Murat Türkün
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Murat Türkün has a total of 53 co-authors. Here are the top co-authors by number of shared publications:
- Hande Kemaloğlu
Ege Üniversitesi, Diş Hekimliği Fakültesi
5 shared publications Esra Uzer Celik
4 shared publications- Cem Peskersoy
Department of Restorative Dentistry, Faculty of Dentistry, Ege University, Izmir 35040, Turkey
3 shared publications - Elif Ercan Devrimci
Department of Restorative Dentistry, Faculty of Dentistry, Ege University, Bornova, Turkey
3 shared publications - Zeynep Ergücü
Department of Restorative Dentistry, Faculty of Dentistry, Ege University, 35040 Izmir, Türkiye
3 shared publications - Aysegul Demirbas
Department of Restorative Dentistry, Faculty of Dentistry, Ege University, Bornova, Turkey
2 shared publications
Latest Publications
- 24 September 2026
- Published by Adnan Menderes University in Meandros Medical and Dental Journal
- Vol. 27 (3) , 414-422
Comparative Evaluation of Microleakage of Biodentine, Glass Ionomer Cement, and Composite Resin Used for Dentin Restoration: An In Vitro Study
Aim: This study aimed to evaluate and compare the microleakage of a calcium silicate–based material (Biodentine) with glass ionomer cement (GIC) and composite resin in standardized coronal dentin cavities in-vitro. Materials and methods: Sixty extracted human third molars were used. Standardized dentin cavities (4×2×2 mm) were prepared and randomly assigned to three groups (n=20 of each): Biodentine, GIC (Fuji IX), and composite resin (Clearfil SE Bond + Filtek Z250). Following restoration, all specimens were stored in distilled water for 24 hours and subjected to 3000 thermal cycles. Microleakage was assessed after 0.5% basic fuchsin dye penetration and scoring under a stereomicroscope. Data were analyzed using Kruskal–Wallis and Bonferroni post hoc tests (p
- 24 September 2026
- Published by Adnan Menderes University in Meandros Medical and Dental Journal
- Vol. 27 (3) , 414-422
Comparative Evaluation of Microleakage of Biodentine, Glass Ionomer Cement, and Composite Resin Used for Dentin Restoration: An In Vitro Study
Aim: This study aimed to evaluate and compare the microleakage of a calcium silicate–based material (Biodentine) with glass ionomer cement (GIC) and composite resin in standardized coronal dentin cavities in-vitro. Materials and methods: Sixty extracted human third molars were used. Standardized dentin cavities (4×2×2 mm) were prepared and randomly assigned to three groups (n=20 of each): Biodentine, GIC (Fuji IX), and composite resin (Clearfil SE Bond + Filtek Z250). Following restoration, all specimens were stored in distilled water for 24 hours and subjected to 3000 thermal cycles. Microleakage was assessed after 0.5% basic fuchsin dye penetration and scoring under a stereomicroscope. Data were analyzed using Kruskal–Wallis and Bonferroni post hoc tests (p
- Open Access
- 12 September 2026
- Published by Springer Nature in BMC Oral Health
Oral health knowledge, beliefs and experiences among outpatients with schizophrenia: a qualitative study
- 12 September 2026
- Published by Springer Nature in BMC Oral Health
Open AccessOral health knowledge, beliefs and experiences among outpatients with schizophrenia: a qualitative study
- Open Access
- 31 August 2026
- Published by Necmettin Erbakan Universitesi Dis Hekimligi Dergisi (NEU Dent J), Necmettin Erbakan University in Necmettin Erbakan Universitesi Dis Hekimligi Dergisi (NEUDentJ), Necmettin Erbakan
- Vol. 8 (2) , 151-158
Evaluation of Subjective Smile Aesthetic Perceptions and Aesthetic Treatment Preferences of Adults Residents of Izmir
Aim: This study aimed to investigate the dental aesthetic satisfaction levels and treatment expectations of adults residents of İzmir, Turkey, and to evaluate the relationship between their subjective aesthetic perceptions and sociodemographic variables. Material and Methods: The cross-sectional study included 400 volunteer participants (200 females, 200 males) residents of İzmir, selected via convenience sampling. Data were collected through a 13-item original Clinical Data Collection Form encompassing demographic information, perception of smile aesthetics, and treatment expectations. A face-to-face interview technique was utilized to ensure data objectivity. Statistical analysis was performed using the Pearson Chi-Square test, with a significance level of p < 0.05. Results: Among the participants, 36.0% were dissatisfied with their general smile aesthetics, and 45.3% expressed dissatisfaction with their current tooth color. A highly significant correlation was found between tooth color dissatisfaction and treatment demand; 79.6% (n=144) of those dissatisfied with their tooth color requested professional whitening (p < 0.001). General aesthetic satisfaction was found to decrease significantly with age (p = 0.040). Female participants reported a significantly higher perceived need for orthodontic treatment (41.5%) and aesthetic restorations (39.0%) compared to males (p < 0.05). Furthermore, satisfaction with tooth color decreased with age, and the perceived need for porcelain crowns peaked at 44.7% in participants aged 45 and over (p < 0.001). Conclusion: Dental aesthetic satisfaction and treatment seeking are primarily determined by tooth color and alignment, which are directly influenced by age and gender. Clinicians should integrate patients' sociodemographic-dependent subjective perceptions into restorative treatment planning.
