Vijay Petley
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Vijay Petley has a total of 35 co-authors. Here are the top co-authors by number of shared publications:
- Shweta Verma
Gas Turbine Research Establishment (GTRE)
5 shared publications - Ranjiitkumar Rajendran
BARC Facilities, Kalpakkam 603 102, India
3 shared publications Shweta Verma
Gas Turbine Research Establishment (GTRE)
3 shared publications- Venkatakrishnan Balasubramanian
Annamalai University
3 shared publications - C. Mukundhan
Centre for Materials Joining and Research (CEMAJOR), Department of Manufacturing Engineering, Annamalai University, Annamalai Nagar, Chidambaram 608002, Tamil Nadu, India
2 shared publications K.H. Thulasi Raman
2 shared publications
Latest Publications
- 15 October 2023
- Published by Springer Nature
- p. 275-285
Rotary Friction Welding of Cast Nickel Base Superalloy with Martensitic Stainless Steel for Aero Engine Application
- 15 October 2023
- Published by Springer Nature
- p. 275-285
Rotary Friction Welding of Cast Nickel Base Superalloy with Martensitic Stainless Steel for Aero Engine Application
- Open Access
- 24 September 2022
- Published by Wiley in Advances in Materials Science and Engineering
- Vol. 2022, 1-10
Microstructural Features, Tensile Properties, and Impact Toughness of Linear Friction Welded High-Temperature Alloy Joints for Blisk Assembly Applications
The main objective of this investigation is to analyze the microstructure, tensile properties, and impact toughness of Ti6Al4V alloy joints developed using optimized parameters of linear friction welding (LFW) for gas turbine blisk assembly applications. The 6mm thick plates of Ti6Al4V alloy were joined using a friction time of 40sec, a friction pressure of 20MPa, a forging pressure of 10MPa, a forging time of 3sec, and an oscillating frequency of 14Hz. The different regions of joints were analyzed using a stereo zoom microscope. Optical and scanning electron microscope (SEM) was used for analysing the microstructural features of joints. The room temperature tensile properties, hardness, and impact toughness of LFW-Ti6Al4V alloy joints were evaluated and correlated to the microstructural features of weld region. The fractured sections of tensile and impact toughness specimens of joints were analyzed using SEM and the failure of joints was correlated with the hardness survey. Results showed that the LFW-Ti6Al4V alloy joints developed using the optimized parameters exhibited a tensile strength (TS) of 1015MPa, a yield strength (YS) of 940MPa, and an elongation (EL) of 8. The joints revealed 98.54, 95.91, and 66.67 of tensile strength, yield strength, and ductility of the parent metal. The LFW joints disclosed impact toughness (IT) of 17.2J which is 89.77 impact toughness of the parent metal. The superior tensile properties and impact toughness of LFW-Ti6Al4V alloy joints are mainly attributed to a greater degree of refinement of α+β grains in the weld interface, which offers greater resistance to tensile deformation and crack propagation.
- 24 September 2022
- Published by Wiley in Advances in Materials Science and Engineering
- Vol. 2022, 1-10
Open AccessMicrostructural Features, Tensile Properties, and Impact Toughness of Linear Friction Welded High-Temperature Alloy Joints for Blisk Assembly Applications
The main objective of this investigation is to analyze the microstructure, tensile properties, and impact toughness of Ti6Al4V alloy joints developed using optimized parameters of linear friction welding (LFW) for gas turbine blisk assembly applications. The 6mm thick plates of Ti6Al4V alloy were joined using a friction time of 40sec, a friction pressure of 20MPa, a forging pressure of 10MPa, a forging time of 3sec, and an oscillating frequency of 14Hz. The different regions of joints were analyzed using a stereo zoom microscope. Optical and scanning electron microscope (SEM) was used for analysing the microstructural features of joints. The room temperature tensile properties, hardness, and impact toughness of LFW-Ti6Al4V alloy joints were evaluated and correlated to the microstructural features of weld region. The fractured sections of tensile and impact toughness specimens of joints were analyzed using SEM and the failure of joints was correlated with the hardness survey. Results showed that the LFW-Ti6Al4V alloy joints developed using the optimized parameters exhibited a tensile strength (TS) of 1015MPa, a yield strength (YS) of 940MPa, and an elongation (EL) of 8. The joints revealed 98.54, 95.91, and 66.67 of tensile strength, yield strength, and ductility of the parent metal. The LFW joints disclosed impact toughness (IT) of 17.2J which is 89.77 impact toughness of the parent metal. The superior tensile properties and impact toughness of LFW-Ti6Al4V alloy joints are mainly attributed to a greater degree of refinement of α+β grains in the weld interface, which offers greater resistance to tensile deformation and crack propagation.
