Yanxin Zhuang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Yanxin Zhuang has a total of 84 co-authors. Here are the top co-authors by number of shared publications:
Pengfei Xing
Department of New Energy Science and Engineering School of Metallurgy Northeastern University Shenyang P. R. China
9 shared publications- Pengfei Xing
School of Metallurgy, Northeastern University, Shenyang, China
7 shared publications Xing Jin
Key Laboratory of Electromagnetic Processing of Materials (Ministry of Education), Northeastern University, Shenyang, China
5 shared publicationsDonghui Wei
4 shared publicationsHaiyu Li
Key Laboratory of Electromagnetic Processing of Materials, Ministry of Education Northeastern University Shenyang China
4 shared publicationsJian Kong
School of Metallurgy, Northeastern University, Shenyang, China
4 shared publications
Latest Publications
- 27 May 2026
- Published by Wiley in Materials and Corrosion
- Vol. 77 (9) , 1567-1578
Corrosion Behavior and Mechanism of Spark Plasma Sintered and Arc‐Melted MoNbTaW Refractory High‐Entropy Alloys in Molten Cerium
Refractory high‐entropy alloys (RHEAs) show promising prospects in nuclear applications due to outstanding radiation tolerance, mechanical performance and corrosion resistance. In this study, MoNbTaW RHEA was synthesized via spark plasma sintering (SPS) at 2200°C, while the alloy with identical composition prepared via arc melting served as the control. The two alloys were first systematically characterized for microstructure, densification, grain size and phase constitution, followed by static immersion corrosion testing in molten cerium at 1400°C for 10 h, as well as systematic testing of their room‐temperature mechanical properties. The results reveal that Ta and W possess higher corrosion resistance than Mo and Nb. Benefiting from refined grains and homogeneous microstructure, the SPS alloy achieves better corrosion resistance and mechanical performance, with a mass loss rate of 3.57%, a corrosion rate of 2.72 μm/h, a Vickers hardness of 570.8 HV and a compressive strength of 2585 MPa.
- 27 May 2026
- Published by Wiley in Materials and Corrosion
- Vol. 77 (9) , 1567-1578
Corrosion Behavior and Mechanism of Spark Plasma Sintered and Arc‐Melted MoNbTaW Refractory High‐Entropy Alloys in Molten Cerium
Refractory high‐entropy alloys (RHEAs) show promising prospects in nuclear applications due to outstanding radiation tolerance, mechanical performance and corrosion resistance. In this study, MoNbTaW RHEA was synthesized via spark plasma sintering (SPS) at 2200°C, while the alloy with identical composition prepared via arc melting served as the control. The two alloys were first systematically characterized for microstructure, densification, grain size and phase constitution, followed by static immersion corrosion testing in molten cerium at 1400°C for 10 h, as well as systematic testing of their room‐temperature mechanical properties. The results reveal that Ta and W possess higher corrosion resistance than Mo and Nb. Benefiting from refined grains and homogeneous microstructure, the SPS alloy achieves better corrosion resistance and mechanical performance, with a mass loss rate of 3.57%, a corrosion rate of 2.72 μm/h, a Vickers hardness of 570.8 HV and a compressive strength of 2585 MPa.
