Dapeng Liu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Dapeng Liu has a total of 46 co-authors. Here are the top co-authors by number of shared publications:
Chenguang Liu
China University of Petroleum (East China), Qingdao 266580, P. R. China
3 shared publicationsAnjie Wang
2 shared publications- Hongjie Zhang
University of Science and Technology of China
2 shared publications Jiangman Zhen
State Key Laboratory of Rare Earth Resource Utilization, Changchun Institute of Applied Chemistry, Chinese Academy of Sciences, Changchun 130022, China
2 shared publicationsRoel Prins
2 shared publicationsAiwen Qin
State Key Lab for Modification of Chemical Fibers and Polymer Materials College of Material Science & Engineering Donghua University, Shanghai 201620, P. R. China
1 shared publication
Latest Publications
- 24 June 2022
- Published by Royal Society of Chemistry (RSC) in Inorganic Chemistry Frontiers
- Vol. 9 (16) , 4216-4224
Rapid “self-healing” behavior induced by chloride anions to renew the Fe–Ni(oxy)hydroxide surface for long-term alkaline seawater electrolysis
Due to the surface adsorption and interlayer insertion behavior of chloride anions, the Fe–Ni(oxy)hydroxide catalytic surface is easily destroyed, making it difficult to be used for long-term seawater electrolysis. Here, we developed a time- and labor-saving rapid surface reconstruction assisted by a directional anodic corrosion strategy to in situ construct a chrysanthemum shaped active catalytic layer of Fe–Ni(oxy)hydroxide used for seawater electrolysis on the surface of commercial self-supported metal materials. The purpose of the initial artificial anodic corrosion process is to directionally control the rapid corrosion of Fe on the surface of Fe–Ni foam to form a relatively stable Ni-rich structure, which can act as the host of Fe* (Fe* or Ni* represent surface active species of high-valence generated by the oxidation activation) redeposition to slow down the loss of active Fe*. Due to the special structure of the Fe–Ni(oxy)hydroxide catalytic layer tightly loaded on the surface of the Fe–Ni alloy, during the later stability test in natural seawater, the Cl− corrosion can accelerate the surface reconstruction of Fe–Ni(oxy)hydroxide to cause “rapid self-healing”, which is not only conducive to the regular renewal of the catalytic layer, but can prolong the stability of its resistance to seawater electrolysis. Eventually, the sample prepared by anodic corrosion and electrochemical reconstruction (named AC-FeNi(O)OH) only required 252 mV of low overpotential to provide a current density of 100 mA cm−2, and also tolerated over 100 hours in alkaline brine and natural seawater.
- 24 June 2022
- Published by Royal Society of Chemistry (RSC) in Inorganic Chemistry Frontiers
- Vol. 9 (16) , 4216-4224
Rapid “self-healing” behavior induced by chloride anions to renew the Fe–Ni(oxy)hydroxide surface for long-term alkaline seawater electrolysis
Due to the surface adsorption and interlayer insertion behavior of chloride anions, the Fe–Ni(oxy)hydroxide catalytic surface is easily destroyed, making it difficult to be used for long-term seawater electrolysis. Here, we developed a time- and labor-saving rapid surface reconstruction assisted by a directional anodic corrosion strategy to in situ construct a chrysanthemum shaped active catalytic layer of Fe–Ni(oxy)hydroxide used for seawater electrolysis on the surface of commercial self-supported metal materials. The purpose of the initial artificial anodic corrosion process is to directionally control the rapid corrosion of Fe on the surface of Fe–Ni foam to form a relatively stable Ni-rich structure, which can act as the host of Fe* (Fe* or Ni* represent surface active species of high-valence generated by the oxidation activation) redeposition to slow down the loss of active Fe*. Due to the special structure of the Fe–Ni(oxy)hydroxide catalytic layer tightly loaded on the surface of the Fe–Ni alloy, during the later stability test in natural seawater, the Cl− corrosion can accelerate the surface reconstruction of Fe–Ni(oxy)hydroxide to cause “rapid self-healing”, which is not only conducive to the regular renewal of the catalytic layer, but can prolong the stability of its resistance to seawater electrolysis. Eventually, the sample prepared by anodic corrosion and electrochemical reconstruction (named AC-FeNi(O)OH) only required 252 mV of low overpotential to provide a current density of 100 mA cm−2, and also tolerated over 100 hours in alkaline brine and natural seawater.
- 27 July 2020
- Published by American Chemical Society (ACS) in ACS Omega
- Vol. 5 (30) , 19111-19119
Effect of Phosphorus Modification on the Acidity, Nanostructure of the Active Phase, and Catalytic Performance of Residue Hydrodenitrogenation Catalysts
A series of NiMoP(x)-Al catalysts with different phosphorus contents were prepared by the incipient wetness co-impregnation method. The effects of phosphorus modification on the acidity, active phase nanostructure, and catalytic properties of the residue hydrodenitrogenation catalysts were investigated to find the role of phosphorus in the catalytic mechanism. The results of temperature-programmed desorption of NH3 and pyridine IR spectroscopy of the catalysts indicate that phosphorus modification can increase the total acid and Brønsted acid. Transmission electron microscopy analysis shows that phosphorus modification increases the stacking number NA, reduces the slab length LA of the active MoS2 phase, and increases the Mo dispersion fMo, leading to the promotion of the sulfidation degree of the active Mo phase and thus increasing the denitrification rate. The catalyst with a 3.4 wt % P2O5 loading shows the highest Brønsted/Lewis acid ratio, the largest amount of three-layer active phases, the smallest LA, the highest fMo, the optimal sulfurization degree, and the highest denitrification rate, 63.6%, indicating the correlation between the nanostructure of the active phase and its catalytic property because of the addition of phosphorus.
