Stuart Bell
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Stuart Bell has a total of 61 co-authors. Here are the top co-authors by number of shared publications:
Geoffrey Will
13 shared publications- Geoffrey Will
University of the Sunshine Coast
8 shared publications Ted Steinberg
Queensland University of Technology
6 shared publicationsTheodore A. Steinberg
6 shared publications- Gaurav Vithalani
Queensland University of Technology
4 shared publications Ralf Raud
Queensland University of Technology 2 George St Brisbane QLD 4000 Australia
4 shared publications
Latest Publications
- Open Access
- 7 October 2026
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 45, 4031-4044
Quantification of early-stage sigma phase nucleation in thermally aged 2205 duplex stainless steel at 850 °C: An integrated experimental, kinetic, and thermodynamic modelling approach
- 7 October 2026
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 45, 4031-4044
Open AccessQuantification of early-stage sigma phase nucleation in thermally aged 2205 duplex stainless steel at 850 °C: An integrated experimental, kinetic, and thermodynamic modelling approach
- Open Access
- 20 July 2026
- Published by Elsevier in SSRN Electronic Journal
Evaluation of performance limitations and fabrication challenges of natural material derived triboelectric nanogenerators
Effective research and development of triboelectric nanogenerators (TENGs) require standardized testing protocol and fabrication method for consistent performance evaluation and comparison across devices. Conventional methods, such as hand tapping/human induced motions, introduce uncontrolled variations that lead to inconsistent and often exaggerated electrical outputs. This work presents, TENG performance analysis using a fatigue capable Mechanical Testing System, enabling precise control of applied force, displacement and frequency. As a proof-of-concept, a sustainable TENG was fabricated using orange peel powder as the triboelectric layer to replicate a natural material based TENG in recent literature. For the first time, under controlled conditions, device exhibited a stable open-circuit voltage (Voc) of ~8 V (1.13% error) and an electrical power of 28 nW (per-cycle), in contrast to the highly variable 88 – 155 Voc measured under manual tapping. These findings demonstrate that standardized testing protocol with reproducibility is required to provide realistic assessments of device performance to address this performance limitation. Beyond showcasing the potential of natural waste-derived materials, this study highlights the requirement of a universal standard for TENG testing to eliminate errors within device fabrication and testing methods. Moreover, this work pinpoints practical measures to improve device performance by addressing key challenges in fabrication.
- 20 July 2026
- Published by Elsevier in SSRN Electronic Journal
Open AccessEvaluation of performance limitations and fabrication challenges of natural material derived triboelectric nanogenerators
Effective research and development of triboelectric nanogenerators (TENGs) require standardized testing protocol and fabrication method for consistent performance evaluation and comparison across devices. Conventional methods, such as hand tapping/human induced motions, introduce uncontrolled variations that lead to inconsistent and often exaggerated electrical outputs. This work presents, TENG performance analysis using a fatigue capable Mechanical Testing System, enabling precise control of applied force, displacement and frequency. As a proof-of-concept, a sustainable TENG was fabricated using orange peel powder as the triboelectric layer to replicate a natural material based TENG in recent literature. For the first time, under controlled conditions, device exhibited a stable open-circuit voltage (Voc) of ~8 V (1.13% error) and an electrical power of 28 nW (per-cycle), in contrast to the highly variable 88 – 155 Voc measured under manual tapping. These findings demonstrate that standardized testing protocol with reproducibility is required to provide realistic assessments of device performance to address this performance limitation. Beyond showcasing the potential of natural waste-derived materials, this study highlights the requirement of a universal standard for TENG testing to eliminate errors within device fabrication and testing methods. Moreover, this work pinpoints practical measures to improve device performance by addressing key challenges in fabrication.
