Current Organizations / Institutes

The organizations/institutes from the scholar's latest article

Previous Organizations / Institutes

The organizations / institutes from the scholar's other articles in the past ten years


David F. Kelley has a total of 43 co-authors. Here are the top co-authors by number of shared publications:

  • Anne Myers Kelley

    Dept. of Chemistry and Biochemistry, U C Merced

    13 shared publications
  • Ilan Jen-La Plante

    Nanosys/Shoei Electronic Materials Inc. 2 , 233 S. Hillview Dr., Milpitas, California 95035

    10 shared publications
  • Christian Ippen

    Nanosys Inc

    8 shared publications
  • Ke Gong

    Chemistry and Chemical Biology, University of California—Merced, 5200 North Lake Road, Merced, California 95343, United States

    8 shared publications
  • Paul Cavanaugh

    Dept. of Chemistry and Biochemistry, U C Merced

    8 shared publications
  • Zhong-Jie Jiang

    Guangzhou Key Laboratory for Surface Chemistry of Energy Materials, Guangdong Engineering and Technology Research Center for Surface Chemistry of Energy Materials, College of Environment and Energy, South China University of Technology, Guangzhou 510006, P. R. China

    7 shared publications

Latest Publications

  • Effect of Surface Chemistry on the Continuum Intensity in CdTe Quantum Dots

    by Adityaa Bajpai, David F. Kelley

    We investigate the surface chemistry dependence of the absorption spectra in 3.2 nm CdTe quantum dots (QDs) using room-temperature absorption spectroscopy. More specifically, we focus on the broad bulk-like contribution commonly referred to as the continuum. Modification of the surface stoichiometry from Cd-rich to Te-rich conditions results in a pronounced increase in the continuum absorption intensity, particularly in the region between the 1Se–1Sh and 1Se–2Sh transitions. In contrast, the absorption at higher energies is comparatively insensitive to surface stoichiometry. We assign the continuum absorption to two distinct types of transitions: (i) low-energy transitions that involve transferring an electron from a surface chalcogenide dangling-bond to a quantum-confined conduction-band state and (ii) high-energy bulk-like transitions that scale with particle volume. We also find that the same considerations apply to continuum transitions involving adsorbed alkylthiols. We further apply this model to interpret the spectroscopic data of metal- and chalcogenide-rich ZnSe and CdSe quantum dots reported in the literature. This analysis provides a consistent interpretation of continuum absorption in semiconductor quantum dots and highlights the role of surface stoichiometry in determining optical spectra.

  • (Invited) Radiative Dynamics in II-VI Quantum Dots

    by Adityaa Bajpai, David Kelley

    Semiconductor quantum dots (QDs) are being pursued for their application in commercial optoelectronic devices, due to their versatility, solution processability, and advances in reliable, high-yield synthetic methods. The advancement of these applications requires a deeper understanding of the role of synthetic factors on the angular momentum fine structure and in turn the photophysical properties and dynamics of the excitonic states in QDs. A perfectly spherical QD has a very simple fine structure, with a fully allowed three-fold degenerate J=1 state and an optically forbidden five-fold degenerate J=2 excitonic states split by and exchange energy. Any deviation from spherical symmetry breaks the degeneracies in the J=1 and J=2 manifolds and a mixing of oscillator strength in certain states in the lower energy manifold. This deviation from spherical symmetry is commonly considered to result from either the crystal field (asymmetry in unit cell) or deviation from spherical symmetry in the morphology of the QDs. In this presentation, we use time-resolved and static spectroscopic measurements on CdTe QDs to show that charged surface ligands introduce internal electric fields that are a major source of spherical symmetry breaking. Specifically, we demonstrate that CdTe QDs with charged (octadecylphosphonic) acid ligands show shorter radiative lifetimes, larger Stokes shifts and larger polarization anisotropies in the photoluminescence excitation spectra than the same particles having uncharged (octanethiol) ligands. The spectroscopic data is analyzed in terms of a simple two-parameter effective mass approximation model (the ‘Efros model’) of angular momentum fine structure states outlined by Efros, et al., Phys. Rev. B 1996, 54, 4843-4856. We show that the results can be qualitatively understood in terms of the Efros model, but it doesn’t explain them quantitatively. This talk will outline how the angular momentum fine structure is considered within the theoretical framework of the ‘Efros model’, and how its quantitative predictions are assessed using well established spectroscopic and synthetic techniques. We show that the fine structure splittings are smaller and/or more complicated and that the lower energy states have more oscillator strength than predicted by the Efros model, and these discrepancies can be understood in terms of more complicated symmetry breaking than is assumed by the model.

