ZCZongzhe Cheng

Zongzhe Cheng

*This is an algorithmically generated author record based on publicly available information.

Zongzhe Cheng has a total of 19 co-authors. Here are the top co-authors by number of shared publications:

  • Michael Hanke

    Paul-Drude-Institut für Festkörperelektronik, Leibniz-Institut im Forschungsverbund Berlin e.V. 1 , Hausvogteiplatz 5-7, 10117 Berlin, Germany

    4 shared publications
  • Oliver Bierwagen

    Paul‐Drude‐Institut für Festkörperelektronik Leibniz‐Institut im Forschungsverbund Berlin e.V. Berlin Germany

    4 shared publications
  • Achim Trampert

    Dep Semiconductor Epitaxy, Paul-Drude-Institut fuer Festkoerperelektronik, Hausvogteiplatz 5/7, D-10117 Berlin, Berlin, GERMANY

    2 shared publications
  • Achim Trampert

    Paul-Drude-Institut für Festkörperelektronik, Leibniz-Institut im Forschungsverbund Berlin e.V., Hausvogteiplatz 5-7, 10117 Berlin, Germany

    2 shared publications
  • Georg Hoffmann

    Paul-Drude-Institut für Festkörperelektronik Leibniz-Institut im Forschungsverbund Berlin e. V Hausvogteiplatz 5-7 10117 Berlin Germany

    2 shared publications
  • Oliver Brandt

    Paul-Drude-Institut für Festkörperelektronik

    2 shared publications

Latest Publications

  • Open Access

    Erratum: “Drastically enhanced cation incorporation in the epitaxy of oxides due to formation and evaporation of suboxides from elemental sources” [APL Mater. 9, 111110 (2021)]

    by Georg Hoffmann, Zongzhe Cheng, Oliver Brandt, Oliver Bierwagen

    It was brought to our attention that the modeling according to Eqs. (4) and (5) did not produce the fits shown in Figs. 4 and 6 in the original article.1 Indeed

  • Open Access

    Drastically enhanced cation incorporation in the epitaxy of oxides due to formation and evaporation of suboxides from elemental sources

    by Georg Hoffmann, Zongzhe Cheng, Oliver Brandt, Oliver Bierwagen

    In the molecular beam epitaxy of oxide films, the cation (Sn, Ga) or dopant (Sn) incorporation does not follow the vapor pressure of the elemental metal sources but is enhanced by several orders of magnitude for low source temperatures. Using line-of-sight quadrupole mass spectrometry, we identify the dominant contribution to the total flux emanating from Sn and Ga sources at these temperatures to be due to the unintentional formation and evaporation of the respective suboxides SnO and Ga2O. We quantitatively describe this phenomenon by using a rate-equation model that takes into account the O2 background pressure, the resulting formation of the suboxides via oxidation of the metal source, and their subsequent thermally activated evaporation. As a result, the total flux composed of the metal and the suboxide fluxes exhibits an S-shaped temperature dependence instead of the expected linear one in an Arrhenius plot, which is in excellent agreement with the available experimental data. Our model reveals that the thermally activated regimes at low and high temperatures are almost exclusively due to suboxide and metal evaporation, respectively, joined by an intermediate plateau-like regime in which the flux is limited by the available amount of O2. An important suboxide contribution is expected for all elemental sources whose suboxide exhibits a higher vapor pressure than that of the element, such as B, Ga, In, La, Si, Ge, Sn, Sb, Mo, Nb, Ru, Ta, V, and W. This contribution can play a decisive role in the molecular beam epitaxy of oxides, including multicomponent or complex oxides, from elemental sources. Finally, our model predicts suboxide-dominated growth in low-pressure chemical vapor deposition of Ga2O3 and In2O3.


  • Open Access

    Plasma-assisted molecular beam epitaxy of NiO on GaN(00.1)

    by Melanie Budde, Thilo Remmele, Carsten Tschammer, Johannes Feldl, Philipp Franz, Jonas Lähnemann, Zongzhe Cheng, Michael Hanke, Manfred Ramsteiner, Martin Albrecht, et al.

