Zhihong Zhong
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Zhihong Zhong has a total of 41 co-authors. Here are the top co-authors by number of shared publications:
Kuijing Song
School of Materials Science and Engineering, Hefei University of Technology, Hefei, People’s Republic of China
3 shared publicationsXin Xian
School of Materials Science and Engineering, Hefei University of Technology, Hefei, China
3 shared publications- Yucheng Wu
School of Materials Science and Engineering, Hefei University of Technology
3 shared publications Ankang Yang
Hefei Univ Technol, Sch Mat Sci & Engn, Hefei 230009, Anhui, Peoples R China
2 shared publicationsChengyong Wang
School of Materials Science and Engineering, Hefei University of Technology, Hefei, People’s Republic of China
2 shared publicationsChunyan Wang
School of Materials Science and Engineering, Hefei University of Technology, Hefei, People’s Republic of China
2 shared publications
Latest Publications
- Open Access
Microstructure and Mechanical Properties of B4C-HfB2-SiC Ceramic Composites Prepared by In Situ Reaction
B4C-HfB2-SiC (BCHS) ceramic composites were fabricated by in situ reaction with B4C and HfSi2 mixed powders through spark plasma sintering in this work. Effects of sintering temperature and sintering additive (HfSi2) content on the density, microstructure, and mechanical properties of the BCHS specimens were studied. The BCHS composite containing 15–30 vol.% HfSi2 reached over 98% theoretical density in the temperature range of 1600–1750 °C under the pressure of 50 MPa. The Vickers hardness, fracture toughness, and room temperature flexural strength of BCHS sintered at 1650 °C with 25 vol.% HfSi2 reached a maximum value of 31.3 GPa, 5.6 MPa·m1/2, and 573.9 MPa, respectively. The flexural strength was not decreased at elevated temperatures, and the flexural strength at temperatures of 400 °C, 600 °C, and 800 °C was evaluated to be 540.7 MPa, 518.8 MPa, and 586.9 MPa, respectively. Dense B4C-HfB2-SiC composites were fabricated by the spark plasma sintering process. The introduction of HfSi2 can significantly enhance the density and mechanical properties of B4C ceramic.
Open AccessMicrostructure and Mechanical Properties of B4C-HfB2-SiC Ceramic Composites Prepared by In Situ Reaction
B4C-HfB2-SiC (BCHS) ceramic composites were fabricated by in situ reaction with B4C and HfSi2 mixed powders through spark plasma sintering in this work. Effects of sintering temperature and sintering additive (HfSi2) content on the density, microstructure, and mechanical properties of the BCHS specimens were studied. The BCHS composite containing 15–30 vol.% HfSi2 reached over 98% theoretical density in the temperature range of 1600–1750 °C under the pressure of 50 MPa. The Vickers hardness, fracture toughness, and room temperature flexural strength of BCHS sintered at 1650 °C with 25 vol.% HfSi2 reached a maximum value of 31.3 GPa, 5.6 MPa·m1/2, and 573.9 MPa, respectively. The flexural strength was not decreased at elevated temperatures, and the flexural strength at temperatures of 400 °C, 600 °C, and 800 °C was evaluated to be 540.7 MPa, 518.8 MPa, and 586.9 MPa, respectively. Dense B4C-HfB2-SiC composites were fabricated by the spark plasma sintering process. The introduction of HfSi2 can significantly enhance the density and mechanical properties of B4C ceramic.
