Sang‐Hoon Rhee
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Sang‐Hoon Rhee has a total of 44 co-authors. Here are the top co-authors by number of shared publications:
- Jung Sang Cho
Department of Engineering Chemistry, Chungbuk National University, Chungbuk, 361-763, Republic of Korea
5 shared publications In Ae Kim
Department of Dental Biomaterials Science, Dental Research Institute and BK21+, School of Dentistry, Seoul National University, Daehakro 101, Jongno, Seoul, 110-749, Korea
4 shared publicationsSeung‐Hoon Um
Department of Dental Biomaterials Science, Dental Research Institute and BK21 Plus, School of Dentistry, Seoul National University, Seoul, 03080, South Korea
4 shared publicationsDong Su Yoo
Department of Materials Science and Engineering, Hanyang University, Seoul, South Korea
3 shared publicationsSeung Jin Lee
Department of Pharmacy, College of Pharmacy, Ewha Womans University, Seodaemun, Seoul 120-750, Korea
3 shared publicationsSeung-Hoon Um
Center for Biomaterials, Biomedical Research Institute, Korea Institute of Science and Technology (KIST), Seoul, 02792, Republic of Korea
3 shared publications
Latest Publications
- 22 August 2026
- Published by Elsevier in Ceramics International
- Vol. 52 (26) , 50925-50938
Biphasic calcium phosphate granules with hierarchical surface topography defined by fracture-exposed multiscale concavities fabricated by spray pyrolysis–gas bubbling
- 22 August 2026
- Published by Elsevier in Ceramics International
- Vol. 52 (26) , 50925-50938
Biphasic calcium phosphate granules with hierarchical surface topography defined by fracture-exposed multiscale concavities fabricated by spray pyrolysis–gas bubbling
- Open Access
- 10 October 2023
- Published by Elsevier in Ceramics International
- Vol. 49 (24) , 40511-40519
Preparation of a thin silica nonwoven fabric composed of nanofibers and micropores by electrospinning after controlled hydrolysis in a sol-gel reaction
- 10 October 2023
- Published by Elsevier in Ceramics International
- Vol. 49 (24) , 40511-40519
Open AccessPreparation of a thin silica nonwoven fabric composed of nanofibers and micropores by electrospinning after controlled hydrolysis in a sol-gel reaction
- Open Access
- 1 October 2021
- Published by KEAI Publishing in Bioactive Materials
- Vol. 6 (10) , 3608-3619
Regulation of cell locomotion by nanosecond-laser-induced hydroxyapatite patterning
Hydroxyapatite, an essential mineral in human bones composed mainly of calcium and phosphorus, is widely used to coat bone graft and implant surfaces for enhanced biocompatibility and bone formation. For a strong implant–bone bond, the bone-forming cells must not only adhere to the implant surface but also move to the surface requiring bone formation. However, strong adhesion tends to inhibit cell migration on the surface of hydroxyapatite. Herein, a cell migration highway pattern that can promote cell migration was prepared using a nanosecond laser on hydroxyapatite coating. The developed surface promoted bone-forming cell movement compared with the unpatterned hydroxyapatite surface, and the cell adhesion and movement speed could be controlled by adjusting the pattern width. Live-cell microscopy, cell tracking, and serum protein analysis revealed the fundamental principle of this phenomenon. These findings are applicable to hydroxyapatite-coated biomaterials and can be implemented easily by laser patterning without complicated processes. The cell migration highway can promote and control cell movement while maintaining the existing advantages of hydroxyapatite coatings. Furthermore, it can be applied to the surface treatment of not only implant materials directly bonded to bone but also various implanted biomaterials implanted that require cell movement control.
- 1 October 2021
- Published by KEAI Publishing in Bioactive Materials
- Vol. 6 (10) , 3608-3619
Open AccessRegulation of cell locomotion by nanosecond-laser-induced hydroxyapatite patterning
Hydroxyapatite, an essential mineral in human bones composed mainly of calcium and phosphorus, is widely used to coat bone graft and implant surfaces for enhanced biocompatibility and bone formation. For a strong implant–bone bond, the bone-forming cells must not only adhere to the implant surface but also move to the surface requiring bone formation. However, strong adhesion tends to inhibit cell migration on the surface of hydroxyapatite. Herein, a cell migration highway pattern that can promote cell migration was prepared using a nanosecond laser on hydroxyapatite coating. The developed surface promoted bone-forming cell movement compared with the unpatterned hydroxyapatite surface, and the cell adhesion and movement speed could be controlled by adjusting the pattern width. Live-cell microscopy, cell tracking, and serum protein analysis revealed the fundamental principle of this phenomenon. These findings are applicable to hydroxyapatite-coated biomaterials and can be implemented easily by laser patterning without complicated processes. The cell migration highway can promote and control cell movement while maintaining the existing advantages of hydroxyapatite coatings. Furthermore, it can be applied to the surface treatment of not only implant materials directly bonded to bone but also various implanted biomaterials implanted that require cell movement control.