  • Radiative dynamics of AgIn(1−x)GaxS2 quantum dots

    by Adityaa Bajpai, Christopher Sunderland, Xudong Wang, David Olmeijer, Ilan Jen-La Plante, Chunming Wang, Anne Myers Kelley, David F. Kelley

    We present and analyze the static spectroscopy and radiative dynamics of very high quality, well characterized silver indium gallium sulfide quantum dots. We find that the static spectroscopy and radiative dynamics are very different from those in II–VI and III–V quantum dots. The absorption spectrum is broad and featureless, but sharp, high quantum yield (90%) band edge photoluminescence is observed. Despite the spectrally sharp photoluminescence, the photoluminescence decays are long and nonexponential, having components ranging from 40 to 150 ns. The spectroscopy and radiative kinetics are understood in the context of the radial composition profile of each element, as determined by energy dispersive x-ray spectroscopy line profiles. The radially dependent compositions show that the core is largely Ag2S with the fraction of gallium increasing with radial distance. We suggest that random spatial fluctuations in the local silver concentration localize holes at the most silver-rich regions of the particle. The lowest energy transition is nominally parity forbidden and the parity selection rule is relaxed in the random alloy crystal environment. The sites at which holes localize have varying degrees of local crystal asymmetry and varying magnitudes of internal electric fields. Both types of perturbations can break the local symmetry and thereby relax the parity selection rule, giving rise to inhomogeneity in the radiative rates. We also consider the possibility that the nonexponential photoluminescence decay kinetics can be explained by a delayed emission model but consider this to be less likely than the inhomogeneous radiative rate model.

  • Ligand effects on the angular momentum fine structure of CdTe quantum dots

    by Adityaa Bajpai, David F. Kelley

    Ligand effects on the angular momentum fine structure of 3.2 nm diameter CdTe quantum dots have been studied using room temperature static spectroscopy and lifetime measurements. This study focuses on the comparison of particles having charged (octadecylphosphonic acid) and uncharged (octanethiol) ligands. In both cases, polarized photoluminescence excitation spectroscopy provides a measure of the extent to which fine structure states with orthogonal polarizations can be selectively excited, and the photoluminescence Stokes shift provides a measure of the amount of luminescence coming from fine structure states with different energies. Radiative lifetime measurements provide a measure of the relative oscillator strengths of fine structure states with different energies. We demonstrate that the changes in the nature of the surface ligands (charged or uncharged) measurably change the polarized photoluminescence excitation spectrum, Stokes shift, and radiative lifetimes. We suggest that this is due to large internal electric fields associated with the charged ligands that alter the angular momentum fine structure mixings and energetics. The results are analyzed in terms of a simple two-parameter effective mass approximation model for quasi-spherical II–VI quantum dots [Efros et al., Phys. Rev. B 54, 4843–4856 (1996)], which is the most commonly used model of angular momentum fine structure states. We find that this model qualitatively explains the results. However, quantitative analysis of these results gives a significant deviation from the model predictions; it requires that the fine structure splittings are smaller and/or more complicated and that the lower energy states have more oscillator strength than predicted by the Efros model.


