Hideki Kakisawa
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Hideki Kakisawa has a total of 46 co-authors. Here are the top co-authors by number of shared publications:
- Ryo Inoue
Department of Mechanical Engineering, Tokyo University of Science, Katsushika-ku, Japan
4 shared publications - Gaku Okuma
Research Center for Structural Materials, National Institute for Materials Science, 1-2-1 Sengen, Tsukuba, Ibaraki 305-0047, Japan
3 shared publications - Fumihiro Wakai
National Institute for Materials Science
2 shared publications Haruki Minagawa
Department of Mechanical Engineering Tokyo University of Science 6-3-1 Niijuku Katsushika-Ku Tokyo 125-8585 Japan
2 shared publications- Kazuya Shimoda
Kyoto University
2 shared publications - Masayuki Uesugi
Japan Synchrotron Radiation Research Institute
2 shared publications
Latest Publications
- 12 September 2026
- Published by Elsevier in Acta Materialia
- Vol. 320
Micromechanics of the sintering force in sintering by bulk diffusion
- 12 September 2026
- Published by Elsevier in Acta Materialia
- Vol. 320
Micromechanics of the sintering force in sintering by bulk diffusion
- 29 October 2023
- Published by Elsevier in Journal of the European Ceramic Society
- Vol. 44 (3) , 1445-1457
Mechanical behaviours of hot-pressed rare-earth oxide (RE = Y and La)-doped TaB2-SiC composites
- 29 October 2023
- Published by Elsevier in Journal of the European Ceramic Society
- Vol. 44 (3) , 1445-1457
Mechanical behaviours of hot-pressed rare-earth oxide (RE = Y and La)-doped TaB2-SiC composites
- Open Access
- 1 March 2023
- Published by Wiley in Advanced Engineering Materials
- Vol. 25 (18)
3D Visualization of Morphological Evolution of Large Defects during Spark Plasma Sintering of Alumina Granules
The mechanical reliability of products must be assured for scaling up and production of complex‐shaped components by spark plasma sintering (SPS) of spray‐dried granules. The evolution of morphologies of pores and defects, which control the mechanical strength, is investigated by using synchrotron X‐ray multiscale tomography during SPS of alumina granules at 1300 °C. While large defects arising from the hierarchical granule packing structure cannot be removed by pressureless sintering, crack‐like defects and branched rodlike defects are almost eliminated by SPS at stresses higher than 30 and 50 MPa, respectively. But, small ellipsoidal porous regions, which may arise from aggregates or dimples of granules, cannot be removed even at a pressure of 50 MPa. A very large defect is also found by using micro‐CT. It is supposed that this defect is formed from a large void in loosely packed granules. The shrinkage of large voids and the elimination of crack‐like defects are explained by the theoretical prediction based on the continuum theory of sintering.
- 1 March 2023
- Published by Wiley in Advanced Engineering Materials
- Vol. 25 (18)
Open Access3D Visualization of Morphological Evolution of Large Defects during Spark Plasma Sintering of Alumina Granules
The mechanical reliability of products must be assured for scaling up and production of complex‐shaped components by spark plasma sintering (SPS) of spray‐dried granules. The evolution of morphologies of pores and defects, which control the mechanical strength, is investigated by using synchrotron X‐ray multiscale tomography during SPS of alumina granules at 1300 °C. While large defects arising from the hierarchical granule packing structure cannot be removed by pressureless sintering, crack‐like defects and branched rodlike defects are almost eliminated by SPS at stresses higher than 30 and 50 MPa, respectively. But, small ellipsoidal porous regions, which may arise from aggregates or dimples of granules, cannot be removed even at a pressure of 50 MPa. A very large defect is also found by using micro‐CT. It is supposed that this defect is formed from a large void in loosely packed granules. The shrinkage of large voids and the elimination of crack‐like defects are explained by the theoretical prediction based on the continuum theory of sintering.