- Open Access
- 5 March 2026
- Published by Elsevier in Engineering Failure Analysis
- Vol. 190
Thermo-Mechanical failure of SS 630 alloy during heat treatment
- 5 March 2026
- Published by Elsevier in Engineering Failure Analysis
- Vol. 190
Open AccessThermo-Mechanical failure of SS 630 alloy during heat treatment
- Open Access
- 22 September 2025
- Published by TIB Open Publishing in SolarPACES Conference Proceedings
- Vol. 3
Development of a Small Punch Test to Evaluate Liquid Metal Embrittlement Susceptibility of 316L Stainless Steel in Liquid Sodium
Liquid sodium is proposed as a heat transfer fluid for solar thermal power receiver designs. It has a long history of use for heat transfer in various industries, with extensive knowledge of its impact on the structural integrity of materials at temperatures ranging from 300 ℃ to 800 ℃. However, the effects at lower temperatures are more poorly understood, which is crucial to studying solar thermal power plant systems. These systems experience diurnal cyclic temperature variation, which causes significant fluctuations in the operating temperature of liquid sodium. Several studies have demonstrated that the susceptibility of metals to Liquid Metal Embrittlement (LME) is highest at temperatures close to the melting point of the liquid metal. Therefore, this study investigates the susceptibility of 316L stainless steel, a common construction material, to sodium induced LME at temperatures between 100 ℃ to 300 ℃ using the Small Punch Test (SPT) method. The test apparatus was validated by using a known embrittling pair of Brass-Galinstan between 10 ℃ to 43 ℃, where the test revealed the expected LME susceptibility of brass. However, no evidence of LME was found in the 316L-sodium pair at temperatures up to 300 ℃.
- 22 September 2025
- Published by TIB Open Publishing in SolarPACES Conference Proceedings
- Vol. 3
Open AccessDevelopment of a Small Punch Test to Evaluate Liquid Metal Embrittlement Susceptibility of 316L Stainless Steel in Liquid Sodium
Liquid sodium is proposed as a heat transfer fluid for solar thermal power receiver designs. It has a long history of use for heat transfer in various industries, with extensive knowledge of its impact on the structural integrity of materials at temperatures ranging from 300 ℃ to 800 ℃. However, the effects at lower temperatures are more poorly understood, which is crucial to studying solar thermal power plant systems. These systems experience diurnal cyclic temperature variation, which causes significant fluctuations in the operating temperature of liquid sodium. Several studies have demonstrated that the susceptibility of metals to Liquid Metal Embrittlement (LME) is highest at temperatures close to the melting point of the liquid metal. Therefore, this study investigates the susceptibility of 316L stainless steel, a common construction material, to sodium induced LME at temperatures between 100 ℃ to 300 ℃ using the Small Punch Test (SPT) method. The test apparatus was validated by using a known embrittling pair of Brass-Galinstan between 10 ℃ to 43 ℃, where the test revealed the expected LME susceptibility of brass. However, no evidence of LME was found in the 316L-sodium pair at temperatures up to 300 ℃.
- Open Access
- 16 September 2024
- Published by TIB Open Publishing in SolarPACES Conference Proceedings
- Vol. 2
Investigation of Factors Affecting Corrosion Mechanisms in Latent Heat Thermal Energy Storage Systems
Concentrated Solar Power (CSP) plants integrated with Latent Heat Thermal Energy Storage (LHTES) systems offer a promising solution for dispatchability, reliability, and economic concerns generally associated with renewable energy technologies. These systems, however, require an operational life of up to 30 years to compete with power plant systems operating on fossil fuels. This is a significant challenge due to the high temperatures and corrosive eutectic salts utilised in LHTES systems. Additionally, these systems and its subcomponents are expected to be under varying degrees of stress due to the diurnal cyclic temperature variations inherent in the plant’s operational cycle. Hence, it is crucial to understand the various factors that can affect the operational life of materials used in such applications and conduct thorough material compatibility studies to assess the combined impact of these operating conditions on corrosion mechanisms. This study presents a novel static immersion test approach using modified Compact Tension (CT) specimens manufactured from 316L to investigate the effects of Na2CO3:NaCl (59.45:40.55 wt.%) salt, elevated temperatures (700 ℃ for up to 1000 hours), and stress on corrosion induced in the alloy. The post-exposure results are characterised with Scanning Electron Microscopy (SEM) and Energy Dispersive Spectroscopy (EDS) shows that corrosion mechanisms are significantly affected by factors such as high operating temperatures leading to changes in both corrosion morphology and rate, high stresses causing localised preferential corrosion, as well as corrosive salt and oxygen availability affecting the type of corrosion induced.