- 11 May 2026
- Published by Springer Nature in Journal of Materials Science
- Vol. 61 (24) , 17415-17426
Thermophysical properties of Zr-based amorphous alloys and their correlation with glass-forming ability via electrostatic levitation measurement
- 11 May 2026
- Published by Springer Nature in Journal of Materials Science
- Vol. 61 (24) , 17415-17426
Thermophysical properties of Zr-based amorphous alloys and their correlation with glass-forming ability via electrostatic levitation measurement
- 9 May 2026
- Published by Springer Nature in High Temperature Corrosion of Materials
- Vol. 103 (3) , 42
High-Temperature Corrosion Behavior of High-Entropy Alloys in Liquid Ce
- 9 May 2026
- Published by Springer Nature in High Temperature Corrosion of Materials
- Vol. 103 (3) , 42
High-Temperature Corrosion Behavior of High-Entropy Alloys in Liquid Ce
- 1 May 2025
- Published by Springer Nature in JOM
- Vol. 77 (7) , 5777-5789
Kinetic and Mechanism of Ca Leaching in the Production of High-Purity Magnesia
- 1 May 2025
- Published by Springer Nature in JOM
- Vol. 77 (7) , 5777-5789
Kinetic and Mechanism of Ca Leaching in the Production of High-Purity Magnesia
- 18 March 2025
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 81 (5) , 456-466
The Corrosion Behavior of Refractory Body-Centered Cubic High-Entropy Alloys in Molten Cerium
Two novel refractory high-entropy alloys (RHEAs), TaNbTiW0.1Cr, and TaNbTiW0.5V, were designed and fabricated to investigate their corrosion behavior after being held in molten cerium at 1,200°C for 50 h. The corrosion performance of these alloys was compared with that of MoNbTaW and MoNbTaWV. Among the four alloys, MoNbTaW demonstrated the best corrosion resistance, with the lowest average corrosion rate of 0.035 μm/h, followed by TaNbTiW0.5V, which exhibited an average corrosion rate of 0.385 μm/h. The MoNbTaW exhibits excellent resistance, with no significant surface changes. In contrast, MoNbTaWV shows deeper, smooth corrosion characterized by minor pitting but no substantial cracking. The TaNbTiW0.1Cr, initially homogeneous, undergoes preferential corrosion in the interdendritic regions, leading to crack formation. The TaNbTiW0.5V displays surface corrosion pits and cracks, with limited diffusion. Energy dispersive spectroscopy (EDS) analysis indicates that Cr is the most susceptible to corrosion, followed by Ti and Nb, while Ta and W exhibit greater resistance. These variations in corrosion behavior are attributed to the differing solubilities of these elements in molten cerium.
- 18 March 2025
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 81 (5) , 456-466
The Corrosion Behavior of Refractory Body-Centered Cubic High-Entropy Alloys in Molten Cerium
Two novel refractory high-entropy alloys (RHEAs), TaNbTiW0.1Cr, and TaNbTiW0.5V, were designed and fabricated to investigate their corrosion behavior after being held in molten cerium at 1,200°C for 50 h. The corrosion performance of these alloys was compared with that of MoNbTaW and MoNbTaWV. Among the four alloys, MoNbTaW demonstrated the best corrosion resistance, with the lowest average corrosion rate of 0.035 μm/h, followed by TaNbTiW0.5V, which exhibited an average corrosion rate of 0.385 μm/h. The MoNbTaW exhibits excellent resistance, with no significant surface changes. In contrast, MoNbTaWV shows deeper, smooth corrosion characterized by minor pitting but no substantial cracking. The TaNbTiW0.1Cr, initially homogeneous, undergoes preferential corrosion in the interdendritic regions, leading to crack formation. The TaNbTiW0.5V displays surface corrosion pits and cracks, with limited diffusion. Energy dispersive spectroscopy (EDS) analysis indicates that Cr is the most susceptible to corrosion, followed by Ti and Nb, while Ta and W exhibit greater resistance. These variations in corrosion behavior are attributed to the differing solubilities of these elements in molten cerium.