- Open Access
- 14 October 2022
- Published by Elsevier in Journal of the European Ceramic Society
- Vol. 43 (2) , 486-492
Heterogeneities and defects in powder compacts and sintered alumina bodies visualized by using the synchrotron X-ray CT
- 14 October 2022
- Published by Elsevier in Journal of the European Ceramic Society
- Vol. 43 (2) , 486-492
Open AccessHeterogeneities and defects in powder compacts and sintered alumina bodies visualized by using the synchrotron X-ray CT
- 18 April 2022
- Published by Springer Nature in Journal of Materials Science
- Vol. 57 (16) , 7767-7777
Fabrication, microstructure, and mechanical properties of all-oxide ceramic matrix composites using high-yield precursors
- 18 April 2022
- Published by Springer Nature in Journal of Materials Science
- Vol. 57 (16) , 7767-7777
Fabrication, microstructure, and mechanical properties of all-oxide ceramic matrix composites using high-yield precursors
- Open Access
- 10 March 2021
- Published by Wiley in International Journal of Ceramic Engineering & Science
- Vol. 3 (3) , 140-149
Optical imaging of surface strain distribution up to 1500°C: Development of micro‐speckle pattern
Micro‐speckle patterns were fabricated using α‐Al2O3 and SiC micro‐particles for in‐plane strain distribution measurement at temperatures up to 1500°C using an ultraviolet high‐temperature observation system (UV‐HTOS) combined with a digital image correlation (DIC) technique. The experimental results showed that the measured mean surface strains of α‐Al2O3 were in good agreement with the calculated values obtained from thermal expansion coefficient and temperature difference. The proposed speckle pattern could be used for strain distribution measurement without degradation even after heating up to 1500°C. The results also demonstrated that the pattern fabricated in this study is effective to understand the heterogeneous deformation mechanism in composite materials applied in high‐temperature structural components.
- 10 March 2021
- Published by Wiley in International Journal of Ceramic Engineering & Science
- Vol. 3 (3) , 140-149
Open AccessOptical imaging of surface strain distribution up to 1500°C: Development of micro‐speckle pattern
Micro‐speckle patterns were fabricated using α‐Al2O3 and SiC micro‐particles for in‐plane strain distribution measurement at temperatures up to 1500°C using an ultraviolet high‐temperature observation system (UV‐HTOS) combined with a digital image correlation (DIC) technique. The experimental results showed that the measured mean surface strains of α‐Al2O3 were in good agreement with the calculated values obtained from thermal expansion coefficient and temperature difference. The proposed speckle pattern could be used for strain distribution measurement without degradation even after heating up to 1500°C. The results also demonstrated that the pattern fabricated in this study is effective to understand the heterogeneous deformation mechanism in composite materials applied in high‐temperature structural components.
- Open Access
Determining Interface Fracture Toughness in Multi Layered Environmental Barrier Coatings with Laser Textured Silicon Bond Coat
In the high temperature combustion atmosphere inside of aircraft turbines, the currently used ceramic matrix composites require a protective environmental barrier coating (EBC) to mitigate corrosion of the turbine parts. Besides thermomechanical and thermochemical properties like matching thermal expansion coefficient (CTE) and a high resistance against corrosive media, mechanical properties like a high adhesion strength are also necessary for a long lifetime of the EBC. In the present work, the adhesion between an air plasma sprayed silicon bond coat and a vacuum plasma sprayed ytterbium disilicate topcoat was aimed to be enhanced by a laser surface structuring of the Si bond coat. An increase in interface toughness was assumed, since the introduction of structures would lead to an increased mechanical interlocking at the rougher bond coat interface. The interface toughness was measured by a new testing method, which allows the testing of specific interfaces. The results demonstrate a clear increase of the toughness from an original bond coat/topcoat interface (8.6 J/m2) compared to a laser structured interface (14.7 J/m2). Observations in the crack propagation indicates that the laser structuring may have led to a strengthening of the upper bond coat area by sintering. Furthermore, in addition to cohesive failure components, adhesive components can also be observed, which could have influenced the determined toughness.
Open AccessDetermining Interface Fracture Toughness in Multi Layered Environmental Barrier Coatings with Laser Textured Silicon Bond Coat
In the high temperature combustion atmosphere inside of aircraft turbines, the currently used ceramic matrix composites require a protective environmental barrier coating (EBC) to mitigate corrosion of the turbine parts. Besides thermomechanical and thermochemical properties like matching thermal expansion coefficient (CTE) and a high resistance against corrosive media, mechanical properties like a high adhesion strength are also necessary for a long lifetime of the EBC. In the present work, the adhesion between an air plasma sprayed silicon bond coat and a vacuum plasma sprayed ytterbium disilicate topcoat was aimed to be enhanced by a laser surface structuring of the Si bond coat. An increase in interface toughness was assumed, since the introduction of structures would lead to an increased mechanical interlocking at the rougher bond coat interface. The interface toughness was measured by a new testing method, which allows the testing of specific interfaces. The results demonstrate a clear increase of the toughness from an original bond coat/topcoat interface (8.6 J/m2) compared to a laser structured interface (14.7 J/m2). Observations in the crack propagation indicates that the laser structuring may have led to a strengthening of the upper bond coat area by sintering. Furthermore, in addition to cohesive failure components, adhesive components can also be observed, which could have influenced the determined toughness.
