Somnath Mandal
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Somnath Mandal has a total of 20 co-authors. Here are the top co-authors by number of shared publications:
- Ilona Jastrzębska
Faculty of Materials Science and Ceramics, AGH University of Kraków, al. A. Mickiewicza 30, 30-059 Kraków, Poland
2 shared publications Joanna Przystaś
2 shared publications- Manoj K. Mahapatra
Mechanical and Materials Engineering University of Alabama at Birmingham Birmingham Alabama USA
2 shared publications Oliwia Pająk
2 shared publicationsA. Piwowarczyk
1 shared publication- Alan Wilmański1 shared publication
Latest Publications
- Open Access
- 11 September 2025
- Published by Elsevier in Journal of the European Ceramic Society
- Vol. 46 (3)
Wettability and reaction of copper slag with MgO, Al2O3, ZrO2, MgCr2O4, MgAl2O4, ZnAl2O4 and Mg2SnO4
- 11 September 2025
- Published by Elsevier in Journal of the European Ceramic Society
- Vol. 46 (3)
Open AccessWettability and reaction of copper slag with MgO, Al2O3, ZrO2, MgCr2O4, MgAl2O4, ZnAl2O4 and Mg2SnO4
- Open Access
- 18 May 2025
- Published by Elsevier in Journal of the European Ceramic Society
- Vol. 45 (14)
Abrasion resistance and hardness of Cr-free zinc and iron co-doped spinel and magnesia-spinel refractory matrices for copper smelting
- 18 May 2025
- Published by Elsevier in Journal of the European Ceramic Society
- Vol. 45 (14)
Open AccessAbrasion resistance and hardness of Cr-free zinc and iron co-doped spinel and magnesia-spinel refractory matrices for copper smelting
- 10 April 2024
- Published by Elsevier in Ceramics International
- Vol. 50 (13) , 23315-23330
Influence of PbO/CuO ratio on phase composition, microstructure, melt wettability and recyclability of copper slag
- 10 April 2024
- Published by Elsevier in Ceramics International
- Vol. 50 (13) , 23315-23330
Influence of PbO/CuO ratio on phase composition, microstructure, melt wettability and recyclability of copper slag
- 7 June 2023
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 106 (10) , 5662-5678
Impact on aggregate/matrix bonding when a refractory contains zinc aluminate instead of spinel and magnesia‐chrome
The high hot strength of MgO–Cr 2 O 3 refractory is often ascribed to its intimate aggregate/matrix bonding. For a fundamental comparison with it, ∼2 mm aggregates of MgO and Al 2 O 3 were separately embedded in ZnAl 2 O 4 and MgAl 2 O 4 matrices, sintered at 1600°C, and examined. It was found that similarity of thermal expansion coefficient (TEC) between the aggregate and the matrix is critical to achieve good bonding and this is more important than the extent of interdiffusion. The TEC mismatch of ≥5.7 × 10 −6 K −1 caused significant undesirable debonding in MgO aggregate/MgAl 2 O 4 matrix sample and MgO/ZnAl 2 O 4 despite >736 μm Zn 2+ diffusion depth in the latter. Direct bonding, as inferred from a thicker interfacial reaction layer and a greater shift of the aggregate/matrix interface before and after firing, was better in MgAl 2 O 4 /ZnAl 2 O 4 combination, followed by tabular Al 2 O 3 /ZnAl 2 O 4 and Al 2 O 3 /MgAl 2 O 4 . Powder X‐ray diffraction indicated that the volatilization of ZnAl 2 O 4 at 1600°C in air was negligible compared to MgO–Cr 2 O 3 .
- 7 June 2023
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 106 (10) , 5662-5678
Impact on aggregate/matrix bonding when a refractory contains zinc aluminate instead of spinel and magnesia‐chrome
The high hot strength of MgO–Cr 2 O 3 refractory is often ascribed to its intimate aggregate/matrix bonding. For a fundamental comparison with it, ∼2 mm aggregates of MgO and Al 2 O 3 were separately embedded in ZnAl 2 O 4 and MgAl 2 O 4 matrices, sintered at 1600°C, and examined. It was found that similarity of thermal expansion coefficient (TEC) between the aggregate and the matrix is critical to achieve good bonding and this is more important than the extent of interdiffusion. The TEC mismatch of ≥5.7 × 10 −6 K −1 caused significant undesirable debonding in MgO aggregate/MgAl 2 O 4 matrix sample and MgO/ZnAl 2 O 4 despite >736 μm Zn 2+ diffusion depth in the latter. Direct bonding, as inferred from a thicker interfacial reaction layer and a greater shift of the aggregate/matrix interface before and after firing, was better in MgAl 2 O 4 /ZnAl 2 O 4 combination, followed by tabular Al 2 O 3 /ZnAl 2 O 4 and Al 2 O 3 /MgAl 2 O 4 . Powder X‐ray diffraction indicated that the volatilization of ZnAl 2 O 4 at 1600°C in air was negligible compared to MgO–Cr 2 O 3 .
