Muhammet Fatih Toksoy
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Muhammet Fatih Toksoy has a total of 30 co-authors. Here are the top co-authors by number of shared publications:
Richard A. Haber
Materials Science and Engineering Rutgers University New Brunswick New Jersey USA
6 shared publications- Kelvin Y. Xie
Department of Materials Science and Engineering, Texas A&M University, College Station, USA
4 shared publications William Rafaniello
Materials Sci. & Eng Rutgers University New Brunswick NJ USA
4 shared publicationsKanak Kuwelkar
2 shared publicationsKevin J. Hemker
2 shared publications- Kevin J. Hemker
Johns Hopkins Univ., Baltimore, MD (United States)
2 shared publications
Latest Publications
- 2 September 2026
- Published by Konya Muhendislik Bilimleri Dergisi in Konya Journal of Engineering Sciences
- Vol. 14 (3) , 1144-1154
ENHANCING THE MECHANICAL PROPERTIES OF BIO-BASED FILMS FOR FOOD PACKAGING
The increase in global population has intensified the need for innovative waste management solutions, making biodegradable plastics increasingly important. Polylactic acid (PLA) is one of the most widely used biobased and biodegradable polymers in the packaging industry due to its biocompatibility and environmental sustainability. However, PLA is inherently brittle and rigid, which limits its processing and packaging performance. To overcome these limitations, this study investigates the incorporation of Mater-Bi, a flexible biobased granule commonly used in shopping bags, into PLA films. Biodegradable films were prepared with varying PLA/Mater-Bi ratios: 100% PLA, 80% PLA–20% Mater-Bi, 70% PLA–30% Mater-Bi, 60% PLA–40% Mater-Bi, and 100% Mater-Bi. The films were characterized for mechanical properties, including thickness, surface density, tensile strength, elongation at break, and puncture resistance. Sealing performance was assessed to ensure food safety, while optical properties were evaluated to meet marketing requirements. FTIR spectroscopy was performed to analyze molecular interactions, and residual solvent levels were verified using gas chromatography to comply with food safety standards. Results indicated that increasing Mater-Bi content enhanced film flexibility and elongation but reduced tensile strength and puncture resistance. Transparency decreased with higher Mater-Bi content, producing a more yellowish tint compared to pure PLA. This study provides a methodology for optimizing PLA-based biodegradable films, offering an alternative for sustainable food packaging with improved mechanical performance.
- 2 September 2026
- Published by Konya Muhendislik Bilimleri Dergisi in Konya Journal of Engineering Sciences
- Vol. 14 (3) , 1144-1154
ENHANCING THE MECHANICAL PROPERTIES OF BIO-BASED FILMS FOR FOOD PACKAGING
The increase in global population has intensified the need for innovative waste management solutions, making biodegradable plastics increasingly important. Polylactic acid (PLA) is one of the most widely used biobased and biodegradable polymers in the packaging industry due to its biocompatibility and environmental sustainability. However, PLA is inherently brittle and rigid, which limits its processing and packaging performance. To overcome these limitations, this study investigates the incorporation of Mater-Bi, a flexible biobased granule commonly used in shopping bags, into PLA films. Biodegradable films were prepared with varying PLA/Mater-Bi ratios: 100% PLA, 80% PLA–20% Mater-Bi, 70% PLA–30% Mater-Bi, 60% PLA–40% Mater-Bi, and 100% Mater-Bi. The films were characterized for mechanical properties, including thickness, surface density, tensile strength, elongation at break, and puncture resistance. Sealing performance was assessed to ensure food safety, while optical properties were evaluated to meet marketing requirements. FTIR spectroscopy was performed to analyze molecular interactions, and residual solvent levels were verified using gas chromatography to comply with food safety standards. Results indicated that increasing Mater-Bi content enhanced film flexibility and elongation but reduced tensile strength and puncture resistance. Transparency decreased with higher Mater-Bi content, producing a more yellowish tint compared to pure PLA. This study provides a methodology for optimizing PLA-based biodegradable films, offering an alternative for sustainable food packaging with improved mechanical performance.
