Rodolfo Antonio Rodriguez-Davila
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Rodolfo Antonio Rodriguez-Davila has a total of 40 co-authors. Here are the top co-authors by number of shared publications:
- Israel Mejia
Centro de Ingeniería y Desarrollo Industrial (CIDESI), Querétaro 76125, Mexico
6 shared publications Manuel Quevedo-Lopez
5 shared publicationsPavel Bolshakov
5 shared publicationsChadwin D. Young
4 shared publications- Chadwin Delin Young
Department of Materials Science and Engineering, The University of Texas at Dallas , 800 W. Campbell Road, Richardson, Texas 75080
4 shared publications - Manuel Angel Quevedo-López
Department of Materials Science and Engineering, University of Texas at Dallas, Richardson, TX 75080, USA
4 shared publications
Latest Publications
- 2 August 2022
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 33 (24) , 19272-19283
Electrical characteristics of lead-free Mn-doped BiFeO3–SrTiO3 thin films deposited on silicon substrate using pulsed laser deposition
- 2 August 2022
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 33 (24) , 19272-19283
Electrical characteristics of lead-free Mn-doped BiFeO3–SrTiO3 thin films deposited on silicon substrate using pulsed laser deposition
- 1 May 2022
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 40 (3) , 033417
Energy storage performance in lead-free antiferroelectric 0.92(Bi0.54Na0.46)TiO3-0.08BaTiO3 ultrathin films by pulsed laser deposition
In this study, we report the recoverable energy density (Urec) of lead-free antiferroelectric perovskite 0.92(Bi0.54Na0.46)TiO3-0.08BaTiO3 (BNT-BT) ultrathin films deposited directly on highly boron-doped silicon (p-Si) by a pulsed laser deposition method. Two pressure values were used in the growing conditions, 4.67 × 10−5 and 13.3 Pa, at a fixed substrate temperature of 700 °C. After that, the films were subjected to postannealing under an oxidizing atmosphere at 700 °C for 1 h. A conventional lithography process was used to define vertical metal–ferroelectric–p-Si structures and evaluate the energy storage characteristics. Cross-sectional SEM images showed achieved thicknesses of about 11–13 nm. The high electric field strengths of 3.8 and 4.5 MV/cm supported for BNT-BT ultrathin films deposited at 4.67 × 10−5 and 13.3 Pa, respectively, imply a high-quality perovskite thin-film growth on p-Si. The 11-nm ultrathin film grown at 13.3 Pa showed higher Urec, efficiency (η), and a maximum applied electric field of 30 J/cm3, 83%, and 4.5 MV/cm, respectively.
- 1 May 2022
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 40 (3) , 033417
Energy storage performance in lead-free antiferroelectric 0.92(Bi0.54Na0.46)TiO3-0.08BaTiO3 ultrathin films by pulsed laser deposition
In this study, we report the recoverable energy density (Urec) of lead-free antiferroelectric perovskite 0.92(Bi0.54Na0.46)TiO3-0.08BaTiO3 (BNT-BT) ultrathin films deposited directly on highly boron-doped silicon (p-Si) by a pulsed laser deposition method. Two pressure values were used in the growing conditions, 4.67 × 10−5 and 13.3 Pa, at a fixed substrate temperature of 700 °C. After that, the films were subjected to postannealing under an oxidizing atmosphere at 700 °C for 1 h. A conventional lithography process was used to define vertical metal–ferroelectric–p-Si structures and evaluate the energy storage characteristics. Cross-sectional SEM images showed achieved thicknesses of about 11–13 nm. The high electric field strengths of 3.8 and 4.5 MV/cm supported for BNT-BT ultrathin films deposited at 4.67 × 10−5 and 13.3 Pa, respectively, imply a high-quality perovskite thin-film growth on p-Si. The 11-nm ultrathin film grown at 13.3 Pa showed higher Urec, efficiency (η), and a maximum applied electric field of 30 J/cm3, 83%, and 4.5 MV/cm, respectively.
