Joseph R. Kish
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Joseph R. Kish has a total of 114 co-authors. Here are the top co-authors by number of shared publications:
S. Shankar
3 shared publicationsY. Zeng
**Natural Resources Canada, CanmetMATERIALS 183 Longwood Rd S, Hamilton, Canada Ontario L8P 0A5
3 shared publications- Alejandro Daniel González
Nemak Monterrey
2 shared publications - Anthony Lombardi
Nemak USA/Canada
2 shared publications C. F. Glover
Swansea University
2 shared publicationsE.K. Asare
Centre for Automotive Materials and Corrosion, McMaster University, 1280 Main St. W, Hamilton, Ontario, Canada L8S 4L8
2 shared publications
Latest Publications
- Open Access
- 22 October 2026
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 173 (20) , 201502
Localized Corrosion Susceptibility of Hypoeutectic Al–Ce Alloy Castings
Hypoeutectic Al–Ce alloys provide improved mechanical strength retention at elevated temperatures relative to other Al alloy cast alloys. However, broader applications, particularly those related to automotive assembly, require demonstrated aqueous corrosion performance. The purpose of this work was to determine the localized corrosion susceptibility of a hypoeutectic Al-6Ce alloy, relative to a hypoeutectic Al–Si alloy (A356), in NaCl (aq). Conventional electrochemical polarization and bulk immersion (ASTM G110) testing, coupled with scanning electron microscopy were used for this purpose. The Al-6Ce alloy exhibited significantly lower localized corrosion susceptibility as determined by ASTM G110 testing. Electrochemical polarization measurements reveal that the lower susceptibility is likely related to the micro-galvanic coupling between the anodic Al 11 Ce 3 eutectic phase and the adjacent cathodic primary Al dendritic phase, which is not sufficiently polarizing to induce passivity breakdown of the anodic Al 11 Ce 3 eutectic phase. The implications of the results are discussed within the context of materials performance in automotive applications.
- 22 October 2026
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 173 (20) , 201502
Open AccessLocalized Corrosion Susceptibility of Hypoeutectic Al–Ce Alloy Castings
Hypoeutectic Al–Ce alloys provide improved mechanical strength retention at elevated temperatures relative to other Al alloy cast alloys. However, broader applications, particularly those related to automotive assembly, require demonstrated aqueous corrosion performance. The purpose of this work was to determine the localized corrosion susceptibility of a hypoeutectic Al-6Ce alloy, relative to a hypoeutectic Al–Si alloy (A356), in NaCl (aq). Conventional electrochemical polarization and bulk immersion (ASTM G110) testing, coupled with scanning electron microscopy were used for this purpose. The Al-6Ce alloy exhibited significantly lower localized corrosion susceptibility as determined by ASTM G110 testing. Electrochemical polarization measurements reveal that the lower susceptibility is likely related to the micro-galvanic coupling between the anodic Al 11 Ce 3 eutectic phase and the adjacent cathodic primary Al dendritic phase, which is not sufficiently polarizing to induce passivity breakdown of the anodic Al 11 Ce 3 eutectic phase. The implications of the results are discussed within the context of materials performance in automotive applications.
