Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Oleksandr Konstantynovskyi has a total of 53 co-authors. Here are the top co-authors by number of shared publications:

  • Pavlo Kryvenko

    Scientific Research Institute for Binders and Materials, Kyiv National University of Construction and Architecture, 03037 Kyiv, Ukraine

    26 shared publications
  • Igor Rudenko

    Scientific Research Institute for Binders and Materials, Kyiv National University of Construction and Architecture, 03037 Kyiv, Ukraine

    25 shared publications
  • Igor Rudenko

    Scientific Research Institute for Binders and Materials, Kyiv National University of Construction and Architecture, 03037 Povitrianykh Syl Avenue, 31, Kyiv, Ukraine

    13 shared publications
  • Oleksandr Gelevera

    Київський національний університет будівництва і архітектури

    5 shared publications
  • Pavlo Kryvenko

    Scientific Research Institute for Binders and Materials, Kyiv National University of Construction and Architecture, 03037 Povitrianykh Syl Avenue, 31, Kyiv, Ukraine

    5 shared publications
  • Oleh Petropavlovskyi

    Kyiv National University of Construction and Architecture

    4 shared publications

Latest Publications

  • Open Access

    Modeling of Basalt Fiber Self-Healing Processes in Aggressive Alkaline Environment of OPC Concrete: The Impact of Metakaolin

    by Pavlo Kryvenko, Igor Rudenko, Oleksandr Gelevera, Oleksandr Konstantynovskyi

    The paper deals with the concept of how to regulate structure formation in the interfacial transition zone (ITZ) between the Ordinary Portland Cement (OPC) matrix and basalt to ensure the durability of basalt fiber-reinforced concretes. It has been demonstrated that the alkali–silica reaction (ASR) can be transformed from a destructive (negative) process into a constructive one in OPC concrete through activation by sodium water glass combined with the incorporation of an Al2O3-containing additive, namely metakaolin. Alkaline activation increased the compressive strength of OPC basalt fiber-reinforced concrete by 1.6–1.9 times. The formation of stable zeolite-like hydration products within the Na2O-CaO-Al2O3-SiO2-H2O system promoted self-healing of the ITZ. This resulted in a 5.6-fold increase in ITZ microhardness compared to the cement matrix, as well as transforming expansion into shrinkage of concrete with a final value of 0.01 mm/m after 360 days. The structure-forming processes in the ITZ ensured a 1.14-fold increase in the compressive strength of 180-day alkali-activated OPC basalt fiber-reinforced concrete compared to its 30-day strength, in contrast to a 0.92-fold decrease in the strength of the non-modified OPC analog under conditions accelerating the development of ASR.

  • Open Access

    High Temperature Resistance of Fly Ash-Enhanced Alkali Activated Portland Cement Mortar: Microstructural Evolution and Strength Retention

    by Pavlo Kryvenko, Igor Rudenko, Oleksandr Konstantynovskyi, Vladyslav Onatii

    The limited high-temperature resistance of Ordinary Portland Cement (OPC) remains a critical challenge for fire-exposed and industrial concrete structures. Its performance deterioration above 500 °C is associated with dehydration and recrystallization of hydration products, leading to structural degradation of the cement matrix. To address this limitation, partial clinker replacement with fly ash combined with sodium water glass activation was proposed to enhance thermal stability. Physico-chemical analysis revealed the absence of portlandite and the formation of C-A-S-H and zeolite-like N–C–A–S–H phases in the fly ash-containing alkali-activated Portland cement. Upon heating, C-A-S-H phases sintered into stable high-temperature calcium aluminosilicate phases and zeolite-like phases underwent topotactic recrystallization into feldspathoid-type structures, preserving matrix integrity at high temperatures. The optimized composition region of cement system (fly ash—12.0–16.5 wt. %, density of water glass—1220–1240 kg/m3) was characterized by residual strength ≥ 50%, while compressive strength at 28 days was ≥80 MPa, exceeding the residual performance typically reported for conventional OPC systems under similar conditions (5–35%). The study was devoted to revealing the potential of low-emission Portland cements in high-temperature-resistant concretes through the utilization of fly ash. The mechanism that controls the compressive strength and temperature resistance of such cements has been demonstrated.