- Open Access
- 1 December 2021
- Published by Wiley in International Journal of Ceramic Engineering & Science
- Vol. 4 (1) , 47-52
Use of dilatometer to screen refractory raw materials
Sudden shortage of a particular raw material due to freight disruptions, competitive market, and COVID restrictions have frequently forced the refractory industry to rapidly develop alternative formulations using available low‐cost materials. These alternative ingredients might cursorily appear to have similar total impurity content, but the presence of certain impurity combinations depending on the refractory type can produce more fluid liquid phase at high temperature, thereby drastically reducing hot strength. Undetected by the commonly used X‐ray fluorescence (XRF) analysis, the low‐cost material might differ in mineral‐phase content, whose phase transformations during firing might create excessive expansion producing warpage of the refractory along with a high porosity reducing strength and corrosion resistance. Finally, those cheap raw materials might have similar sieve analysis to that of the standard ingredient but might have much lower tapped density, which would introduce detrimental porosity into the resulting refractory. Hence, time‐consuming trials are often performed. Dilatometer studies on pressed or cast samples in a single test can identify reaction temperatures of spinel or mullite formation, which expand during firing, along with the amount of expansion and exact times at which firing needs to be done. It can also compare relative shrinkage due to liquid‐phase formation among impure raw materials like recycled grogs or low‐grade ores. Finally, dilatometric step scan is shown as a fast technique to prepare in‐house, low‐cost reactive spinel powder, which can also work for mullite.
- 1 December 2021
- Published by Wiley in International Journal of Ceramic Engineering & Science
- Vol. 4 (1) , 47-52
Open AccessUse of dilatometer to screen refractory raw materials
Sudden shortage of a particular raw material due to freight disruptions, competitive market, and COVID restrictions have frequently forced the refractory industry to rapidly develop alternative formulations using available low‐cost materials. These alternative ingredients might cursorily appear to have similar total impurity content, but the presence of certain impurity combinations depending on the refractory type can produce more fluid liquid phase at high temperature, thereby drastically reducing hot strength. Undetected by the commonly used X‐ray fluorescence (XRF) analysis, the low‐cost material might differ in mineral‐phase content, whose phase transformations during firing might create excessive expansion producing warpage of the refractory along with a high porosity reducing strength and corrosion resistance. Finally, those cheap raw materials might have similar sieve analysis to that of the standard ingredient but might have much lower tapped density, which would introduce detrimental porosity into the resulting refractory. Hence, time‐consuming trials are often performed. Dilatometer studies on pressed or cast samples in a single test can identify reaction temperatures of spinel or mullite formation, which expand during firing, along with the amount of expansion and exact times at which firing needs to be done. It can also compare relative shrinkage due to liquid‐phase formation among impure raw materials like recycled grogs or low‐grade ores. Finally, dilatometric step scan is shown as a fast technique to prepare in‐house, low‐cost reactive spinel powder, which can also work for mullite.
- 7 August 2020
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 103 (12) , 7095-7114
Designing environment‐friendly chromium‐free Spinel‐Periclase‐Zirconia refractories for Ruhrstahl Heraeus degasser
Ruhrstahl Heraeus (RH) degassers are globally used to manufacture vacuum‐treated steel for automotive and railroad applications. The state‐of‐the‐art environment‐friendly chromium‐free alternatives for direct‐bonded magnesia‐chrome refractories used in RH degassers are expensive, and the scientific literature lacks direct correlation between materials chemistry, processing, and functional properties. We have designed a novel spinel‐periclase‐15 wt% ZrO 2 composition containing 14 wt% in situ spinel which exhibited 7.2 MPa hot modulus of rupture (1500℃), exceeding all reported Cr‐free refractories for RH degasser applications. Investigation with scanning electron microscopy coupled with energy dispersive spectroscopy (SEM‐EDS) attributed this improvement to a reduction in interparticle Ca and Si content which forms low‐melting phases, as supported by FactSage thermodynamic simulations. The spinel‐periclase composition SP exhibited superior thermal shock resistance because thermal shock‐induced cracks were stopped by fracture porosity around MgO particles, formed due to thermal expansion mismatch. SEM‐EDS analysis of the SP composition corroded by RH slag at 1650°C revealed that Fe is the most corrosive element followed by Ca and Si. Contradicting the consensus, it was observed that corrosion resistance of fused MgO was better than that of ZrO 2 . The cubic ZrO 2 phase reduced FeO x penetration locally by incorporating CaO from the RH slag into a solid solution and forming a CaZrO 3 phase creating a “slag barrier”. Lastly, pore size was found to greatly exacerbate slag penetration following the Washburn percolation model.
