Gelson Luis Adabo
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Gelson Luis Adabo has a total of 99 co-authors. Here are the top co-authors by number of shared publications:
- Renata Garcia Fonseca
Department of Dental Materials and Prosthodontics, School of Dentistry São Paulo State University (UNESP) Araraquara São Paulo Brazil
18 shared publications Diogo Longhini
São Paulo State University (UNESP)
7 shared publicationsSicknan Soares da Rocha
Federal University of Goiás, Goiânia Department of Prevention and Oral Rehabilitation Dental Clinic
7 shared publications- Ricardo Faria Ribeiro
Department of Dental Materials and Prosthodontics, Ribeirão Preto School of Dentistry, University of São Paulo, Ribeirão Preto, Brazil
6 shared publications Isabella Gagliardi Haneda
5 shared publications- Laiza Maria Grassi Fais
Department of Dental Material and Prosthodontics, School of Dentistry, São Paulo State University (UNESP), Araraquara 14800900, Brazil
5 shared publications
Latest Publications
- 6 April 2023
- Published by Springer Nature in Clinical Oral Investigations
- Vol. 27 (7) , 3827-3838
Reliability and lifetime of lithium disilicate, 3Y-TZP, and 5Y-TZP zirconia crowns with different occlusal thicknesses
Objectives To assess the probability of survival of crowns made with a 3Y-TZP, a 5Y-TZP, and a lithium disilicate. Materials and methods CAD-CAM premolar crowns with occlusal thicknesses of 1.0 mm or 1.5 mm and cemented on a metal dye. Step-stress accelerated life testing (SSALT) was performed to access the use level probability Weibull curves and reliability were calculated for the completion of a mission of 100,000 cycles at 300 to 1200 N. Results All ceramics showed a high probability of survival (87–99%) at 300 N, irrespective of thickness. 3Y-TZP shows no significant decrease in the probability of survival up to 1200 N (83–96%). Lithium disilicate presented lower reliability than zirconia under the 600 N mission. 5Y-TZP showed lower reliability than 3Y-TZP at 1200 N. There was no significant difference in the Weibull modulus (3.23–7.12). 3Y-TZP had the highest characteristic strength (2483–2972 N), followed by 5Y-TZP (1512–1547 N) and lithium disilicate (971–1154 N). Conclusion Zirconia ceramics have a high probability of survival (up to 900 N-load), while lithium disilicate survives up to 300 N load only, irrespective of the thickness (1.0 mm or 1.5 mm). Clinical relevance The probability of survival of posterior crowns made with zirconia ceramics resists extreme loads while glass ceramics resist normal chewing loads. In addition, crowns with thinner occlusal face showed sufficient mechanical behavior.
- 6 April 2023
- Published by Springer Nature in Clinical Oral Investigations
- Vol. 27 (7) , 3827-3838
Reliability and lifetime of lithium disilicate, 3Y-TZP, and 5Y-TZP zirconia crowns with different occlusal thicknesses
Objectives To assess the probability of survival of crowns made with a 3Y-TZP, a 5Y-TZP, and a lithium disilicate. Materials and methods CAD-CAM premolar crowns with occlusal thicknesses of 1.0 mm or 1.5 mm and cemented on a metal dye. Step-stress accelerated life testing (SSALT) was performed to access the use level probability Weibull curves and reliability were calculated for the completion of a mission of 100,000 cycles at 300 to 1200 N. Results All ceramics showed a high probability of survival (87–99%) at 300 N, irrespective of thickness. 3Y-TZP shows no significant decrease in the probability of survival up to 1200 N (83–96%). Lithium disilicate presented lower reliability than zirconia under the 600 N mission. 5Y-TZP showed lower reliability than 3Y-TZP at 1200 N. There was no significant difference in the Weibull modulus (3.23–7.12). 3Y-TZP had the highest characteristic strength (2483–2972 N), followed by 5Y-TZP (1512–1547 N) and lithium disilicate (971–1154 N). Conclusion Zirconia ceramics have a high probability of survival (up to 900 N-load), while lithium disilicate survives up to 300 N load only, irrespective of the thickness (1.0 mm or 1.5 mm). Clinical relevance The probability of survival of posterior crowns made with zirconia ceramics resists extreme loads while glass ceramics resist normal chewing loads. In addition, crowns with thinner occlusal face showed sufficient mechanical behavior.
