Weibing Ma
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Weibing Ma has a total of 45 co-authors. Here are the top co-authors by number of shared publications:
Jingdong Guo
9 shared publicationsHuaidang Zhao
Tianjin University
7 shared publicationsMinjie Ma
Tianjin University
7 shared publicationsXiangrong Zang
Tianjin University
5 shared publications- Hongwei Zhang
Key Laboratory of Advanced Ceramics and Machining Technology of Ministry of Education, Tianjin University, Tianjin 300072, China
4 shared publications Jing Li
4 shared publications
Latest Publications
- Open Access
- 18 May 2026
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 16 (29) , 26238-26248
Low-temperature fabrication of BTO-based relaxor ferroelectric thick films with multi-layered architecture
A screen‑printed BTO-based thick film with lead-free glass and sandwich structure enables low-temperature sintering (900 ℃). It achieves a high energy density of 1.65 J cm −3 , efficiency of 74.3%.
- 18 May 2026
- Published by Royal Society of Chemistry (RSC) in RSC Advances
- Vol. 16 (29) , 26238-26248
Open AccessLow-temperature fabrication of BTO-based relaxor ferroelectric thick films with multi-layered architecture
A screen‑printed BTO-based thick film with lead-free glass and sandwich structure enables low-temperature sintering (900 ℃). It achieves a high energy density of 1.65 J cm −3 , efficiency of 74.3%.
- Open Access
Low-Temperature Sintering and Piezoelectric Properties of Pb(Fe2/3W1/3)O3-Doped 0.7Pb(Zr0.46Ti0.54)O3–0.1Pb(Zn1/3Nb2/3)O3–0.2Pb(Ni1/3Nb2/3)O3 Ceramics for Free-Standing Silver-Electrode Co-Fired Multilayer Piezoelectric Devices
In this study, the sintering behavior and electrical properties of 0.7Pb(Zr0.46Ti0.54)O3 (PZT)–0.1Pb(Zn1/3Nb2/3)O3 (PZN)–0.2Pb(Ni1/3Nb2/3)O3 (PNN) piezoelectric ceramics with different Pb(Fe2/3W1/3)O3 (PFW) doping contents were investigated to obtain a formulation that can be co-fired with silver (Ag) electrodes below 900 °C for multilayer ceramics. PFW was introduced as a sintering aid, which effectively reduced the sintering temperature of the ceramics from 1200 °C to 850 °C. The sample with x = 0.12 exhibited the largest average grain size of 1.72 μm, achieving excellent comprehensive properties with piezoelectric constant (d33) = 477 pC/N, planar electromechanical coupling factor (kp) = 0.68, dielectric loss tangent (tanδ) = 0.0154, and relative density of 98.2%. Furthermore, the feasibility of fabricating piezoelectric actuators based on this optimized composition was verified. Multilayer piezoelectric devices were prepared via screen printing combined with a carbon-based sacrificial layer method. No obvious interdiffusion was observed at the interface between the Ag internal electrodes and the ceramic matrix. The 9-layer device attained a high d33 = 1470 pC/N and produced a large displacement of 5.5 μm (corresponding to a strain = 1.83%) with a voltage of 500 V. The thickness of the multilayer piezoelectric film was approximately 0.3 mm. Through this, the feasibility of manufacturing a multilayered actuator with an Ag electrode was confirmed through the composition of 0.58PZT–0.1PZN–0.2PNN–0.12PFW.