- Open Access
- 3 January 2021
- Published by Springer Nature in Journal of Materials Science
- Vol. 56 (9) , 5493-5508
Defect structures of sodium and chloride co-substituted hydroxyapatite and its osseointegration capacity
A defect structure and osseointegration capacity of sodium and chloride co-substituted hydroxyapatite (NaClAp) were newly studied. The NaClAp was prepared by reacting H3PO4 and Ca(OH)2 with NaNO3 and NH4Cl followed by sintering; pure hydroxyapatite (HAp) was synthesized as a control. After sintering, the co-substitution of Ca and OH with Na and Cl, respectively, produced charged point defects at Ca and PO4 sites. Also, OH molecules partially adopted a head-on structure. The calculated total system energy of NaClAp was higher, whereas the binding energies between each constituent elements and system were lower than those of HAp. These results suggest that NaClAp was less stable than HAp, due to the formation of various defects by co-substitution of Na and Cl. Indeed, NaClAp exhibited higher dissolution behavior in simulated body fluid (SBF) compared with HAp. Accordingly, this increased the capability to produce low crystalline hydroxyl carbonate apatite, likely due to the increasing degree of apatite supersaturation in SBF. Besides, the NaClAp granules showed noticeable improvements in osseointegration capacity four weeks after in vivo test compared with HAp. Collectively, these results imply that the defects made by multiple ion substitutions are useful to increase osseointegration capacity of hydroxyapatite.
- 3 January 2021
- Published by Springer Nature in Journal of Materials Science
- Vol. 56 (9) , 5493-5508
Open AccessDefect structures of sodium and chloride co-substituted hydroxyapatite and its osseointegration capacity
A defect structure and osseointegration capacity of sodium and chloride co-substituted hydroxyapatite (NaClAp) were newly studied. The NaClAp was prepared by reacting H3PO4 and Ca(OH)2 with NaNO3 and NH4Cl followed by sintering; pure hydroxyapatite (HAp) was synthesized as a control. After sintering, the co-substitution of Ca and OH with Na and Cl, respectively, produced charged point defects at Ca and PO4 sites. Also, OH molecules partially adopted a head-on structure. The calculated total system energy of NaClAp was higher, whereas the binding energies between each constituent elements and system were lower than those of HAp. These results suggest that NaClAp was less stable than HAp, due to the formation of various defects by co-substitution of Na and Cl. Indeed, NaClAp exhibited higher dissolution behavior in simulated body fluid (SBF) compared with HAp. Accordingly, this increased the capability to produce low crystalline hydroxyl carbonate apatite, likely due to the increasing degree of apatite supersaturation in SBF. Besides, the NaClAp granules showed noticeable improvements in osseointegration capacity four weeks after in vivo test compared with HAp. Collectively, these results imply that the defects made by multiple ion substitutions are useful to increase osseointegration capacity of hydroxyapatite.
- Open Access
- 1 January 2020
- Published by SAGE Publications in Journal of Applied Biomaterials & Functional Materials
- Vol. 18
Effect of grain size of dental zirconia on shear bond strength of composite resin cement
The effect of grain size of dental zirconia on the shear bond strength of composite resin cement was newly studied. Disc-shaped dental zirconia with small (sample S) and large (sample L) grains were made by sintering of pre-sintered dental zirconia at 1450°C for 0.5 h and 40 h, respectively. After the sintering, the average grain size of sample S was 1.37 ± 0.15 µm, while that of sample L was 3.74 ± 0.50 µm. The sintered discs were successively polished with different grades of diamond and alumina slurries. The interfacial free energies were 63.5 ± 4.2 dyne/cm for sample S and 52.1 ± 5.5 dyne/cm for sample L. Stainless steel cylinders, previously sandblasted with 50 µm alumina powder, were bonded to the zirconia discs using composite resin cement. Next, samples were kept in an oven for 7 d at 36.5°C. The shear bond strength of sample S was 23.0 ± 4.5 MPa while that of sample L was 17.5 ± 4.6 MPa. After the fracture, the areal % values of composite resin cement remaining on the zirconia surfaces were 89.7 ± 5.9% for sample S and 61.6 ± 5.5% for sample L. The results suggest that grain size reduction has a potential to enhance the degree of bonding between a composite resin cement and a dental zirconia due to the increase of interfacial free energy.
