Chayanee Tippayasam
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Chayanee Tippayasam has a total of 30 co-authors. Here are the top co-authors by number of shared publications:
- Attaphon Kaewvilai
King Mongkut’s University of Technology North Bangkok
5 shared publications - Duangrudee Chaysuwan
Department of Materials Engineering, Faculty of Engineering, Kasetsart University, Bangkok, Thailand
3 shared publications - Cristina Leonelli
Department of Engineering “Enzo Ferrari”, University of Modena and Reggio Emilia, 41125 Modena, Italy
2 shared publications - Jednupong Palomas
King Mongkut’s University of Technology North Bangkok
2 shared publications Parjaree Thavorniti
2 shared publicationsThammanoon Thaweechai
School of Integrated Science, Kasetsart University, Bangkok, Thailand
2 shared publications
Latest Publications
- Open Access
- 15 September 2026
- Published by Rangsit University in Journal of Current Science and Technology
- Vol. 16 (4) , 209
Utilization of Waste Silicone Sealant and Aluminium Scraps as Additives in Fly Ash–Based Geopolymer for Lightweight Construction Blocks
This study presents a pathway for using waste silicone sealant (Si-s) and aluminium scraps (Al-s) to produce lightweight geopolymer materials. Fly ash, sodium hydroxide, and sodium silicate were used as the starting materials for geopolymerization. Ground Si-s and Al-s were added to the mixtures, which were then cured for 28 days under ambient conditions (25°C). The structural composition and morphology were analyzed using Fourier-transform infrared spectroscopy (FTIR), X-ray diffraction (XRD), and scanning electron microscopy equipped with energy-dispersive X-ray spectroscopy (SEM–EDS). The results showed that Si-s acted as a dispersed additive in the geopolymer matrix and affected the reaction, possibly because its acidity neutralized the alkaline solution. It also increased the crystallite size to 51.68 nm, compared with 20.25 nm for the control geopolymer. The addition of Al-s produced a porous structure and reduced the crystallite size to 14.94 nm because it reacted with the alkaline solution, generating an exothermic reaction and hydrogen gas. The physical and mechanical properties, including density, apparent porosity, water absorption, compressive strength, and ultrasonic pulse velocity, were evaluated. The proportions of Al-s and Si-s were expressed as parts per hundred mixtures (phm), with the mixture comprising fly ash, NaOH, and Na₂SiO₃ used in the geopolymerization process. The addition of 0.4–0.6 phm Al-s and 40 phm Si-s resulted in geopolymers with densities of 1,292–1,438 kg/m³, apparent porosities of 18.18%–25.87%, and water absorption values of 6.97%–10.15%. The compressive strength ranged from 13.25 to 41.91 ksc, depending on the Si-s content. These geopolymers exhibited physical properties and compressive strengths that complied with the requirements for Type C12 lightweight concrete blocks specified in Thai Industrial Standard TIS 2601-2556. Therefore, waste Si-s and Al-s can be effectively recycled to produce lightweight geopolymer materials with properties suitable for construction applications.
- 15 September 2026
- Published by Rangsit University in Journal of Current Science and Technology
- Vol. 16 (4) , 209
Open AccessUtilization of Waste Silicone Sealant and Aluminium Scraps as Additives in Fly Ash–Based Geopolymer for Lightweight Construction Blocks
This study presents a pathway for using waste silicone sealant (Si-s) and aluminium scraps (Al-s) to produce lightweight geopolymer materials. Fly ash, sodium hydroxide, and sodium silicate were used as the starting materials for geopolymerization. Ground Si-s and Al-s were added to the mixtures, which were then cured for 28 days under ambient conditions (25°C). The structural composition and morphology were analyzed using Fourier-transform infrared spectroscopy (FTIR), X-ray diffraction (XRD), and scanning electron microscopy equipped with energy-dispersive X-ray spectroscopy (SEM–EDS). The results showed that Si-s acted as a dispersed additive in the geopolymer matrix and affected the reaction, possibly because its acidity neutralized the alkaline solution. It also increased the crystallite size to 51.68 nm, compared with 20.25 nm for the control geopolymer. The addition of Al-s produced a porous structure and reduced the crystallite size to 14.94 nm because it reacted with the alkaline solution, generating an exothermic reaction and hydrogen gas. The physical and mechanical properties, including density, apparent porosity, water absorption, compressive strength, and ultrasonic pulse velocity, were evaluated. The proportions of Al-s and Si-s were expressed as parts per hundred mixtures (phm), with the mixture comprising fly ash, NaOH, and Na₂SiO₃ used in the geopolymerization process. The addition of 0.4–0.6 phm Al-s and 40 phm Si-s resulted in geopolymers with densities of 1,292–1,438 kg/m³, apparent porosities of 18.18%–25.87%, and water absorption values of 6.97%–10.15%. The compressive strength ranged from 13.25 to 41.91 ksc, depending on the Si-s content. These geopolymers exhibited physical properties and compressive strengths that complied with the requirements for Type C12 lightweight concrete blocks specified in Thai Industrial Standard TIS 2601-2556. Therefore, waste Si-s and Al-s can be effectively recycled to produce lightweight geopolymer materials with properties suitable for construction applications.
