Nagendra S. Bhairamadgi
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Nagendra S. Bhairamadgi has a total of 15 co-authors. Here are the top co-authors by number of shared publications:
Pandurang N. Honkhambe
Polymer Science and Engineering Division, National Chemical Laboratory, Pune 411008, India
3 shared publications- Prakash P. Wadgaonkar
CSIR-National Chemical Laboratory
3 shared publications Mahesh V. Biyani
Polymer Science and Engineering Division, National Chemical Laboratory, Pune 411008, India
2 shared publications- Manikrao M. Salunkhe
Department of Chemistry , Institute of Science , Mumbai, India
2 shared publications A. S. Patil
Solapur University
1 shared publicationKishor P. Kumbhar
Polymer Science and Engineering Division, National Chemical Laboratory, Pune 411008, India
1 shared publication
Latest Publications
- 31 May 2011
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 122 (3) , 1607-1613
Poly(ether ether ketone)s and poly(ether ether ketone ketone)s containing cardo decahydronaphthalene groups: Synthesis and characterization
New poly(ether ether ketone)s and poly (ether ether ketone ketone)s were synthesized by polycondensation of each of the three bisphenols, viz., 4,4′‐(octahydro‐2(1H)‐naphthylidene)bisphenol, 4,4′‐(octahydro‐2(1H)‐naphthylidene)bis‐3‐methylphenol, and 4,4′‐(octahydro‐2(1H)‐naphthylidene)bis‐3,5‐dimethylphenol with 4,4′‐difluorobenzophenone and 1,3‐bis(4‐fluorobenzoyl)benzene in a mixture of N,N‐dimethylacetamide and toluene [1 : 1 (v/v)] in the presence of anhydrous potassium carbonate. Inherent viscosities of poly(ether ether ketone)s and poly (ether ether ketone ketone)s were in the range 0.32–0.80 dL/g and number‐average molecular weights were in the range 16,100–55,900 g/mol. Poly(ether ether ketone)s and poly(ether ether ketone ketone)s were soluble in organic solvents such as dichloromethane, chloroform, tetrahydrofuran, meta‐cresol, pyridine, and 1‐methyl‐2‐pyrrolidinone at room temperature and could be cast into tough, transparent, and flexible films from their chloroform solutions. Wide angle x‐ray diffraction measurements revealed the amorphous nature of poly(ether ether ketone)s and poly (ether ether ketone ketone)s. The glass transition temperature poly(ether ether ketone)s and poly(ether ether ketone ketone)s were in the range 185–251°C. The temperature at 10% weight loss, determined from thermogravimetric analysis, of poly(ether ether ketone)s and poly(ether ether ketone ketone)s in nitrogen atmosphere was in the range 462–493°C indicating their good thermal stability. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2011
- 31 May 2011
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 122 (3) , 1607-1613
Poly(ether ether ketone)s and poly(ether ether ketone ketone)s containing cardo decahydronaphthalene groups: Synthesis and characterization
New poly(ether ether ketone)s and poly (ether ether ketone ketone)s were synthesized by polycondensation of each of the three bisphenols, viz., 4,4′‐(octahydro‐2(1H)‐naphthylidene)bisphenol, 4,4′‐(octahydro‐2(1H)‐naphthylidene)bis‐3‐methylphenol, and 4,4′‐(octahydro‐2(1H)‐naphthylidene)bis‐3,5‐dimethylphenol with 4,4′‐difluorobenzophenone and 1,3‐bis(4‐fluorobenzoyl)benzene in a mixture of N,N‐dimethylacetamide and toluene [1 : 1 (v/v)] in the presence of anhydrous potassium carbonate. Inherent viscosities of poly(ether ether ketone)s and poly (ether ether ketone ketone)s were in the range 0.32–0.80 dL/g and number‐average molecular weights were in the range 16,100–55,900 g/mol. Poly(ether ether ketone)s and poly(ether ether ketone ketone)s were soluble in organic solvents such as dichloromethane, chloroform, tetrahydrofuran, meta‐cresol, pyridine, and 1‐methyl‐2‐pyrrolidinone at room temperature and could be cast into tough, transparent, and flexible films from their chloroform solutions. Wide angle x‐ray diffraction measurements revealed the amorphous nature of poly(ether ether ketone)s and poly (ether ether ketone ketone)s. The glass transition temperature poly(ether ether ketone)s and poly(ether ether ketone ketone)s were in the range 185–251°C. The temperature at 10% weight loss, determined from thermogravimetric analysis, of poly(ether ether ketone)s and poly(ether ether ketone ketone)s in nitrogen atmosphere was in the range 462–493°C indicating their good thermal stability. © 2011 Wiley Periodicals, Inc. J Appl Polym Sci, 2011
- 10 July 2010
- Published by Springer Nature in Polymer Bulletin