- 31 August 2026
- Published by Necmettin Erbakan Universitesi Dis Hekimligi Dergisi (NEU Dent J), Necmettin Erbakan University in Necmettin Erbakan Universitesi Dis Hekimligi Dergisi (NEUDentJ), Necmettin Erbakan
- Vol. 8 (2) , 151-158
Open AccessEvaluation of Subjective Smile Aesthetic Perceptions and Aesthetic Treatment Preferences of Adults Residents of Izmir
Aim: This study aimed to investigate the dental aesthetic satisfaction levels and treatment expectations of adults residents of İzmir, Turkey, and to evaluate the relationship between their subjective aesthetic perceptions and sociodemographic variables. Material and Methods: The cross-sectional study included 400 volunteer participants (200 females, 200 males) residents of İzmir, selected via convenience sampling. Data were collected through a 13-item original Clinical Data Collection Form encompassing demographic information, perception of smile aesthetics, and treatment expectations. A face-to-face interview technique was utilized to ensure data objectivity. Statistical analysis was performed using the Pearson Chi-Square test, with a significance level of p < 0.05. Results: Among the participants, 36.0% were dissatisfied with their general smile aesthetics, and 45.3% expressed dissatisfaction with their current tooth color. A highly significant correlation was found between tooth color dissatisfaction and treatment demand; 79.6% (n=144) of those dissatisfied with their tooth color requested professional whitening (p < 0.001). General aesthetic satisfaction was found to decrease significantly with age (p = 0.040). Female participants reported a significantly higher perceived need for orthodontic treatment (41.5%) and aesthetic restorations (39.0%) compared to males (p < 0.05). Furthermore, satisfaction with tooth color decreased with age, and the perceived need for porcelain crowns peaked at 44.7% in participants aged 45 and over (p < 0.001). Conclusion: Dental aesthetic satisfaction and treatment seeking are primarily determined by tooth color and alignment, which are directly influenced by age and gender. Clinicians should integrate patients' sociodemographic-dependent subjective perceptions into restorative treatment planning.
- Open Access
Impact of Anti-Discoloration System (ADS) on the Optical Stability of Alkasite and Composite Resins: A Comparative Study on the Synergistic Staining Effect of Chlorhexidine and Coffee
This study investigated the impact of conventional chlorhexidine (CHX) and anti-discoloration system (ADS)-containing CHX mouthrinses on the color stability of diverse dental polymers, both alone and in combination with coffee. Specimens (n = 180) were prepared from a nanohybrid composite (Charisma Diamond; Kulzer GmbH, Hanau, Germany), a monochromatic composite (Vittra Unique APS; FGM Dental Group, Joinville, Brazil), and a dual-cure alkasite (Cention Forte; Ivoclar Vivadent, Schaan, Liechtenstein). Following a 14-day cycle of mouthrinse immersion (2 min/daily) and coffee exposure (15 min/daily at 85 °C), color changes (ΔE00) were analyzed using the CIEDE2000 system. All materials exhibited significant discoloration across all protocols (p < 0.001). Cention Forte showed the highest susceptibility to staining, particularly in the CHX + coffee group (ΔE00 = 21.10), while Charisma Diamond remained the most stable (0.95–8.60). Conventional CHX (Kloroben; Drogsan Pharmaceuticals, Ankara, Turkey) induced significantly higher staining than ADS-CHX (Curasept ADS; Curasept S.p.A., Saronno, Italy) across all materials (p < 0.05). Notably, ADS technology significantly inhibited coffee-induced pigmentation in Cention Forte (p = 0.003) and Charisma Diamond (p = 0.046), effectively reducing the synergistic staining layer. In conclusion, while coffee consumption dramatically increases discoloration following CHX use, ADS technology serves as a protective barrier, reducing pigment adhesion. For patients with high dietary pigment intake, ADS-containing mouthrinses offer a significant clinical advantage in preserving the aesthetic longevity of polymeric restorations.