- 27 July 2020
- Published by American Chemical Society (ACS) in ACS Omega
- Vol. 5 (30) , 19111-19119
Effect of Phosphorus Modification on the Acidity, Nanostructure of the Active Phase, and Catalytic Performance of Residue Hydrodenitrogenation Catalysts
A series of NiMoP(x)-Al catalysts with different phosphorus contents were prepared by the incipient wetness co-impregnation method. The effects of phosphorus modification on the acidity, active phase nanostructure, and catalytic properties of the residue hydrodenitrogenation catalysts were investigated to find the role of phosphorus in the catalytic mechanism. The results of temperature-programmed desorption of NH3 and pyridine IR spectroscopy of the catalysts indicate that phosphorus modification can increase the total acid and Brønsted acid. Transmission electron microscopy analysis shows that phosphorus modification increases the stacking number NA, reduces the slab length LA of the active MoS2 phase, and increases the Mo dispersion fMo, leading to the promotion of the sulfidation degree of the active Mo phase and thus increasing the denitrification rate. The catalyst with a 3.4 wt % P2O5 loading shows the highest Brønsted/Lewis acid ratio, the largest amount of three-layer active phases, the smallest LA, the highest fMo, the optimal sulfurization degree, and the highest denitrification rate, 63.6%, indicating the correlation between the nanostructure of the active phase and its catalytic property because of the addition of phosphorus.
- 1 December 2019
- Published by Elsevier in Journal of Energy Chemistry
- Vol. 39, 182-187
Facile synthesis of V-doped CoP nanoparticles as bifunctional electrocatalyst for efficient water splitting
- 1 December 2019
- Published by Elsevier in Journal of Energy Chemistry
- Vol. 39, 182-187
Facile synthesis of V-doped CoP nanoparticles as bifunctional electrocatalyst for efficient water splitting
- 1 September 2017
- Published by Elsevier in Catalysis Today
- Vol. 292, 133-142
Ni 2 P/Al 2 O 3 hydrodesulfurization catalysts prepared by separating the nickel compound and hypophosphite
- 1 September 2017
- Published by Elsevier in Catalysis Today
- Vol. 292, 133-142
Ni 2 P/Al 2 O 3 hydrodesulfurization catalysts prepared by separating the nickel compound and hypophosphite
- 13 April 2017
- Published by Royal Society of Chemistry (RSC) in Dalton Transactions
- Vol. 46 (19) , 6366-6378
Disproportionation of hypophosphite and phosphite
31P NMR spectra showing that NaH2PO2 first disproportionates to NaH2PO3, Na2HPO3, Na2H2P2O5 and Na4P2O7, and finally reacts to yield Na5P3O10.
- 13 April 2017
- Published by Royal Society of Chemistry (RSC) in Dalton Transactions
- Vol. 46 (19) , 6366-6378
Disproportionation of hypophosphite and phosphite
31P NMR spectra showing that NaH2PO2 first disproportionates to NaH2PO3, Na2HPO3, Na2H2P2O5 and Na4P2O7, and finally reacts to yield Na5P3O10.
- 1 March 2016
- Published by Elsevier in Catalysis Communications
- Vol. 77, 13-17
Bulk and Al2O3-supported Ni2P HDS catalysts prepared by separating the nickel and hypophosphite sources
- 1 March 2016
- Published by Elsevier in Catalysis Communications
- Vol. 77, 13-17
Bulk and Al2O3-supported Ni2P HDS catalysts prepared by separating the nickel and hypophosphite sources
- 13 July 2015
- Published by Royal Society of Chemistry (RSC) in Physical Chemistry Chemical Physics
- Vol. 17 (34) , 21856-21865
Drawing dependent structures, mechanical properties and cyclization behaviors of polyacrylonitrile and polyacrylonitrile/carbon nanotube composite fibers prepared by plasticized spinning
Drawing to change the structural properties and cyclization behaviors of the polyacrylonitrile (PAN) chains in crystalline and amorphous regions is carried out on PAN and PAN/carbon nanotube (CNT) composite fibers. Various characterization methods including Fourier transform infrared spectroscopy, differential scanning calorimetry, X-ray diffraction and thermal gravimetric analysis are used to monitor the structural evolution and cyclization behaviors of the fibers. With an increase of the draw ratio during the plasticized spinning process, the structural parameters of the fibers, i.e. crystallinity and planar zigzag conformation, are decreased at first, and then increased, which are associated with the heat exchange rate and the oriented-crystallization rate. A possible mechanism for plasticized spinning is proposed to explain the changing trends of crystallinity and planar zigzag conformation. PAN and PAN/CNT fibers exhibit various cyclization behaviors induced by drawing, e.g., the initiation temperature for the cyclization (Ti) of PAN fibers is increased with increasing draw ratio, while Ti of PAN/CNT fibers is decreased. Drawing also facilitates cyclization and lowers the percentage of β-amino nitrile for PAN/CNT fibers during the stabilization.
