Jai-Lin Tsai
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Jai-Lin Tsai has a total of 74 co-authors. Here are the top co-authors by number of shared publications:
- Cheng Dai
Department of Materials Science and Engineering, National Chung Hsing University, Taichung 402, Taiwan
4 shared publications - Jyun-You Chen
Department of Materials Science and Engineering, National Chung Hsing University, Taichung 402, Taiwan
4 shared publications - Ting-Wei Hsu
Department of Materials Science and Engineering, National Chung Hsing University, Taichung 402, Taiwan
4 shared publications - Shi-Min Weng
Department of Materials Science and Engineering, National Chung Hsing University, Taichung 402, Taiwan
3 shared publications C.J. Hsu
Department of Materials Engineering, National Chung Hsing University, Taichung, Taiwan, ROC
2 shared publicationsChen Pi
2 shared publications
Latest Publications
- 15 August 2025
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Magnetics
- Vol. 62 (3) , 1-6
Magnetic Properties and Microstructure of FePt (BN/AlN, Ag, C) Film
The FePt (BN/AlN, Ag, C) and reference FePt (BN, Ag, C) films exhibit close ordering degrees (0.84), indicating that the hard L10 FePt phase is nearly identical in both films. The reference FePt (BN, Ag, C) film presents perpendicular magnetic anisotropy and the highest out-of-plane coercivity (31.7 kOe). Still, the disordered fcc FePt contributed to the in-plane magnetization and wider hard-axis hysteresis loop. In contrast, the FePt (BN/AlN, Ag, C) film exhibits higher c-axis alignment, as evidenced by lower rocking width in the (001) / (002) diffraction peaks (3.94 °/2.5 °). The more c-axis anisotropic crystal grains also respond to the higher magneto-crystalline anisotropy, and lower hard-/easy-axis remanence ratio than the reference sample. However, the out-of-plane coercivity is significantly smaller in the FePt (BN/AlN, Ag, C) film (16.7 kOe) due to the formation of soft magnetic FeB grains, where the hard- and soft-magnetic phases are exchange-coupled, which enhances the magnetic remanence and saturation magnetization. From microstructure image mapping, AlN segregated at the grain boundaries, but part of Al was present in the FePt lattice and was supposed to initiate the formation of FeB due to high atomic diffusivity at high deposition temperature.
- 15 August 2025
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Magnetics
- Vol. 62 (3) , 1-6
Magnetic Properties and Microstructure of FePt (BN/AlN, Ag, C) Film
The FePt (BN/AlN, Ag, C) and reference FePt (BN, Ag, C) films exhibit close ordering degrees (0.84), indicating that the hard L10 FePt phase is nearly identical in both films. The reference FePt (BN, Ag, C) film presents perpendicular magnetic anisotropy and the highest out-of-plane coercivity (31.7 kOe). Still, the disordered fcc FePt contributed to the in-plane magnetization and wider hard-axis hysteresis loop. In contrast, the FePt (BN/AlN, Ag, C) film exhibits higher c-axis alignment, as evidenced by lower rocking width in the (001) / (002) diffraction peaks (3.94 °/2.5 °). The more c-axis anisotropic crystal grains also respond to the higher magneto-crystalline anisotropy, and lower hard-/easy-axis remanence ratio than the reference sample. However, the out-of-plane coercivity is significantly smaller in the FePt (BN/AlN, Ag, C) film (16.7 kOe) due to the formation of soft magnetic FeB grains, where the hard- and soft-magnetic phases are exchange-coupled, which enhances the magnetic remanence and saturation magnetization. From microstructure image mapping, AlN segregated at the grain boundaries, but part of Al was present in the FePt lattice and was supposed to initiate the formation of FeB due to high atomic diffusivity at high deposition temperature.