- 15 May 2026
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 35 (32) , 33115-33125
Experimental Evaluation of Recycled GG25 Cast Iron as a Partial Steel Fiber Substitute for Aviation Clutches
- 15 May 2026
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 35 (32) , 33115-33125
Experimental Evaluation of Recycled GG25 Cast Iron as a Partial Steel Fiber Substitute for Aviation Clutches
- Open Access
- 20 March 2025
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 22 (4)
Regression analysis of material properties and hardness of dense boron carbide
Material properties directly affect the final performance of the produced articles. This study aims to establish a correlation between materials properties and hardness of boron carbide samples. Ten different boron carbide powders were sintered to high densities by spark plasma sintering, and material properties (grain size, density, stoichiometry, and free carbon) were analyzed. Hardness tests were conducted on these samples. All experimental procedures were completed by a single operator, and the same instruments were used for all the samples. Multiple linear regressions using the ordinary least squares method in SPSS were carried out to identify the relationship between hardness and material properties. Analyses showed density is the most dominant property, surpassing any other parameter. Grain size became more dominant at higher densities (>99%) and affected hardness results. Both grain size and density are the result of the starting powder and the densification procedure. This study showed that 80% of the hardness variation can be explained by this model.
- 20 March 2025
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 22 (4)
Open AccessRegression analysis of material properties and hardness of dense boron carbide
Material properties directly affect the final performance of the produced articles. This study aims to establish a correlation between materials properties and hardness of boron carbide samples. Ten different boron carbide powders were sintered to high densities by spark plasma sintering, and material properties (grain size, density, stoichiometry, and free carbon) were analyzed. Hardness tests were conducted on these samples. All experimental procedures were completed by a single operator, and the same instruments were used for all the samples. Multiple linear regressions using the ordinary least squares method in SPSS were carried out to identify the relationship between hardness and material properties. Analyses showed density is the most dominant property, surpassing any other parameter. Grain size became more dominant at higher densities (>99%) and affected hardness results. Both grain size and density are the result of the starting powder and the densification procedure. This study showed that 80% of the hardness variation can be explained by this model.
- Open Access
- 1 January 2025
- Published by National Library of Serbia in Processing and Application of Ceramics
- Vol. 19 (1) , 108-113
Homogeneity enhancement of oxide additives in boron carbide by precipitation method
This study elucidates the use of the precipitation method to enhance the uniformity of oxide additives in boron carbide ceramics. Achieving a homogeneous distribution of additives is critical, as higher additive content tends to degrade the mechanical properties of boron carbide. In this research, yttrium and aluminium hydroxide salts were dispersed and incorporated into boron carbide slurry under highly alkaline conditions. The mixture was aged and subsequently calcined to produce metal oxide layers around the boron carbide particles. The additive-to-boron carbide ratio and calcination conditions were systematically varied and the resulting powders were characterized using SEM, EDX and zeta potential analyses. The precipitation method effectively improved additive dispersion, achieving a uniform distribution. Furthermore, samples processed through precipitation exhibited higher densities compared to conventional benchmark samples.
- 1 January 2025
- Published by National Library of Serbia in Processing and Application of Ceramics
- Vol. 19 (1) , 108-113
Open AccessHomogeneity enhancement of oxide additives in boron carbide by precipitation method
This study elucidates the use of the precipitation method to enhance the uniformity of oxide additives in boron carbide ceramics. Achieving a homogeneous distribution of additives is critical, as higher additive content tends to degrade the mechanical properties of boron carbide. In this research, yttrium and aluminium hydroxide salts were dispersed and incorporated into boron carbide slurry under highly alkaline conditions. The mixture was aged and subsequently calcined to produce metal oxide layers around the boron carbide particles. The additive-to-boron carbide ratio and calcination conditions were systematically varied and the resulting powders were characterized using SEM, EDX and zeta potential analyses. The precipitation method effectively improved additive dispersion, achieving a uniform distribution. Furthermore, samples processed through precipitation exhibited higher densities compared to conventional benchmark samples.