- Open Access
- 25 October 2022
- Published by Springer Nature in Research Square
Fatigue failure of lithium disilicate and translucent zirconia crowns with different occlusal thicknesses
Objectives: To assess the probability of survival of crowns made of high translucent 3rd generation zirconia (Prettau Anterior - PA), 2nd generation zirconia (Prettau - P), and the glass-ceramic lithium disilicate (IPS e.max CAD - EM). Materials and Methods: CAD-CAM premolar crowns were fabricated with occlusal thicknesses of 1.0 mm or 1.5 mm and cemented on a metal dye. Step-stress accelerated life testing (SSALT) was performed using 3 profiles: mild (n=9), moderate (n=6), and aggressive (n=3). The use-level probability Weibull curves and reliability were calculated for completion of a mission of 100,000 cycles at 300, 600, 900, and 1200 N. Results: A high probability of survival was found for all ceramics (87-99%) at 300 N, irrespective of thickness. There was no significant decrease in the probability of survival for all P crowns up to 1200 N (83-96%). EM crowns presented lower reliability than P or PA crowns under the 600-900 N mission. PA crowns showed lower reliability than P crowns at higher loads of 1200 N. There was no significant difference in the Weibull modulus (3.23-7.12). P demonstrated the highest characteristic strength (2483-2972 N), followed by PA (1512-1547 N) and EM (971-1154 N). Conclusion: High translucent 3rd generation zirconia has a high probability of survival (up to 900 N-load), while lithium disilicate survives up to 300 N load only, irrespective of thickness (1.0 mm or 1.5 mm). Clinical Relevance: The probability of survival of posterior crowns made with zirconia ceramics has sufficient strength for parafunctional loads, while glass ceramics resist normal chewing loads only.
- 25 October 2022
- Published by Springer Nature in Research Square
Open AccessFatigue failure of lithium disilicate and translucent zirconia crowns with different occlusal thicknesses
Objectives: To assess the probability of survival of crowns made of high translucent 3rd generation zirconia (Prettau Anterior - PA), 2nd generation zirconia (Prettau - P), and the glass-ceramic lithium disilicate (IPS e.max CAD - EM). Materials and Methods: CAD-CAM premolar crowns were fabricated with occlusal thicknesses of 1.0 mm or 1.5 mm and cemented on a metal dye. Step-stress accelerated life testing (SSALT) was performed using 3 profiles: mild (n=9), moderate (n=6), and aggressive (n=3). The use-level probability Weibull curves and reliability were calculated for completion of a mission of 100,000 cycles at 300, 600, 900, and 1200 N. Results: A high probability of survival was found for all ceramics (87-99%) at 300 N, irrespective of thickness. There was no significant decrease in the probability of survival for all P crowns up to 1200 N (83-96%). EM crowns presented lower reliability than P or PA crowns under the 600-900 N mission. PA crowns showed lower reliability than P crowns at higher loads of 1200 N. There was no significant difference in the Weibull modulus (3.23-7.12). P demonstrated the highest characteristic strength (2483-2972 N), followed by PA (1512-1547 N) and EM (971-1154 N). Conclusion: High translucent 3rd generation zirconia has a high probability of survival (up to 900 N-load), while lithium disilicate survives up to 300 N load only, irrespective of thickness (1.0 mm or 1.5 mm). Clinical Relevance: The probability of survival of posterior crowns made with zirconia ceramics has sufficient strength for parafunctional loads, while glass ceramics resist normal chewing loads only.
- 1 February 2020
- Published by Elsevier in The Journal of Prosthetic Dentistry
- Vol. 123 (2) , 330-337
The mechanical behavior of high-translucent monolithic zirconia after adjustment and finishing procedures and artificial aging
- 1 February 2020
- Published by Elsevier in The Journal of Prosthetic Dentistry
- Vol. 123 (2) , 330-337
The mechanical behavior of high-translucent monolithic zirconia after adjustment and finishing procedures and artificial aging
- 1 January 2020
- Published by Elsevier in The Journal of Prosthetic Dentistry
- Vol. 123 (1) , 155-162
Does airborne-particle abrasion before, rather than after, zirconia sintering lead to higher mechanical strength even under aging challenge?
- 1 January 2020
- Published by Elsevier in The Journal of Prosthetic Dentistry
- Vol. 123 (1) , 155-162
Does airborne-particle abrasion before, rather than after, zirconia sintering lead to higher mechanical strength even under aging challenge?