- 11 May 2024
- Published by Elsevier in Thin Solid Films
- Vol. 798
Segregation effects of doped VN and ZrN on magnetic and microstructural characteristics of FePt-based films
- 11 May 2024
- Published by Elsevier in Thin Solid Films
- Vol. 798
Segregation effects of doped VN and ZrN on magnetic and microstructural characteristics of FePt-based films
- Open Access
- 29 January 2023
- Published by MDPI AG in Nanomaterials
- Vol. 13 (3) , 539
Magnetic Properties and Microstructure of FePt(BN, X, C) (X = Ag, Re) Films
A sputtered FePt(BN, Re, C) film, here boron nitride (BN), was compared to a reference sample FePt(BN, Ag, C). Intrinsically, these films illustrate a high anisotropy field (Hk) and perpendicular magnetocrystalline anisotropy (Ku),although the reference sample shows a higher value (Hk = 69.5 kOe, Ku = 1.74 × 107 erg/cm3) than the FePt(BN, Re, C) film (Hk = 66.9 kOe, Ku = 1.46 × 107 erg/cm3). However, the small difference in the anisotropy constant (K2/K1) ratio presents a close tendency in the angular dependence of the switching field. Extrinsically, the out-of-plane coercivity for the reference sample is 32 kOe, which is also higher than the FePt(BN, Re, C) film (Hc = 27 kOe), and both films present lower remanence (Mr(parallel)/Mr(perpendicular) = 0.08~0.12), that is, the index for perpendicular magnetic anisotropy. The higher perpendicular magnetization for both films was due to highly (001) textured FePt films, which was also evidenced by the tight rocking width of 4.1°/3.0° for (001)/(002) X-ray diffraction peaks, respectively, and high-enough ordering degree. The reference sample was measured to have a higher ordering degree (S = 0.84) than FePt(BN, Re, C) (S = 0.63). As a result, the Ag segregant shows stronger ability to promote the ordering of the FePt film; however, the FePt(BN, Re, C) film still has comparable magnetic properties without Ag doping. From the surface and elemental composition analysis, the metallic Re atoms found in the FePt lattice result in a strong spin–orbital coupling between transition metal Fe (3d electron) and heavy metals (Re, Pt) (5d electron) and we conducted high magnetocrystalline anisotropy (Ku). Above is the explanation that the lower-ordered FePt(BN, Re, C) film still has high-enough Ku and out-of-plane Hc. Regarding the microstructure, both the reference sample and FePt(BN, Re, C) show granular structure and columnar grains, and the respective average grain size and distributions are 6.60 nm (12.5%) and 11.2 nm (15.9%). The average widths of the grain boundaries and the aspect ratio of the columnar grain height are 2.05 nm, 1.00 nm, 2.35 nm, and 1.70 nm, respectively.
- 29 January 2023
- Published by MDPI AG in Nanomaterials
- Vol. 13 (3) , 539
Open AccessMagnetic Properties and Microstructure of FePt(BN, X, C) (X = Ag, Re) Films
A sputtered FePt(BN, Re, C) film, here boron nitride (BN), was compared to a reference sample FePt(BN, Ag, C). Intrinsically, these films illustrate a high anisotropy field (Hk) and perpendicular magnetocrystalline anisotropy (Ku),although the reference sample shows a higher value (Hk = 69.5 kOe, Ku = 1.74 × 107 erg/cm3) than the FePt(BN, Re, C) film (Hk = 66.9 kOe, Ku = 1.46 × 107 erg/cm3). However, the small difference in the anisotropy constant (K2/K1) ratio presents a close tendency in the angular dependence of the switching field. Extrinsically, the out-of-plane coercivity for the reference sample is 32 kOe, which is also higher than the FePt(BN, Re, C) film (Hc = 27 kOe), and both films present lower remanence (Mr(parallel)/Mr(perpendicular) = 0.08~0.12), that is, the index for perpendicular magnetic anisotropy. The higher perpendicular magnetization for both films was due to highly (001) textured FePt films, which was also evidenced by the tight rocking width of 4.1°/3.0° for (001)/(002) X-ray diffraction peaks, respectively, and high-enough ordering degree. The reference sample was measured to have a higher ordering degree (S = 0.84) than FePt(BN, Re, C) (S = 0.63). As a result, the Ag segregant shows stronger ability to promote the ordering of the FePt film; however, the FePt(BN, Re, C) film still has comparable magnetic properties without Ag doping. From the surface and elemental composition analysis, the metallic Re atoms found in the FePt lattice result in a strong spin–orbital coupling between transition metal Fe (3d electron) and heavy metals (Re, Pt) (5d electron) and we conducted high magnetocrystalline anisotropy (Ku). Above is the explanation that the lower-ordered FePt(BN, Re, C) film still has high-enough Ku and out-of-plane Hc. Regarding the microstructure, both the reference sample and FePt(BN, Re, C) show granular structure and columnar grains, and the respective average grain size and distributions are 6.60 nm (12.5%) and 11.2 nm (15.9%). The average widths of the grain boundaries and the aspect ratio of the columnar grain height are 2.05 nm, 1.00 nm, 2.35 nm, and 1.70 nm, respectively.