  • (Invited) Luminescent InP Quantum Dots: They're Not Just Like CdSe

    by Paul Cavanaugh, Haochen Sun, Ilan Jen-La Plante, Xudong Wang, Maria Bautista, Christian Ippen, Anne Myers Kelley, David Kelley

    Time-resolved photoluminescence (PL) and transient absorption (TA) spectroscopy have been used to elucidate the electron and hole dynamics in high quality InP/ZnSe/ZnS quantum dots (QDs) at room temperature. These dynamics depend critically on the overall In:P ratio. Stoichiometric QDs (those having an In:P ratio close to unity), have PL quantum yields of > 90% and exhibit dynamics that are very simple: both electron and hole relaxation to the bandedge is fast compared to the ~ 40 ps time-correlated photon-counting instrument response and the PL follows a single exponential decay having a time constant of about 26 ns. However, QDs having an In:P ratio greater than about 1.1 maintain PL quantum yields > 90%, but show much more complicated PL kinetics. In the non-stoichiometric QDs, a significant fraction of the PL exhibits a slower risetime. The PL rises over a range of timescales varying from close to the instrument response to approximately 2.0 ns. The time constant of the slowest component increases with increasing InP core size and the fraction of the PL that has the slow risetime increases with excess indium in the particle. The slow risetime is absent in the TA results, indicating that the slow dynamics may be assigned to relaxation in the valence band. The risetime increases with the thickness of the ZnSe shell, varying from < 40 ps for the thinnest (1.1 nm) to about 2.0 ns for the thickest (2.7 nm) ZnSe shells. In addition to the slow risetime, the QDs having excess indium show a significant long-lived (>100 ns) decay component. The magnitude and time constant of this slow decay also increases with ZnSe shell thickness. These results suggest that holes are transiently trapped at sites associated with indium dopants in the ZnSe shell. The trapped hole has negligible overlap with the conduction band electron, making this an optically dark state. The holes are in an equilibrium between the shell traps and the valence band, giving rise to the delayed emission. Several possible assignments of the trapping species can be considered, and a substitutional indium adjacent to a zinc vacancy, In3+/VZn 2-, is the most likely. This assignment is consistent with the observation that trapping occurs only when the QD has excess indium and is supported by experiments showing that the addition of zinc oleate or acetate decreases the extent of trapping, presumably by filling some of the vacancy traps. Further experiments show that addition of alkyl carboxylic acids causes increased trapping, presumably by the formation of zinc oleate, thereby creating additional zinc vacancies. Chloride ion is a common impurity in the synthesis of InP/ZnSe/ZnS QDs and the possibility of In3+/Cl- impurities acting as the hole trap can be also considered. However, additional experimental data on InP/ZnSe/ZnS QDs synthesized in the absence of chloride show the same PL risetimes and delayed emission, eliminating this possibility. Density functional theory calculations further corroborate assignment of the trapping species to In3+/VZn 2-. These calculations show that either a single In2+ ion or an In2+-In3+ dimer is much too easily oxidized to form the reversible traps observed experimentally, while In3+ is far too difficult to oxidize. However, a zinc vacancy adjacent to a substitutional indium is calculated to have its highest occupied orbitals about 1 eV above the top of the valence band of bulk ZnSe, in the appropriate energy range to act as reversible traps for quantum confined holes in the InP valence band.

  • Angular Momentum Fine Structure in InP/ZnSe Quantum Dots

    by David F. Kelley

    There is a large experimental and theoretical literature on the angular momentum fine structure of the lowest energy exciton in InP-based quantum dots. This literature is highly contradictory, and no clear picture of the fine structure accounting for all these results is available. This paper presents a quantitative analysis of recently published luminescence anisotropy results and presents an analysis of the different proposed fine structure models that compares radiative lifetimes calculated from those models with experimental values. These analyses show that the lowest energy (dark) state is the mj = ±2 state and the lowest energy bright state is a vibronically allowed phonon level. The splittings between the ±2/±1L states and the ±1U/0U states are the same, about 28 meV. We also find that the manifold of J = 1 states is about 60 meV above the manifold of J = 2 states.


  • (Invited) Luminescent InP Quantum Dots: They're Not Just Like CdSe

    by Paul Cavanaugh, Haochen Sun, Ilan Jen-La Plante, Xudong Wang, Maria Bautista, Christian Ippen, Anne Myers Kelley, David Kelley

    There are significant similarities and differences in the spectroscopy and photophysics between CdSe-based and InP-based quantum dots. One of the more important differences is the presence of reversibly populated hole traps in InP/ZnSe quantum dots (QDs). These traps affect many aspects of the overall excited state dynamics. In this paper we elucidate the hole relaxation dynamics in high quality InP/ZnSe/ZnS QDs at room temperature and focus on the role of these traps. Specifically, we show that the presence of transiently populated traps results in extremely slow (tens of picoseconds to nanoseconds) hole cooling as evidenced by a significant fraction of the photoluminescence exhibiting a slow risetime following photoexcitation. Through a combination of chemical derivatization studies and density functional theory calculations, they are assigned to substitutional indium adjacent to a zinc vacancy, In3+/VZn 2-, in the ZnSe shell.


