Franz Josef Lanyi
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Franz Josef Lanyi has a total of 13 co-authors. Here are the top co-authors by number of shared publications:
Dirk W. Schubert
Institute of Polymer Materials Friedrich-Alexander-University Erlangen-Nuremberg Martensstraße 7 91058 Erlangen Germany
3 shared publicationsJoachim Kaschta
Institute of Polymer Materials Friedrich-Alexander-University Erlangen-Nuremberg Martensstraße 7 91058 Erlangen Germany
3 shared publications- Dirk Wolfram Schubert
Institute of Polymer Materials, Department of Materials Science, Faculty of Engineering, Friedrich-Alexander University Erlangen-Nürnberg (FAU), Martensstr. 7, 91058 Erlangen, Germany
2 shared publications Nicolai Wenzke
Institute of Polymer Materials Friedrich-Alexander-University Erlangen-Nuremberg Martensstraße 7 91058 Erlangen Germany
2 shared publicationsAnja Goblirsch
1 shared publicationBastian Wölfel
Institute of Polymer Materials, Friedrich-Alexander-University Erlangen-Nuremberg 1, Germany
1 shared publication
Latest Publications
- Open Access
- 31 October 2019
- Published by Wiley in Advanced Engineering Materials
- Vol. 22 (9)
On the Determination of the Enthalpy of Fusion of α‐Crystalline Isotactic Polypropylene Using Differential Scanning Calorimetry, X‐Ray Diffraction, and Fourier‐Transform Infrared Spectroscopy: An Old Story Revisited
The crystallinity determination of polymers using differential scanning calorimetry (DSC) is a standard procedure in industrial and university research. Its value strongly depends on the enthalpy of fusion, which cannot be determined directly using DSC, but must be calibrated using external methods such as X‐ray diffraction (XRD) or density measurements. In addition, the determination of the enthalpy or heat of fusion is not trivial and thus error‐prone; hence, values from 60 to 260 J g−1 are quoted for polypropylene in the literature. It is therefore of great relevance to devise a consistent method to determine the heat of fusion. To determine the heat of fusion for polypropylene, a sample set with a broad range of crystallinities is produced using cooling rates between 1 and ≈3500 K min−1. The melting enthalpy of the samples is determined using DSC measurements. The determination of the melting enthalpy based on XRD measurements is discussed in detail, validated using Fourier‐transform infrared spectroscopy (FTIR), and compared with values quoted in the open literature. Although two different approaches are used to determine the enthalpy of fusion, a value of 170 ± 3 J g−1 is determined.
- 31 October 2019
- Published by Wiley in Advanced Engineering Materials
- Vol. 22 (9)
Open AccessOn the Determination of the Enthalpy of Fusion of α‐Crystalline Isotactic Polypropylene Using Differential Scanning Calorimetry, X‐Ray Diffraction, and Fourier‐Transform Infrared Spectroscopy: An Old Story Revisited
The crystallinity determination of polymers using differential scanning calorimetry (DSC) is a standard procedure in industrial and university research. Its value strongly depends on the enthalpy of fusion, which cannot be determined directly using DSC, but must be calibrated using external methods such as X‐ray diffraction (XRD) or density measurements. In addition, the determination of the enthalpy or heat of fusion is not trivial and thus error‐prone; hence, values from 60 to 260 J g−1 are quoted for polypropylene in the literature. It is therefore of great relevance to devise a consistent method to determine the heat of fusion. To determine the heat of fusion for polypropylene, a sample set with a broad range of crystallinities is produced using cooling rates between 1 and ≈3500 K min−1. The melting enthalpy of the samples is determined using DSC measurements. The determination of the melting enthalpy based on XRD measurements is discussed in detail, validated using Fourier‐transform infrared spectroscopy (FTIR), and compared with values quoted in the open literature. Although two different approaches are used to determine the enthalpy of fusion, a value of 170 ± 3 J g−1 is determined.