- Open Access
- 6 March 2022
- Published by MDPI AG in Nanomaterials
- Vol. 12 (5) , 874
Switching Field Distribution in BN/FePtCAg/MgTiON and FePtCAg/MgTiOBN Films
BN is the currently required segregant for perpendicular FePt media. We found that BN can be diffused from the MgTiOBN intermediate layer during a high temperature process. The FePtCAg film sputtered on MgTiOBN layers illustrates higher perpendicular magnetocrystalline anisotropy (Ku) (1.43 × 107 erg/cm3) and coercivity (normal to film surface) (17 kOe) at 350 K compared to BN/FePtCAg/MgTiON film. From the microstructure, the FePtCAg film shows the granular structure on the MgTiOBN intermediate layer, but parts of the irregular FePt grains are agglomerated and partially separated in the matrix, with grains size being, on average, 26.7 nm. Cross-sectional imaging showed that the FePt grains have a truncated pyramid shape with a lower wetting angle, which is influenced by the surface energy of MgTiOBN. BN segregation at FePt grains or boundaries is still not clear. Using the electron energy loss spectrum (EELS), we found that part of the BN atoms were clearly observed in the FePt lattice and iron-boride oxide was indexed in the x-ray photoelectron spectroscopy (XPS) spectra. To determine the effects of BN segregant (from capping layer or intermediate layer) on the magnetic switching behavior of FePtCAg film, the intrinsic-(ΔHint = 6.17 kOe, 6.54 kOe) and extrinsic- (ΔHext = 0.80 kOe, 0.39 kOe) switching field distribution (SFD) were measured by plotting saturated major- and unsaturated minor- hysteresis loops to evaluate the crystal orientation and microstructure (grains volume and distribution) for BN/FePtCAg/MgTiON and FePtCAg/MgTiOBN films, respectively. The main contribution of intrinsic SFD is the c-axis misalignment for the BN/FePt/MgTiON sample; however, the dispersed magnetic anisotropy has a higher input to intrinsic SFD for FePtCAg/MgTiOBN/CrRu film.
- 6 March 2022
- Published by MDPI AG in Nanomaterials
- Vol. 12 (5) , 874
Open AccessSwitching Field Distribution in BN/FePtCAg/MgTiON and FePtCAg/MgTiOBN Films
BN is the currently required segregant for perpendicular FePt media. We found that BN can be diffused from the MgTiOBN intermediate layer during a high temperature process. The FePtCAg film sputtered on MgTiOBN layers illustrates higher perpendicular magnetocrystalline anisotropy (Ku) (1.43 × 107 erg/cm3) and coercivity (normal to film surface) (17 kOe) at 350 K compared to BN/FePtCAg/MgTiON film. From the microstructure, the FePtCAg film shows the granular structure on the MgTiOBN intermediate layer, but parts of the irregular FePt grains are agglomerated and partially separated in the matrix, with grains size being, on average, 26.7 nm. Cross-sectional imaging showed that the FePt grains have a truncated pyramid shape with a lower wetting angle, which is influenced by the surface energy of MgTiOBN. BN segregation at FePt grains or boundaries is still not clear. Using the electron energy loss spectrum (EELS), we found that part of the BN atoms were clearly observed in the FePt lattice and iron-boride oxide was indexed in the x-ray photoelectron spectroscopy (XPS) spectra. To determine the effects of BN segregant (from capping layer or intermediate layer) on the magnetic switching behavior of FePtCAg film, the intrinsic-(ΔHint = 6.17 kOe, 6.54 kOe) and extrinsic- (ΔHext = 0.80 kOe, 0.39 kOe) switching field distribution (SFD) were measured by plotting saturated major- and unsaturated minor- hysteresis loops to evaluate the crystal orientation and microstructure (grains volume and distribution) for BN/FePtCAg/MgTiON and FePtCAg/MgTiOBN films, respectively. The main contribution of intrinsic SFD is the c-axis misalignment for the BN/FePt/MgTiON sample; however, the dispersed magnetic anisotropy has a higher input to intrinsic SFD for FePtCAg/MgTiOBN/CrRu film.