- 26 December 2024
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 22 (3)
Recycling boron carbide dust waste for preparing high‐performance ceramics by hot‐pressed sintering
B 4 C dust waste causes environmental pollution and is difficult to be recycled. This paper proposes a method of recycling B 4 C dust waste to fabricate high‐performance ceramics via the processes of raw material treatment and hot pressing. The characteristics of B 4 C dust waste are analyzed and the existing states of the impurities are detected. Dust wastes, removed different impurities via different processes, are simultaneously hot pressed at 2050°C for 15 min under 20 MPa pressure, and the microstructure and mechanical property of the fabricated ceramics are detected and compared. Results indicate that the particle size of dust waste is fine (2.7 µm), and the impurities B 2 O 3 /H 3 BO 3 , Fe, and BN exist in dust waste. The mechanical properties of the ceramics fabricated with dust wastes treated via different methods are similar or even superior to those of the commercial ceramics, and among them, the ceramics fabricated with the dust waste removed oxygen with ethanol show the excellent comprehensive performance, of which the hardness, flexural strength, and fractural toughness reach 30.78 GPa, 410 MPa, 4.3 MPa m 1/2 , respectively. Removing oxygen of dust waste can effectively enhance the densification, and the impurity Fe can also improve the densification owing to the formed low‐melting‐point FeB from the reaction between Fe and boron carbide in the dust waste. The pullout of FeB, BN particles, and the loosening area induced by residual stress of FeB contributes to the promotion of fracture toughness. This paper proves the feasibility of preparing high‐performance ceramics with B 4 C dust waste and lays a theoretical and practical foundation for the recycling and value‐added reuse of B 4 C dust waste, and for the low‐cost preparing of high‐performance B 4 C ceramics.
- 26 December 2024
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 22 (3)
Recycling boron carbide dust waste for preparing high‐performance ceramics by hot‐pressed sintering
B 4 C dust waste causes environmental pollution and is difficult to be recycled. This paper proposes a method of recycling B 4 C dust waste to fabricate high‐performance ceramics via the processes of raw material treatment and hot pressing. The characteristics of B 4 C dust waste are analyzed and the existing states of the impurities are detected. Dust wastes, removed different impurities via different processes, are simultaneously hot pressed at 2050°C for 15 min under 20 MPa pressure, and the microstructure and mechanical property of the fabricated ceramics are detected and compared. Results indicate that the particle size of dust waste is fine (2.7 µm), and the impurities B 2 O 3 /H 3 BO 3 , Fe, and BN exist in dust waste. The mechanical properties of the ceramics fabricated with dust wastes treated via different methods are similar or even superior to those of the commercial ceramics, and among them, the ceramics fabricated with the dust waste removed oxygen with ethanol show the excellent comprehensive performance, of which the hardness, flexural strength, and fractural toughness reach 30.78 GPa, 410 MPa, 4.3 MPa m 1/2 , respectively. Removing oxygen of dust waste can effectively enhance the densification, and the impurity Fe can also improve the densification owing to the formed low‐melting‐point FeB from the reaction between Fe and boron carbide in the dust waste. The pullout of FeB, BN particles, and the loosening area induced by residual stress of FeB contributes to the promotion of fracture toughness. This paper proves the feasibility of preparing high‐performance ceramics with B 4 C dust waste and lays a theoretical and practical foundation for the recycling and value‐added reuse of B 4 C dust waste, and for the low‐cost preparing of high‐performance B 4 C ceramics.
- 26 December 2024
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 22 (3)
Synergistically reinforced boron carbide ceramics by introduction of Fe and BN
Boron carbide (B 4 C)‐FeB ceramics and B 4 C‐FeB‐BN ceramics are prepared via hot pressing with B 4 C plus different contents of iron (Fe) and B 4 C plus 5 wt% Fe and different contents of boron nitride (BN), respectively. The phase composition, microstructure, and mechanical properties of the prepared ceramics are studied in detail. The synergistic effect of Fe and BN on hot‐pressed B 4 C ceramics is discussed. Results indicate that Fe can react with B 4 C to form FeB, and enhance the densification and mechanical property of B 4 C ceramics. 5 wt% Fe is the optimal addition amount. Fe and BN can synergistically reinforce B 4 C ceramics. The ceramics fabricated with B 4 C‐5 wt% Fe‐4 wt% BN have the optimal comprehensive performance, of which the relative density, hardness, flexural strength, and fracture toughness reach 98.5%, 32.74 GPa, 668.92 MPa, and 4.09 MPa·m 1/2 , respectively, higher than those of the ceramics fabricated with B 4 C or with B 4 C plus Fe. The liquid formed by Fe during sintering enhances the dispersion of BN, which is beneficial to realizing the function of pinning grain boundary and pulling out. The toughening phenomena include intergranular and transgranular fracture, particle pulling out, and bridging.