Open AccessImpact of Anti-Discoloration System (ADS) on the Optical Stability of Alkasite and Composite Resins: A Comparative Study on the Synergistic Staining Effect of Chlorhexidine and Coffee
This study investigated the impact of conventional chlorhexidine (CHX) and anti-discoloration system (ADS)-containing CHX mouthrinses on the color stability of diverse dental polymers, both alone and in combination with coffee. Specimens (n = 180) were prepared from a nanohybrid composite (Charisma Diamond; Kulzer GmbH, Hanau, Germany), a monochromatic composite (Vittra Unique APS; FGM Dental Group, Joinville, Brazil), and a dual-cure alkasite (Cention Forte; Ivoclar Vivadent, Schaan, Liechtenstein). Following a 14-day cycle of mouthrinse immersion (2 min/daily) and coffee exposure (15 min/daily at 85 °C), color changes (ΔE00) were analyzed using the CIEDE2000 system. All materials exhibited significant discoloration across all protocols (p < 0.001). Cention Forte showed the highest susceptibility to staining, particularly in the CHX + coffee group (ΔE00 = 21.10), while Charisma Diamond remained the most stable (0.95–8.60). Conventional CHX (Kloroben; Drogsan Pharmaceuticals, Ankara, Turkey) induced significantly higher staining than ADS-CHX (Curasept ADS; Curasept S.p.A., Saronno, Italy) across all materials (p < 0.05). Notably, ADS technology significantly inhibited coffee-induced pigmentation in Cention Forte (p = 0.003) and Charisma Diamond (p = 0.046), effectively reducing the synergistic staining layer. In conclusion, while coffee consumption dramatically increases discoloration following CHX use, ADS technology serves as a protective barrier, reducing pigment adhesion. For patients with high dietary pigment intake, ADS-containing mouthrinses offer a significant clinical advantage in preserving the aesthetic longevity of polymeric restorations.
- Open Access
- 29 January 2026
- Published by MDPI AG in Journal of Functional Biomaterials
- Vol. 17 (2) , 67
In Vitro Evaluation of the Effect of Microabrasion and Resin Infiltration Materials on Enamel Microhardness and Penetration Depth
Background: This in vitro study aimed to evaluate the effect of microabrasion as a surface pretreatment and to compare an experimental resin infiltrant with a commercially available system (ICON) in terms of enamel surface microhardness recovery and resin penetration depth in artificially demineralized enamel lesions. Methods: Forty-eight caries-free human third molars were prepared to obtain standardized enamel specimens, and artificial enamel lesions were created using a pH-cycling model. Specimens were randomly allocated into four groups (n = 12): experimental resin with microabrasion, experimental resin without microabrasion, ICON resin with microabrasion, and ICON resin without microabrasion. When indicated, microabrasion was performed using a 6.6% hydrochloric acid paste for a total application time of 30 s, followed by standard hydrochloric acid etching as part of the infiltration protocol. Enamel surface microhardness was measured at baseline, after demineralization, and after resin infiltration. Resin penetration depth was assessed using confocal laser scanning microscopy, with six specimens per group (n = 6). Data were analyzed using repeated-measures mixed-effects models and one-way ANOVA (p < 0.05). Results: Resin infiltration resulted in a partial recovery of enamel surface microhardness following demineralization; however, baseline hardness values were not fully restored, and no statistically significant differences were observed among the study groups (p > 0.05). These findings indicate surface stabilization rather than complete mechanical or mineral restoration. The ICON resin demonstrated significantly greater penetration depth than the experimental resin. In both resin systems, microabrasion significantly increased penetration depth. Conclusions: Within the limitations of this in vitro study, resin infiltration primarily contributed to the stabilization of demineralized enamel surfaces rather than true remineralization or full mechanical recovery. Although microabrasion enhanced resin penetration depth, this effect should be interpreted with caution due to the potential for cumulative enamel loss. From a clinical perspective, these findings support the selective use of microabrasion to enhance resin infiltration in early enamel lesions with pronounced surface barriers, while emphasizing the need to balance penetration benefits against enamel preservation.