- 6 February 2026
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 1042, 43-51
Enhanced Weldability and Microstructural Characteristics of A536–A36 Dissimilar Joints Using Buttering and Preheating Techniques
Welding process is widely used as a metal assembly technique in various industries, including construction, automotive manufacturing, pressurization, and shipbuilding. In ship repair and fabrication, dissimilar welding between carbon steel and cast iron is often required, for example, in assembling appendages such as propeller shafts, yokes, and other equipment. Although cast iron offers high strength about 700 MPa and weight reduction benefits, its poor weldability due to high carbon content often leads to cracking when joined to carbon steel. Previous studies have found that preheating before welding mitigates rapid cooling and martensite formation, while buttering with Ni-based filler reduces carbon diffusion and carbide precipitation at the fusion boundary. This research has been carried out to investigate various procedures for dissimilar welding ductile cast iron A536 and carbon steel A36, as follows: (1) no preheat or buttering (Control), (2) preheating only (PH), (3) buttering only (BT), and (4) combined preheat and buttering (PHBT) to evaluate their effects on tensile strength, hardness, and microstructural evolution. Successful study of dissimilar welding between carbon steel and cast iron will reduce the cost of ship maintenance, increase its service life, and provide a path for more sustainable development.
- 6 February 2026
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 1042, 43-51
Enhanced Weldability and Microstructural Characteristics of A536–A36 Dissimilar Joints Using Buttering and Preheating Techniques
Welding process is widely used as a metal assembly technique in various industries, including construction, automotive manufacturing, pressurization, and shipbuilding. In ship repair and fabrication, dissimilar welding between carbon steel and cast iron is often required, for example, in assembling appendages such as propeller shafts, yokes, and other equipment. Although cast iron offers high strength about 700 MPa and weight reduction benefits, its poor weldability due to high carbon content often leads to cracking when joined to carbon steel. Previous studies have found that preheating before welding mitigates rapid cooling and martensite formation, while buttering with Ni-based filler reduces carbon diffusion and carbide precipitation at the fusion boundary. This research has been carried out to investigate various procedures for dissimilar welding ductile cast iron A536 and carbon steel A36, as follows: (1) no preheat or buttering (Control), (2) preheating only (PH), (3) buttering only (BT), and (4) combined preheat and buttering (PHBT) to evaluate their effects on tensile strength, hardness, and microstructural evolution. Successful study of dissimilar welding between carbon steel and cast iron will reduce the cost of ship maintenance, increase its service life, and provide a path for more sustainable development.
- 6 February 2026
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 1042, 33-41
Hardness Reduction in SA-335 P11 Welds by GTAW Using Controlled Interpass Temperature and the Temper Bead Technique without Post Weld Heat Treatment
Regulations governing welding in the oil and gas industry mandate post-weld heat treatment (PWHT) for all welded joints, regardless of pipe wall thickness. The maximum permissible hardness is limited to 248 HV to prevent cracking. However, PWHT is time-consuming, energy-intensive, and costly. This study investigates the use of interpass temperature control and the temper bead welding technique as alternative methods for reducing weld hardness without PWHT. SA-335 Grade P11 low alloy steel pipes were welded using the GTAW process with ER80S-B2 filler metal and 99.99% argon gas. A preheat temperature of 250 °C was applied in all conditions. Four experimental groups were investigated: (1) PWHT at 650 °C for 1 hour, (2) low interpass temperature at 250 °C, (3) high interpass temperature at 600 °C, and (4) temper bead welding with 17 overlapping beads. The first three groups used 7 beads for comparison. Weld quality was assessed using VT, PT, and RT. Hardness testing served as the primary evaluation method, followed by tensile, bend, macrostructural, and microstructural analysis. Hardness results showed that the PWHT and high interpass groups remained below 248 HV, with the temper bead group achieving the lowest weld metal hardness (215.5 HV). The low interpass group exceeded the limit (up to 256.3 HV). All specimens failed in the base metal during tensile testing, with average strengths ranging from 498.3 MPa (PWHT) to 526.3 MPa (temper bead). No critical defects were found in bend tests. Microstructural comparison revealed that temper bead welding produced finer and more uniform grains, contributing to lower hardness and improved thermal softening in the HAZ.
