Chao Peng
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Chao Peng has a total of 17 co-authors. Here are the top co-authors by number of shared publications:
- Benjamin Paul Wilson
School of Chemical Engineering, Aalto University
7 shared publications Mari Lundström
5 shared publicationsFupeng Liu
Aalto University
3 shared publications- Fupeng Liu
Jiangxi University of Science and Technology
3 shared publications - Mari Lundström
Aalto University
2 shared publications Zulin Wang
Hydrometallurgy and Corrosion, Department of Chemical and Metallurgical Engineering (CMET), School of Chemical Engineering, Aalto University, Espoo 02150, Finland
2 shared publications
Latest Publications
- Open Access
- 1 February 2020
- Published by Elsevier in Journal of Power Sources
- Vol. 450
Role of impurity copper in Li-ion battery recycling to LiCoO2 cathode materials
- 1 February 2020
- Published by Elsevier in Journal of Power Sources
- Vol. 450
Open AccessRole of impurity copper in Li-ion battery recycling to LiCoO2 cathode materials
- Open Access
- 3 October 2019
- Published by Springer Nature in JOM
- Vol. 72 (2) , 978
Correction to: Recovery of High-Purity MnO2 from the Acid Leaching Solution of Spent Li-Ion Batteries
- 3 October 2019
- Published by Springer Nature in JOM
- Vol. 72 (2) , 978
Open AccessCorrection to: Recovery of High-Purity MnO2 from the Acid Leaching Solution of Spent Li-Ion Batteries
- Open Access
- 23 September 2019
- Published by Springer Nature in JOM
- Vol. 72 (2) , 790-799
Recovery of High-Purity MnO2 from the Acid Leaching Solution of Spent Li-Ion Batteries
Hydrometallurgical recycling processes for spent Li-ion batteries (LIBs) often produce pregnant leach solutions (PLS) that contain metals like Co, Ni, Mn, Li, Al, etc. Although significant research has focused on the recovery of the most valuable materials (e.g., Co, Ni, Li), the reclamation of Mn from PLS is often neglected. In this study, recovery of Mn via a multi-step process based on solvent extraction with di-2-ethylhexyl phosphoric acid, scrubbing, stripping and oxidative Mn precipitation has been undertaken. The results demonstrate that more than 99% of Mn can be successfully recovered as a high-purity MnO2 product (purity > 99.5%) with almost no loss of Co, Ni and Li. In addition, the behavior of other metal elements present in the PLS were also studied in detail. Overall, this study investigates the fundamentals of Mn recovery from the complicated PLS of LIBs waste and outlines industrial process feasibility based on known unit process steps.
- 23 September 2019
- Published by Springer Nature in JOM
- Vol. 72 (2) , 790-799
Open AccessRecovery of High-Purity MnO2 from the Acid Leaching Solution of Spent Li-Ion Batteries
Hydrometallurgical recycling processes for spent Li-ion batteries (LIBs) often produce pregnant leach solutions (PLS) that contain metals like Co, Ni, Mn, Li, Al, etc. Although significant research has focused on the recovery of the most valuable materials (e.g., Co, Ni, Li), the reclamation of Mn from PLS is often neglected. In this study, recovery of Mn via a multi-step process based on solvent extraction with di-2-ethylhexyl phosphoric acid, scrubbing, stripping and oxidative Mn precipitation has been undertaken. The results demonstrate that more than 99% of Mn can be successfully recovered as a high-purity MnO2 product (purity > 99.5%) with almost no loss of Co, Ni and Li. In addition, the behavior of other metal elements present in the PLS were also studied in detail. Overall, this study investigates the fundamentals of Mn recovery from the complicated PLS of LIBs waste and outlines industrial process feasibility based on known unit process steps.
- Open Access
- 19 September 2019
- Published by American Chemical Society (ACS) in ACS Sustainable Chemistry & Engineering
- Vol. 7 (20) , 17372-17378
Oxalic Acid Recovery from High Iron Oxalate Waste Solution by a Combination of Ultrasound-Assisted Conversion and Cooling Crystallization
In order to achieve the global goals related to renewable energy and responsible production, technologies that ensure the circular economy of metals and chemicals in recycling processes are a necessity. The recycling of spent Nd-Fe-B magnets typically results in rare earth elements (REEs) free wastewaters that have a high ferric ion concentration as well as oxalate groups and for which, there are only a few economically viable methods for disposal or reuse. The current research provides a new approach for the effective recovery of oxalic acid and the results suggest that during the initial oxalate groups separation stage, > 99% of oxalate ions can be precipitated as ferrous oxalate (FeC2O4·2H2O) by an ultrasound-assisted iron powder replacement method (Fe/Fe(III) = 2, tu/s = 5 min, T = 50 °C). Subsequently, almost all of the FeC2O4·2H2O was dissolved using 6 mol/L HCl (T = 65 °C, t = 5 min) and the dissolved oxalates were found to mainly exist in form of H2C2O4. Furthermore, over 80% of the oxalic acid was recovered via crystallization by cooling the oxalate containing HCl solution to 5 °C. After oxalic acid crystallization, the residual raffinate acid solution can then be recirculated back to the ferrous oxalate leaching stage, in order to decrease any oxalic acid losses. This treatment protocol for high iron REEs-free solution not only avoids the potential harm to the environment due to the wastewater but also significantly improves the circular economy of chemicals in the typical utilized in permanent magnet recycling processes.