- 29 January 2026
- Published by MDPI AG in Journal of Functional Biomaterials
- Vol. 17 (2) , 67
Open AccessIn Vitro Evaluation of the Effect of Microabrasion and Resin Infiltration Materials on Enamel Microhardness and Penetration Depth
Background: This in vitro study aimed to evaluate the effect of microabrasion as a surface pretreatment and to compare an experimental resin infiltrant with a commercially available system (ICON) in terms of enamel surface microhardness recovery and resin penetration depth in artificially demineralized enamel lesions. Methods: Forty-eight caries-free human third molars were prepared to obtain standardized enamel specimens, and artificial enamel lesions were created using a pH-cycling model. Specimens were randomly allocated into four groups (n = 12): experimental resin with microabrasion, experimental resin without microabrasion, ICON resin with microabrasion, and ICON resin without microabrasion. When indicated, microabrasion was performed using a 6.6% hydrochloric acid paste for a total application time of 30 s, followed by standard hydrochloric acid etching as part of the infiltration protocol. Enamel surface microhardness was measured at baseline, after demineralization, and after resin infiltration. Resin penetration depth was assessed using confocal laser scanning microscopy, with six specimens per group (n = 6). Data were analyzed using repeated-measures mixed-effects models and one-way ANOVA (p < 0.05). Results: Resin infiltration resulted in a partial recovery of enamel surface microhardness following demineralization; however, baseline hardness values were not fully restored, and no statistically significant differences were observed among the study groups (p > 0.05). These findings indicate surface stabilization rather than complete mechanical or mineral restoration. The ICON resin demonstrated significantly greater penetration depth than the experimental resin. In both resin systems, microabrasion significantly increased penetration depth. Conclusions: Within the limitations of this in vitro study, resin infiltration primarily contributed to the stabilization of demineralized enamel surfaces rather than true remineralization or full mechanical recovery. Although microabrasion enhanced resin penetration depth, this effect should be interpreted with caution due to the potential for cumulative enamel loss. From a clinical perspective, these findings support the selective use of microabrasion to enhance resin infiltration in early enamel lesions with pronounced surface barriers, while emphasizing the need to balance penetration benefits against enamel preservation.
- Open Access
- 1 January 2026
- Published by Nihon University School of Dentistry in Journal of Oral Science
- Vol. 68 (4) , 255-260
Comparative effects of integrated and post-applied nano-hydroxyapatite on enamel properties following high-concentration hydrogen peroxide bleaching
Purpose: This study investigated whether nano-hydroxyapatite (nHAp) can reduce the adverse effects of high-concentration hydrogen peroxide (HP) bleaching – such as mineral loss and surface softening – while maintaining whitening efficacy. Incorporation of nHAp into the bleaching gel was also compared with its application after bleaching.Methods: Sixty bovine enamel specimens were randomly assigned to six groups and treated with different HP-based protocols with or without nHAp. Color change (ΔE) was measured using spectrophotometry, microhardness with the Vickers test, and surface morphology and elemental composition using scanning electron microscopy (SEM) and energy-dispersive X-ray spectroscopy (EDS).Results: All HP-treated groups showed significant color improvement (ΔE > 3.3, P < 0.05). Post-bleaching nHAp application produced higher ΔE values than bleaching alone, though not to a significant degree. The highest ΔE was observed in the group receiving HP followed by nHAp. Post-bleaching nHAp significantly improved microhardness and calcium content in the Opalescence group, while effects in the BioWhiten group were limited and not significant. SEM analysis revealed superficial granular deposits and partial surface coverage in nHAp-treated specimens, particularly after post-bleaching application.Conclusion: Incorporation of nHAp during or after HP bleaching can reduce enamel alterations while preserving whitening efficacy, particularly when applied after bleaching in systems lacking intrinsic remineralizing components.