- 1 February 2020
- Published by Elsevier in Solid-State Electronics
- Vol. 164
On the DC extraction of the asymmetric parasitic source and drain resistances for MOSFETs
- 1 February 2020
- Published by Elsevier in Solid-State Electronics
- Vol. 164
On the DC extraction of the asymmetric parasitic source and drain resistances for MOSFETs
- 11 November 2019
- Published by Taylor & Francis
- p. 375-395
Reliability Assessment of Low-Temperature ZnO-Based Thin-Film Transistors
Large-area/flexible electronics for Internet of Things (IoT) applications have garnered significant consideration recently. In addition, oxide-based semiconductors, namely, zinc oxide-based (i.e., ZnO and indium gallium zinc oxide, IGZO) materials, are attractive for use in flexible electronics due to their current or potential use in display technology, their transparency, and because they can be processed at low temperature, which is compatible with large-area/flex technology needs. Furthermore, these semiconductors have demonstrated noteworthy thin-film transistor (TFT) performance [1–3] when compared to organic-based semiconductors. Thus, ZnO-based semiconductors as potential candidates for use as an active layer in TFTs in flexible circuitry [3] are a viable option. Although this is the case, low-temperature deposition parameter impact of ultra-thin semiconducting ZnO-based layers on TFT performance is required. In addition, other critical materials are required to fabricate a TFT, such as the gate dielectric—a critical component of any metal-oxide-semiconductor field effect transistor (MOSFET). Currently in mainstream silicon-based transistor technologies, optimized high-k gate dielectrics, such as hafnium-based films are used. However, early hafnium dioxide (HfO2) gate-first dielectric development in MOSFETs saw the impact of fast transient charge trapping and its effect on threshold voltage (Vt ) instability. These high-k dielectrics were deposited and annealed at higher temperatures to achieve a low-leakage dielectric. This fast trapping phenomenon has been extensively investigated over the years, where channel electrons would be readily trapped in the HfO2 rather than participate in the channel current [4–18]. This fast electron trapping can have trapping times on the order of microseconds and manifest itself as a shift in the threshold voltage (∆Vt ), and subsequently lower the drive current (Figure 16.1). The results demonstrate that electrically active defects that impact performance and reliability behave differently for low process temperature (100°C) HfO2 gate dielectrics compared to HfO2 processed at temperatures (~400°C + source/drain [S/D] anneal) for silicon complimentary 376metal-oxide-semiconductor (CMOS) gate-first technology [19–21]. The instability characteristics illustrate that, after an initially large shift for the TFT, the Vt remains shifted after each subsequent measurement (more details in this chapter), while a conventional Si transistor demonstrated large shifts as well, but demonstrated complete recovery with each subsequent measurement. These electrically active defects—also known as traps—affect device performance and reliability as a function time and the trap fundamental nature [22]; and therefore, need intense investigation to understand low temperature HfO2 deposition’s impact on non-Si, TFT Vt instability. Figure 16.1 (a) ‘Conventional’ gate-first HfO2 using [23,24] where complete recovery (tr ) of Vt is observed with repetitive measurements while (b) ZnO TFT HfO2 using DC I-V does not recover after first measurement.