- 19 September 2019
- Published by American Chemical Society (ACS) in ACS Sustainable Chemistry & Engineering
- Vol. 7 (20) , 17372-17378
Open AccessOxalic Acid Recovery from High Iron Oxalate Waste Solution by a Combination of Ultrasound-Assisted Conversion and Cooling Crystallization
In order to achieve the global goals related to renewable energy and responsible production, technologies that ensure the circular economy of metals and chemicals in recycling processes are a necessity. The recycling of spent Nd-Fe-B magnets typically results in rare earth elements (REEs) free wastewaters that have a high ferric ion concentration as well as oxalate groups and for which, there are only a few economically viable methods for disposal or reuse. The current research provides a new approach for the effective recovery of oxalic acid and the results suggest that during the initial oxalate groups separation stage, > 99% of oxalate ions can be precipitated as ferrous oxalate (FeC2O4·2H2O) by an ultrasound-assisted iron powder replacement method (Fe/Fe(III) = 2, tu/s = 5 min, T = 50 °C). Subsequently, almost all of the FeC2O4·2H2O was dissolved using 6 mol/L HCl (T = 65 °C, t = 5 min) and the dissolved oxalates were found to mainly exist in form of H2C2O4. Furthermore, over 80% of the oxalic acid was recovered via crystallization by cooling the oxalate containing HCl solution to 5 °C. After oxalic acid crystallization, the residual raffinate acid solution can then be recirculated back to the ferrous oxalate leaching stage, in order to decrease any oxalic acid losses. This treatment protocol for high iron REEs-free solution not only avoids the potential harm to the environment due to the wastewater but also significantly improves the circular economy of chemicals in the typical utilized in permanent magnet recycling processes.
- Open Access
- 29 August 2019
- Published by American Chemical Society (ACS) in ACS Sustainable Chemistry & Engineering
- Vol. 7 (19) , 16103-16111
Synergistic Recovery of Valuable Metals from Spent Nickel–Metal Hydride Batteries and Lithium-Ion Batteries
This research presents a sustainable approach for the simultaneous recycling of spent lithium-ion batteries (LIBs) and nickel-metal hydride batteries (NiMHs). Firstly, dissolution of LIBs and NiMHs were found to be mutually co-promoted, resulting in above 98% extraction of Li, Co, Ni and rare earth elements (REEs) without the need for any oxidant or reductant additions. After leaching, > 97% of REEs were recovered as a REEs-alkali double sulfate precipitate with the addition of NaOH and Na2SO4 precipitants. This REEs-free solution was then further processed in order to separate and recover the battery metals present: Mn, Co, Ni and Li. The resultant residual solution (rich in NaOH and Na2SO4) was redirected to the REEs precipitation step, decreasing both the need of precipitants (e.g. Na2SO4) as well as the costs related to the treatment of the high-Na waste solution. Moreover, the Li remaining in the waste solution can be circulated back into the main process, resulting in an exceptionally high Li recovery of > 93% in the form of high-purity Li3PO4 (99.95%). This is a marked improvement over the previously reported Li recovery levels of 60% - 80%. Overall, this newly developed process has considerable environmental and economic advantages for the recovery of valuable metals from mixed LIBs and NiMHs wastes
- 29 August 2019
- Published by American Chemical Society (ACS) in ACS Sustainable Chemistry & Engineering
- Vol. 7 (19) , 16103-16111
Open AccessSynergistic Recovery of Valuable Metals from Spent Nickel–Metal Hydride Batteries and Lithium-Ion Batteries
This research presents a sustainable approach for the simultaneous recycling of spent lithium-ion batteries (LIBs) and nickel-metal hydride batteries (NiMHs). Firstly, dissolution of LIBs and NiMHs were found to be mutually co-promoted, resulting in above 98% extraction of Li, Co, Ni and rare earth elements (REEs) without the need for any oxidant or reductant additions. After leaching, > 97% of REEs were recovered as a REEs-alkali double sulfate precipitate with the addition of NaOH and Na2SO4 precipitants. This REEs-free solution was then further processed in order to separate and recover the battery metals present: Mn, Co, Ni and Li. The resultant residual solution (rich in NaOH and Na2SO4) was redirected to the REEs precipitation step, decreasing both the need of precipitants (e.g. Na2SO4) as well as the costs related to the treatment of the high-Na waste solution. Moreover, the Li remaining in the waste solution can be circulated back into the main process, resulting in an exceptionally high Li recovery of > 93% in the form of high-purity Li3PO4 (99.95%). This is a marked improvement over the previously reported Li recovery levels of 60% - 80%. Overall, this newly developed process has considerable environmental and economic advantages for the recovery of valuable metals from mixed LIBs and NiMHs wastes
- 1 May 2019
- Published by Elsevier in Hydrometallurgy
- Vol. 185, 38-45
Recovery and separation of silver and mercury from hazardous zinc refinery residues produced by zinc oxygen pressure leaching
- 1 May 2019
- Published by Elsevier in Hydrometallurgy
- Vol. 185, 38-45
Recovery and separation of silver and mercury from hazardous zinc refinery residues produced by zinc oxygen pressure leaching
- Top Cited PapersOpen Access
- 1 March 2019
- Published by Elsevier in Journal of Power Sources
- Vol. 415, 179-188
Selective extraction of lithium (Li) and preparation of battery grade lithium carbonate (Li2CO3) from spent Li-ion batteries in nitrate system
- 1 March 2019
- Published by Elsevier in Journal of Power Sources
- Vol. 415, 179-188
Top Cited PapersOpen AccessSelective extraction of lithium (Li) and preparation of battery grade lithium carbonate (Li2CO3) from spent Li-ion batteries in nitrate system