- 1 January 2026
- Published by Nihon University School of Dentistry in Journal of Oral Science
- Vol. 68 (4) , 255-260
Open AccessComparative effects of integrated and post-applied nano-hydroxyapatite on enamel properties following high-concentration hydrogen peroxide bleaching
Purpose: This study investigated whether nano-hydroxyapatite (nHAp) can reduce the adverse effects of high-concentration hydrogen peroxide (HP) bleaching – such as mineral loss and surface softening – while maintaining whitening efficacy. Incorporation of nHAp into the bleaching gel was also compared with its application after bleaching.Methods: Sixty bovine enamel specimens were randomly assigned to six groups and treated with different HP-based protocols with or without nHAp. Color change (ΔE) was measured using spectrophotometry, microhardness with the Vickers test, and surface morphology and elemental composition using scanning electron microscopy (SEM) and energy-dispersive X-ray spectroscopy (EDS).Results: All HP-treated groups showed significant color improvement (ΔE > 3.3, P < 0.05). Post-bleaching nHAp application produced higher ΔE values than bleaching alone, though not to a significant degree. The highest ΔE was observed in the group receiving HP followed by nHAp. Post-bleaching nHAp significantly improved microhardness and calcium content in the Opalescence group, while effects in the BioWhiten group were limited and not significant. SEM analysis revealed superficial granular deposits and partial surface coverage in nHAp-treated specimens, particularly after post-bleaching application.Conclusion: Incorporation of nHAp during or after HP bleaching can reduce enamel alterations while preserving whitening efficacy, particularly when applied after bleaching in systems lacking intrinsic remineralizing components.
- Open Access
- 31 August 2025
- Published by Korean Academy of Conservative Dentistry in Restorative Dentistry & Endodontics
- Vol. 50 (3) , e22
Comparative study of the effectiveness of different bleaching agents on blood-colored extracted teeth and investigation of recoloring after bleaching: an in vitro experimental study
Objectives: This study evaluated the efficacy of three distinct bleaching agents over time on blood-stained, devitalized teeth. Furthermore, the recoloring subsequent to bleaching will be monitored.Methods: The study was conducted on 60 caries-free, unfilled, upper human incisors. The Freccia and Peters blood staining technique was employed, and four groups (n = 15) were identified: control, 35% hydrogen peroxide-treated, 37% carbamide peroxide-treated, and sodium perborate-treated groups. Color differences were measured using ΔE00, ΔWID, L*, a*, and b* values. To investigate tooth discoloration after bleaching, 10 unbleached teeth with three groups of 10 bleached teeth were compared by vine staining. The group of bleached teeth was restored immediately, another group waited one week, and the third group had sodium ascorbate applied and analyzed using one-way analysis of variance tests (p < 0.05).Results: Among the groups, carbamide peroxide exhibited the most significant whitening during the 6-day bleaching process, followed by hydrogen peroxide and sodium perborate. Subsequent examination of the wine recoloring of post-bleaching samples demonstrated that bleached teeth exhibited a heightened propensity for recoloration in contrast to unbleached teeth. Notably, sodium ascorbate treatments for hydrogen peroxide neutralization and the wait-and-restore approach were not statistically significant in terms of preventing recoloration.Conclusions: Sodium perborate is less effective and more time-consuming than hydrogen peroxide or carbamide peroxide for bleaching purposes. Carbamide peroxide is the most effective bleaching agent. The sodium ascorbate treatment and the wait-and-restore approach are ineffective in preventing recoloring. Bleached teeth have more discoloration than unbleached teeth.