- 1 April 2019
- Published by Elsevier in Chemical Engineering Science
- Vol. 197, 11-25
Production of polyamide 11 microparticles for Additive Manufacturing by liquid-liquid phase separation and precipitation
- 1 April 2019
- Published by Elsevier in Chemical Engineering Science
- Vol. 197, 11-25
Production of polyamide 11 microparticles for Additive Manufacturing by liquid-liquid phase separation and precipitation
- 1 October 2018
- Published by Elsevier in Polymer Testing
- Vol. 71, 49-55
A method to reveal bulk and surface crystallinity of Polypropylene by FTIR spectroscopy - Suitable for fibers and nonwovens
- 1 October 2018
- Published by Elsevier in Polymer Testing
- Vol. 71, 49-55
A method to reveal bulk and surface crystallinity of Polypropylene by FTIR spectroscopy - Suitable for fibers and nonwovens
- 28 July 2016
- Published by Wiley in Macromolecular Symposia
- Vol. 365 (1) , 194-202
Novel Chart for Representation of Material Performance and Reliability
Summary: In modern industrial production lines various process and material parameters determine the properties of the final product. Thus, a process optimization procedure has to take into account a large design space containing several parameters. As a consequence, the evaluation of the influence of single process parameters on the final product properties can be quite complicated. Usually a certain property of a product, for example the mechanical strength, has to satisfy a defined specification. In terms of quality control not only the performance of the material but also the reliability of the specified values has to be considered. The Weibull statistic gives an interesting approach to evaluate both, material's performance and reliability. Regarding the mechanical properties e.g. in terms of the stress at break σb the Weibull analysis leads to a characteristic failure constant σb,0 at which 63.2 % of the samples will break. Additionally, the Weibull modulus m can be regarded as a measure for the width of the distribution of the measuring results. High values of m represent a narrow distribution and thus a better reliability. Moreover, the Weibull modulus m is independent of the absolute value of the measuring data. Therefore, it is possible to compare samples produced under different conditions. The standard deviation and the interquartile range are often used to quantify the scatter of empirical data. It is shown within this work that the Weibull modulus m can be a more precise discriminator for the evaluation of the reliability because it is rather stable against outlaying values. As an example this study concentrates on the mechanical properties of melt spun fibres consisting of blends from polypropylenes with different molar masses produced under various process conditions. This work presents a novel chart which allows one to compare different samples on the basis of the Weibull statistics whereat the Weibull modulus m is plotted over σb,0. Defining a reference material, the m‐σb,0‐map can be split into quadrants, whereat each quadrant designates an improvement or worsening of material's performance and reliability with respect to the reference. An evaluation in terms of performance and reliability of great sets of data is easily applicable. It will be shown that the Weibull statistic can also be applied to Young's Modulus, the elongation at break and the tensile energy absorption.
- 28 July 2016
- Published by Wiley in Macromolecular Symposia
- Vol. 365 (1) , 194-202
Novel Chart for Representation of Material Performance and Reliability
Summary: In modern industrial production lines various process and material parameters determine the properties of the final product. Thus, a process optimization procedure has to take into account a large design space containing several parameters. As a consequence, the evaluation of the influence of single process parameters on the final product properties can be quite complicated. Usually a certain property of a product, for example the mechanical strength, has to satisfy a defined specification. In terms of quality control not only the performance of the material but also the reliability of the specified values has to be considered. The Weibull statistic gives an interesting approach to evaluate both, material's performance and reliability. Regarding the mechanical properties e.g. in terms of the stress at break σb the Weibull analysis leads to a characteristic failure constant σb,0 at which 63.2 % of the samples will break. Additionally, the Weibull modulus m can be regarded as a measure for the width of the distribution of the measuring results. High values of m represent a narrow distribution and thus a better reliability. Moreover, the Weibull modulus m is independent of the absolute value of the measuring data. Therefore, it is possible to compare samples produced under different conditions. The standard deviation and the interquartile range are often used to quantify the scatter of empirical data. It is shown within this work that the Weibull modulus m can be a more precise discriminator for the evaluation of the reliability because it is rather stable against outlaying values. As an example this study concentrates on the mechanical properties of melt spun fibres consisting of blends from polypropylenes with different molar masses produced under various process conditions. This work presents a novel chart which allows one to compare different samples on the basis of the Weibull statistics whereat the Weibull modulus m is plotted over σb,0. Defining a reference material, the m‐σb,0‐map can be split into quadrants, whereat each quadrant designates an improvement or worsening of material's performance and reliability with respect to the reference. An evaluation in terms of performance and reliability of great sets of data is easily applicable. It will be shown that the Weibull statistic can also be applied to Young's Modulus, the elongation at break and the tensile energy absorption.