- Open Access
- 1 July 2019
- Published by FapUNIFESP (SciELO) in Brazilian Dental Journal
- Vol. 30 (4) , 333-341
Influence of Zirconia-Coated Bioactive Glass on Gingival Fibroblast Behavior
The objective of this study was the development of a bioactive glass coating on zirconia (Zr) to modulate the gingival fibroblast phenotype. For this purpose, Biosilicate® (BS) particles in a water/isopropyl alcohol (1:1) vehicle (6 mg/mL) were applied to zirconia discs followed by thermal treatment at 1100 °C for 20 min. The surface topography (SEM), chemical composition (EDX), surface roughness (Ra; confocal microscopy), surface free energy (goniometry), and color alteration (UV-vis spectrophotometry) were assessed (n=6). Thereafter, L929 fibroblasts were seeded onto Zr and Zr+BS discs, and cell proliferation (Alamar Blue; n=6), morphology (SEM; n=2), migration (wound healing; n=4), and collagen synthesis (Sirius Red; n=6) were evaluated up to 7 days. Data were analyzed by ANOVA/Tukey tests (a=5%). A homogeneous coating consisting of Si, Na, O, and Ca was detected on the Zr surface after thermal treatment with BS, which led to a significant increase in surface roughness and free energy (p0.05). Cells seeded on the Zr+BS surface featured increased proliferation, collagen expression, and migration capability in comparison with those cultured on plain Zr (p<0.05). SEM images revealed that cell spreading occurred faster in the presence of BS. Therefore, it was concluded that thermal treatment of the Zr surface with BS led to the deposition of a bioactive coating, which induced gingival fibroblast spread, proliferation, migration, and collagen expression in vitro.
- 1 July 2019
- Published by FapUNIFESP (SciELO) in Brazilian Dental Journal
- Vol. 30 (4) , 333-341
Open AccessInfluence of Zirconia-Coated Bioactive Glass on Gingival Fibroblast Behavior
The objective of this study was the development of a bioactive glass coating on zirconia (Zr) to modulate the gingival fibroblast phenotype. For this purpose, Biosilicate® (BS) particles in a water/isopropyl alcohol (1:1) vehicle (6 mg/mL) were applied to zirconia discs followed by thermal treatment at 1100 °C for 20 min. The surface topography (SEM), chemical composition (EDX), surface roughness (Ra; confocal microscopy), surface free energy (goniometry), and color alteration (UV-vis spectrophotometry) were assessed (n=6). Thereafter, L929 fibroblasts were seeded onto Zr and Zr+BS discs, and cell proliferation (Alamar Blue; n=6), morphology (SEM; n=2), migration (wound healing; n=4), and collagen synthesis (Sirius Red; n=6) were evaluated up to 7 days. Data were analyzed by ANOVA/Tukey tests (a=5%). A homogeneous coating consisting of Si, Na, O, and Ca was detected on the Zr surface after thermal treatment with BS, which led to a significant increase in surface roughness and free energy (p0.05). Cells seeded on the Zr+BS surface featured increased proliferation, collagen expression, and migration capability in comparison with those cultured on plain Zr (p<0.05). SEM images revealed that cell spreading occurred faster in the presence of BS. Therefore, it was concluded that thermal treatment of the Zr surface with BS led to the deposition of a bioactive coating, which induced gingival fibroblast spread, proliferation, migration, and collagen expression in vitro.
- Open Access
- 1 December 2018
- Published by FapUNIFESP (SciELO) in Cerâmica
- Vol. 64 (372) , 491-497
Bending strength and reliability of porcelains used in all-ceramic dental restorations
Four dental porcelains for covering zirconia were sintered (fired) at 910-960 °C and characterized, focusing in analyzing reliability, physical and mechanical properties. Samples with relative density close to 99% presented leucite crystallization apart from residual amorphous phase. Hardness between 491±23 and 575±32 HV was different among all ceramics. Fracture toughness between 1.13±0.11 and 1.42±0.25 MPa.m1/2 was statistically different. Bending strength results were not different for three porcelain groups (73±9 to 75±12 MPa), with the exception of one specific group (62±4 MPa). Weibull analysis indicated bending strength between 73 and 75 MPa, Weibull modulus (m) between 5.7 and 7.1, while the ceramic with strength of 60 MPa presented m=13.6. The use of classical theory of fracture mechanics associated to the results of properties obtained in this work indicated the critical failure size in these ceramics lays between 65 and 90 μm and the theoretical fracture energy of porcelains is approximately from 10.5 to 16.3 J/m. It was concluded that the porcelains had different behavior, and it seems that there is no clear relationship among the studied properties.
