Yusuf Musa Abubakar
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Yusuf Musa Abubakar has a total of 10 co-authors. Here are the top co-authors by number of shared publications:
Abdel Malik Abdel Gaffar Amoka
Department of Physics, Ahmadu Bello University, Zaria, Nigeria
1 shared publication- Abdullahi Lawal
Department of Physics, Faculty of Physical Sciences, Ahmadu Bello University, Zaria, Nigeria
1 shared publication - Abdulsalam Ismaila Galadima
Department of Physics, Ahmadu Bello University, Zaria, Nigeria
1 shared publication - Alhassan Shuaibu
Department of Physics, Kaduna State University, Kaduna, Nigeria
1 shared publication - Aliyu Abdulraheem
Department of Physics, Ahmadu Bello University, Zaria, Nigeria
1 shared publication - Annika Lohstroh
Univ Surrey, Dept Phys, Guildford GU2 7XH, Surrey, England
1 shared publication
Latest Publications
- Open Access
- 30 March 2025
- Published by Umaru Musa YarAdua University Katsina NG in UMYU Scientifica
- Vol. 4 (1) , 297-304
DFT Investigation of Magnesium-Doped Zirconolite for High-Level Nuclear Waste Immobilization
Study’s Excerpt: • A DFT method was used to investigate the structural and electronic properties of Mg-doped zirconolite. • A Quantum ESPRESSO code was implemented for the DFT study. • Mg-doped zirconolite showed a stable structure. • Findings accentuate the need for further investigation into the physical and thermal properties of Mg-doped zirconolite. Full Abstract: The black mineral zirconolite (CaZrTi2O7), which is made up of calcium zirconium titanate, has been considered an appropriate waste form for immobilizing radioactive waste. Using Density Functional Theory (DFT), this study examined the impact of magnesium substitution on ceramic nuclear waste from Zirconolite. To explore the material's structural stability and electronic characteristics, a computational simulation was conducted using Quantum ESPRESSO within the Perdew-Burke-Ernzerhof generalized gradient approximation (PBE-GGA) and Broyden-Fletcher-Golfarb-Shannon (BFGS) relaxation calculations. From the energy range of -2.0 eV to 2.0 eV, the computed electronic band structure was displayed along the symmetry routes. An indirect band gap material with 0.06 eV was revealed by the energy gap between the valence band maximum (VBm) and the conduction band minimum (CBm) at the R2 and Γ sites. The behavior of semiconductors is consistent with this energy gap value. The dopant substitution energy effect was determined to be 1.424 eV, indicating that the Mg-doped Zirconolite's molecular structure remained stable. To sum up, doping CaZrTi2O7 ceramic may promote the production of oxygen, which enhances Magnesium's mobility to the subterranean water molecules inside the geological disposal facility.
- 30 March 2025
- Published by Umaru Musa YarAdua University Katsina NG in UMYU Scientifica
- Vol. 4 (1) , 297-304
Open AccessDFT Investigation of Magnesium-Doped Zirconolite for High-Level Nuclear Waste Immobilization
Study’s Excerpt: • A DFT method was used to investigate the structural and electronic properties of Mg-doped zirconolite. • A Quantum ESPRESSO code was implemented for the DFT study. • Mg-doped zirconolite showed a stable structure. • Findings accentuate the need for further investigation into the physical and thermal properties of Mg-doped zirconolite. Full Abstract: The black mineral zirconolite (CaZrTi2O7), which is made up of calcium zirconium titanate, has been considered an appropriate waste form for immobilizing radioactive waste. Using Density Functional Theory (DFT), this study examined the impact of magnesium substitution on ceramic nuclear waste from Zirconolite. To explore the material's structural stability and electronic characteristics, a computational simulation was conducted using Quantum ESPRESSO within the Perdew-Burke-Ernzerhof generalized gradient approximation (PBE-GGA) and Broyden-Fletcher-Golfarb-Shannon (BFGS) relaxation calculations. From the energy range of -2.0 eV to 2.0 eV, the computed electronic band structure was displayed along the symmetry routes. An indirect band gap material with 0.06 eV was revealed by the energy gap between the valence band maximum (VBm) and the conduction band minimum (CBm) at the R2 and Γ sites. The behavior of semiconductors is consistent with this energy gap value. The dopant substitution energy effect was determined to be 1.424 eV, indicating that the Mg-doped Zirconolite's molecular structure remained stable. To sum up, doping CaZrTi2O7 ceramic may promote the production of oxygen, which enhances Magnesium's mobility to the subterranean water molecules inside the geological disposal facility.