- 31 August 2025
- Published by Korean Academy of Conservative Dentistry in Restorative Dentistry & Endodontics
- Vol. 50 (3) , e22
Open AccessComparative study of the effectiveness of different bleaching agents on blood-colored extracted teeth and investigation of recoloring after bleaching: an in vitro experimental study
Objectives: This study evaluated the efficacy of three distinct bleaching agents over time on blood-stained, devitalized teeth. Furthermore, the recoloring subsequent to bleaching will be monitored.Methods: The study was conducted on 60 caries-free, unfilled, upper human incisors. The Freccia and Peters blood staining technique was employed, and four groups (n = 15) were identified: control, 35% hydrogen peroxide-treated, 37% carbamide peroxide-treated, and sodium perborate-treated groups. Color differences were measured using ΔE00, ΔWID, L*, a*, and b* values. To investigate tooth discoloration after bleaching, 10 unbleached teeth with three groups of 10 bleached teeth were compared by vine staining. The group of bleached teeth was restored immediately, another group waited one week, and the third group had sodium ascorbate applied and analyzed using one-way analysis of variance tests (p < 0.05).Results: Among the groups, carbamide peroxide exhibited the most significant whitening during the 6-day bleaching process, followed by hydrogen peroxide and sodium perborate. Subsequent examination of the wine recoloring of post-bleaching samples demonstrated that bleached teeth exhibited a heightened propensity for recoloration in contrast to unbleached teeth. Notably, sodium ascorbate treatments for hydrogen peroxide neutralization and the wait-and-restore approach were not statistically significant in terms of preventing recoloration.Conclusions: Sodium perborate is less effective and more time-consuming than hydrogen peroxide or carbamide peroxide for bleaching purposes. Carbamide peroxide is the most effective bleaching agent. The sodium ascorbate treatment and the wait-and-restore approach are ineffective in preventing recoloring. Bleached teeth have more discoloration than unbleached teeth.
- Open Access
- 22 July 2025
- Published by MDPI AG in Applied Sciences
- Vol. 15 (15) , 8159
Shear Bond Strength and Finite Element Stress Analysis of Composite Repair Using Various Adhesive Strategies With and Without Silane Application
This study evaluated the effect of various adhesive systems, particularly silane application, on the repair bond strength of a nanofill resin composite and associated stress distribution using finite element analysis (FEA). A total of 105 composite specimens (4 × 6 mm) were aged by thermal cycling (10,000 cycles), roughened, etched with phosphoric acid, and assigned to seven groups (n = 15): G1. control—no adhesive; G2. Single Bond Universal Adhesive; G3. composite primer; G4. PQ1; G5. Silane + PQ1; G6. Clearfil Universal Bond; G7. All-Bond Universal. Shear bond strength was measured using a universal testing machine (1 mm/min), and failure modes were microscopically classified. FEA was conducted under static and fatigue conditions using 3D models built in Fusion-360. Mechanical properties were obtained from technical data and the literature. A 300 N load was applied and contact detection (0.05 mm) and constraint zones were defined. Statistical analysis was performed using one-way ANOVA and Tukey’s HSD (p = 0.05). Pearson’s correlation was used to assess the relationship between bond strength and von Mises stress. The highest bond strength was found in G2 (21.54 MPa) while G1 showed the lowest (8.86 MPa). Silane-treated groups exhibited favorable stress distribution and a strong correlation between experimental and simulated outcomes. Silane applications significantly enhance composite repair performance.
- 22 July 2025
- Published by MDPI AG in Applied Sciences
- Vol. 15 (15) , 8159
Open AccessShear Bond Strength and Finite Element Stress Analysis of Composite Repair Using Various Adhesive Strategies With and Without Silane Application
This study evaluated the effect of various adhesive systems, particularly silane application, on the repair bond strength of a nanofill resin composite and associated stress distribution using finite element analysis (FEA). A total of 105 composite specimens (4 × 6 mm) were aged by thermal cycling (10,000 cycles), roughened, etched with phosphoric acid, and assigned to seven groups (n = 15): G1. control—no adhesive; G2. Single Bond Universal Adhesive; G3. composite primer; G4. PQ1; G5. Silane + PQ1; G6. Clearfil Universal Bond; G7. All-Bond Universal. Shear bond strength was measured using a universal testing machine (1 mm/min), and failure modes were microscopically classified. FEA was conducted under static and fatigue conditions using 3D models built in Fusion-360. Mechanical properties were obtained from technical data and the literature. A 300 N load was applied and contact detection (0.05 mm) and constraint zones were defined. Statistical analysis was performed using one-way ANOVA and Tukey’s HSD (p = 0.05). Pearson’s correlation was used to assess the relationship between bond strength and von Mises stress. The highest bond strength was found in G2 (21.54 MPa) while G1 showed the lowest (8.86 MPa). Silane-treated groups exhibited favorable stress distribution and a strong correlation between experimental and simulated outcomes. Silane applications significantly enhance composite repair performance.