- 9 January 2026
- Published by Springer Nature in JOM
- Vol. 78 (4) , 3228-3239
Towards Controlling Corrosion of Structural Alloys for Molten Salt Reactors with Surface Modifications
- 9 January 2026
- Published by Springer Nature in JOM
- Vol. 78 (4) , 3228-3239
Towards Controlling Corrosion of Structural Alloys for Molten Salt Reactors with Surface Modifications
- Open Access
- 25 November 2025
- Published by Elsevier in Corrosion Science
- Vol. 259
Oxygen-accelerated corrosion of Alloy 800 in a molten LiCl-KCl-MgCl2 eutectic mixture
- 25 November 2025
- Published by Elsevier in Corrosion Science
- Vol. 259
Open AccessOxygen-accelerated corrosion of Alloy 800 in a molten LiCl-KCl-MgCl2 eutectic mixture
- 1 July 2025
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 172 (8) , 081502
Localized Corrosion Susceptibility of AA7050 Produced by Controlled Diffusion Solidification
Controlled diffusion solidification (CDS) is a process designed to enable net-shape casting of high-strength AA7xxx alloys by mitigating hot tearing during solidification. The objective of this work was to benchmark the localized corrosion susceptibility of AA7050 produced by CDS against the conventional wrought rolled plate counterpart (both in the peak-aged T6 temper). Relative localized corrosion susceptibility was determined by electrochemical polarization measurements and cyclic corrosion testing (ASTM G85 - Annex 2) and rationalized by differences in the microstructure, as revealed by light optical and scanning electron microscopy. The localized corrosion mode was a combination of intergranular corrosion and selective grain attack, with the dominant mode depending on material: selective grain attack for the CDS material (equiaxed grain structure) and intergranular (exfoliation) corrosion for wrought material (elongated grain structure). The presence of large intermetallic particles that decorate grain boundaries, which are cathodic relative to the Al matrix phase, combined with a Cu-depleted zone adjacent to grain boundaries, were implicated as critical factors driving selective grain attack of the CDS material, as observed in the through-thickness direction.
- 1 July 2025
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 172 (8) , 081502
Localized Corrosion Susceptibility of AA7050 Produced by Controlled Diffusion Solidification
Controlled diffusion solidification (CDS) is a process designed to enable net-shape casting of high-strength AA7xxx alloys by mitigating hot tearing during solidification. The objective of this work was to benchmark the localized corrosion susceptibility of AA7050 produced by CDS against the conventional wrought rolled plate counterpart (both in the peak-aged T6 temper). Relative localized corrosion susceptibility was determined by electrochemical polarization measurements and cyclic corrosion testing (ASTM G85 - Annex 2) and rationalized by differences in the microstructure, as revealed by light optical and scanning electron microscopy. The localized corrosion mode was a combination of intergranular corrosion and selective grain attack, with the dominant mode depending on material: selective grain attack for the CDS material (equiaxed grain structure) and intergranular (exfoliation) corrosion for wrought material (elongated grain structure). The presence of large intermetallic particles that decorate grain boundaries, which are cathodic relative to the Al matrix phase, combined with a Cu-depleted zone adjacent to grain boundaries, were implicated as critical factors driving selective grain attack of the CDS material, as observed in the through-thickness direction.
- 22 May 2025
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 81 (7) , 671-681
Selective Oxidation of Fe-Cr-Mn Stainless Steel in Supercritical Water
Oxidation of austenitic Fe-Cr-Mn stainless steel (Nitronic® 32) in supercritical water (25 MPa) was assessed to determine the (i) ability to form a ferrite surface layer from selective oxidation of Mn and (ii) protection provided by the oxide scale. X-ray diffraction and electron microscopy techniques revealed a layered oxide scale forms, complete with a ferrite surface layer within a zone depleted of alloying elements after 500 h at 550°C. While intact during immersion, the oxide spalled during cooling, indicating a sensitivity to thermal stresses. The suitability of Fe-Cr-Mn alloy fuel claddings for the supercritical water-cooled reactor concept is discussed.
- 22 May 2025
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 81 (7) , 671-681
Selective Oxidation of Fe-Cr-Mn Stainless Steel in Supercritical Water
Oxidation of austenitic Fe-Cr-Mn stainless steel (Nitronic® 32) in supercritical water (25 MPa) was assessed to determine the (i) ability to form a ferrite surface layer from selective oxidation of Mn and (ii) protection provided by the oxide scale. X-ray diffraction and electron microscopy techniques revealed a layered oxide scale forms, complete with a ferrite surface layer within a zone depleted of alloying elements after 500 h at 550°C. While intact during immersion, the oxide spalled during cooling, indicating a sensitivity to thermal stresses. The suitability of Fe-Cr-Mn alloy fuel claddings for the supercritical water-cooled reactor concept is discussed.