- 23 September 2024
- Published by Springer Nature in JOM
- Vol. 76 (11) , 6313-6324
Effect of Bonding Temperature on the Interfacial Microstructure and Mechanical Properties of W/Steel Joints Diffusion-Bonded with a CoFeNi Interlayer
- 23 September 2024
- Published by Springer Nature in JOM
- Vol. 76 (11) , 6313-6324
Effect of Bonding Temperature on the Interfacial Microstructure and Mechanical Properties of W/Steel Joints Diffusion-Bonded with a CoFeNi Interlayer
- 15 September 2021
- Published by Springer Nature in Advanced Composites and Hybrid Materials
- Vol. 5 (2) , 1508-1515
Microstructure and compression properties of a dual-phase FeCoCrMn high-entropy alloy
- 15 September 2021
- Published by Springer Nature in Advanced Composites and Hybrid Materials
- Vol. 5 (2) , 1508-1515
Microstructure and compression properties of a dual-phase FeCoCrMn high-entropy alloy
- 19 June 2020
- Published by Taylor & Francis in Journal of Adhesion Science and Technology
- Vol. 34 (24) , 2638-2651
Microstructure and mechanical properties of W/steel joints diffusion bonded with Nb and Nb/Ni interlayers by spark plasma sintering
Tungsten/steel joints are desired for fusion reactors and militarily applications, as it could combine the unique properties of these two dissimilar metals. In view of the large differences of physical and chemical properties between W and steel, diffusion bonding is considered to be the proper technique for joining of W to steel. In this paper, diffusion bonding of W to low activation ferritic/martensitic steel at 1050 °C with 50 MPa for 20 min by spark plasma sintering (SPS) were investigated. The results showed that direct diffusion bonding of W to steel was feasible. However, the formation of ferrite and carbide at the W/steel interface lowered the joint strength. Effects of the insertion of ductile interlayers (Nb, Nb/Ni) on the joining interface microstructure and mechanical properties of W/steel joints were studied. The detailed microstructural characterization revealed that Nb could prevent the formation of ferrite and carbide at the W/steel interface. The Ni promoted the interfacial diffusion between Nb and steel. The shear strength and Vickers hardness of the joints were evaluated.
- 19 June 2020
- Published by Taylor & Francis in Journal of Adhesion Science and Technology
- Vol. 34 (24) , 2638-2651
Microstructure and mechanical properties of W/steel joints diffusion bonded with Nb and Nb/Ni interlayers by spark plasma sintering
Tungsten/steel joints are desired for fusion reactors and militarily applications, as it could combine the unique properties of these two dissimilar metals. In view of the large differences of physical and chemical properties between W and steel, diffusion bonding is considered to be the proper technique for joining of W to steel. In this paper, diffusion bonding of W to low activation ferritic/martensitic steel at 1050 °C with 50 MPa for 20 min by spark plasma sintering (SPS) were investigated. The results showed that direct diffusion bonding of W to steel was feasible. However, the formation of ferrite and carbide at the W/steel interface lowered the joint strength. Effects of the insertion of ductile interlayers (Nb, Nb/Ni) on the joining interface microstructure and mechanical properties of W/steel joints were studied. The detailed microstructural characterization revealed that Nb could prevent the formation of ferrite and carbide at the W/steel interface. The Ni promoted the interfacial diffusion between Nb and steel. The shear strength and Vickers hardness of the joints were evaluated.
- 18 November 2019
- Published by Springer Nature in Metals and Materials International
- Vol. 26 (8) , 1192-1199
Microstructure Stability and Its Influence on the Mechanical Properties of CrMnFeCoNiAl0.25 High Entropy Alloy
- 18 November 2019
- Published by Springer Nature in Metals and Materials International
- Vol. 26 (8) , 1192-1199
Microstructure Stability and Its Influence on the Mechanical Properties of CrMnFeCoNiAl0.25 High Entropy Alloy
- 20 November 2018
- Published by Wiley in Rare Metals
- Vol. 41 (3) , 1015-1021
Tailoring strength and ductility of high‐entropy CrMnFeCoNi alloy by adding Al
High‐entropy alloys with high strength and acceptable ductility at both room and elevated temperatures for high‐temperature structural applications are desired. In this paper, CrMnFeCoNi alloy with outstanding ductility but low strength was selected as baseline alloy to study the formation of hard phase to strengthen this ductile alloy by adding Al into it. The results indicate that there is a phase structure transition from fcc to bcc when adding enough Al into CrMnFeCoNi. The yield strength and hardness increase with the content of Al increasing, due to the formation of hard bcc phase in the ductile CrMnFeCoNi alloy. The CrMnFeCoNiAl alloy with a bcc structure shows a high yield strength and adequate ductility at elevated temperatures. At 400 and 500 °C, the yield strength and ductility of CrMnFeCoNiAl alloy are 975.59 MPa and 6.39% and 989.48 MPa and 9.15%, respectively. An example of tailoring the strength and ductility of high‐entropy alloy is demonstrated in this paper.