- Open Access
- 16 September 2024
- Published by MDPI AG in Applied Sciences
- Vol. 14 (18) , 8335
Evaluation of Proximal Contact Tightness and Contact Area of Posterior Composite Resin Restorations
The purpose of this study is to evaluate the influence of the matrix system on proximal contact tightness (PCT) of posterior composite resin restorations. Standardized class II cavities on 180 first lower molar dentiform model teeth (Frasaco GmbH, Tettnang, Germany) were prepared. Three groups were formed considering the matrix system: Group-IM: Ivory matrix (Hahnenkratt GmbH, Königsbach-Stein, Germany), Group-OM: Omni matrix (Ultradent, South Jordan, UT, USA), and Group-PM: Palodent V3 sectional matrix (Dentsply, Charlotte, NC, USA). Teeth were restored with resin composite mounted in a manikin head to simulate the clinical environment. Proximal contact tightness (PCT) was measured using a custom-made portable dental pressure meter (PDPM), and the validation of the PCT results was performed with a histogram analysis acquired from bite-wing radiography. All data were statistically analyzed by ANOVA and t-test in SPSS software (v.27.0) (p < 0.05). PM group showed statistically tighter contacts on both mesial (PCTm: 228.28 ± 59.17 N) and distal surfaces (PCTd: 254.91 ± 65.69 N) (p > 0.05). Mesial contacts were found to be significantly tighter than distal contacts among all (p < 0.05). According to the histogram results, only in the PM group, the difference between the mesial and distal areas is significant (p < 0.05). Histogram results confirmed that the tightest contact values were achieved in the PM group, followed by the OM and IM groups, respectively (p < 0.05). The use of sectional matrix systems and separation rings is more effective in creating tighter contact than conventional matrix systems. The use of anatomical wedges will help to create a more natural approximal contour and narrow contact area.
- 16 September 2024
- Published by MDPI AG in Applied Sciences
- Vol. 14 (18) , 8335
Open AccessEvaluation of Proximal Contact Tightness and Contact Area of Posterior Composite Resin Restorations
The purpose of this study is to evaluate the influence of the matrix system on proximal contact tightness (PCT) of posterior composite resin restorations. Standardized class II cavities on 180 first lower molar dentiform model teeth (Frasaco GmbH, Tettnang, Germany) were prepared. Three groups were formed considering the matrix system: Group-IM: Ivory matrix (Hahnenkratt GmbH, Königsbach-Stein, Germany), Group-OM: Omni matrix (Ultradent, South Jordan, UT, USA), and Group-PM: Palodent V3 sectional matrix (Dentsply, Charlotte, NC, USA). Teeth were restored with resin composite mounted in a manikin head to simulate the clinical environment. Proximal contact tightness (PCT) was measured using a custom-made portable dental pressure meter (PDPM), and the validation of the PCT results was performed with a histogram analysis acquired from bite-wing radiography. All data were statistically analyzed by ANOVA and t-test in SPSS software (v.27.0) (p < 0.05). PM group showed statistically tighter contacts on both mesial (PCTm: 228.28 ± 59.17 N) and distal surfaces (PCTd: 254.91 ± 65.69 N) (p > 0.05). Mesial contacts were found to be significantly tighter than distal contacts among all (p < 0.05). According to the histogram results, only in the PM group, the difference between the mesial and distal areas is significant (p < 0.05). Histogram results confirmed that the tightest contact values were achieved in the PM group, followed by the OM and IM groups, respectively (p < 0.05). The use of sectional matrix systems and separation rings is more effective in creating tighter contact than conventional matrix systems. The use of anatomical wedges will help to create a more natural approximal contour and narrow contact area.