- 11 November 2019
- Published by Taylor & Francis
- p. 375-395
Reliability Assessment of Low-Temperature ZnO-Based Thin-Film Transistors
Large-area/flexible electronics for Internet of Things (IoT) applications have garnered significant consideration recently. In addition, oxide-based semiconductors, namely, zinc oxide-based (i.e., ZnO and indium gallium zinc oxide, IGZO) materials, are attractive for use in flexible electronics due to their current or potential use in display technology, their transparency, and because they can be processed at low temperature, which is compatible with large-area/flex technology needs. Furthermore, these semiconductors have demonstrated noteworthy thin-film transistor (TFT) performance [1–3] when compared to organic-based semiconductors. Thus, ZnO-based semiconductors as potential candidates for use as an active layer in TFTs in flexible circuitry [3] are a viable option. Although this is the case, low-temperature deposition parameter impact of ultra-thin semiconducting ZnO-based layers on TFT performance is required. In addition, other critical materials are required to fabricate a TFT, such as the gate dielectric—a critical component of any metal-oxide-semiconductor field effect transistor (MOSFET). Currently in mainstream silicon-based transistor technologies, optimized high-k gate dielectrics, such as hafnium-based films are used. However, early hafnium dioxide (HfO2) gate-first dielectric development in MOSFETs saw the impact of fast transient charge trapping and its effect on threshold voltage (Vt ) instability. These high-k dielectrics were deposited and annealed at higher temperatures to achieve a low-leakage dielectric. This fast trapping phenomenon has been extensively investigated over the years, where channel electrons would be readily trapped in the HfO2 rather than participate in the channel current [4–18]. This fast electron trapping can have trapping times on the order of microseconds and manifest itself as a shift in the threshold voltage (∆Vt ), and subsequently lower the drive current (Figure 16.1). The results demonstrate that electrically active defects that impact performance and reliability behave differently for low process temperature (100°C) HfO2 gate dielectrics compared to HfO2 processed at temperatures (~400°C + source/drain [S/D] anneal) for silicon complimentary 376metal-oxide-semiconductor (CMOS) gate-first technology [19–21]. The instability characteristics illustrate that, after an initially large shift for the TFT, the Vt remains shifted after each subsequent measurement (more details in this chapter), while a conventional Si transistor demonstrated large shifts as well, but demonstrated complete recovery with each subsequent measurement. These electrically active defects—also known as traps—affect device performance and reliability as a function time and the trap fundamental nature [22]; and therefore, need intense investigation to understand low temperature HfO2 deposition’s impact on non-Si, TFT Vt instability. Figure 16.1 (a) ‘Conventional’ gate-first HfO2 using [23,24] where complete recovery (tr ) of Vt is observed with repetitive measurements while (b) ZnO TFT HfO2 using DC I-V does not recover after first measurement.
- 1 September 2019
- Published by Elsevier in Microelectronic Engineering
- Vol. 217
Impact of Al2O3 deposition temperature on the performance and initial stability of nanocrystalline ZnO thin-film transistors
- 1 September 2019
- Published by Elsevier in Microelectronic Engineering
- Vol. 217
Impact of Al2O3 deposition temperature on the performance and initial stability of nanocrystalline ZnO thin-film transistors
- 13 August 2019
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Electron Devices
- Vol. 66 (9) , 3861-3866
Performance and Reliability Comparison of ZnO and IGZO Thin-Film Transistors and Inverters Fabricated at a Maximum Process Temperature of 115 °C
Performance and reliability comparison of oxide-based thin-film transistors fabricated at a maximum process temperature of 115 °C is presented. A fully patterned and passivated process was successfully evaluated and implemented using polycrystalline ZnO and amorphous indium–gallium–zinc–oxide (IGZO) as an active layer in glass substrates. Saturation mobilities of 14.2 and 9.0 cm $^{{2}}\cdot \text{V}^{-{1}}\cdot \text{s}^{-{1}}$ were obtained for ZnO and IGZO, respectively, with threshold voltages of 2.2 and 2.0 V, an ON/ OFF ratio $> {1} \times 10^{{8}}$ , and an ${I}_{{\text {off}}}< {1} \times 10^{-{12}}$ A. The small mobility change in IGZO with gate voltage is due to its amorphous character. Longer variation is observed in polycrystalline ZnO due to its grain boundaries. Reliability studies show a threshold voltage shifting of 0.4 and 1.8 V for ZnO and IGZO devices, testing after 1200-s stress. Devices were successfully implemented in ZnO- and IGZO-based inverters using saturation and zero-drive structures, showing a maximum dc gain of 2.4- and 25-V/V, respectively.