- Open Access
- 7 February 2021
- Published by MDPI AG in Nanomaterials
- Vol. 11 (2) , 419
Temperature Dependence and Microstructure Effects on Magnetic Properties of FePt(B, Ag, C) Film
A FePt(B, Ag, C) granular film was formed from post-annealed B4C(1.0 nm)/FePt(Ag, C) layers at a substrate temperature of 470 °C for 2 min. The 6 nm thick FePt(B, Ag, C) film demonstrates high perpendicular magnetic anisotropy (Ku = 2.83 × 107 erg/cm3 at 100 K) and out-of-plane coercivity (Hc = 38.0 kOe at 100 K). The Ku and out-of-plane Hc are respectively increased from 38% and 46% between 350 K and 50 K. The sample with a thickness of 8 nm also shows a similar trend for magnetic properties; however, the tiny magnetization kink which may come from rare Fe-B or disordered FePt grains was observed in the easy axis loop. The intrinsic (ΔHint = 12.6 kOe) and extrinsic switching field distribution (ΔHext = 1.62 kOe) were characterized by major and minor loops to correlate the microstructural grains. The coupled FePt grains grown on a single MgTiON grain were observed in a high-resolution transmission electron microstructure (HRTEM) image. This small intergranular exchange coupling was defined by estimating the magnetic cluster size (46.6 nm) from ΔHext and the average grains size (28.2 nm) from TEM images. The temperature dependence of coercivity was fitted to further understand the magnetization reversal process. The lower microstructural parameter was evidenced in the imperfect grain morphology.
- 7 February 2021
- Published by MDPI AG in Nanomaterials
- Vol. 11 (2) , 419
Open AccessTemperature Dependence and Microstructure Effects on Magnetic Properties of FePt(B, Ag, C) Film
A FePt(B, Ag, C) granular film was formed from post-annealed B4C(1.0 nm)/FePt(Ag, C) layers at a substrate temperature of 470 °C for 2 min. The 6 nm thick FePt(B, Ag, C) film demonstrates high perpendicular magnetic anisotropy (Ku = 2.83 × 107 erg/cm3 at 100 K) and out-of-plane coercivity (Hc = 38.0 kOe at 100 K). The Ku and out-of-plane Hc are respectively increased from 38% and 46% between 350 K and 50 K. The sample with a thickness of 8 nm also shows a similar trend for magnetic properties; however, the tiny magnetization kink which may come from rare Fe-B or disordered FePt grains was observed in the easy axis loop. The intrinsic (ΔHint = 12.6 kOe) and extrinsic switching field distribution (ΔHext = 1.62 kOe) were characterized by major and minor loops to correlate the microstructural grains. The coupled FePt grains grown on a single MgTiON grain were observed in a high-resolution transmission electron microstructure (HRTEM) image. This small intergranular exchange coupling was defined by estimating the magnetic cluster size (46.6 nm) from ΔHext and the average grains size (28.2 nm) from TEM images. The temperature dependence of coercivity was fitted to further understand the magnetization reversal process. The lower microstructural parameter was evidenced in the imperfect grain morphology.