- 14 October 2018
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 16 (3) , 1120-1125
Modification of commercial boron carbide powder using Rapid Carbothermal Reduction
- 14 October 2018
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 16 (3) , 1120-1125
Modification of commercial boron carbide powder using Rapid Carbothermal Reduction
- 1 December 2017
- Published by Elsevier in Materials Characterization
- Vol. 134, 274-278
The effect of Si on the microstructure and mechanical properties of spark plasma sintered boron carbide
- 1 December 2017
- Published by Elsevier in Materials Characterization
- Vol. 134, 274-278
The effect of Si on the microstructure and mechanical properties of spark plasma sintered boron carbide
- 13 February 2017
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 14 (3) , 443-453
Densification and characterization of rapid carbothermal synthesized boron carbide
Submicrometer boron carbide powders were synthesized using rapid carbothermal reduction (RCR) method. Synthesized boron carbide powders had smaller particle size, lower free carbon, and high density of twins compared to commercial samples. Powders were sintered using spark plasma sintering at different temperatures and dwell times to compare sintering behavior. Synthesized boron carbide powders reached >99% TD at lower temperature and shorter dwell times compared to commercial powders. Improved microhardness observed in the densified RCR samples was likely caused by the combination of higher purity, better stoichiometry control, finer grain size, and a higher density of twin boundaries.
- 13 February 2017
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 14 (3) , 443-453
Densification and characterization of rapid carbothermal synthesized boron carbide
Submicrometer boron carbide powders were synthesized using rapid carbothermal reduction (RCR) method. Synthesized boron carbide powders had smaller particle size, lower free carbon, and high density of twins compared to commercial samples. Powders were sintered using spark plasma sintering at different temperatures and dwell times to compare sintering behavior. Synthesized boron carbide powders reached >99% TD at lower temperature and shorter dwell times compared to commercial powders. Improved microhardness observed in the densified RCR samples was likely caused by the combination of higher purity, better stoichiometry control, finer grain size, and a higher density of twin boundaries.
- 14 November 2016
- Published by American Chemical Society (ACS) in Nano Letters
- Vol. 16 (12) , 7573-7579
Superstrength through Nanotwinning
The theoretical strength of a material is the minimum stress to deform or fracture the perfect single crystal material that has no defects. This theoretical strength is considered as an upper bound on the attainable strength for a real crystal. In contradiction to this expectation, we use quantum mechanics (QM) simulations to show that for the boron carbide (B4C) hard ceramic, this theoretical shear strength can be exceeded by 11% by imposing nano-scale twins. We also predict from QM that the indentation strength of nano-twinned B4C is 12% higher than that of the perfect crystal. Further we validate this effect experimentally, showing that nano-twinned samples are harder by 2.3% than the twin-free counterpart of B4C. The origin of this strengthening mechanism is suppression of twin boundary (TB) slip within the nano-twins due to the directional nature of covalent bonds at the TB.
- 14 November 2016
- Published by American Chemical Society (ACS) in Nano Letters
- Vol. 16 (12) , 7573-7579
Superstrength through Nanotwinning
The theoretical strength of a material is the minimum stress to deform or fracture the perfect single crystal material that has no defects. This theoretical strength is considered as an upper bound on the attainable strength for a real crystal. In contradiction to this expectation, we use quantum mechanics (QM) simulations to show that for the boron carbide (B4C) hard ceramic, this theoretical shear strength can be exceeded by 11% by imposing nano-scale twins. We also predict from QM that the indentation strength of nano-twinned B4C is 12% higher than that of the perfect crystal. Further we validate this effect experimentally, showing that nano-twinned samples are harder by 2.3% than the twin-free counterpart of B4C. The origin of this strengthening mechanism is suppression of twin boundary (TB) slip within the nano-twins due to the directional nature of covalent bonds at the TB.