    The growth of NiO on GaN(00.1) substrates by plasma-assisted molecular beam epitaxy under oxygen-rich conditions was investigated at growth temperatures between 100 ° C and 850 ° C . Epitaxial growth of NiO(111) with two rotational domains, with epitaxial relation NiO ( 1 1 ¯ 0 ) ‖ GaN ( 11.0 ) and NiO ( 10 1 ¯ ) ‖ GaN ( 11.0 ) , was observed by X-ray diffraction and confirmed by in situ reflection high-energy electron diffraction as well as transmission electron microscopy (TEM) and electron backscatter diffraction. With respect to the high lattice mismatch of 8.1% and a measured low residual tensile layer strain, growth by lattice matching epitaxy or domain-matching epitaxy is discussed. The morphology measured by atomic force microscopy showed a grainy surface, probably arising from the growth by columnar rotational domains visible in TEM micrographs. The domain sizes measured by AFM and TEM increase with the growth temperature, indicating an increasing surface diffusion length. Growth at 850 ° C , however, involved local decomposition of the GaN substrate that leads to an interfacial β - Ga 2 O 3 ( 2 ¯ 01 ) layer and a high NiO surface roughness. Raman measurements of the quasiforbidden one-phonon peak indicate increasing layer quality (decreasing defect density) with increasing growth temperature.


  • Open Access

    Lattice matched Volmer–Weber growth of Fe3Si on GaAs(001)—the influence of the growth rate

    by B Jenichen, Zongzhe Cheng, Michael Hanke, Jens Herfort, Achim Trampert

    We investigate the formation of lattice matched single-crystalline Fe3Si/GaAs(001) ferromagnet/semiconductor hybrid structures by Volmer–Weber island growth, starting from the epitaxial growth of isolated Fe3Si islands up to the formation of continuous films as a result of island coalescence. We find coherent defect-free layers exhibiting compositional disorder near the Fe3Si/GaAs—interface for higher growth rates, whereas they are fully ordered for lower growth rates.


  • Thermal expansion of single-crystalline β-Ga2O3 from RT to 1200 K studied by synchrotron-based high resolution x-ray diffraction

    by Zongzhe Cheng, Michael Hanke, Zbigniew Galazka, Achim Trampert

    The anisotropic coefficient of thermal expansion for single-crystalline monoclinic β-Ga2O3 has been precisely measured by synchrotron-based high resolution x-ray diffraction in the temperature range from 298 to 1200 K. We derived values along the three main crystallographic directions, based on spacings for (600), (020), and ( 2 ¯ 04 ) lattice planes. αa changes non-linearly between 0.10 × 10–6 K–1 and 2.78 × 10–6 K–1 in the temperature range of 298 to 1200 K, while the values of αb and αc along the further two directions are nearly double. Within the Einstein model, we have numerically modeled the functional dependencies applying a single phonon mode.


  • Growth mode evolution during (100)-oriented β -Ga 2 O 3 homoepitaxy

    by Zongzhe Cheng, Michael Hanke, Zbigniew Galazka, Achim Trampert

    This work focuses on homoepitaxial growth of β -Ga 2 O 3 on (100)-oriented substrates during molecular beam epitaxy. It provides a comprehensive study on the growth mode by combining in situ with ex situ tools. In situ reflection high-energy electron diffraction (RHEED) indicates 2D layer-by-layer mode accompanied by (1 × 1) surface reconstruction. The homoepitaxial layers are grown pseudomorphic with the substrate without in-plane strain as probed by in-plane azimuthal RHEED and out-of-plane synchrotron-based high resolution x-ray diffraction. In contrast to the substrate, stacking faults and twin domains are present in the layer.


  • Phase formation and strain relaxation of Ga2O3 on c-plane and a-plane sapphire substrates as studied by synchrotron-based x-ray diffraction

    by Zongzhe Cheng, Michael Hanke, Patrick Vogt, Oliver Bierwagen, Achim Trampert

    Heteroepitaxial Ga2O3 was deposited on c-plane and a-plane oriented sapphire by plasma-assisted molecular beam epitaxy and probed by ex-situ and in-situ synchrotron-based x-ray diffraction. The investigation on c-plane sapphire determined a critical thickness of around 33 Å, at which the monoclinic β-phase forms on top of the hexagonal α-phase. A 143 Å thick single phase α-Ga2O3 was observed on a-plane sapphire, much thicker than the α-Ga2O3 on c-plane sapphire. The α-Ga2O3 relaxed very fast in the first 30 Å in both out-of-plane and in-plane directions as measured by the in-situ study.