Mikael Broas
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Mikael Broas has a total of 13 co-authors. Here are the top co-authors by number of shared publications:
Mervi Paulasto-Kröckel
5 shared publications- Vesa Vuorinen
Department of Electrical Engineering and Automation, School of Electrical Engineering, Aalto University, Aalto, Finland
5 shared publications - Timo Sajavaara
Department of Physics, University of Jyväskylä, Jyväskylä, Finland
3 shared publications - Markku Tilli
Laboratory of Physical Metallurgy, Helsinki University of Technology, SF-02150 Espoo, Finland
2 shared publications - Alexander Pyymaki Perros
Nanovate Oy, Micronova, Espoo, Finland
1 shared publication Andreas Graff
Fraunhofer Institute for Microstructure of Materials and Systems IMWS 3 , Walter-Huelse-Str. 1, 06120 Halle, Germany
1 shared publication
Latest Publications
- 1 July 2019
- Published by Elsevier in Thin Solid Films
- Vol. 682, 147-155
In-situ annealing characterization of atomic-layer-deposited Al2O3 in N2, H2 and vacuum atmospheres
- 1 July 2019
- Published by Elsevier in Thin Solid Films
- Vol. 682, 147-155
In-situ annealing characterization of atomic-layer-deposited Al2O3 in N2, H2 and vacuum atmospheres
- 2 October 2017
- Published by AIP Publishing in Applied Physics Letters
- Vol. 111 (14)
Blistering mechanisms of atomic-layer-deposited AlN and Al2O3 films
Blistering of protective, structural, and functional coatings is a reliability risk pestering films ranging from elemental to ceramic ones. The driving force behind blistering comes from either excess hydrogen at the film-substrate interface or stress-driven buckling. Contrary to the stress-driven mechanism, the hydrogen-initiated one is poorly understood. Recently, it was shown that in the bulk Al-Al2O3 system, the blistering is preceded by the formation of nano-sized cavities on the substrate. The stress- and hydrogen-driven mechanisms in atomic-layer-deposited (ALD) films are explored here. We clarify issues in the hydrogen-related mechanism via high-resolution microscopy and show that at least two distinct mechanisms can cause blistering in ALD films.
- 2 October 2017
- Published by AIP Publishing in Applied Physics Letters
- Vol. 111 (14)
Blistering mechanisms of atomic-layer-deposited AlN and Al2O3 films
Blistering of protective, structural, and functional coatings is a reliability risk pestering films ranging from elemental to ceramic ones. The driving force behind blistering comes from either excess hydrogen at the film-substrate interface or stress-driven buckling. Contrary to the stress-driven mechanism, the hydrogen-initiated one is poorly understood. Recently, it was shown that in the bulk Al-Al2O3 system, the blistering is preceded by the formation of nano-sized cavities on the substrate. The stress- and hydrogen-driven mechanisms in atomic-layer-deposited (ALD) films are explored here. We clarify issues in the hydrogen-related mechanism via high-resolution microscopy and show that at least two distinct mechanisms can cause blistering in ALD films.
- Open Access
- 11 July 2017
- Published by American Chemical Society (ACS) in ACS Omega
- Vol. 2 (7) , 3390-3398
Chemically Stable Atomic-Layer-Deposited Al2O3 Films for Processability
Atomic-layer-deposited alumina (ALD Al2O3) can be utilized for passivation, structural, and functional purposes in electronics. In all cases, the deposited film is usually expected to maintain chemical stability over the lifetime of the device or during processing. However, as-deposited ALD Al2O3 is typically amorphous with poor resistance to chemical attack by aggressive solutions employed in electronics manufacturing. Therefore, such films may not be suitable for further processing as solvent treatments could weaken the protective barrier properties of the film or dissolved material could contaminate the solvent baths, which can cause cross-contamination of a production line used to manufacture different products. On the contrary, heat-treated, crystalline ALD Al2O3 has shown resistance to deterioration in solutions, such as standard clean (SC) 1 and 2. In this study, ALD Al2O3 was deposited from four different precursor combinations and subsequently annealed either at 600, 800, or 1000 °C for 1 h. Crystalline Al2O3 was achieved after the 800 and 1000 °C heat treatments. The crystalline films showed apparent stability in SC-1 and HF solutions. However, ellipsometry and electron microscopy showed that a prolonged exposure (60 min) to SC-1 and HF had induced a decrease in the refractive index and nanocracks in the films annealed at 800 °C. The degradation mechanism of the unstable crystalline film and the microstructure of the film, fully stable in SC-1 and with minor reaction with HF, were studied with transmission electron microscopy. Although both crystallized films had the same alumina transition phase, the film annealed at 800 °C in N2, with a less developed microstructure such as embedded amorphous regions and an uneven interfacial reaction layer, deteriorates at the amorphous regions and at the substrate–film interface. On the contrary, the stable film annealed at 1000 °C in N2 had considerably less embedded amorphous regions and a uniform Al–O–Si interfacial layer.