- 7 August 2020
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 103 (12) , 7095-7114
Designing environment‐friendly chromium‐free Spinel‐Periclase‐Zirconia refractories for Ruhrstahl Heraeus degasser
Ruhrstahl Heraeus (RH) degassers are globally used to manufacture vacuum‐treated steel for automotive and railroad applications. The state‐of‐the‐art environment‐friendly chromium‐free alternatives for direct‐bonded magnesia‐chrome refractories used in RH degassers are expensive, and the scientific literature lacks direct correlation between materials chemistry, processing, and functional properties. We have designed a novel spinel‐periclase‐15 wt% ZrO 2 composition containing 14 wt% in situ spinel which exhibited 7.2 MPa hot modulus of rupture (1500℃), exceeding all reported Cr‐free refractories for RH degasser applications. Investigation with scanning electron microscopy coupled with energy dispersive spectroscopy (SEM‐EDS) attributed this improvement to a reduction in interparticle Ca and Si content which forms low‐melting phases, as supported by FactSage thermodynamic simulations. The spinel‐periclase composition SP exhibited superior thermal shock resistance because thermal shock‐induced cracks were stopped by fracture porosity around MgO particles, formed due to thermal expansion mismatch. SEM‐EDS analysis of the SP composition corroded by RH slag at 1650°C revealed that Fe is the most corrosive element followed by Ca and Si. Contradicting the consensus, it was observed that corrosion resistance of fused MgO was better than that of ZrO 2 . The cubic ZrO 2 phase reduced FeO x penetration locally by incorporating CaO from the RH slag into a solid solution and forming a CaZrO 3 phase creating a “slag barrier”. Lastly, pore size was found to greatly exacerbate slag penetration following the Washburn percolation model.
- 29 July 2017
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 15 (1) , 161-170
Microstructure and phase evolution of Indian magnesite‐derived MgAl 2 O 4 as a function of stoichiometry and ZrO 2 doping
To aid development of cost‐effective sintered spinel as a refractory raw material, this paper presents an extensive analysis of microstructure and complex phase evolution of Al‐rich, Mg‐rich, and stoichiometric spinel aggregates derived from Indian magnesite and calcined alumina. Pore morphology in Al‐rich spinel was transformed upon sintering at 1650°C and corundum laths embedded in porous Al‐rich spinel matrix was formed. Stoichiometric spinel sintered at 1600°C consisted of mostly direct bonded angular equiaxed spinel grains which incorporated the impurities in solid solution. Mg‐rich spinel was composed of spinel grains with reduced angularity along with intergranular amorphous phase, small round monticellite grains, and periclase. EDS line scan revealed impurity‐free joins existed between direct bonded spinel grains. Mg‐rich spinel containing 0.65 wt% ZrO 2 formed cubic ZrO 2 ‐CaO‐MgO solid solution located along spinel boundaries, which reduced both intergranular amorphous phase and monticellite. This increased SiO 2 and MgO content in spinel solid solution triggering exsolution of metastable cubic forsterite manifested as split spinel peaks in XRD pattern. A 14.7% reduction in slag penetration was exhibited upon doping Mg‐rich spinel with 0.21% ZrO 2 . Stoichiometric and Mg‐rich spinels attained 0.35% and 0.54% apparent porosity at 1600°C, which is better than most commercial sintered refractory spinels.
- 29 July 2017
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 15 (1) , 161-170
Microstructure and phase evolution of Indian magnesite‐derived MgAl 2 O 4 as a function of stoichiometry and ZrO 2 doping
To aid development of cost‐effective sintered spinel as a refractory raw material, this paper presents an extensive analysis of microstructure and complex phase evolution of Al‐rich, Mg‐rich, and stoichiometric spinel aggregates derived from Indian magnesite and calcined alumina. Pore morphology in Al‐rich spinel was transformed upon sintering at 1650°C and corundum laths embedded in porous Al‐rich spinel matrix was formed. Stoichiometric spinel sintered at 1600°C consisted of mostly direct bonded angular equiaxed spinel grains which incorporated the impurities in solid solution. Mg‐rich spinel was composed of spinel grains with reduced angularity along with intergranular amorphous phase, small round monticellite grains, and periclase. EDS line scan revealed impurity‐free joins existed between direct bonded spinel grains. Mg‐rich spinel containing 0.65 wt% ZrO 2 formed cubic ZrO 2 ‐CaO‐MgO solid solution located along spinel boundaries, which reduced both intergranular amorphous phase and monticellite. This increased SiO 2 and MgO content in spinel solid solution triggering exsolution of metastable cubic forsterite manifested as split spinel peaks in XRD pattern. A 14.7% reduction in slag penetration was exhibited upon doping Mg‐rich spinel with 0.21% ZrO 2 . Stoichiometric and Mg‐rich spinels attained 0.35% and 0.54% apparent porosity at 1600°C, which is better than most commercial sintered refractory spinels.