- Open Access
- 20 October 2015
- Published by American Physical Society (APS) in Physical Review Letters
- Vol. 115 (17) , 175501
Atomic-Level Understanding of “Asymmetric Twins” in Boron Carbide
Recent observations of planar defects in boron carbide have been shown to deviate from perfect mirror symmetry and are referred to as “asymmetric twins.” Here, we demonstrate that these asymmetric twins are really phase boundaries that form in stoichiometric (i.e., ) but not in . TEM observations and ab initio simulations have been coupled to show that these planar defects result from an interplay of stoichiometry, atomic positioning, icosahedral twinning, and structural hierarchy. The composition of icosahedra in is and translation of the carbon atom from a polar to equatorial site leads to a shift in bonding and a slight distortion of the lattice. No such distortion is observed in boron-rich because the icosahedra do not contain carbon. Implications for tailoring boron carbide with stoichiometry and extrapolations to other hierarchical crystalline materials are discussed.- 20 October 2015
- Published by American Physical Society (APS) in Physical Review Letters
- Vol. 115 (17) , 175501
Open AccessAtomic-Level Understanding of “Asymmetric Twins” in Boron Carbide
Recent observations of planar defects in boron carbide have been shown to deviate from perfect mirror symmetry and are referred to as “asymmetric twins.” Here, we demonstrate that these asymmetric twins are really phase boundaries that form in stoichiometric (i.e., ) but not in . TEM observations and ab initio simulations have been coupled to show that these planar defects result from an interplay of stoichiometry, atomic positioning, icosahedral twinning, and structural hierarchy. The composition of icosahedra in is and translation of the carbon atom from a polar to equatorial site leads to a shift in bonding and a slight distortion of the lattice. No such distortion is observed in boron-rich because the icosahedra do not contain carbon. Implications for tailoring boron carbide with stoichiometry and extrapolations to other hierarchical crystalline materials are discussed. - 10 February 2015
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 5 (25) , 19067-19073
Improvement of crystallization and particle size distribution of boric acid in the processing of a boron carbide precursor
In the processing of crystalline boron carbide, boron oxide and carbon precursors are used as feedstock into a carbothermal reduction process reactor. The uniformity of the precursor blends has a dramatic effect on the homogeneity of the resultant boron carbide. In boron carbide precursor preparation via a wet process, boric acid is usually dissolved into water at 80 °C and then mixed with carbon and dried at 120 °C, followed by calcination then comminution to obtain the desired feed particle size. However, controlling the crystallization and particle size of boric acid is challenging and there are no prior published studies dealing with this issue. In this study, a simple process demonstrated that adding hexane to the boric acid water solution during the drying can achieve a highly crystallized powder with a narrow particle size distribution. Hexane generates supersaturation during the recrystallization of boric acid by increasing boric acid nucleation. The hexane can inhibit boric acid crystal growth by isolating the formed nuclei thus providing a barrier to molecular diffusion. The water to hexane volumetric ratio, suitable processing parameters, and optimized dispersant amount were investigated. It was found that the process of mixing the optimum solution at room temperature and then drying it at 120 °C produced the relatively uniform 0.3 μm particles. By adding 1.5 wt% dispersant (Triton X-100) to the mixture, 20 nm boric acid particle size can be obtained. The boron carbide powder fabricated by carbothermal process from the modified precursor demonstrated a finer and more uniform particle size with lower free carbon content. The precursor calcination temperature could be lowered from 600 °C to 450 °C.
- 10 February 2015
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 5 (25) , 19067-19073
Improvement of crystallization and particle size distribution of boric acid in the processing of a boron carbide precursor
In the processing of crystalline boron carbide, boron oxide and carbon precursors are used as feedstock into a carbothermal reduction process reactor. The uniformity of the precursor blends has a dramatic effect on the homogeneity of the resultant boron carbide. In boron carbide precursor preparation via a wet process, boric acid is usually dissolved into water at 80 °C and then mixed with carbon and dried at 120 °C, followed by calcination then comminution to obtain the desired feed particle size. However, controlling the crystallization and particle size of boric acid is challenging and there are no prior published studies dealing with this issue. In this study, a simple process demonstrated that adding hexane to the boric acid water solution during the drying can achieve a highly crystallized powder with a narrow particle size distribution. Hexane generates supersaturation during the recrystallization of boric acid by increasing boric acid nucleation. The hexane can inhibit boric acid crystal growth by isolating the formed nuclei thus providing a barrier to molecular diffusion. The water to hexane volumetric ratio, suitable processing parameters, and optimized dispersant amount were investigated. It was found that the process of mixing the optimum solution at room temperature and then drying it at 120 °C produced the relatively uniform 0.3 μm particles. By adding 1.5 wt% dispersant (Triton X-100) to the mixture, 20 nm boric acid particle size can be obtained. The boron carbide powder fabricated by carbothermal process from the modified precursor demonstrated a finer and more uniform particle size with lower free carbon content. The precursor calcination temperature could be lowered from 600 °C to 450 °C.