- 20 November 2018
- Published by Wiley in Rare Metals
- Vol. 41 (3) , 1015-1021
Tailoring strength and ductility of high‐entropy CrMnFeCoNi alloy by adding Al
High‐entropy alloys with high strength and acceptable ductility at both room and elevated temperatures for high‐temperature structural applications are desired. In this paper, CrMnFeCoNi alloy with outstanding ductility but low strength was selected as baseline alloy to study the formation of hard phase to strengthen this ductile alloy by adding Al into it. The results indicate that there is a phase structure transition from fcc to bcc when adding enough Al into CrMnFeCoNi. The yield strength and hardness increase with the content of Al increasing, due to the formation of hard bcc phase in the ductile CrMnFeCoNi alloy. The CrMnFeCoNiAl alloy with a bcc structure shows a high yield strength and adequate ductility at elevated temperatures. At 400 and 500 °C, the yield strength and ductility of CrMnFeCoNiAl alloy are 975.59 MPa and 6.39% and 989.48 MPa and 9.15%, respectively. An example of tailoring the strength and ductility of high‐entropy alloy is demonstrated in this paper.
- 1 September 2018
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 735, 104-113
Microstructure and mechanical properties of SiC joint with an in-situ formed SiC-TiB2 composite interlayer
- 1 September 2018
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 735, 104-113
Microstructure and mechanical properties of SiC joint with an in-situ formed SiC-TiB2 composite interlayer
- 5 April 2018
- Published by Taylor & Francis in Journal of Adhesion Science and Technology
- Vol. 32 (18) , 2041-2053
Effect of adding of SiC particulate on the microstructure and shear strength of SiC ceramic joint brazed with Si-24Ti alloy
In order to refine the grain size of TiSi2 silicide and reduce the formation of micro-defects in the joint, and thereby increasing the joint strength of SiC ceramic brazed with Si-24Ti (wt.%), a small amount of SiC particulates were added in the brazing alloy. The microstructure and mechanical strength of SiC joints was investigated by using field emission scanning electron microscopy, energy dispersive X-ray spectroscopy, X-ray diffraction spectrometer, and shear strength test. The results indicated that SiC particulates enhanced the nucleation and grain refinement of the TiSi2 and Si phase. The adding of appropriate content of SiC (2 phase and increase the fraction of Si-TiSi2 eutectic zone. However, excess addition of 1.5 wt.% SiC caused the coarsening of TiSi2 phase due to the clustering of added fine SiC particulates. With the increasing of SiC particulate content, the shear strength of the joints increased at first and then decreased. The maximum shear strength of 106.3 MPa of SiC joint was obtained for the joint brazed with 1 wt.% SiC addition, which was ~19% higher than that of the joint brazed without SiC particulates.
- 5 April 2018
- Published by Taylor & Francis in Journal of Adhesion Science and Technology
- Vol. 32 (18) , 2041-2053
Effect of adding of SiC particulate on the microstructure and shear strength of SiC ceramic joint brazed with Si-24Ti alloy
In order to refine the grain size of TiSi2 silicide and reduce the formation of micro-defects in the joint, and thereby increasing the joint strength of SiC ceramic brazed with Si-24Ti (wt.%), a small amount of SiC particulates were added in the brazing alloy. The microstructure and mechanical strength of SiC joints was investigated by using field emission scanning electron microscopy, energy dispersive X-ray spectroscopy, X-ray diffraction spectrometer, and shear strength test. The results indicated that SiC particulates enhanced the nucleation and grain refinement of the TiSi2 and Si phase. The adding of appropriate content of SiC (2 phase and increase the fraction of Si-TiSi2 eutectic zone. However, excess addition of 1.5 wt.% SiC caused the coarsening of TiSi2 phase due to the clustering of added fine SiC particulates. With the increasing of SiC particulate content, the shear strength of the joints increased at first and then decreased. The maximum shear strength of 106.3 MPa of SiC joint was obtained for the joint brazed with 1 wt.% SiC addition, which was ~19% higher than that of the joint brazed without SiC particulates.
- 18 June 2015
- Published by Springer Nature in Metals and Materials International
- Vol. 21 (4) , 659-665
Tensile and creep deformation of a newly developed Ni-Fe-based superalloy for 700 °C advanced ultra-supercritical boiler applications
- 18 June 2015
- Published by Springer Nature in Metals and Materials International
- Vol. 21 (4) , 659-665
Tensile and creep deformation of a newly developed Ni-Fe-based superalloy for 700 °C advanced ultra-supercritical boiler applications