- 26 December 2024
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 22 (3)
Synergistically reinforced boron carbide ceramics by introduction of Fe and BN
Boron carbide (B 4 C)‐FeB ceramics and B 4 C‐FeB‐BN ceramics are prepared via hot pressing with B 4 C plus different contents of iron (Fe) and B 4 C plus 5 wt% Fe and different contents of boron nitride (BN), respectively. The phase composition, microstructure, and mechanical properties of the prepared ceramics are studied in detail. The synergistic effect of Fe and BN on hot‐pressed B 4 C ceramics is discussed. Results indicate that Fe can react with B 4 C to form FeB, and enhance the densification and mechanical property of B 4 C ceramics. 5 wt% Fe is the optimal addition amount. Fe and BN can synergistically reinforce B 4 C ceramics. The ceramics fabricated with B 4 C‐5 wt% Fe‐4 wt% BN have the optimal comprehensive performance, of which the relative density, hardness, flexural strength, and fracture toughness reach 98.5%, 32.74 GPa, 668.92 MPa, and 4.09 MPa·m 1/2 , respectively, higher than those of the ceramics fabricated with B 4 C or with B 4 C plus Fe. The liquid formed by Fe during sintering enhances the dispersion of BN, which is beneficial to realizing the function of pinning grain boundary and pulling out. The toughening phenomena include intergranular and transgranular fracture, particle pulling out, and bridging.
Enhancing the removal of Fe and Ti from metallurgical silicon by slagging-directional solidification
- 13 December 2023
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 21 (3) , 1372-1381
Synthesize and crystallization behavior of SiOC/SiC nanocomposites derived from organosilane slurry residue
A route preparing SiOC/SiC nanocomposites directly by pyrolysis of organosilane slurry residue was investigated. Organosilane slurry residue's unique composition, containing both silicon and carbon, offers an intriguing platform for developing advanced ceramic materials. The pyrolysis process is examined comprehensively, revealing the chemical reactions and structural changes leading to SiC crystals formation. The phase evolution at various annealing temperatures was revealed. Crystallization behavior in the process were studied. The results reveal that SiOC matrix was generated at annealed temperature 800°C and SiC nanoparticles were formed at 1300°C. In comparison to phase separation of SiOC, carbothermal reduction of SiO 2 was domain in SiC formation. This research advances the understanding of SiOC/SiC nanocomposites, highlighting the value of repurposing industrial byproducts for sustainable and innovative materials development.
- 13 December 2023
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 21 (3) , 1372-1381
Synthesize and crystallization behavior of SiOC/SiC nanocomposites derived from organosilane slurry residue
A route preparing SiOC/SiC nanocomposites directly by pyrolysis of organosilane slurry residue was investigated. Organosilane slurry residue's unique composition, containing both silicon and carbon, offers an intriguing platform for developing advanced ceramic materials. The pyrolysis process is examined comprehensively, revealing the chemical reactions and structural changes leading to SiC crystals formation. The phase evolution at various annealing temperatures was revealed. Crystallization behavior in the process were studied. The results reveal that SiOC matrix was generated at annealed temperature 800°C and SiC nanoparticles were formed at 1300°C. In comparison to phase separation of SiOC, carbothermal reduction of SiO 2 was domain in SiC formation. This research advances the understanding of SiOC/SiC nanocomposites, highlighting the value of repurposing industrial byproducts for sustainable and innovative materials development.