- Open Access
Crack Initiation Criteria in EBC under Thermal Stress
For design of multi-layered environmental barrier coatings (EBCs), it is essential to assure mechanical reliability against interface crack initiation and propagation induced by thermal stress owing to a misfit of the coefficients of thermal expansion between the coating layers and SiC/SiC substrate. We conducted finite element method (FEM) analyses to evaluate energy release rate (ERR) for interface cracks and performed experiment to obtain interface fracture toughness to assess mechanical reliability of an EBC with a function of thermal barrier (T/EBC; SiC/SiAlON/mullite/Yb-silicate gradient composition layer/Yb2SiO5 with porous segment structure) on an SiC/SiC substrate under thermal stress due to cooling in fabrication process. Our FEM analysis revealed that a thinner SiAlON layer and a thicker mullite layer are most suitable to reduce ERRs for crack initiation at the SiC/SiAlON, SiAlON/mullite and mullite/Yb2Si2O7 interfaces. Interface fracture tests of the T/EBC with layer thicknesses within the proposed range exhibited fracture at the SiC/SiAlON and SiAlON/mullite interfaces. We also estimated the approximate fracture toughness for the SiC/SiAlON and SiAlON/mullite interfaces and lower limit of fracture toughness for the mullite/Yb2Si2O7 interface. Comparison between ERR and fracture toughness indicates that the fabricated T/EBC possesses sufficient mechanical reliability against interface crack initiation and propagation.
Open AccessCrack Initiation Criteria in EBC under Thermal Stress
For design of multi-layered environmental barrier coatings (EBCs), it is essential to assure mechanical reliability against interface crack initiation and propagation induced by thermal stress owing to a misfit of the coefficients of thermal expansion between the coating layers and SiC/SiC substrate. We conducted finite element method (FEM) analyses to evaluate energy release rate (ERR) for interface cracks and performed experiment to obtain interface fracture toughness to assess mechanical reliability of an EBC with a function of thermal barrier (T/EBC; SiC/SiAlON/mullite/Yb-silicate gradient composition layer/Yb2SiO5 with porous segment structure) on an SiC/SiC substrate under thermal stress due to cooling in fabrication process. Our FEM analysis revealed that a thinner SiAlON layer and a thicker mullite layer are most suitable to reduce ERRs for crack initiation at the SiC/SiAlON, SiAlON/mullite and mullite/Yb2Si2O7 interfaces. Interface fracture tests of the T/EBC with layer thicknesses within the proposed range exhibited fracture at the SiC/SiAlON and SiAlON/mullite interfaces. We also estimated the approximate fracture toughness for the SiC/SiAlON and SiAlON/mullite interfaces and lower limit of fracture toughness for the mullite/Yb2Si2O7 interface. Comparison between ERR and fracture toughness indicates that the fabricated T/EBC possesses sufficient mechanical reliability against interface crack initiation and propagation.
- 31 October 2018
- Published by Springer Nature in Journal of Materials Science
- Vol. 54 (4) , 2824-2835
In situ observation and strain distribution measurements of atmospheric plasma-sprayed mullite and Si multilayered coatings on SiC substrates
- 31 October 2018
- Published by Springer Nature in Journal of Materials Science
- Vol. 54 (4) , 2824-2835
In situ observation and strain distribution measurements of atmospheric plasma-sprayed mullite and Si multilayered coatings on SiC substrates
- 15 October 2010
- Published by Elsevier in Materials Science and Engineering: B
- Vol. 173 (1-3) , 94-98
Room temperature fabrication of SiO2/polyacrylic ester multilayer composites by spin-coating
- 15 October 2010
- Published by Elsevier in Materials Science and Engineering: B
- Vol. 173 (1-3) , 94-98
Room temperature fabrication of SiO2/polyacrylic ester multilayer composites by spin-coating