Open AccessLow-Temperature Sintering and Piezoelectric Properties of Pb(Fe2/3W1/3)O3-Doped 0.7Pb(Zr0.46Ti0.54)O3–0.1Pb(Zn1/3Nb2/3)O3–0.2Pb(Ni1/3Nb2/3)O3 Ceramics for Free-Standing Silver-Electrode Co-Fired Multilayer Piezoelectric Devices
In this study, the sintering behavior and electrical properties of 0.7Pb(Zr0.46Ti0.54)O3 (PZT)–0.1Pb(Zn1/3Nb2/3)O3 (PZN)–0.2Pb(Ni1/3Nb2/3)O3 (PNN) piezoelectric ceramics with different Pb(Fe2/3W1/3)O3 (PFW) doping contents were investigated to obtain a formulation that can be co-fired with silver (Ag) electrodes below 900 °C for multilayer ceramics. PFW was introduced as a sintering aid, which effectively reduced the sintering temperature of the ceramics from 1200 °C to 850 °C. The sample with x = 0.12 exhibited the largest average grain size of 1.72 μm, achieving excellent comprehensive properties with piezoelectric constant (d33) = 477 pC/N, planar electromechanical coupling factor (kp) = 0.68, dielectric loss tangent (tanδ) = 0.0154, and relative density of 98.2%. Furthermore, the feasibility of fabricating piezoelectric actuators based on this optimized composition was verified. Multilayer piezoelectric devices were prepared via screen printing combined with a carbon-based sacrificial layer method. No obvious interdiffusion was observed at the interface between the Ag internal electrodes and the ceramic matrix. The 9-layer device attained a high d33 = 1470 pC/N and produced a large displacement of 5.5 μm (corresponding to a strain = 1.83%) with a voltage of 500 V. The thickness of the multilayer piezoelectric film was approximately 0.3 mm. Through this, the feasibility of manufacturing a multilayered actuator with an Ag electrode was confirmed through the composition of 0.58PZT–0.1PZN–0.2PNN–0.12PFW.
- Open Access
Study on Efficient Separation of Amorphous Silica from High-Alumina Coal Gangue
Coal gangue, a major industrial solid waste from coal mining and processing, requires efficient alumina and silica separation for high-value utilization. This study focused on mineral reaction mechanisms and characteristics of coal gangue during calcination and alkaline leaching. Results showed calcination at 900–1200 °C altered its phase composition, affecting silica separation efficiency, with the optimal calcination range being 960–1120 °C. Poorly crystallized mullite and Al2O3 in calcined gangue were insoluble under low-alkaline and low-temperature conditions. On the contrary, amorphous silica is soluble and forms a sodium silicate solution in the proper alkaline conditions. This characteristic facilitates the efficient separation of alumina and silica. It was determined that the suitable conditions for silica removal from coal gangue are as follows: 1080 °C calcination for 90 min, leaching at 75 °C with 200 g/L NaOH (solid–liquid ratio of 1:4) for 4 h. Under these selected conditions, the silica leaching efficiency was 77.31%, the alumina leaching efficiency was 12.21%, the Na2O content in the leached residue was 1.94%, and the mass ratio of alumina to silica (A/S) in the leached residue increased from 0.88 to 3.42. A potential desilication mechanism was also analyzed.
Open AccessStudy on Efficient Separation of Amorphous Silica from High-Alumina Coal Gangue
Coal gangue, a major industrial solid waste from coal mining and processing, requires efficient alumina and silica separation for high-value utilization. This study focused on mineral reaction mechanisms and characteristics of coal gangue during calcination and alkaline leaching. Results showed calcination at 900–1200 °C altered its phase composition, affecting silica separation efficiency, with the optimal calcination range being 960–1120 °C. Poorly crystallized mullite and Al2O3 in calcined gangue were insoluble under low-alkaline and low-temperature conditions. On the contrary, amorphous silica is soluble and forms a sodium silicate solution in the proper alkaline conditions. This characteristic facilitates the efficient separation of alumina and silica. It was determined that the suitable conditions for silica removal from coal gangue are as follows: 1080 °C calcination for 90 min, leaching at 75 °C with 200 g/L NaOH (solid–liquid ratio of 1:4) for 4 h. Under these selected conditions, the silica leaching efficiency was 77.31%, the alumina leaching efficiency was 12.21%, the Na2O content in the leached residue was 1.94%, and the mass ratio of alumina to silica (A/S) in the leached residue increased from 0.88 to 3.42. A potential desilication mechanism was also analyzed.