- 13 August 2019
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Electron Devices
- Vol. 66 (9) , 3861-3866
Performance and Reliability Comparison of ZnO and IGZO Thin-Film Transistors and Inverters Fabricated at a Maximum Process Temperature of 115 °C
Performance and reliability comparison of oxide-based thin-film transistors fabricated at a maximum process temperature of 115 °C is presented. A fully patterned and passivated process was successfully evaluated and implemented using polycrystalline ZnO and amorphous indium–gallium–zinc–oxide (IGZO) as an active layer in glass substrates. Saturation mobilities of 14.2 and 9.0 cm $^{{2}}\cdot \text{V}^{-{1}}\cdot \text{s}^{-{1}}$ were obtained for ZnO and IGZO, respectively, with threshold voltages of 2.2 and 2.0 V, an ON/ OFF ratio $> {1} \times 10^{{8}}$ , and an ${I}_{{\text {off}}}< {1} \times 10^{-{12}}$ A. The small mobility change in IGZO with gate voltage is due to its amorphous character. Longer variation is observed in polycrystalline ZnO due to its grain boundaries. Reliability studies show a threshold voltage shifting of 0.4 and 1.8 V for ZnO and IGZO devices, testing after 1200-s stress. Devices were successfully implemented in ZnO- and IGZO-based inverters using saturation and zero-drive structures, showing a maximum dc gain of 2.4- and 25-V/V, respectively.
- 30 April 2019
- Published by The Electrochemical Society in ECS Transactions
- Vol. 90 (1) , 89-97
Relatively Low-Temperature Processing and Its Impact on Device Performance and Reliability
Fabrication of MoS2, ZnO, and IGZO transistors at low enough temperatures that are suitable for large-area/flexible electronics is presented. Evaluating critical processing conditions and approaches on device performance is critical to understanding and improving devices to enable large-area/flexible circuits for the IoT. For MoS2, a study of the implications of photoresist residue on MoS2 in the source/drain contact region was done. Results determined that an O2 plasma exposure in this location can remove the resist residue and create a robust TiOx/MoS2 contact, where an ~15x increase in mobility and ~20x reduction in contact resistance was achieved for O2 plasma treated transistors. Thin-film transistor fabrication of ZnO and IGZO as the semiconductor yielded saturation mobilities of 14.2 and 9.0 cm2/V•s, respectively. Among other parameters, the contact resistance was noticeably lower for ZnO due to its polycrystalline morphology compared to the amorphous IGZO, which was determined to be more resistive.
- 30 April 2019
- Published by The Electrochemical Society in ECS Transactions
- Vol. 90 (1) , 89-97
Relatively Low-Temperature Processing and Its Impact on Device Performance and Reliability
Fabrication of MoS2, ZnO, and IGZO transistors at low enough temperatures that are suitable for large-area/flexible electronics is presented. Evaluating critical processing conditions and approaches on device performance is critical to understanding and improving devices to enable large-area/flexible circuits for the IoT. For MoS2, a study of the implications of photoresist residue on MoS2 in the source/drain contact region was done. Results determined that an O2 plasma exposure in this location can remove the resist residue and create a robust TiOx/MoS2 contact, where an ~15x increase in mobility and ~20x reduction in contact resistance was achieved for O2 plasma treated transistors. Thin-film transistor fabrication of ZnO and IGZO as the semiconductor yielded saturation mobilities of 14.2 and 9.0 cm2/V•s, respectively. Among other parameters, the contact resistance was noticeably lower for ZnO due to its polycrystalline morphology compared to the amorphous IGZO, which was determined to be more resistive.
- 1 March 2019
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- No. 10719032,p. 190-193
Understanding the Effects of Low-Temperature Passivation and Annealing on ZnO TFTs Test Structures
Back-gate ZnO TFTs - with and without top-side passivation - were fabricated and electrically characterized. Passivation layers consisting of HfO 2 , Al 2 O 3 , and Parylene were introduced to study their impact on the TFT performance. Annealing was done to improve the electrical characteristics of passivated devices by neutralizing the initial charge introduced as a result of the low-temperature passivation. Low-temperature annealing combined with an Al 2 O 3 passivation layer demonstrates an I-V response comparable to ZnO TFTs without any passivation layer, indicating the viability of Al 2 O 3 as a good candidate for passivating ZnO TFTs.
