Current Organizations / Institutes

The organizations/institutes from the scholar's latest article

Previous Organizations / Institutes

The organizations / institutes from the scholar's other articles in the past ten years


Aziz Barış Başyiğit has a total of 22 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Comparison of dry sliding wear behavior and microstructural properties of AISI 8620 steel after gas carburization, gas nitriding, and pack boronization surface treatments

    by Aziz Baris Basyigit, Omer Sahin, Salih Ugur Bayca, Volkan Kilicli

    AISI 8620 steel is used in gears and machine parts where surface wear resistance is important. The presented study focuses on different surface hardening treatments on microstructural properties and the dry sliding wear behavior of the AISI 8620 steel. The dry sliding wear test used a tribometer with constant wear test parameters according to ASTM G-99 standard. The microstructures were characterized by optical and scanning electron microscopy (SEM), energy-dispersive X-ray (EDX), and X-ray diffraction (XRD). The highest surface hardness (∼1,507 HV) occurs in the boronized sample, attributed to the hard, iron borides (FeB, Fe 2 B, Fe 3 B) layers. The minimum surface hardness (∼507 HV) is determined in nitrided samples. The maximum case hardening depth (∼0.90 mm) is obtained in nitrided samples, as the minimum value of case depth (∼0.1 mm) was found in boronized samples. The mean coefficient of friction was highest for nitrided (0.622) and lowest for boronized (0.367) samples. Boronizing also gave the minimum wear (1.705 mm 3 , 1 mg), compared with nitriding (13.5 mm 3 , 1.8 mg) and carburizing (43.57 mm 3 , 4.9 mg). The boronized samples exhibited the best wear properties. According to the optical profilometer results of worn samples; the carburized sample exhibits a broad and deep wear track (volume loss 43.57 mm 3 ), indicating severe abrasive wear due to lower surface hardness, the boronized sample showed the narrowest and shallowest wear track (volume loss 1.705 mm 3 ), because of superior wear resistance from the dense, hard iron boride layer while the nitrided sample having moderate wear depth and volume loss (13.5 mm 3 ), indicating intermediate wear resistance attributed to a thinner, harder nitride layer providing moderate protection.


  • Open Access

    Correction to: Wear Resistance of Aluminum Alloy A356 After Thorough Anodic Oxidation

    by A. B. Başyiğit, Z. Azakli, R. Gümrük, O. Bican

  • Wear Resistance of Aluminum Alloy A356 After Thorough Anodic Oxidation

    by Aziz Bariş Başyiğit, Zeki Azakli, Recep Gümrük, Osman Bican

  • EFFECT OF CASE DEPTHS ON CORROSION PROPERTIES OF HARD ANODIC OXIDIZED A356 ALUMINUM ALLOY

    by Murat Haciosmanoğlu, Azi̇z Bariş Başyi̇ğİt, Ali̇ Paşa Heki̇mOğlu, Osman Bi̇cAn

    In this work, A356 alloy samples having a dimension of [ ][ ]mm were coated by hard anodic oxidation method at eight different thicknesses up to [ ]80[ ][ ]m. The sample surfaces and longitudinal section of these surfaces in both coated and uncoated conditions were investigated with a scanning electron microscope (SEM). Microhardness of the coating layers and core regions (base metal) were determined with the microvickers hardness testing method. Corrosion properties of the coated and uncoated samples were investigated by an electrochemical corrosion test set up according to ASTM G5 standard. The test results obtained from the coated and uncoated surfaces were compared to each other. Coated surfaces exhibited fluctuant surface profile. Microcracks were formed on these surfaces. Microhardness of the coating layers increased with increasing coating layer thickness. Energy dispersed X-ray spectroscopy (EDS) analysis of the surfaces showed that oxygen rate on the surfaces increased after the corrosion tests. Corrosion rate of the A356 alloy coated by hard anodic oxidation decreased with increasing coating thickness up to 40–50[ ][ ]m, but after this coating thickness, the corrosion rate increased. The results obtained from the investigations were discussed based on the characteristics of the coated surfaces.

  • Effects of filler material selection on the microstructural, mechanical and corrosion properties of TIG welded AISI/SAE 304L stainless steel sheets and rings

    by Oğuz Akgül, Aziz Barış Başyiğit

    Austenitic stainless steels are mainly preferred especially for resistance to aggressive oxidizing medias and high temperature applications such as equipments and mechanical parts which are used in defense and conventional industries. In this study; 3 mm thick 304L austenitic stainless steel sheets and rings are joined to each other by using Tungsten Inert Gas welding method under pure argon shielding gas with ER316L and ER2209 filler metals. Weld metals and heat-affected zones of welded joints were examined by metallurgical and scanning electron microscopes. Microhardness, tensile and Charpy impact tests of weld regions are investigated. It has been determined that the filler metals have dominantly changed the microstructure of weld metals. The microhardness values of the welded samples joined with ER2209 filler metal was lower than the sample joined with ER316L filler metal in weld metal regions. Besides, corrosion tests indicated that the corrosion rates of welded samples joined with ER2209 filler metal is lower than the samples joined with ER316L filler metal.