- 13 July 2015
- Published by Royal Society of Chemistry (RSC) in Physical Chemistry Chemical Physics
- Vol. 17 (34) , 21856-21865
Drawing dependent structures, mechanical properties and cyclization behaviors of polyacrylonitrile and polyacrylonitrile/carbon nanotube composite fibers prepared by plasticized spinning
Drawing to change the structural properties and cyclization behaviors of the polyacrylonitrile (PAN) chains in crystalline and amorphous regions is carried out on PAN and PAN/carbon nanotube (CNT) composite fibers. Various characterization methods including Fourier transform infrared spectroscopy, differential scanning calorimetry, X-ray diffraction and thermal gravimetric analysis are used to monitor the structural evolution and cyclization behaviors of the fibers. With an increase of the draw ratio during the plasticized spinning process, the structural parameters of the fibers, i.e. crystallinity and planar zigzag conformation, are decreased at first, and then increased, which are associated with the heat exchange rate and the oriented-crystallization rate. A possible mechanism for plasticized spinning is proposed to explain the changing trends of crystallinity and planar zigzag conformation. PAN and PAN/CNT fibers exhibit various cyclization behaviors induced by drawing, e.g., the initiation temperature for the cyclization (Ti) of PAN fibers is increased with increasing draw ratio, while Ti of PAN/CNT fibers is decreased. Drawing also facilitates cyclization and lowers the percentage of β-amino nitrile for PAN/CNT fibers during the stabilization.
- Open Access
- 27 February 2015
- Published by Royal Society of Chemistry (RSC) in Chemical Science
- Vol. 6 (5) , 2877-2884
γ-Al 2 O 3 supported Pd@CeO 2 core@shell nanospheres: salting-out assisted growth and self-assembly, and their catalytic performance in CO oxidation
Highly active Pd@CeO 2 core@shell nanospheres with tunable Pd core sizes for catalytic CO oxidation.
- 27 February 2015
- Published by Royal Society of Chemistry (RSC) in Chemical Science
- Vol. 6 (5) , 2877-2884
Open Accessγ-Al 2 O 3 supported Pd@CeO 2 core@shell nanospheres: salting-out assisted growth and self-assembly, and their catalytic performance in CO oxidation
Highly active Pd@CeO 2 core@shell nanospheres with tunable Pd core sizes for catalytic CO oxidation.
- 15 December 2014
- Published by Royal Society of Chemistry (RSC) in Dalton Transactions
- Vol. 44 (5) , 2425-2430
l-Lysine-assisted fabrication of PdxPt1−x/Ni(OH)2 (0 ≤ x ≤ 1) hybrids with composition-dependent catalytic properties
A fast and facile self-assembly method has been developed to deposit 3–5 nm sized PdxPt1−x (0 ≤ x ≤ 1) nanoparticles (NPs) on Ni(OH)2 nanosheets. The biomolecule L-lysine has been used here as the linker to hybridize PdxPt1−x NPs and Ni(OH)2 nanosheets together. The catalytic properties of the obtained PdxPt1−x/Ni(OH)2 hybrids were evaluated by employing the reduction of 4-nitrophenol (4-NP) to 4-aminophenol (4-AP) by NaBH4 as a model reaction. The results reveal that the stability, activity and recyclability of PdxPt1−x NPs have been remarkably enhanced after being supported on Ni(OH)2 nanosheets. Moreover, the influence of the composition of noble metals on the catalytic properties has been studied in depth and Pd0.5Pt0.5/Ni(OH)2 hybrids show the optimal catalytic properties.
- 15 December 2014
- Published by Royal Society of Chemistry (RSC) in Dalton Transactions
- Vol. 44 (5) , 2425-2430
l-Lysine-assisted fabrication of PdxPt1−x/Ni(OH)2 (0 ≤ x ≤ 1) hybrids with composition-dependent catalytic properties
A fast and facile self-assembly method has been developed to deposit 3–5 nm sized PdxPt1−x (0 ≤ x ≤ 1) nanoparticles (NPs) on Ni(OH)2 nanosheets. The biomolecule L-lysine has been used here as the linker to hybridize PdxPt1−x NPs and Ni(OH)2 nanosheets together. The catalytic properties of the obtained PdxPt1−x/Ni(OH)2 hybrids were evaluated by employing the reduction of 4-nitrophenol (4-NP) to 4-aminophenol (4-AP) by NaBH4 as a model reaction. The results reveal that the stability, activity and recyclability of PdxPt1−x NPs have been remarkably enhanced after being supported on Ni(OH)2 nanosheets. Moreover, the influence of the composition of noble metals on the catalytic properties has been studied in depth and Pd0.5Pt0.5/Ni(OH)2 hybrids show the optimal catalytic properties.