- 11 July 2017
- Published by American Chemical Society (ACS) in ACS Omega
- Vol. 2 (7) , 3390-3398
Open AccessChemically Stable Atomic-Layer-Deposited Al2O3 Films for Processability
Atomic-layer-deposited alumina (ALD Al2O3) can be utilized for passivation, structural, and functional purposes in electronics. In all cases, the deposited film is usually expected to maintain chemical stability over the lifetime of the device or during processing. However, as-deposited ALD Al2O3 is typically amorphous with poor resistance to chemical attack by aggressive solutions employed in electronics manufacturing. Therefore, such films may not be suitable for further processing as solvent treatments could weaken the protective barrier properties of the film or dissolved material could contaminate the solvent baths, which can cause cross-contamination of a production line used to manufacture different products. On the contrary, heat-treated, crystalline ALD Al2O3 has shown resistance to deterioration in solutions, such as standard clean (SC) 1 and 2. In this study, ALD Al2O3 was deposited from four different precursor combinations and subsequently annealed either at 600, 800, or 1000 °C for 1 h. Crystalline Al2O3 was achieved after the 800 and 1000 °C heat treatments. The crystalline films showed apparent stability in SC-1 and HF solutions. However, ellipsometry and electron microscopy showed that a prolonged exposure (60 min) to SC-1 and HF had induced a decrease in the refractive index and nanocracks in the films annealed at 800 °C. The degradation mechanism of the unstable crystalline film and the microstructure of the film, fully stable in SC-1 and with minor reaction with HF, were studied with transmission electron microscopy. Although both crystallized films had the same alumina transition phase, the film annealed at 800 °C in N2, with a less developed microstructure such as embedded amorphous regions and an uneven interfacial reaction layer, deteriorates at the amorphous regions and at the substrate–film interface. On the contrary, the stable film annealed at 1000 °C in N2 had considerably less embedded amorphous regions and a uniform Al–O–Si interfacial layer.
- 1 December 2016
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 688, 388-398
Thermodynamic reassessment of the Au-Pt-Sn system and microstructural evolution of the (AuSn)eut-Pt interconnection
- 1 December 2016
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 688, 388-398
Thermodynamic reassessment of the Au-Pt-Sn system and microstructural evolution of the (AuSn)eut-Pt interconnection
- 3 June 2016
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 34 (4) , 041506
Structural and chemical analysis of annealed plasma-enhanced atomic layer deposition aluminum nitride films
Plasma-enhanced atomic layer deposition was utilized to grow aluminum nitride (AlN) films on Si from trimethylaluminum and N2:H2 plasma at 200 °C. Thermal treatments were then applied on the films which caused changes in their chemical composition and nanostructure. These changes were observed to manifest in the refractive indices and densities of the films. The AlN films were identified to contain light element impurities, namely, H, C, and excess N due to nonideal precursor reactions. Oxygen contamination was also identified in the films. Many of the embedded impurities became volatile in the elevated annealing temperatures. Most notably, high amounts of H were observed to desorb from the AlN films. Furthermore, dinitrogen triple bonds were identified with infrared spectroscopy in the films. The triple bonds broke after annealing at 1000 °C for 1 h which likely caused enhanced hydrolysis of the films. The nanostructure of the films was identified to be amorphous in the as-deposited state and to become nanocrystalline after 1 h of annealing at 1000 °C.
- 3 June 2016
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 34 (4) , 041506
Structural and chemical analysis of annealed plasma-enhanced atomic layer deposition aluminum nitride films
Plasma-enhanced atomic layer deposition was utilized to grow aluminum nitride (AlN) films on Si from trimethylaluminum and N2:H2 plasma at 200 °C. Thermal treatments were then applied on the films which caused changes in their chemical composition and nanostructure. These changes were observed to manifest in the refractive indices and densities of the films. The AlN films were identified to contain light element impurities, namely, H, C, and excess N due to nonideal precursor reactions. Oxygen contamination was also identified in the films. Many of the embedded impurities became volatile in the elevated annealing temperatures. Most notably, high amounts of H were observed to desorb from the AlN films. Furthermore, dinitrogen triple bonds were identified with infrared spectroscopy in the films. The triple bonds broke after annealing at 1000 °C for 1 h which likely caused enhanced hydrolysis of the films. The nanostructure of the films was identified to be amorphous in the as-deposited state and to become nanocrystalline after 1 h of annealing at 1000 °C.