  • Open Access

    The Physico-Chemical Aspects of Enhancing the Fracture Toughness of Rapid-Hardening High Strength Blast Furnace Cement

    by Pavlo Kryvenko, Igor Rudenko, Oleksandr Konstantynovskyi

    This study investigates the influence of the structure formation rate and the morphology of hydration products on the fracture toughness of rapid-hardening high-strength cement matrix. The issue of brittle failure in such cements was demonstrated using blast furnace cement CEM III/C (slag content – 95 wt. %). A complex admixture based on the «glycerol – polyacrylamide» system promoted the early formation of low-calcium silicate hydrates, followed by the polycondensation of polymeric xerogel structures. The mentioned sequence of structure formation processes delayed the setting, promoting the development of a homogeneous structure with stable strength. The increased formation of low-calcium silicate hydrates in the form of fibrous and thin hexagonal structures contributed to the self-reinforcement and densification of the cement matrix. Additionally, the modification led to the formation of compounds analogous to silicon glycerolates, which acted as dampers and supported stress redistribution within the matrix. The enhanced fracture toughness of concrete (compressive strength class C70/85) based on modified alkali-activated CEM III/C, unlike that of the portland cement counterpart, was confirmed by a reduction in the brittleness coefficient to ≤ 8, indicating a transition to ductile failure. This effect was supported by a 39…52 % increase in fracture energy and a 10.7 % improvement in bending deflection under load.

  • Open Access

    OPC/GBFS-Based Alkali-Activated Reactive Powder Concrete: Properties and Age Factor

    by Oleksandr Helevera, Pavlo Kryvenko, Igor Rudenko, Oleksandr Konstantynovskyi

    The development of reactive powder concrete (further, RPC) based on portland cements, containing granulated blast furnace slag (further, GBFS) and activated by soluble sodium silicates, is globally significant in terms of protecting critical infrastructure. Using an activated binder system (further, AAC) made with sodium metasilicate in liquid form, instead of powder, and reducing the OPC content in AAC from 45 wt. % to 5 wt. %, increased the RPC compressive strength from 87.5 MPa to 108.7 MPa at 28 days. Ductile failure at 28 days was confirmed by a brittleness coefficient of 5.3…5.5 and 10.5 % higher impact strength compared to OPC-based analogue. Reducing the OPC content from 45 wt. % to 5 wt. % at a water glass silicate modulus of 2.6…2.7 determined a slight decrease in the early compressive strength of super-rapid-hardening RPC, however, provided a significant increase in compressive strength from 112.5 MPa to 132.4 MPa at 28 days. The ductile failure at 28 days was confirmed by the brittleness coefficient of 5.5…5.9 and 28.7 % higher impact strength compared to analogue made with sodium metasilicate. RPCs with stable long-term strength, and impact strength were obtained

  • Open Access

    The Plasticization of Alkali-Activated Cement System Na2O-CaO-Al2O3-SiO2-H2O: Problems and Decisions

    by Pavlo Kryvenko, Igor Rudenko, Oleksandr Konstantynovskyi

    The paper is devoted to the plasticization mechanisms of alkali-activated cement system Na2O-CaO-Al2O3-SiO2-H2O. The fundamentals and basic factors determining the effectiveness of plasticizing surfactants for alkali-activated cement materials are discussed. The factors under consideration in the study were alkali-activated cement basicity (the content of granulated blast furnace slag), the anion of the alkaline component or activator, and the degree of dispersing of the cement particles in the system. The action effect of plasticizers was determined by finding the interrelation between the stability of its molecular structure, degree of adsorption, and molecular weight depending on mentioned basic factors. A systematic approach to the systematization of surfactants and their choice to be taken into consideration to control technology-related and physico-mechanical properties of alkali-activated cement-based heavyweight concretes, building mortars, and lightened grouts has been proposed.


  • Open Access

    Perspective Chapter: Performance of Geopolymer-Based Coating for Protection of Concrete Surface after Coupling Effect of Wetting-Drying Cycles and Seawater

    by Pavlo Kryvenko, Igor Rudenko, Oleksandr Konstantynovskyi

    In marine structures, the risk of degradation of both the concrete structure and the initiation of corrosion of steel reinforcement is precisely caused by the periodicity of wetting in seawater and drying under the influence of atmospheric CO2. To protect reinforced concrete from the influence of the mentioned ions under coupling exposure classes XS3 and XC4, a coating based on geopolymer of the formula (0,2K2O + 0,8Na2O)·4,5SiO2·Al2O3·nH2O was designed. The effect of the wastes and industrial by-products as the modifying additives on the acceleration of the synthesis of water-resistant zeolite-like matrices of geopolymer at normal temperatures (t = 20 ± 2°С) was studied. The water resistance coefficient of the geopolymer-based mortars was the highest (> 0.9) for both the slaked lime (Ca(OH)2) and aluminum fluoride (AlF3) modifications. The effectiveness of geopolymer-based coatings was confirmed by acceptable changes in water absorption (≤ 1 kg/m2) and adhesion (≤ 23%) after 50 cycles and 200 cycles of wetting in seawater and further drying at t = 105 ± 2°С. Diffusion permeability of Cl−, SO42−-ions into the coatings was to a depth of no more than 1…2 mm, and the coating’s thickness ≥ 2 mm was determined as appropriate value.