- Open Access
- 31 July 2024
- Published by Ondokuz Mayis Universitesi in Türk Diş Hekimliği Araştırma Dergisi
Biyoaktif Cam İçeren Deneysel Bir Remineralizasyon Ajanının Minenin Yüzey Sertliğine Etkisi
Amaç: Bu in vitro çalışmanın amacı, biyoaktif cam içeren deneysel bir remineralizasyon ajanının minenin yüzey sertliği üzerindeki etkisini araştırmaktır. Gereç ve Yöntem: Onbeş adet insan 3. molar dişinden toplam otuz adet mine kesiti hazırlandı. Örnekler akrilik içine gömüldükten sonra rastgele üç gruba ayrıldı: G1. Kazein fosfopeptid-amorf kalsiyum fosfat [GC Tooth Mousse]; G2. Biyoaktif cam içeren deneysel remineralizasyon ajanı; G3. Yapay tükürük çözeltisi. Örnekler, remineralizasyon ajanlarının uygulanmasından önce 30 saniye süreyle %37’lik fosforik asit kullanılarak demineralizasyona tabi tutuldu. Daha sonra örneklerin yüzeylerine 5 dakikalık bir süre boyunca günde iki kez olmak üzere remineralizasyon ajanları uygulandı. Ajanların pamuk peletler ile temizlenmesinin ardından, örnekler bir sonraki tekrara kadar yapay bir tükürük çözeltisinde saklandı. İşlem 10 gün boyunca günlük olarak tekrarlandı. Örneklerin yüzey sertliği Vickers mikrosertlik testi kullanılarak başlangıçta, demineralizasyonu takiben ve remineralizasyondan sonra olmak üzere üç ayrı zamanda değerlendirildi. Bulgular: Fosforik asitle demineralizasyon sonrasında grupların mikrosertlik değerlerinde anlamlı bir azalma tespit edildi (p0.05). Her iki remineralizasyon ajanı karşılaştırıldığında, mine yüzeyinde meydana getirdikleri mikrosertlik artışları arasında istatistiksel olarak anlamlı bir fark saptanmadı. Sonuç: Biyoaktif cam içeren deneysel ajanın demineralize mine yüzeylerinin mikrosertlik değerlerini anlamlı şekilde artırdığı tespit edildi. Ancak, deneysel ajanın fiziksel ve biyolojik özelliklerinin daha ileri araştırmalarla incelenmesi gerekmektedir. Ayrıca, yapay tükürük solüsyonunun tek başına demineralize mine yüzeylerinin sertliğini artırmadığı belirlenmiştir.
- 31 July 2024
- Published by Ondokuz Mayis Universitesi in Türk Diş Hekimliği Araştırma Dergisi
Open AccessBiyoaktif Cam İçeren Deneysel Bir Remineralizasyon Ajanının Minenin Yüzey Sertliğine Etkisi
Amaç: Bu in vitro çalışmanın amacı, biyoaktif cam içeren deneysel bir remineralizasyon ajanının minenin yüzey sertliği üzerindeki etkisini araştırmaktır. Gereç ve Yöntem: Onbeş adet insan 3. molar dişinden toplam otuz adet mine kesiti hazırlandı. Örnekler akrilik içine gömüldükten sonra rastgele üç gruba ayrıldı: G1. Kazein fosfopeptid-amorf kalsiyum fosfat [GC Tooth Mousse]; G2. Biyoaktif cam içeren deneysel remineralizasyon ajanı; G3. Yapay tükürük çözeltisi. Örnekler, remineralizasyon ajanlarının uygulanmasından önce 30 saniye süreyle %37’lik fosforik asit kullanılarak demineralizasyona tabi tutuldu. Daha sonra örneklerin yüzeylerine 5 dakikalık bir süre boyunca günde iki kez olmak üzere remineralizasyon ajanları uygulandı. Ajanların pamuk peletler ile temizlenmesinin ardından, örnekler bir sonraki tekrara kadar yapay bir tükürük çözeltisinde saklandı. İşlem 10 gün boyunca günlük olarak tekrarlandı. Örneklerin yüzey sertliği Vickers mikrosertlik testi kullanılarak başlangıçta, demineralizasyonu takiben ve remineralizasyondan sonra olmak üzere üç ayrı zamanda değerlendirildi. Bulgular: Fosforik asitle demineralizasyon sonrasında grupların mikrosertlik değerlerinde anlamlı bir azalma tespit edildi (p0.05). Her iki remineralizasyon ajanı karşılaştırıldığında, mine yüzeyinde meydana getirdikleri mikrosertlik artışları arasında istatistiksel olarak anlamlı bir fark saptanmadı. Sonuç: Biyoaktif cam içeren deneysel ajanın demineralize mine yüzeylerinin mikrosertlik değerlerini anlamlı şekilde artırdığı tespit edildi. Ancak, deneysel ajanın fiziksel ve biyolojik özelliklerinin daha ileri araştırmalarla incelenmesi gerekmektedir. Ayrıca, yapay tükürük solüsyonunun tek başına demineralize mine yüzeylerinin sertliğini artırmadığı belirlenmiştir.