- 22 November 2024
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 81 (2) , 109-121
Corrosion of Surface-Treated Type 304 Stainless Steel in Alkaline Subcritical Water
Surface treatment can reduce corrosion of stainless steel in hot-pressurized (subcritical/supercritical) water and, thus is being considered to control corrosion of austenitic stainless steel Type 304 (Fe-18Cr-8Ni) for application to hydrothermal liquefaction (HTL) conversion of biomass. Typical HTL conversion processes involve hot (250°C to 374°C), pressurized (4 MPa to 22 MPa) subcritical water as the conversion medium with the addition of a homogenous alkaline catalyst. The objective of this research was to determine the relative extent to which well-established surface treatments could reduce corrosion of Type 304 in simulated HTL alkaline water, with the chromia-forming Alloy 33 (Fe-33Cr-32Ni) serving as a comparative baseline. Surface treatments examined include grinding, shot peening, sandblasting, and chemical pickling. Corrosion was assessed using gravimetric measurements made after 10 d of immersion in simulated HTL alkaline water at 310°C and 10 MPa in a static autoclave test system. Analysis of the starting (preimmersion) and corroded (postimmersion) surfaces was conducted using a variety of surface characterization techniques. None of the surface treatments reduced corrosion of Type 304, relative to the mechanically-ground surface, despite achieving the desired outcomes before and during immersion. Alloy 33 is less susceptible to corrosion than Type 304 due to the formation of a more protective Cr2O3 sublayer at the oxide/metal interface.
- 22 November 2024
- Published by Association for Materials Protection and Performance (AMPP) in Corrosion
- Vol. 81 (2) , 109-121
Corrosion of Surface-Treated Type 304 Stainless Steel in Alkaline Subcritical Water
Surface treatment can reduce corrosion of stainless steel in hot-pressurized (subcritical/supercritical) water and, thus is being considered to control corrosion of austenitic stainless steel Type 304 (Fe-18Cr-8Ni) for application to hydrothermal liquefaction (HTL) conversion of biomass. Typical HTL conversion processes involve hot (250°C to 374°C), pressurized (4 MPa to 22 MPa) subcritical water as the conversion medium with the addition of a homogenous alkaline catalyst. The objective of this research was to determine the relative extent to which well-established surface treatments could reduce corrosion of Type 304 in simulated HTL alkaline water, with the chromia-forming Alloy 33 (Fe-33Cr-32Ni) serving as a comparative baseline. Surface treatments examined include grinding, shot peening, sandblasting, and chemical pickling. Corrosion was assessed using gravimetric measurements made after 10 d of immersion in simulated HTL alkaline water at 310°C and 10 MPa in a static autoclave test system. Analysis of the starting (preimmersion) and corroded (postimmersion) surfaces was conducted using a variety of surface characterization techniques. None of the surface treatments reduced corrosion of Type 304, relative to the mechanically-ground surface, despite achieving the desired outcomes before and during immersion. Alloy 33 is less susceptible to corrosion than Type 304 due to the formation of a more protective Cr2O3 sublayer at the oxide/metal interface.
- 19 November 2024
- Published by Springer Nature
- p. 529-532
An Accelerated Bulk Immersion Surrogate for ASTM B117 Corrosion Testing for Secondary A356-T6 (AlSi7Mg0.3) Al Alloy Low-Pressure Die Castings
- 19 November 2024
- Published by Springer Nature
- p. 529-532
An Accelerated Bulk Immersion Surrogate for ASTM B117 Corrosion Testing for Secondary A356-T6 (AlSi7Mg0.3) Al Alloy Low-Pressure Die Castings
- 19 November 2024
- Published by Springer Nature
- p. 561-565
Corrosion of Extruded Mg Alloys: Effect of Major Alloying Elements
- 19 November 2024
- Published by Springer Nature
- p. 561-565
Corrosion of Extruded Mg Alloys: Effect of Major Alloying Elements
- 19 November 2024
- Published by Springer Nature
- p. 435-438
Effect of Zn Content on Corrosion of As-Cast Al-Fe-Zn-Mg Dilute Eutectic Alloys for Automotive Applications
- 19 November 2024
- Published by Springer Nature
- p. 435-438
Effect of Zn Content on Corrosion of As-Cast Al-Fe-Zn-Mg Dilute Eutectic Alloys for Automotive Applications