- Open Access
- 20 June 2023
- Published by Umaru Musa YarAdua University Katsina NG in UMYU Scientifica
- Vol. 2 (2) , 037-043
Influence of Blending on Mechanical Behavior of Low-Density Polyethylene, Polypropylene, Polyvinylchloride
Three thermoplastic polymers, low-density polyethylene (LDPE), polypropylene(PP), and polyvinyl chloride (PVC),were synthesized from their raw pellets.Three blends of 1:1 wt.% of low-density polyethylene/polypropylene, low-density polyethylene/polyvinylchloride, polypropylene/polyvinylchloride, and one blend of 1:1:1 wt.% of low-density polyethylene/polypropylene/polyvinylchloride were produced via compression mould method using Two-roll Mill machine and Compression Mould machine. Using the Tensile Strength Tester machine, the pristine polymer and the blends were cut into dumbbell shapes for mechanical testing. The resultsobtained are 9.8MPa and 67.5% maximum stress and strain, respectively, for LDPE, 29MPa, and 12.4% maximum stress and strain, respectively, for neat PP. 25.8MPa and 35% maximum stress and strain respectively for pristine PVC, 19.2MPa and 44% maximum stress and strain respectively for LDPE/PVC blend, 19MPa and 29% maximum stress and strain respectively for LDPE/PP blend, 27.5MPa and10.75% maximum stress and strain respectively for PP/PVC, 21MPa and 10.4% maximum stress and stain respectively for LDPE/PP/PVC blend. The force at peak and the respective peak elongation are; 85.612N and 0.008387m for pristineLDPE, 344.810N and 0.004810m for pristinePP, 264.976N and 0.005496m forpristine PVC, 188.288N and 0.005980m for LDPE/PVC blend, 174.755N and 0.005109m for LDPE/PP blend, 250.196N and0.004287m for PP/PVC blend, 275.175N and 4.009mm for LDPE/PP/PVC blend. The maximum energies expended to have maximum extension are 0.71802784J (LDPE), 2.04578339J (PP), 1.70308635J (PVC), 1.12596224J (LDPE/PVC),0.8928233J (LDPE/PP), 1.50129025J (PP/PVC) and 1.10317658J (LDPE/PP/PVC). These results show improvement in the mechanical properties of the blends when compared with those of the constituent polymers. It also indicatesthat polymeric properties modification via an immiscible polymer blend is possible and easy to achieve.