- 1 March 2019
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- No. 10719032,p. 190-193
Understanding the Effects of Low-Temperature Passivation and Annealing on ZnO TFTs Test Structures
Back-gate ZnO TFTs - with and without top-side passivation - were fabricated and electrically characterized. Passivation layers consisting of HfO 2 , Al 2 O 3 , and Parylene were introduced to study their impact on the TFT performance. Annealing was done to improve the electrical characteristics of passivated devices by neutralizing the initial charge introduced as a result of the low-temperature passivation. Low-temperature annealing combined with an Al 2 O 3 passivation layer demonstrates an I-V response comparable to ZnO TFTs without any passivation layer, indicating the viability of Al 2 O 3 as a good candidate for passivating ZnO TFTs.
- 1 March 2019
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 1-5
Positive Bias Instability in ZnO TFTs with Al2O3 Gate Dielectric
Positive bias instability stress (PBI) was done on ZnO thin-film transistors (TFTs) with Al 2 O 3 deposition at 100°C and 250°C. The threshold voltage (VT), transconductance (g m ), and subthreshold slope (SS) were monitored where the 100°C samples demonstrated a “turn-around” phenomenon in the ΔV T compared to the 250°C samples. The 250°C samples show consistent ΔV T , suggesting a higher Al 2 O 3 deposition temperature results in the absence of the defect responsible for the “turn-around” effect. Both sets also demonstrate negligible degradation in Δg m and ASS-suggesting little to no influence on the V T shift by interfacial state generation.
- 1 March 2019
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 1-5
Positive Bias Instability in ZnO TFTs with Al2O3 Gate Dielectric
Positive bias instability stress (PBI) was done on ZnO thin-film transistors (TFTs) with Al 2 O 3 deposition at 100°C and 250°C. The threshold voltage (VT), transconductance (g m ), and subthreshold slope (SS) were monitored where the 100°C samples demonstrated a “turn-around” phenomenon in the ΔV T compared to the 250°C samples. The 250°C samples show consistent ΔV T , suggesting a higher Al 2 O 3 deposition temperature results in the absence of the defect responsible for the “turn-around” effect. Both sets also demonstrate negligible degradation in Δg m and ASS-suggesting little to no influence on the V T shift by interfacial state generation.
- 1 July 2018
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 1-4
Hot Carrier Stress Investigation of Zinc Oxide Thin Film Transistors with an Al2O3 Gate Dielectric
Hot carrier stress, where the gate and drain voltages were stressed simultaneously, was executed on ZnO thin-film transistors (TFTs) with different PLD ZnO or ALD Al 2 O 3 deposition parameters. The threshold voltage and transconductance were monitored where 30 mTorr samples had greater threshold voltage shifts and transconductance (gm) degradation compared to the 20 mTorr ZnO film. For samples with and without a 400°C forming gas anneal, greater degradation was seen in the annealed sample, which indicates 400°C may be too aggressive. The correlation between gm degradation (i.e., interface degradation) and ΔVt demonstrate that there is influence to the Vt shift from electrically active defects generated in the interfacial region.
- 1 July 2018
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 1-4
Hot Carrier Stress Investigation of Zinc Oxide Thin Film Transistors with an Al2O3 Gate Dielectric
Hot carrier stress, where the gate and drain voltages were stressed simultaneously, was executed on ZnO thin-film transistors (TFTs) with different PLD ZnO or ALD Al 2 O 3 deposition parameters. The threshold voltage and transconductance were monitored where 30 mTorr samples had greater threshold voltage shifts and transconductance (gm) degradation compared to the 20 mTorr ZnO film. For samples with and without a 400°C forming gas anneal, greater degradation was seen in the annealed sample, which indicates 400°C may be too aggressive. The correlation between gm degradation (i.e., interface degradation) and ΔVt demonstrate that there is influence to the Vt shift from electrically active defects generated in the interfacial region.