PHPhilip Hulsmann

Philip Hulsmann

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article

Previous Organizations / Institutes

The organizations / institutes from the scholar's other articles in the past ten years


Philip Hulsmann has a total of 7 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Simulation of Water Vapor Ingress into PV-Modules under Different Climatic Conditions

    by Philip Hülsmann, Markus Heck, Michael Köhl

    This work deals with the simulation of water vapor ingress into wafer-based PV-modules for long-term exposure under different climatic conditions. Measured material parameters together with climatic data sets from four test sites (tropic, moderate, alpine, and arid) were used to calculate the water concentration inside of the encapsulant between solar cell and glass for a lifetime of 20 years. Two back-sheet materials (PET-based and PA-based) combined with EVA as encapsulant were used in respect to their influence on water ingress. The results show faster water ingress for warmer regions, but the highest concentrations were found for the moderate test site. The water ingress was additionally influenced by the used encapsulant and back-sheet combination. In particular the temperature dependency of the mass transfer, which differs from material to material, was the focus of this investigation.


  • Permeation impact on metallization degradation

    by C Peike, S Hoffmann, Philip Hulsmann, K A Weis, Michael Koehl, P Bentz

    The degradation of the inorganic components in a PV module is, besides polymer degradation, one of the most important aspects of PV module aging. Especially the corrosion of the cell metallization may lead to significant decreases in PV module performance. But in which way the metallization corrosion is affected by the permeation of atmospheric gases is not understood, yet. In order to investigate this permeation impact, laminates with a systematic variation of back-sheet and encapsulation materials as well as different laminate set-ups were made. Two different kinds of encapsulation (EVA and PVB) and four different back-sheet materials (TAPT, PA and two different TPT foils) were used. Standard cells with a two and three bus bar set-up were used. The laminates were subjected to damp-heat aging tests with a relative humidity of 80% at 80°C and 90°C, respectively. The degradation was investigated by means of electroluminescence imaging, Raman spectroscopy and microscopy. Special attention was paid to the spatial distribution of corrosion effects on the cell. Furthermore, the occurrence of a typical damp-heat induced damage, apparent as a shaded area in the electroluminescence images, should be investigated. A corrosion of the grid and the ribbons could be observed. EDX measurements revealed the grid corrosion to go along with the formation of needles of lead compounds from the silver paste.