- 1 December 2018
- Published by FapUNIFESP (SciELO) in Cerâmica
- Vol. 64 (372) , 491-497
Open AccessBending strength and reliability of porcelains used in all-ceramic dental restorations
Four dental porcelains for covering zirconia were sintered (fired) at 910-960 °C and characterized, focusing in analyzing reliability, physical and mechanical properties. Samples with relative density close to 99% presented leucite crystallization apart from residual amorphous phase. Hardness between 491±23 and 575±32 HV was different among all ceramics. Fracture toughness between 1.13±0.11 and 1.42±0.25 MPa.m1/2 was statistically different. Bending strength results were not different for three porcelain groups (73±9 to 75±12 MPa), with the exception of one specific group (62±4 MPa). Weibull analysis indicated bending strength between 73 and 75 MPa, Weibull modulus (m) between 5.7 and 7.1, while the ceramic with strength of 60 MPa presented m=13.6. The use of classical theory of fracture mechanics associated to the results of properties obtained in this work indicated the critical failure size in these ceramics lays between 65 and 90 μm and the theoretical fracture energy of porcelains is approximately from 10.5 to 16.3 J/m. It was concluded that the porcelains had different behavior, and it seems that there is no clear relationship among the studied properties.
- 1 February 2018
- Published by Elsevier in The Journal of Prosthetic Dentistry
- Vol. 119 (2) , 286-291
Effect of surface treatments on repair with composite resin of a partially monoclinic phase transformed yttrium-stabilized tetragonal zirconia
- 1 February 2018
- Published by Elsevier in The Journal of Prosthetic Dentistry
- Vol. 119 (2) , 286-291
Effect of surface treatments on repair with composite resin of a partially monoclinic phase transformed yttrium-stabilized tetragonal zirconia
- Open Access
- 7 August 2017
- Published by FapUNIFESP (SciELO) in Materials Research
- Vol. 20 (5) , 1418-1424
Effect of the Cooling Rate on the Properties of Veneer Porcelain for Zirconia Dental Prosthesis
To solve chipping of veneer porcelain in zirconia dental prosthesis it has been studied different cooling rates in firing schedules to control residual stresses generated by differences in thermal properties between the ceramics. However, cooling rates may affect the porcelain, irrespectively of interaction with zirconia. This study analyzed the effect of cooling rate on the three-point flexural strength (FS), residual stress, Vickers hardness (VH) and V-notch fracture toughness (SEVNB) on a feldspathic porcelain (Vita VM9) indicated for covering zirconia. Bar-shaped specimens were sintered according manufacturer's schedule firing and cooled at different rates (slow, normal or fast). Specimens were tested for FS (n=30), VH (n=15) and SEVNB tests (n=15). Weibull analysis were performed from FS values to measure reliability and probability of failure (PF). One-way ANOVA was significant for VH (p<0.001), and Tukey's test showed that slow cooling led to higher values. There was no significant difference for FS (p=0.654) and SEVNB (p=0.734). Fast cooling led to the lowest PF, but cooling rate factor was not significant for Weibull modulus. All cooling group showed residual tensile stress (MPa): Slow = 34.81; Normal = 27.04; Fast = 18,98. It was concluded that cooling rate produce minor changes in the porcelain properties.
