SPS. V. Proidak

S. V. Proidak

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


S. V. Proidak has a total of 11 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Strain Hardening of Low-Carbon Steel in the Area of Jerky Flow

    by I. O. Vakulenko, D. M Bolotova, S. V Proidak, B Kurt, A. E Erdogdu, H. O Chaikovska, K Asgarov

    Purpose. The aim of this work is to assess the effect of ferrite grain size of low-carbon steel on the development of strain hardening processes in the area of nucleation and propagation of deformation bands. Methodology. Low-carbon steels with a carbon content of 0.06–0.1% C in various structural states were used as the material for study. The sample for the study was a wire with a diameter of 1mm. The structural studies of the metal were carried out using an Epiquant light microscope. Ferrite grain size was determined using quantitative metallographic techniques. Different ferrite grain size was obtained as a result of combination of thermal and termo mechanical treatment. Vary by heating temperature and the cooling rate, using cold plastic deformation and subsequent annealing, made it possible to change the ferrite grain size at the level of two orders of magnitude. Deformation curves were obtained during stretching the samples on the Instron testing machine. Findings. Based on the analysis of stretching curves of low-carbon steels with different ferrite grain sizes, it has been established that the initiation and propagation of plastic deformation in the jerky flow area is accompanied by the development of strain hardening processes. The study of the nature of increase at dislocation density depending on ferrite grain size of low-carbon steel, starting from the moment of initiation of plastic deformation, confirmed the existence of relationship between the development of strain hardening at the area of jerky flow and the area of parabolic hardening curve. Originality. One of the reasons for decrease in Luders deformation with an increase of ferrite grain size of low-carbon steel is an increase in strain hardening indicator, which accelerates decomposition of uniform dislocations distribution in the front of deformation band. The flow stress during initiation of plastic deformation is determined by the additive contribution from the frictional stress of the crystal lattices, the state of ferrite grain boundaries, and the density of mobile dislocations. It was found that the size of dislocation cell increases in proportion to the diameter of ferrite grain, which facilitates the development of dislocation annihilation during plastic deformation. Practical value. Explanation of qualitative dependence of the influence of ferrite grain size of a low-carbon steel on the strain hardening degree and the magnitude of Luders deformation will make it possible to determine the optimal structural state of steels subjected to cold plastic deformation.

  • Open Access

    FORMATION OF CARBON STEEL STRUCTURE DURING HOT PLASTIC DEFORMATION

    by I. O. Vakulenko, D. M. Bolotova, S. V. Proidak, H. Askerov, H. Cug, H. O. Tchaikovska

    FORMATION OF CARBON STEEL STRUCTURE DURING HOT PLASTIC DEFORMATION

  • Open Access

    SOFTENING OF HARDENED MEDIUM-CARBON STEEL DURING HEATING

    by I. O. Vakulenko, S. V. Proidak, L. I. Vakulenko, N. A. Grischenko

    Purpose. The work is aimed to clarify the softening mechanism during the heating of martensite hardened carbon steel, which is of practical importance, especially in the development of the production technology of rolled products with different levels of hardening. Methodology. The samples after martensite hardening were tempered at the temperatures of 300-500˚С. The microstructure was investigated under the electron microscope. Thin foils were made using the Bolman and tweezer methods in chlorous-acetic solution and Morris reagent. Phase distortions of crystalline lattice were determined by the methods of X-ray structural analysis, using the diffractometer. The cold-worked layer of metal after grinding was removed by electrolytic dissolution. Tensile strength brake of the metal was determined using the tensile diagrams of samples using the Instron type machine. Microhardness was measured using the PMT-3 device with indentation load 0.49 N. Findings. When heating the hardened steel to a temperature of 300˚C, the softening effect is mainly related to the rate of reduction of the accumulated as a result of martensitic transformation, density of the crystalline structure defects. The total result is caused by the development of dislocations recombination and strengthening because of the emergence of additional number of cementite particles during the martensitic crystals decomposition. Starting from the heating temperatures of 400˚C and above, the development of polygonization processes in the ferrite is accompanied by the emergence of additional sub-boundaries, which enhance the effect of metal strengthening. With increase in the heating temperature of the hardened steel, the level of strength properties is determined by the progressive softening from the decrease in carbon atoms saturation degree of the solid solution, dislocations density and increase in the size of cementite particles over the effect of strengthening from hindering of mobile dislocations by carbon atoms and the emergence of additional sub-boundaries. Originality. For the tempering temperature of 300-400˚C, the absence of the phase distortion change indicates the emergence of additional factor in strengthening the metal from the formation of sub-boundaries and the dispersion strengthening from the carbide particles. Practical value. The given explanation of the mechanism of structural transformations in the process of tempering in the average temperature range of the hardened carbon steel can be used to optimize the technology of thermal strengthening of rolled metal.

  • Open Access

    INFLUENCE OF SELF-TEMPERING TEMPERATURE ON STRENGTH OF RAILWAY WHEEL DISK AFTER ACCELERATED COOLING

    by L. I. Vakulenko, D. M. Bolotova, S. V. Proydak, M. A. Grischenko, I. O. Vakulenko

    Purpose. The paper aims at estimation of resource of strength increase for railway wheel disk. Methodology. The material for research was carbon steel of railway wheel containing 0.57%C, 0.65%Si, 0.45%Mn, 0.0029%S, 0,014%P, 0,11%Cr. A railway wheel was heated to the temperatures above and was held at this temperature until the completion of аustenite homogenization processes and then the disk was cooled at a growing rate to a certain temperature. A temperature interval of completion of the speed-up wheel disk cooling was 200-450C. Structure was studied with the use of research methods under electronic and light microscopes. After accelerated cooling the estimation of metal structure imperfection degree was carried out with the use of X-ray structural analysis method. The stress and yielding limit of carbon steel were determined at tension, at a speed of deformation . The microhardness of steel structural components was estimated using the microhardness tester of PMT-3 type. Findings. The properties complex of railway wheel carbon steel depending on the temperature of the accelerated cooling termination is determined by the correlation of soften and work-hardening processes development. The effect of work-hardening is based on blocking of mobile dislocations due to a precipitation carbon atoms and dispersion work-hardening from the formed particles of carbidic phase. At the temperatures of the accelerated cooling termination of carbon steel higher than 300-350C the decrease rate of strength properties is determined by the exceeding of total soften effect from disintegration of solid solution, acceleration of spheroidithation and coalescence of cementite particles above the dislocations blocking by the carbon atoms and dispersion work-hardening. Originality. Authors proved that the strength level of the railway wheel carbon steel from the temperature of accelerated cooling completion is determined by the influence ratio of the solid solution satiety degree and dispersion work-hardening from a carbidic phase. For the temperatures of accelerated cooling termination 200-300C a decrease of solid solution satiety degree is a basic factor, which determines the level of the strength characteristic. Practical value. When making the whole-rolled railway wheel one can increase the strength limit of disk metal using the accelerated cooling to the middle interval of temperatures, which was successfully proven by authors.