- 17 October 2019
- Published by Springer Nature
- p. 741-749
Effect of Holding Time on Microstructural Characteristics and Mechanical Properties of Ti64 Diffusion Bonds
- 17 October 2019
- Published by Springer Nature
- p. 741-749
Effect of Holding Time on Microstructural Characteristics and Mechanical Properties of Ti64 Diffusion Bonds
- 25 February 2017
- Published by Springer Nature in Transactions of the Indian Institute of Metals
- Vol. 70 (3) , 769-774
Evaluation of Metal–Ceramic Composite Joint Under Tensile Loads at Elevated Temperature
- 25 February 2017
- Published by Springer Nature in Transactions of the Indian Institute of Metals
- Vol. 70 (3) , 769-774
Evaluation of Metal–Ceramic Composite Joint Under Tensile Loads at Elevated Temperature
- 1 February 2017
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 695, 2253-2260
Stress evolution mechanism of NiCr thin films on titanium alloy
- 1 February 2017
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 695, 2253-2260
Stress evolution mechanism of NiCr thin films on titanium alloy
- 1 September 2015
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 643, 64-71
Microstructural and mechanical characterization of Ti6Al4V refurbished parts obtained by laser metal deposition
- 1 September 2015
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 643, 64-71
Microstructural and mechanical characterization of Ti6Al4V refurbished parts obtained by laser metal deposition
- 1 June 2015
- Published by Elsevier in Materials Research Bulletin
- Vol. 66, 59-64
Microstructural and mechanical characteristics of Ni–Cr thin films
- 1 June 2015
- Published by Elsevier in Materials Research Bulletin
- Vol. 66, 59-64
Microstructural and mechanical characteristics of Ni–Cr thin films
- 5 December 2013
- Published by ASME International
Weld Ductility Evaluation of Aeroengine Materials by Performing Bend Tests
Welding is an integral part of the fabrication process for realization of the components and sub-components for any structural system. The weld process and the evaluation of the weld zone properties become more significant for the critical application like structural components of an aero engine. Standard tensile testing of the welded specimens provides the ductility for the composite joint i.e. the parent, heat affected zone and the weld zone. Standard bend tests (Three point bend) are specified as the qualitative tests for evaluating the ductility of the welded joints. For these bend tests, the ductility of the parent specimens are utilized for calculating the bend test parameters and the bend angles are specified after performing the tests on the parent specimens. But during the bend tests on the TIG welded specimens of specific materials and the thickness combinations like Ti-64 with thickness of 1.2 and 4.0 mm, it was observed that the specimens used to get fractured during bend tests before the specified bend angle is achieved. Though this suggests that the ductility of the welded joint is lesser than that of the parent specimens, it is not quantified with the premature failure of the test specimen. In the present study, bend tests on these material samples are performed on TIG welded specimens. Load and the displacement were monitored during the bend tests and maximum plunger depth and bend angle was recorded. A term called virtual plunger diameter is introduced in this work. Based on this plunger depth, span length, virtual plunger diameter is estimated at the onset of the fracture. From this plunger diameter the ductility of the weld joint is recalculated and is found to be lesser than the ductility of the welded joint as observed during the tensile test. The proposed bend test result analysis technique provides the quantitative results i.e. weld ductility from the bend test data.
- 5 December 2013
- Published by ASME International
Weld Ductility Evaluation of Aeroengine Materials by Performing Bend Tests
Welding is an integral part of the fabrication process for realization of the components and sub-components for any structural system. The weld process and the evaluation of the weld zone properties become more significant for the critical application like structural components of an aero engine. Standard tensile testing of the welded specimens provides the ductility for the composite joint i.e. the parent, heat affected zone and the weld zone. Standard bend tests (Three point bend) are specified as the qualitative tests for evaluating the ductility of the welded joints. For these bend tests, the ductility of the parent specimens are utilized for calculating the bend test parameters and the bend angles are specified after performing the tests on the parent specimens. But during the bend tests on the TIG welded specimens of specific materials and the thickness combinations like Ti-64 with thickness of 1.2 and 4.0 mm, it was observed that the specimens used to get fractured during bend tests before the specified bend angle is achieved. Though this suggests that the ductility of the welded joint is lesser than that of the parent specimens, it is not quantified with the premature failure of the test specimen. In the present study, bend tests on these material samples are performed on TIG welded specimens. Load and the displacement were monitored during the bend tests and maximum plunger depth and bend angle was recorded. A term called virtual plunger diameter is introduced in this work. Based on this plunger depth, span length, virtual plunger diameter is estimated at the onset of the fracture. From this plunger diameter the ductility of the weld joint is recalculated and is found to be lesser than the ductility of the welded joint as observed during the tensile test. The proposed bend test result analysis technique provides the quantitative results i.e. weld ductility from the bend test data.
- 1 November 2013
- Published by Elsevier in Scripta Materialia
- Vol. 69 (9) , 698-701
Strain-controlled fatigue in B-modified Ti–6Al–4V alloys
- 1 November 2013
- Published by Elsevier in Scripta Materialia
- Vol. 69 (9) , 698-701
Strain-controlled fatigue in B-modified Ti–6Al–4V alloys