- 7 August 2017
- Published by FapUNIFESP (SciELO) in Materials Research
- Vol. 20 (5) , 1418-1424
Open AccessEffect of the Cooling Rate on the Properties of Veneer Porcelain for Zirconia Dental Prosthesis
To solve chipping of veneer porcelain in zirconia dental prosthesis it has been studied different cooling rates in firing schedules to control residual stresses generated by differences in thermal properties between the ceramics. However, cooling rates may affect the porcelain, irrespectively of interaction with zirconia. This study analyzed the effect of cooling rate on the three-point flexural strength (FS), residual stress, Vickers hardness (VH) and V-notch fracture toughness (SEVNB) on a feldspathic porcelain (Vita VM9) indicated for covering zirconia. Bar-shaped specimens were sintered according manufacturer's schedule firing and cooled at different rates (slow, normal or fast). Specimens were tested for FS (n=30), VH (n=15) and SEVNB tests (n=15). Weibull analysis were performed from FS values to measure reliability and probability of failure (PF). One-way ANOVA was significant for VH (p<0.001), and Tukey's test showed that slow cooling led to higher values. There was no significant difference for FS (p=0.654) and SEVNB (p=0.734). Fast cooling led to the lowest PF, but cooling rate factor was not significant for Weibull modulus. All cooling group showed residual tensile stress (MPa): Slow = 34.81; Normal = 27.04; Fast = 18,98. It was concluded that cooling rate produce minor changes in the porcelain properties.
- 1 August 2017
- Published by Elsevier in Journal of Dentistry
- Vol. 63, 94-102
The effects of mechanical and hydrothermal aging on microstructure and biaxial flexural strength of an anterior and a posterior monolithic zirconia
- 1 August 2017
- Published by Elsevier in Journal of Dentistry
- Vol. 63, 94-102
The effects of mechanical and hydrothermal aging on microstructure and biaxial flexural strength of an anterior and a posterior monolithic zirconia
- Open Access
- 20 April 2017
- Published by Instituto de Filosofia e Ciências Humanas - UNICAMP in Brazilian Journal of Oral Sciences
- Vol. 15 (2) , 109-112
Comparison of the indentation strength and single-edge-v-notched beam methods for dental ceramic fracture toughness testing
Aim: To study influence of the cooling rate after sintering a veneering porcelain (Vita VM9) on fracture toughness by indentation strength (IS) and single-edge-v-notched beam (SEVNB) methods. Methods: Vita VM9 bars were sintered according to the manufacturer’s recommendation and cooled under three conditions: Slow (inside the furnace from sintering temperature to room temperature); Normal (inside the furnace from sintering temperature to 500 ºC and outside the furnace from 500 ºC to room temperature); and Fast (outside the furnace from sintering temperature to room temperature). Fracture toughness was measured by IS (n=10) and SEVNB (n=10) methods. Data were analyzed by two-way ANOVA (α=0.05). Results: The fracture toughness obtained from SEVNB (slow - 1.02±0.10; normal - 1.09±0.13; and fast - 1,02±0.18 MPa.m1/2 cooling techniques) was significantly lower than IS (slow - 1.19±0.13; normal - 1.17±0.07; and fast - 1.16±0.06 MPa. m1/2 cooling techniques). There was no significant influence of the cooling technique (p=0.012). Conclusions: The measurement technique influenced the fracture toughness values . IS method overestimated the fracture toughness values. Irrespective of the measuring method, cooling rate did not influence the Vita VM9 veneering porcelain fracture toughness.
- 20 April 2017
- Published by Instituto de Filosofia e Ciências Humanas - UNICAMP in Brazilian Journal of Oral Sciences
- Vol. 15 (2) , 109-112
Open AccessComparison of the indentation strength and single-edge-v-notched beam methods for dental ceramic fracture toughness testing
Aim: To study influence of the cooling rate after sintering a veneering porcelain (Vita VM9) on fracture toughness by indentation strength (IS) and single-edge-v-notched beam (SEVNB) methods. Methods: Vita VM9 bars were sintered according to the manufacturer’s recommendation and cooled under three conditions: Slow (inside the furnace from sintering temperature to room temperature); Normal (inside the furnace from sintering temperature to 500 ºC and outside the furnace from 500 ºC to room temperature); and Fast (outside the furnace from sintering temperature to room temperature). Fracture toughness was measured by IS (n=10) and SEVNB (n=10) methods. Data were analyzed by two-way ANOVA (α=0.05). Results: The fracture toughness obtained from SEVNB (slow - 1.02±0.10; normal - 1.09±0.13; and fast - 1,02±0.18 MPa.m1/2 cooling techniques) was significantly lower than IS (slow - 1.19±0.13; normal - 1.17±0.07; and fast - 1.16±0.06 MPa. m1/2 cooling techniques). There was no significant influence of the cooling technique (p=0.012). Conclusions: The measurement technique influenced the fracture toughness values . IS method overestimated the fracture toughness values. Irrespective of the measuring method, cooling rate did not influence the Vita VM9 veneering porcelain fracture toughness.