- Open Access
Surface and Microstructure Analysis of CoCrPt Film on RuCoCrX (X = Ti, Re) Intermediate Layers
The microstructural and magnetic properties of perpendicular anisotropic CoCrPt films deposited on Ru or RuCoCrX (X = Ti, Re) intermediate layers were studied. The c-axis of CoCrPt grains were promoted by (0002) textured RuCoCr, and RuCoCrX (X = Ti, Re) intermediate layers due to smaller lattice misfit as compared to Ru. The narrower rocking width (Δθ50 = 3.76°) in RuCoCrRe intermediate layer and CoCrPt shows higher out of plane coercivity (Hc = 6.2 kOe), magnetic anisotropy constant (Ku = 6.2 × 106 erg/cm3) and nucleation field (HN = −2.8kOe) as compared to the Ru intermediate layer (Hc = 5.4 kOe, Ku = 5.9 × 106 erg/cm3, HN = −1.6 kOe). The partial intergranular exchange decoupling of CoCrPt grains was observed. The grain boundaries oxides were formed by the residual oxygen in targets and sputtering processes. The minor Cr2O3, CoO, TiO2, ReO3 oxides were investigated by surface analysis. Due to the minor oxides and Cr segregation at grains boundaries, the CoCrPt films present high coercivity. Samples CoCrPt/RuCoCr and CoCrPt/RuCoCrTi present a minimum at 45° but the values are much higher than the ideal Stoner-Wohlfarth theoretical value 0.5 which could be due to fewer natural oxides for magnetic grains separation. In sample CoCrPt/RuCoCrRe, there is an increase of intergranular interaction as indicated by the large asymmetry and the shift of the minimum at lower angles.
Open AccessSurface and Microstructure Analysis of CoCrPt Film on RuCoCrX (X = Ti, Re) Intermediate Layers
The microstructural and magnetic properties of perpendicular anisotropic CoCrPt films deposited on Ru or RuCoCrX (X = Ti, Re) intermediate layers were studied. The c-axis of CoCrPt grains were promoted by (0002) textured RuCoCr, and RuCoCrX (X = Ti, Re) intermediate layers due to smaller lattice misfit as compared to Ru. The narrower rocking width (Δθ50 = 3.76°) in RuCoCrRe intermediate layer and CoCrPt shows higher out of plane coercivity (Hc = 6.2 kOe), magnetic anisotropy constant (Ku = 6.2 × 106 erg/cm3) and nucleation field (HN = −2.8kOe) as compared to the Ru intermediate layer (Hc = 5.4 kOe, Ku = 5.9 × 106 erg/cm3, HN = −1.6 kOe). The partial intergranular exchange decoupling of CoCrPt grains was observed. The grain boundaries oxides were formed by the residual oxygen in targets and sputtering processes. The minor Cr2O3, CoO, TiO2, ReO3 oxides were investigated by surface analysis. Due to the minor oxides and Cr segregation at grains boundaries, the CoCrPt films present high coercivity. Samples CoCrPt/RuCoCr and CoCrPt/RuCoCrTi present a minimum at 45° but the values are much higher than the ideal Stoner-Wohlfarth theoretical value 0.5 which could be due to fewer natural oxides for magnetic grains separation. In sample CoCrPt/RuCoCrRe, there is an increase of intergranular interaction as indicated by the large asymmetry and the shift of the minimum at lower angles.
- 1 April 2020
- Published by Elsevier in Applied Surface Science
- Vol. 509
Surface modification of FePt(Ag, C) granular film by ultrathin B4C capping layer
- 1 April 2020
- Published by Elsevier in Applied Surface Science
- Vol. 509
Surface modification of FePt(Ag, C) granular film by ultrathin B4C capping layer
- 1 January 2020
- Published by Elsevier in Thin Solid Films
- Vol. 693
CoCrPt@(TiO2,CoO) granular thin films grown on Ru/Ni Pd100-/NiTa (x = 20, 50, 80)
- 1 January 2020
- Published by Elsevier in Thin Solid Films
- Vol. 693
CoCrPt@(TiO2,CoO) granular thin films grown on Ru/Ni Pd100-/NiTa (x = 20, 50, 80)