- 16 September 2024
- Published by TIB Open Publishing in SolarPACES Conference Proceedings
- Vol. 2
Open AccessInvestigation of Factors Affecting Corrosion Mechanisms in Latent Heat Thermal Energy Storage Systems
Concentrated Solar Power (CSP) plants integrated with Latent Heat Thermal Energy Storage (LHTES) systems offer a promising solution for dispatchability, reliability, and economic concerns generally associated with renewable energy technologies. These systems, however, require an operational life of up to 30 years to compete with power plant systems operating on fossil fuels. This is a significant challenge due to the high temperatures and corrosive eutectic salts utilised in LHTES systems. Additionally, these systems and its subcomponents are expected to be under varying degrees of stress due to the diurnal cyclic temperature variations inherent in the plant’s operational cycle. Hence, it is crucial to understand the various factors that can affect the operational life of materials used in such applications and conduct thorough material compatibility studies to assess the combined impact of these operating conditions on corrosion mechanisms. This study presents a novel static immersion test approach using modified Compact Tension (CT) specimens manufactured from 316L to investigate the effects of Na2CO3:NaCl (59.45:40.55 wt.%) salt, elevated temperatures (700 ℃ for up to 1000 hours), and stress on corrosion induced in the alloy. The post-exposure results are characterised with Scanning Electron Microscopy (SEM) and Energy Dispersive Spectroscopy (EDS) shows that corrosion mechanisms are significantly affected by factors such as high operating temperatures leading to changes in both corrosion morphology and rate, high stresses causing localised preferential corrosion, as well as corrosive salt and oxygen availability affecting the type of corrosion induced.
- Open Access
- 28 August 2024
- Published by TIB Open Publishing in SolarPACES Conference Proceedings
- Vol. 2
Effect of Load Cycling on High Temperature Creep of 316L Stainless Steel
For components in concentrating solar thermal plants, the creep mechanism will cause a significant portion of material damage to receivers, storage tanks, turbines and pipework. These components will undergo conditions where loads, temperature, or both load and temperature are not constatnly applied. This creep damage process will not resemble the constant load creep tests used to characterise creep of materials. Therefore, creep tests incorporating a load cycle were undertaken to obtain a better understanding of how high temperature materials respond to these cyclic conditions. These tests showed that when time under load was considered, creep undertaken under load cycling conditions were accelerated relative to constant load conditions. A modified Larson-Miller approach was used to assess this effect and determine an equivalent stress where constant load test data agrees with the cycled test data. This found that cycling the load was equivalent to if the system were under 3 and 7 MPa higher stress, for tests which were loaded for 12 hrs and 6 hrs per 24 hrs respectively. This could be a potential approach to simply and easily consider these load cycling effects for design and life analysis.
- 28 August 2024
- Published by TIB Open Publishing in SolarPACES Conference Proceedings
- Vol. 2
Open AccessEffect of Load Cycling on High Temperature Creep of 316L Stainless Steel
For components in concentrating solar thermal plants, the creep mechanism will cause a significant portion of material damage to receivers, storage tanks, turbines and pipework. These components will undergo conditions where loads, temperature, or both load and temperature are not constatnly applied. This creep damage process will not resemble the constant load creep tests used to characterise creep of materials. Therefore, creep tests incorporating a load cycle were undertaken to obtain a better understanding of how high temperature materials respond to these cyclic conditions. These tests showed that when time under load was considered, creep undertaken under load cycling conditions were accelerated relative to constant load conditions. A modified Larson-Miller approach was used to assess this effect and determine an equivalent stress where constant load test data agrees with the cycled test data. This found that cycling the load was equivalent to if the system were under 3 and 7 MPa higher stress, for tests which were loaded for 12 hrs and 6 hrs per 24 hrs respectively. This could be a potential approach to simply and easily consider these load cycling effects for design and life analysis.
- Open Access
- 13 May 2024
- Published by Elsevier in Solar Energy Materials and Solar Cells
- Vol. 272
Corrosion effects of Na2CO3/NaCl molten salt eutectic on 316L stainless steel under isothermal and cycling conditions
- 13 May 2024
- Published by Elsevier in Solar Energy Materials and Solar Cells
- Vol. 272
Open AccessCorrosion effects of Na2CO3/NaCl molten salt eutectic on 316L stainless steel under isothermal and cycling conditions
- Open Access
- 3 December 2023
- Published by Elsevier in Solar Energy Materials and Solar Cells
- Vol. 266
Novel method for evaluation of stress assisted corrosion through compact tension specimens to assess material compatibility in latent heat thermal energy storage systems
- 3 December 2023
- Published by Elsevier in Solar Energy Materials and Solar Cells
- Vol. 266
Open AccessNovel method for evaluation of stress assisted corrosion through compact tension specimens to assess material compatibility in latent heat thermal energy storage systems
- 13 April 2023
- Published by Elsevier in Solar Energy Materials and Solar Cells
- Vol. 256
Corrosion of iron–nickel–chromium alloys in high temperature carbonate salt under argon atmosphere
- 13 April 2023
- Published by Elsevier in Solar Energy Materials and Solar Cells
- Vol. 256
Corrosion of iron–nickel–chromium alloys in high temperature carbonate salt under argon atmosphere