- Vol. 66 (9) , 1207-1218
Synthesis and characterization of soluble polyamides from bis-[(4′-aminobenzyl)-4-benzamide] ether and various diacids
- 10 July 2010
- Published by Springer Nature in Polymer Bulletin
- Vol. 66 (9) , 1207-1218
Synthesis and characterization of soluble polyamides from bis-[(4′-aminobenzyl)-4-benzamide] ether and various diacids
- 13 April 2010
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 117 (5) , 2545-2552
Synthesis and characterization of new aromatic polyesters containing pendent naphthyl units
Two bisphenols, viz., 4,4′‐[1‐(2‐naphthalenyl)ethylidene]bisphenol and 4,4′‐[1‐(2‐naphthalenyl) ethylidene]bis‐3‐methylphenol were prepared by condensation of commercially available 2‐acetonaphthanone with phenol and o‐cresol, respectively. A series of new aromatic polyesters containing pendent naphthyl units was synthesized by phase‐transfer‐catalyzed interfacial polycondensation of these bisphenols with isophthaloyl chloride, terephthaloyl chloride, and a mixture of isophthaloyl chloride/terephthaloyl chloride (50 : 50 mol %). Inherent viscosities of polyesters were in the range 0.83–1.76 dL g−1, while number average molecular weights (Mn) were in the range 61,000–235,000 g mol−1. Polyesters were readily soluble in organic solvents such as dichloromethane, chloroform, tetrahydrofuran, m‐cresol, pyridine, N,N‐dimethylformamide, N,N‐dimethylacetamide, and 1‐methyl‐2‐pyrrolidinone at room temperature. Tough, transparent, and flexible films were cast from a solution of polyesters in chloroform. X‐Ray diffraction measurements displayed a broad halo at 2θ ≅ 19° indicating the amorphous nature of polyesters. Glass transition temperatures of polyesters were in the range 209–259°C. The temperature at 10% weight loss (T10), determined by TGA in nitrogen atmosphere, of polyesters was in the range 435–500°C indicating their good thermal stability. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2010
- 13 April 2010
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 117 (5) , 2545-2552
Synthesis and characterization of new aromatic polyesters containing pendent naphthyl units
Two bisphenols, viz., 4,4′‐[1‐(2‐naphthalenyl)ethylidene]bisphenol and 4,4′‐[1‐(2‐naphthalenyl) ethylidene]bis‐3‐methylphenol were prepared by condensation of commercially available 2‐acetonaphthanone with phenol and o‐cresol, respectively. A series of new aromatic polyesters containing pendent naphthyl units was synthesized by phase‐transfer‐catalyzed interfacial polycondensation of these bisphenols with isophthaloyl chloride, terephthaloyl chloride, and a mixture of isophthaloyl chloride/terephthaloyl chloride (50 : 50 mol %). Inherent viscosities of polyesters were in the range 0.83–1.76 dL g−1, while number average molecular weights (Mn) were in the range 61,000–235,000 g mol−1. Polyesters were readily soluble in organic solvents such as dichloromethane, chloroform, tetrahydrofuran, m‐cresol, pyridine, N,N‐dimethylformamide, N,N‐dimethylacetamide, and 1‐methyl‐2‐pyrrolidinone at room temperature. Tough, transparent, and flexible films were cast from a solution of polyesters in chloroform. X‐Ray diffraction measurements displayed a broad halo at 2θ ≅ 19° indicating the amorphous nature of polyesters. Glass transition temperatures of polyesters were in the range 209–259°C. The temperature at 10% weight loss (T10), determined by TGA in nitrogen atmosphere, of polyesters was in the range 435–500°C indicating their good thermal stability. © 2010 Wiley Periodicals, Inc. J Appl Polym Sci, 2010
- 1 April 2010
- Published by Elsevier in Materials Science and Engineering: B
- Vol. 168 (1-3) , 186-192
Synthesis and characterization of polyesters from 2,3-bis (4′-hydroxy phenyl) quinoxaline and 2,3-bis (2′-hydroxynaphthalene-6′-yl) quinoxaline
- 1 April 2010
- Published by Elsevier in Materials Science and Engineering: B
- Vol. 168 (1-3) , 186-192
Synthesis and characterization of polyesters from 2,3-bis (4′-hydroxy phenyl) quinoxaline and 2,3-bis (2′-hydroxynaphthalene-6′-yl) quinoxaline
- 11 January 2010
- Published by Elsevier in European Polymer Journal
- Vol. 46 (4) , 709-718
Synthesis and characterization of new aromatic polyesters containing cardo decahydronaphthalene groups
- 11 January 2010
- Published by Elsevier in European Polymer Journal
- Vol. 46 (4) , 709-718
Synthesis and characterization of new aromatic polyesters containing cardo decahydronaphthalene groups