- 6 February 2026
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 1042, 33-41
Hardness Reduction in SA-335 P11 Welds by GTAW Using Controlled Interpass Temperature and the Temper Bead Technique without Post Weld Heat Treatment
Regulations governing welding in the oil and gas industry mandate post-weld heat treatment (PWHT) for all welded joints, regardless of pipe wall thickness. The maximum permissible hardness is limited to 248 HV to prevent cracking. However, PWHT is time-consuming, energy-intensive, and costly. This study investigates the use of interpass temperature control and the temper bead welding technique as alternative methods for reducing weld hardness without PWHT. SA-335 Grade P11 low alloy steel pipes were welded using the GTAW process with ER80S-B2 filler metal and 99.99% argon gas. A preheat temperature of 250 °C was applied in all conditions. Four experimental groups were investigated: (1) PWHT at 650 °C for 1 hour, (2) low interpass temperature at 250 °C, (3) high interpass temperature at 600 °C, and (4) temper bead welding with 17 overlapping beads. The first three groups used 7 beads for comparison. Weld quality was assessed using VT, PT, and RT. Hardness testing served as the primary evaluation method, followed by tensile, bend, macrostructural, and microstructural analysis. Hardness results showed that the PWHT and high interpass groups remained below 248 HV, with the temper bead group achieving the lowest weld metal hardness (215.5 HV). The low interpass group exceeded the limit (up to 256.3 HV). All specimens failed in the base metal during tensile testing, with average strengths ranging from 498.3 MPa (PWHT) to 526.3 MPa (temper bead). No critical defects were found in bend tests. Microstructural comparison revealed that temper bead welding produced finer and more uniform grains, contributing to lower hardness and improved thermal softening in the HAZ.
- 3 February 2026
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 1041, 35-42
Effect of Post Weld Heat Treatment and Filler Metal on the Microstructure, Mechanical Properties, and Corrosion Resistance of Dissimilar Welds between Carbon Steel and Stainless Steel
Food-grade piping and water transportation systems extensively use dissimilar welding between stainless steel and carbon steel, where cost-effectiveness and corrosion resistance are essential consideration. However, the fusion zone of dissimilar welds often observed microstructural inhomogeneities and hardness changes, thus compromising mechanical qualities and corrosion resistance. This study was seperated in two phases to investigate and optimize dissimilar welding between carbon steel and stainless steel in both plate and pipe applications. Phase 1 studied welding A36 carbon steel plate and A304 stainless steel using gas tungsten arc welding (GTAW) with ER308L filler metal, the effect of post-weld heat treatment (PWHT) holding time on the mechanical and microstructural propertie. PWHT was performed at 650 °C for 20 and 60 minutes. The 20-minute condition yielded an optimal combination of mechanical strength and microstructural refinement, while the 60-minute condition led to grain coarsening and reduced strength. Phase 2 extended the findings to pipe welding applications, adopting the 20-minute PWHT condition. Welding was performed on dissimilar joints between A106-B carbon steel pipe and A312 TP304L stainless steel pipe (2-inch OD) using ER308L and ER309L filler metals under 99.99% argon shielding. Tensile and hardness testing indicated that welds with ER309L offered superior mechanical performance. Microstructural analysis revealed delta-ferrite and stabilized austenite in the fusion zone, with enhanced Cr and Ni concentrations contributing to improved corrosion resistance, as confirmed by electrochemical testing.
- 3 February 2026
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 1041, 35-42
Effect of Post Weld Heat Treatment and Filler Metal on the Microstructure, Mechanical Properties, and Corrosion Resistance of Dissimilar Welds between Carbon Steel and Stainless Steel
Food-grade piping and water transportation systems extensively use dissimilar welding between stainless steel and carbon steel, where cost-effectiveness and corrosion resistance are essential consideration. However, the fusion zone of dissimilar welds often observed microstructural inhomogeneities and hardness changes, thus compromising mechanical qualities and corrosion resistance. This study was seperated in two phases to investigate and optimize dissimilar welding between carbon steel and stainless steel in both plate and pipe applications. Phase 1 studied welding A36 carbon steel plate and A304 stainless steel using gas tungsten arc welding (GTAW) with ER308L filler metal, the effect of post-weld heat treatment (PWHT) holding time on the mechanical and microstructural propertie. PWHT was performed at 650 °C for 20 and 60 minutes. The 20-minute condition yielded an optimal combination of mechanical strength and microstructural refinement, while the 60-minute condition led to grain coarsening and reduced strength. Phase 2 extended the findings to pipe welding applications, adopting the 20-minute PWHT condition. Welding was performed on dissimilar joints between A106-B carbon steel pipe and A312 TP304L stainless steel pipe (2-inch OD) using ER308L and ER309L filler metals under 99.99% argon shielding. Tensile and hardness testing indicated that welds with ER309L offered superior mechanical performance. Microstructural analysis revealed delta-ferrite and stabilized austenite in the fusion zone, with enhanced Cr and Ni concentrations contributing to improved corrosion resistance, as confirmed by electrochemical testing.