- Open Access
Modification of LaB6 with ZrO2-Al2O3-TiO2 for Improvement of Density and Mechanical and Electrical Properties
Pure lanthanum hexaboride (LaB6) ceramics were prepared using powders of different grain sizes. The ceramics could reach a relative density of 98.2% at high temperatures and pressures, but had a low flexural strength (136.9 MPa). LaB6 ceramics were synthesized using ZrO2-Al2O3-TiO2 (ZAT) as sintering additives. The ceramics demonstrate high density and excellent mechanical properties. The hot pressure sintering (HPS) method was utilized in the synthesis of the ceramics. Investigations were conducted on the effects of ZAT content, as well as the effects of the sintering temperature and pressure on the sintering behavior, microstructure, and mechanical and electrical properties of LaB6 ceramics. LaB6 ceramics fabricated with a ZAT addition of 6 wt.%, at a sintering temperature of 1700 °C, and under a pressure of 50 MPa, exhibited superior sintering and electrical properties, including a relative density of 97%, a conductivity of 7.2 MS/m, a flexural strength of 281.5 MPa, and a Vickers hardness of 21.2 GPa. The LaB6 ceramics synthesized in this research exhibit promising potential as electron-emitting cathodes for field emission applications.
Open AccessModification of LaB6 with ZrO2-Al2O3-TiO2 for Improvement of Density and Mechanical and Electrical Properties
Pure lanthanum hexaboride (LaB6) ceramics were prepared using powders of different grain sizes. The ceramics could reach a relative density of 98.2% at high temperatures and pressures, but had a low flexural strength (136.9 MPa). LaB6 ceramics were synthesized using ZrO2-Al2O3-TiO2 (ZAT) as sintering additives. The ceramics demonstrate high density and excellent mechanical properties. The hot pressure sintering (HPS) method was utilized in the synthesis of the ceramics. Investigations were conducted on the effects of ZAT content, as well as the effects of the sintering temperature and pressure on the sintering behavior, microstructure, and mechanical and electrical properties of LaB6 ceramics. LaB6 ceramics fabricated with a ZAT addition of 6 wt.%, at a sintering temperature of 1700 °C, and under a pressure of 50 MPa, exhibited superior sintering and electrical properties, including a relative density of 97%, a conductivity of 7.2 MS/m, a flexural strength of 281.5 MPa, and a Vickers hardness of 21.2 GPa. The LaB6 ceramics synthesized in this research exhibit promising potential as electron-emitting cathodes for field emission applications.
- 24 April 2023
- Published by Elsevier in Ceramics International
- Vol. 49 (14) , 23349-23357
Improving the performance of flexible composites based on 3-3 interconnected skeletons for piezoelectric energy harvesting
- 24 April 2023
- Published by Elsevier in Ceramics International
- Vol. 49 (14) , 23349-23357
Improving the performance of flexible composites based on 3-3 interconnected skeletons for piezoelectric energy harvesting
- 26 May 2022
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 33 (17) , 14097-14107
Valence transition of cerium during the synthesis of powders and densification of CeB6 polycrystalline
- 26 May 2022
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 33 (17) , 14097-14107
Valence transition of cerium during the synthesis of powders and densification of CeB6 polycrystalline
- 28 February 2022
- Published by Elsevier in Materials Chemistry and Physics
- Vol. 282
Microwave dielectric properties of Sr3Ti2O7 ceramics with composite element doping of Nd & Al
- 28 February 2022
- Published by Elsevier in Materials Chemistry and Physics
- Vol. 282
Microwave dielectric properties of Sr3Ti2O7 ceramics with composite element doping of Nd & Al
- 9 March 2021
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 32 (7) , 8450-8459
Influences of (LiCe) co-doping on the structure and properties of Na0.15Bi2.85Ti0.7Nb1.3O9 piezoceramics
- 9 March 2021
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 32 (7) , 8450-8459
Influences of (LiCe) co-doping on the structure and properties of Na0.15Bi2.85Ti0.7Nb1.3O9 piezoceramics
- 14 November 2019
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 30 (24) , 21435-21443
Effect of NaCl on the microstructure and electrical properties of K0.5Na0.5NbO3 ceramics prepared by cold sintering process
- 14 November 2019
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 30 (24) , 21435-21443
Effect of NaCl on the microstructure and electrical properties of K0.5Na0.5NbO3 ceramics prepared by cold sintering process
- 2 January 2019
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 30 (3) , 2854-2863
Effects of V2O5 doping on the structure and electrical properties of BCZT lead-free piezoelectric ceramics
- 2 January 2019
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 30 (3) , 2854-2863
Effects of V2O5 doping on the structure and electrical properties of BCZT lead-free piezoelectric ceramics