  • Open Access

    Reactionary powder concrete based on alkali-activated cement

    by Igor Rudenko, Oleksandr Gelevera, Oleksandr Konstantynovs''KYj, Andrij Razsamakin, Ігор Руденко, Андрій Разсамакін

    The development of reactive powder concretes based on alkali-activated cements for the construction and protection of critical infrastructure is of woldwide importance for improving the safety of their exploitation. The factors influencing the kinetics of strength gain and drying shrinkage of reactive powder concretes using sodium silicate pentahydrate as an alkaline activator were determined.It was shown that increasing the ratio of alkali-activated cement to sand from 1:3 to 1:1 and using the activator in the liquid state increased the concrete strength gain: the compressive strength was 52.3 MPa, 85.0 MPa, 100.6 MPa, and 124.7 MPa at the ages of 1, 3, 28, and 90 days of hardening, respectively. The ratio of compressive strength to flexural strength was 5.3...5.9 at an age of 28 days, indicating a high fracture toughness of the obtained material. An increase in the content of alkali-activated cement in concrete determined a decrease in the influence of sand granulometry on concrete strength,due to its “floating” placement in the cement matrix.The introduction of a fine calcite additive ensured to reduce the shrinkage of concrete by 1.3...1.5 times at an age of 90 days due to the densification of the microstructure and the intensification of crystallisation processes. The implementation of these measures resulted in a high strength alkali-activated cement reactive powder concrete of strength classC80/95, high fracture toughness and reduced drying shrinkage.

  • Open Access

    Development Mix Design Alkali-Activated Cement Powder Concrete

    by Oleksandr Helevera, Andrii Razsamakin, Igor Rudenko, Oleksandr Konstantynovskyi, Volodymyr Smeshko

    The development of reactive powder concretes based on alkali-activated cements for the construction and protection of critical infrastructure is of worldwide importance for improving the safety of their exploitation. The factors influencing the kinetics of strength gain and drying shrinkage of reactive powder concretes using sodium silicate pentahydrate as an alkaline activator were determined. It was shown that increasing the ratio of alkali-activated cement to sand from 1/3 to 1/1 and using the activator in the liquid state increased the concrete strength gain: the compressive strength was 52.3 MPa, 85.0 MPa, 100.6 MPa, and 116.7 MPa at 1, 3, 28, and 90 d. The ratio of compressive strength to flexural strength was in the range of 5.3…5.9 after 28 d, indicating high fracture toughness of the concrete. Higher content of alkali-activated cement caused a decrease in the influence of sand granulometry on concrete strength. This was due to “floating” placement of aggregate in the cement matrix. The introduction of fine calcite as an additive ensured to reduce the shrinkage of concrete by 1.3…1.5 times at 90 d due to the densification of the microstructure and the intensification of crystallization processes. The implementation of these measures resulted in high strength alkali-activated cement reactive powder concrete of strength class C80/95, high fracture toughness, and reduced drying shrinkage.

  • Open Access

    Improvement of Early Strength of Slag Containing Portland Cements

    by Pavlo Kryvenko, Igor Rudenko, Oleksandr Konstantynovskyi, Artem Kovalchuk

    The implementation of alkali-activated Portland cements (or alkali-activated slag cement as per the Ukrainian National Standard DSTU B V.2.7-181:2009) in materials for repair and retrofitting (repair concretes and mortars, shotcrete concretes, reactive powder concretes) is effective is due to their conformity with modern trends in construction. The actuality to produce of alkali-activated Portland cements using the one-part technology causes the application of sodium silicate as the most effective activator in a solid aggregate state. Application of proposed alkali-activated Portland cements in mentioned materials for repair and retrofitting requires finding ways to maximize early strength. The factors affecting early strength were determined using alkali-activated Portland cement based on sodium metasilicate pentahydrate. Modification of alkali-activated Portland cement with a complex additive of the system “surfactant – salt of a strong acid” resulted in an increase in strength from class 42.5 N to 42.5 R due to a reduction in water content and an increase in the crystallization of hydrates. The application of a complex additive also ensured the extension of initial setting time from 30 min up to 40 min and the final setting time – from 40 min to 50 min. An additional increase in the activity of the cement aluminosilicate component was achieved by increasng the specific surface area and introducing nanosilica. The combination of these recipe and technological factors resulted in a rapid-hardening alkali-activated Portland cement with a strength class of 52.5 R.