Matin Saessi
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Matin Saessi has a total of 6 co-authors. Here are the top co-authors by number of shared publications:
- Ali Alizadeh
Faculty of Materials and Manufacturing Processes, Malek Ashtar University of Technology, Tehran, Iran
4 shared publications Alireza Abdollahi
Metals research center, Malek-Ashtar University of Technology, Tehran
1 shared publication- Alireza Abdollahi
Metallic Materials Research Center, Malek-Ashtar University of Technology, Tehran, Iran
1 shared publication Hossein Sarpoolaky
Department of Materials Engineering, Iran University of Science and Technology, Tehran, Iran
1 shared publicationMohammad Maleki
Faculty of Materials & Manufacturing Processes, Malek Ashtar University of Technology, Tehran, Iran
1 shared publicationNasser Ehsani
Composite research center, Malek-Ashtar University of Technology, Tehran
1 shared publication
Latest Publications
- 13 July 2026
- Published by Springer Nature in Sādhanā
- Vol. 51 (3) , 177
Mechanical behavior and degradation performance of white Portland cements containing a processed rich-TiO2 solution
- 13 July 2026
- Published by Springer Nature in Sādhanā
- Vol. 51 (3) , 177
Mechanical behavior and degradation performance of white Portland cements containing a processed rich-TiO2 solution
- 26 June 2019
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (9) , 096549
Room temperature wear performance and mechanical properties of hot extruded ultrafine-grained Al5083-5 wt%B4C-Al2024 tri-modal composites
In this paper, the mechanical properties and wear performance of Al5083-5 wt. %B4C-Al2024 tri-modal composites at room temperature has been discussed. Al2024 alloy powders were added to mechanically milled Al5083-5wt. %B4C powders as coarse grains and the samples consolidated using the hot press and hot extrusion techniques. Results indicated that by adding Al2024 coarse grains, tensile strength of Al5083-5 wt. %B4C composite decreased up to 35% from 508 MPa to 327 MPa however, ductility increased from 2.8 to 5%. Moreover, by adding 50wt. % of Al2024 coarse grains, hardness decreased from 355 to 288 HV which had a significant role on the room temperature wear performance of the tri-modal samples and wear rate increased from 3.5×10-6 to 4.7×10-6 (mm3/m). It seemed that room temperature wear performance of Al5083-5 wt. %B4C-Al2024 composites is directly dependent to the hardness and the weight percentage of the Al2024 coarse grains.
- 26 June 2019
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (9) , 096549
Room temperature wear performance and mechanical properties of hot extruded ultrafine-grained Al5083-5 wt%B4C-Al2024 tri-modal composites
In this paper, the mechanical properties and wear performance of Al5083-5 wt. %B4C-Al2024 tri-modal composites at room temperature has been discussed. Al2024 alloy powders were added to mechanically milled Al5083-5wt. %B4C powders as coarse grains and the samples consolidated using the hot press and hot extrusion techniques. Results indicated that by adding Al2024 coarse grains, tensile strength of Al5083-5 wt. %B4C composite decreased up to 35% from 508 MPa to 327 MPa however, ductility increased from 2.8 to 5%. Moreover, by adding 50wt. % of Al2024 coarse grains, hardness decreased from 355 to 288 HV which had a significant role on the room temperature wear performance of the tri-modal samples and wear rate increased from 3.5×10-6 to 4.7×10-6 (mm3/m). It seemed that room temperature wear performance of Al5083-5 wt. %B4C-Al2024 composites is directly dependent to the hardness and the weight percentage of the Al2024 coarse grains.