- 20 June 2023
- Published by Umaru Musa YarAdua University Katsina NG in UMYU Scientifica
- Vol. 2 (2) , 037-043
Open AccessInfluence of Blending on Mechanical Behavior of Low-Density Polyethylene, Polypropylene, Polyvinylchloride
Three thermoplastic polymers, low-density polyethylene (LDPE), polypropylene(PP), and polyvinyl chloride (PVC),were synthesized from their raw pellets.Three blends of 1:1 wt.% of low-density polyethylene/polypropylene, low-density polyethylene/polyvinylchloride, polypropylene/polyvinylchloride, and one blend of 1:1:1 wt.% of low-density polyethylene/polypropylene/polyvinylchloride were produced via compression mould method using Two-roll Mill machine and Compression Mould machine. Using the Tensile Strength Tester machine, the pristine polymer and the blends were cut into dumbbell shapes for mechanical testing. The resultsobtained are 9.8MPa and 67.5% maximum stress and strain, respectively, for LDPE, 29MPa, and 12.4% maximum stress and strain, respectively, for neat PP. 25.8MPa and 35% maximum stress and strain respectively for pristine PVC, 19.2MPa and 44% maximum stress and strain respectively for LDPE/PVC blend, 19MPa and 29% maximum stress and strain respectively for LDPE/PP blend, 27.5MPa and10.75% maximum stress and strain respectively for PP/PVC, 21MPa and 10.4% maximum stress and stain respectively for LDPE/PP/PVC blend. The force at peak and the respective peak elongation are; 85.612N and 0.008387m for pristineLDPE, 344.810N and 0.004810m for pristinePP, 264.976N and 0.005496m forpristine PVC, 188.288N and 0.005980m for LDPE/PVC blend, 174.755N and 0.005109m for LDPE/PP blend, 250.196N and0.004287m for PP/PVC blend, 275.175N and 4.009mm for LDPE/PP/PVC blend. The maximum energies expended to have maximum extension are 0.71802784J (LDPE), 2.04578339J (PP), 1.70308635J (PVC), 1.12596224J (LDPE/PVC),0.8928233J (LDPE/PP), 1.50129025J (PP/PVC) and 1.10317658J (LDPE/PP/PVC). These results show improvement in the mechanical properties of the blends when compared with those of the constituent polymers. It also indicatesthat polymeric properties modification via an immiscible polymer blend is possible and easy to achieve.
- 18 September 2015
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Nuclear Science
- Vol. 62 (5) , 2360-2366
Stability of Silicon Carbide Particle Detector Performance at Elevated Temperatures
The alpha spectroscopy performance and electric current stability of 4H-silicon carbide Schottky devices with 50 μm epitaxial layer was examined at temperatures between 300 to 500 K at 50 K intervals. An activation energy of 5.98 ±0.64 meV was extracted from temperature dependent resistivity measurements. The Schottky barrier height decreases from 1.33 eV at 300 K to 1.11 eV at 500 K and the ideality factor increases from 1.17 at 300 K to 1.79 at 500 K. The reverse bias leakage currents stabilizes faster at higher temperatures. The charge collection efficiency is above 90% for temperatures up to 500 K. Pulse height spectra collected for 24 hours at constant voltage and temperature show improvements with time within the first 8 hours and remained stable for the remainder of the acquisition time. The peak width of the alpha spectra reduces significantly with increasing temperature at applied bias voltages below 50 V, which indicates that leakage currents are not the limiting factor in those conditions even at 500 K in our set up. So far, the devices indicate reasonable stability for extended periods of operation and highlight possible applications in harsh radiation media.
- 18 September 2015
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Nuclear Science
- Vol. 62 (5) , 2360-2366
Stability of Silicon Carbide Particle Detector Performance at Elevated Temperatures
The alpha spectroscopy performance and electric current stability of 4H-silicon carbide Schottky devices with 50 μm epitaxial layer was examined at temperatures between 300 to 500 K at 50 K intervals. An activation energy of 5.98 ±0.64 meV was extracted from temperature dependent resistivity measurements. The Schottky barrier height decreases from 1.33 eV at 300 K to 1.11 eV at 500 K and the ideality factor increases from 1.17 at 300 K to 1.79 at 500 K. The reverse bias leakage currents stabilizes faster at higher temperatures. The charge collection efficiency is above 90% for temperatures up to 500 K. Pulse height spectra collected for 24 hours at constant voltage and temperature show improvements with time within the first 8 hours and remained stable for the remainder of the acquisition time. The peak width of the alpha spectra reduces significantly with increasing temperature at applied bias voltages below 50 V, which indicates that leakage currents are not the limiting factor in those conditions even at 500 K in our set up. So far, the devices indicate reasonable stability for extended periods of operation and highlight possible applications in harsh radiation media.