  • Open Access

    Stable Cadmium-Free Quantum Dot Optical Down-Converters for Solid State Lighting

    by Ilan Jen-La Plante, David F Kelley

    Quantum dots (QDs) have been used in commercial solid-state lighting (SSL) applications to improve the energy efficiency of light generation at warm color temperatures. By increasing the amount of QDs used in each product, further energy savings are possible; however, traditional QDs contain cadmium, which has regulatory limits on its concentration in consumer products. As described within this final technical report, we have established that heavy-metal free QDs made from indium phosphide (InP) exhibit highly efficient emission at the temperatures and fluxes relevant to SSL. However, the maintenance of this emission is compromised during long term operation due to QD oxidation. We have identified multiple methods to slow the oxidation rate, which has improved the operational stability of these materials more than 200 times longer than at the project start. Beyond these improvements, heavy-metal free QDs require a further hundred-fold increase in stability to enable use in mid-power SSL and a ten-fold increase in stability to enable use in diffuse SSL applications. The outcomes of this project demonstrate feasibility for the use of heavy-metal free QDs in commercial SSL applications with potential use in diffuse SSL applications in the near term (1-2 years) pending market need.


  • Open Access

    Spectral widths and Stokes shifts in InP-based quantum dots

    by Paul Cavanaugh, Xudong Wang, Maria J. Bautista, Ilan Jen-La Plante, David F. Kelley

    InP-based quantum dots (QDs) have Stokes shifts and photoluminescence (PL) line widths that are larger than in II–VI semiconductor QDs with comparable exciton energies. The mechanisms responsible for these spectral characteristics are investigated in this paper. Upon comparing different semiconductors, we find the Stokes shift decreases in the following order: InP > CdTe > CdSe. We also find that the Stokes shift decreases with core size and decreases upon deposition of a ZnSe shell. We suggest that the Stokes shift is largely due to different absorption and luminescent states in the angular momentum fine structure. The energy difference between the fine structure levels, and hence the Stokes shifts, are controlled by the electron–hole exchange interaction. Luminescence polarization results are reported and are consistent with this assignment. Spectral widths are controlled by the extent of homogeneous and inhomogeneous broadening. We report PL and PL excitation (PLE) spectra that facilitate assessing the roles of homogeneous and different inhomogeneous broadening mechanisms in the spectra of zinc-treated InP and InP/ZnSe/ZnS particles. There are two distinct types of inhomogeneous broadening: size inhomogeneity and core–shell interface inhomogeneity. The latter results in a distribution of core–shell band offsets and is caused by interfacial dipoles associated with In–Se or P–Zn bonding. Quantitative modeling of the spectra shows that the offset inhomogeneity is comparable to but somewhat smaller than the size inhomogeneity. The combination of these two types of inhomogeneity also explains several aspects of reversible hole trapping dynamics involving localized In3+/VZn2− impurity states in the ZnSe shells.


  • Comment on “Dependence of the Fluorescent Lifetime τ on the Concentration at High Dilution”

    by Anne Myers Kelley, David F. Kelley

    A recent Letter in this Journal (Langhals and Schlücker, J. Phys. Chem. Lett. 202213, 7568-7573) reported a dependence of the fluorescence lifetime of a dye on concentration and attributed it to "electromagnetic interactions with distant resonating structures" on a length scale of more than 100 nm. We show that their results can be explained as a straightforward result of absorption and re-emission of the fluorescence ("radiative energy transport"), which lengthens the apparent lifetime at higher concentrations. This effect has been well-documented in the literature many times. We show that simulations of the fluorescence decays accounting for radiative transport can reproduce the authors' results without postulating any new electromagnetic mechanism.