- 3 February 2026
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 1041, 91-98
Development of Geopolymer-Based Weld Backing Using Recycled Industrial Waste for A36 Steel Welding Using GMAW Process
Geopolymer is an alkali-activated aluminosilicate material that combine ceramic-like thermal performance with low thermal conductivity, high-temperature resistance, while remaining castable and structurally adaptable. It is synthesized from calcined kaolin (metakaolin) and fly ash, which react with alkaline solutions to form strong covalent bonds through geopolymerization. This material offers a viable alternative to conventional refractories and imported ceramic products.In this study, a geopolymer material was developed for welding applications and utilized as a weld backing strip for gas metal arc welding (GMAW) of ASTM A36 carbon steel. Weld backing strips are essential for achieving full penetration and consistent root quality in large-scale steel fabrication, particularly in structural, shipbuilding, and heavy industrial construction. The geopolymer binder consisted of 35 wt% metakaolin, 15 wt% fly ash, and a 1:1 ratio of 10 M NaOH and sodium silicate solution. To enhance thermal resistance, river sand, fine glass powder, or recycled SAW flux was incorporated as an external solid phase. Geopolymer specimens were thermally cured and fired at 500 °C to eliminate moisture and organic. Moreover, it was heated to 900 °C to simulate welding heat exposure. Microstructural, mineralogical, and functional group transformations were evaluated using XRD, SEM, and FTIR, while mechanical strength, thermal conductivity, and density were also assessed. The results indicated that glass-enhanced geopolymer exhibited the lowest thermal conductivity (0.89 W/m·K) and highest compressive strength retention after firing, owing to its partial crystallinity and preserved amorphous phase. Flux-based composites showed extensive ceramic phase formation, while sand-based composites retained high thermal conductivity and suffered severe strength loss. Welding trials confirmed that geopolymer backings effectively supported root bead formation with no cracking.
- 3 February 2026
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 1041, 91-98
Development of Geopolymer-Based Weld Backing Using Recycled Industrial Waste for A36 Steel Welding Using GMAW Process
Geopolymer is an alkali-activated aluminosilicate material that combine ceramic-like thermal performance with low thermal conductivity, high-temperature resistance, while remaining castable and structurally adaptable. It is synthesized from calcined kaolin (metakaolin) and fly ash, which react with alkaline solutions to form strong covalent bonds through geopolymerization. This material offers a viable alternative to conventional refractories and imported ceramic products.In this study, a geopolymer material was developed for welding applications and utilized as a weld backing strip for gas metal arc welding (GMAW) of ASTM A36 carbon steel. Weld backing strips are essential for achieving full penetration and consistent root quality in large-scale steel fabrication, particularly in structural, shipbuilding, and heavy industrial construction. The geopolymer binder consisted of 35 wt% metakaolin, 15 wt% fly ash, and a 1:1 ratio of 10 M NaOH and sodium silicate solution. To enhance thermal resistance, river sand, fine glass powder, or recycled SAW flux was incorporated as an external solid phase. Geopolymer specimens were thermally cured and fired at 500 °C to eliminate moisture and organic. Moreover, it was heated to 900 °C to simulate welding heat exposure. Microstructural, mineralogical, and functional group transformations were evaluated using XRD, SEM, and FTIR, while mechanical strength, thermal conductivity, and density were also assessed. The results indicated that glass-enhanced geopolymer exhibited the lowest thermal conductivity (0.89 W/m·K) and highest compressive strength retention after firing, owing to its partial crystallinity and preserved amorphous phase. Flux-based composites showed extensive ceramic phase formation, while sand-based composites retained high thermal conductivity and suffered severe strength loss. Welding trials confirmed that geopolymer backings effectively supported root bead formation with no cracking.