  • Investigating the Microstructural Properties and Phase Distributions of TIG Welded AISI/SAE 304L Stainless Steel Runners in TNT Filled Ammunutions

    by Oğuz Akgül, Aziz Barış BAŞYİĞİT

    Among the stainless steels, the most widely used group is austenitic stainless steels. The prominent reason why austenitic stainless steels are preferred in welded stainless steel fabrications is their good weldability. AISI/SAE 304L austenitic stainless steels exhibit adequate corrosion resistance in oxidizing environments. AISI/SAE 304L austenitic stainless steels are also used in filling interfaces of runners between the Tri-Nitro-Toluen filling vessel and ammunitions in defense industry. For the manufacture of the runners, the stainless steel plates and the stainless steel pipes are mainly joined by fusion welding. In this study; 3 mm thick 304L austenitic stainless steel plates and rings are welded to each other with two different filler weld wires of ER316L and ER2209 by Tungsten Inert Gas welding method under pure argon shielding gas. Weld metals and heat-affected zones of welded joints were examined using optical metallurgical microscope. It has been determined that the additional filler weld wires have changed the weld metal and the heat affected zone microstructures and phase distributions dominantly. Microstructures of all welded joints have been compared. Besides, phase distributions of weld metals and heat effected zones are made by image analysis sofware and Schaefflers diagram. ER 2209 welding filler metal increased the phase fraction of delta-ferrite in weld metals while it decreased the austenite phase fraction as compared to ER316L filler metal.


  • Open Access

    Investigating the Mechanical and Microstructural properties of Aluminium based Alloy Wheel Rims after TIG Welding

    by Aziz Barış BAŞYİĞİT

    En tr The quantity of motor vehicles is increasing in our country as also seen in the world. From the fact that usage of minimum 4 wheels per a motor vehicle, increasing traffic accidents results by deformation of vehicles parts especially wheels in economic considerations. As nowadays road conditions taken into account, the accidents damage especially tires, wheels and deform the rims and even can break them. The rims that produced from aluminium based alloys that presents a nice view and also maintains satisfactory mechanical values versus their weights are deformed by customary road conditions are being unbended and even welded by automobile wheel repairers. Because of the aluminium based alloy made motor vehicles wheel rims are too expensive to buy, they may be repaired. Hence; the aim of this research will be helpfull in determining and questioning whether qualification of their strength properties is adequate or not after the rims have been repaired by welding. For this purpose in this study; mechanical and microstructural properties of weld metal of motor vehicles Aluminium based alloy wheel rims were investigated after TIG welding. The microstructures of base and weld metals are determined to be in close structure and microvickers hardness test results are also in near values between each other regionally. Aluminium bases alloy wheel rims can be repaired by TIG welding after deformation of them. Dünyada olduğu üzere, Ülkemizde de motorlu taşıt sayısı her geçen gün artmaktadır. Binek taşıtlar başına en az 4 adet tekerleğin kullanılması gerçeğinden hareketle istatistiksel olarak yaşanan trafik kazalarındaki artışlar araçların çeşitli aksamlarında yüksek bir maliyetle zarar görmesine neden olmaktadır. Ayrıca mevcut yol koşulları da göz önüne alındığında kazalar taşıtların tekerlekleri başta olmak üzere lastiklerin zarar görmesinin yanı sıra jantların da eğilmelerine çatlamalarına ve hatta kırılmalarına yol açmaktadır. Göze hoş görünmelerinin yanında mekanik dayanım değerlerinin ağırlıklarına göre tatminkar sonuçlar sunduğu Alüminyum esaslı alaşımlardan üretilen jantlar mevcut yol koşullarında bahse konu nedenlerle deformasyona uğramakta ve oto lastik tamircileri tarafından doğrultma işlemine tabi tutulmakta ve hatta bazen kaynak edilmektedir. Alüminyum esaslı motorlu taşıt jantlarının ilk satın alış maliyetinin yüksek olması nedeniyle tamir edilebilmektedirler. Bu sebeple, kaynaklı tamir sonrası kaynak bölgelerinin mukavemet yeterliliklerini karşılama durumları bu proje ile sorgulanabilir ve değerlendirilebilir hale geleceği hedeflenmiştir. Bu amaçla; alüminyum esaslı taşıt jantlarının TIG kaynak işlemi sonrası kaynak bölgesinin mekanik ve mikroyapısal özellikleri incelenmiştir. TIG kaynak işlemi sonrasında ana malzeme ile kaynak metalinin yakın karakterde mikroyapılara sahip olduğu ve mikrovikers sertlik tarama sonuçlarının bölgesel olarak yaklaşık yakın değerlerde olduğu tespit edilmiştir. Alüminyum alaşımlı jantların muhtemel deformasyonları sonrasında TIG kaynak yöntemi ile tamir edilebileceği anlaşılmıştır.


  • Open Access

    S235 Yapı Çeliğinin Tozaltı Kaynağında Toz Türünün Mekanik ve Mikroyapısal Özelliklere Etkileri

    by Aziz Barış BAŞYİĞİT, Büşra Solak

    S235 ince taneli yapı çelikleri; bilhassa akma mukavemeti değerlerinin en az 235 megapaskal istendiği yapılar, fabrikalar ve makine parçalarında tercih edilmektedir. Düşük alaşımlı çelik gruplarında sınıflandırıldıklarından bu alaşımların fiyatlarının ucuz oluşu tüketimlerinin artmasını da beraberinde getirmiştir. Bu çalışmada; 15 mm kalınlığındaki S235 Yapı çeliği 2 farklı kaynak tozu kullanılarak tozaltı kaynak yöntemiyle kaynak edilmiştir. Kaynak tozu bileşiminin kaynak edilmiş S235 çelik alaşımının mikro-yapısal ve mekanik özellikleri üzerindeki etkileri incelenmiştir. Bu iki tür kaynak tozunun karşılaştırılması amacıyla; ana malzeme ve kaynaklı bağlantının ısının tesiri altındaki bölgeleri ve kaynak metalinin mikro-vikers sertlik taramaları, enine çekme deneyleri, mikroyapısal incelemeler uygulanmıştır.