- 16 December 2025
- Published by Springer Nature in Journal of the Australian Ceramic Society
- Vol. 62 (4) , 1-18
Heat-resistant geopolymer derived from metakaolin–fly ash blend with bagasse ash addition: an innovative curved backing for steel pipe welding
- 16 December 2025
- Published by Springer Nature in Journal of the Australian Ceramic Society
- Vol. 62 (4) , 1-18
Heat-resistant geopolymer derived from metakaolin–fly ash blend with bagasse ash addition: an innovative curved backing for steel pipe welding
- 9 February 2023
- Published by Elsevier in Materials Today Communications
- Vol. 35
Effects of flux-cored arc welding technology on microstructure and wear resistance of Fe-Cr-C hardfacing alloy
- 9 February 2023
- Published by Elsevier in Materials Today Communications
- Vol. 35
Effects of flux-cored arc welding technology on microstructure and wear resistance of Fe-Cr-C hardfacing alloy
- 14 August 2020
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 1007, 65-70
Geopolymer Synthesis Using Metakaolin and High Calcium Fly Ash as Binary System Geopolymer
Conventional cement production process emits tons of carbon dioxide gas which is one of the greenhouse gases that influence the environment across the world. Discovering the alternative construction material with the eco-friendly process and the performance similar to or greater than ordinary Portland cement has been attractive to find out. This research presented green construction materials or so-called geopolymers from metakaolin substituted by high calcium fly ash by 20, 40, 60, 80 and 100 wt%. Some researches reported that geopolymer produced from metakaolin and fly ash with alkali solution gave a great result, but usually, they used fly ash containing very low calcium component. Compressive strength at 3, 7 and 28 curing days and flowability were conducted. The compressive strength of geopolymers blended with high calcium fly ash was still developed as the curing day increased and revealed the highest at 28 days especially on MK40 (high calcium fly ash 60 wt%). Geopolymer pastes prepared with a higher amount of high calcium fly ash exhibited less viscous. It was proved that the high amount of high calcium fly ash could be applied and gave extraordinary compressive strength. Furthermore, X-ray diffraction and X-ray fluorescence were used to investigate chemical properties as well as microstructure by a scanning electron microscope. For phase analysis, the existence of oxides of calcium and sulfur in high calcium fly ash resulted in the formation of thenardite, calcite, portlandite and C-S-H phase associating with geopolymeric phase. Therefore, this research proposed the opportunity for geopolymer production by using abundant high calcium fly ash to raise the value of the industrial waste products and green alternative construction material compared with OPC.
- 14 August 2020
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 1007, 65-70
Geopolymer Synthesis Using Metakaolin and High Calcium Fly Ash as Binary System Geopolymer
Conventional cement production process emits tons of carbon dioxide gas which is one of the greenhouse gases that influence the environment across the world. Discovering the alternative construction material with the eco-friendly process and the performance similar to or greater than ordinary Portland cement has been attractive to find out. This research presented green construction materials or so-called geopolymers from metakaolin substituted by high calcium fly ash by 20, 40, 60, 80 and 100 wt%. Some researches reported that geopolymer produced from metakaolin and fly ash with alkali solution gave a great result, but usually, they used fly ash containing very low calcium component. Compressive strength at 3, 7 and 28 curing days and flowability were conducted. The compressive strength of geopolymers blended with high calcium fly ash was still developed as the curing day increased and revealed the highest at 28 days especially on MK40 (high calcium fly ash 60 wt%). Geopolymer pastes prepared with a higher amount of high calcium fly ash exhibited less viscous. It was proved that the high amount of high calcium fly ash could be applied and gave extraordinary compressive strength. Furthermore, X-ray diffraction and X-ray fluorescence were used to investigate chemical properties as well as microstructure by a scanning electron microscope. For phase analysis, the existence of oxides of calcium and sulfur in high calcium fly ash resulted in the formation of thenardite, calcite, portlandite and C-S-H phase associating with geopolymeric phase. Therefore, this research proposed the opportunity for geopolymer production by using abundant high calcium fly ash to raise the value of the industrial waste products and green alternative construction material compared with OPC.
- 1 February 2016
- Published by Elsevier in Construction and Building Materials
- Vol. 104, 293-297
Potassium alkali concentration and heat treatment affected metakaolin-based geopolymer
- 1 February 2016
- Published by Elsevier in Construction and Building Materials
- Vol. 104, 293-297
Potassium alkali concentration and heat treatment affected metakaolin-based geopolymer
- 1 February 2014
- Published by Elsevier in Construction and Building Materials
- Vol. 53, 455-459
Effect of Thai Kaolin on properties of agricultural ash blended geopolymers
- 1 February 2014
- Published by Elsevier in Construction and Building Materials
- Vol. 53, 455-459
Effect of Thai Kaolin on properties of agricultural ash blended geopolymers