- 1 January 2020
- Published by SAGE Publications in Journal of Applied Biomaterials & Functional Materials
- Vol. 18
Open AccessEffect of grain size of dental zirconia on shear bond strength of composite resin cement
The effect of grain size of dental zirconia on the shear bond strength of composite resin cement was newly studied. Disc-shaped dental zirconia with small (sample S) and large (sample L) grains were made by sintering of pre-sintered dental zirconia at 1450°C for 0.5 h and 40 h, respectively. After the sintering, the average grain size of sample S was 1.37 ± 0.15 µm, while that of sample L was 3.74 ± 0.50 µm. The sintered discs were successively polished with different grades of diamond and alumina slurries. The interfacial free energies were 63.5 ± 4.2 dyne/cm for sample S and 52.1 ± 5.5 dyne/cm for sample L. Stainless steel cylinders, previously sandblasted with 50 µm alumina powder, were bonded to the zirconia discs using composite resin cement. Next, samples were kept in an oven for 7 d at 36.5°C. The shear bond strength of sample S was 23.0 ± 4.5 MPa while that of sample L was 17.5 ± 4.6 MPa. After the fracture, the areal % values of composite resin cement remaining on the zirconia surfaces were 89.7 ± 5.9% for sample S and 61.6 ± 5.5% for sample L. The results suggest that grain size reduction has a potential to enhance the degree of bonding between a composite resin cement and a dental zirconia due to the increase of interfacial free energy.
- 18 September 2019
- Published by SAGE Publications in Advances in Applied Ceramics: Structural, Functional and Bioceramics
- Vol. 118 (8) , 484-490
In vivo evaluations of hydroxyapatites with small and large grain sizes
The effect of grain size of hydroxyapatite on its osteoconductivity was newly investigated. The hydroxyapatite discs, which had small (specimen S) and large grain size (specimen L), were prepared through microwave sintering at 1100°C for 6 and 720 min, respectively. The average grain size of specimen S was about 15 times smaller than that of specimen L. The surface energy of specimen S was about 1.6 times higher than that of specimen L under the same surface roughness. For the osteoconductivity test, porous hydroxyapatite granules were prepared using PEG porogen. The osteoconductivity of specimen S was superior to that of specimen L four weeks after implantation in calvarial defects of New Zealand white rabbits. Taken together, it can be concluded that the hydroxyapatite with small grain size had a higher osteoconductivity compared with the hydroxyapatite with large grain size due to its high surface energy.
- 18 September 2019
- Published by SAGE Publications in Advances in Applied Ceramics: Structural, Functional and Bioceramics
- Vol. 118 (8) , 484-490
In vivo evaluations of hydroxyapatites with small and large grain sizes
The effect of grain size of hydroxyapatite on its osteoconductivity was newly investigated. The hydroxyapatite discs, which had small (specimen S) and large grain size (specimen L), were prepared through microwave sintering at 1100°C for 6 and 720 min, respectively. The average grain size of specimen S was about 15 times smaller than that of specimen L. The surface energy of specimen S was about 1.6 times higher than that of specimen L under the same surface roughness. For the osteoconductivity test, porous hydroxyapatite granules were prepared using PEG porogen. The osteoconductivity of specimen S was superior to that of specimen L four weeks after implantation in calvarial defects of New Zealand white rabbits. Taken together, it can be concluded that the hydroxyapatite with small grain size had a higher osteoconductivity compared with the hydroxyapatite with large grain size due to its high surface energy.
- 31 December 2018
- Published by Korean Society for Dental Materials in Korean Journal of Dental Materials
- Vol. 45 (4) , 233-242
Effect of resin cement color on the color of commercially available zirconia crown
- 31 December 2018
- Published by Korean Society for Dental Materials in Korean Journal of Dental Materials
- Vol. 45 (4) , 233-242
Effect of resin cement color on the color of commercially available zirconia crown
- 1 October 2018
- Published by Wiley in Journal of Biomedical Materials Research Part B: Applied Biomaterials
- Vol. 107 (5) , 1440-1451
Synthesis of a Ca3SiO5–Ca2SiO4–Ca3Al2O6 cement system with rapid setting capacity by spray‐pyrolysis coupled with sol–gel method
A modified mineral‐trioxide‐aggregate (mMTA) with rapid setting capacity was newly synthesized by spray‐pyrolysis following a sol–gel reaction. Its faster setting capacity and initially higher compressive strength compared with Portland cement (PC) were evaluated. The precursor solution of the mMTA was prepared through condensation following hydrolysis among Ca(NO3)2·4H2O, Si(OC2H5)4, and Al(NO3)3·9H2O under nitric acid. The mMTA powder was then synthesized by spray‐pyrolysis at 1500°C. The particle shape was spherical with an average particle size of 0.8 ± 0.3 μm, while PC particles were irregular and 3.9 ± 3.0 μm in size. The mMTA consisted of mostly Ca3SiO5, Ca3Al2O6, and partial Ca2SiO4 phases, while the PC comprised mainly Ca3SiO5, Ca2SiO4, and partial Ca3Al2O6 phases. The final setting times of mMTA and PC measured under 95% relative humidity were about 11 min and 3 h, respectively. The early stage of setting in mMTA was dominated by the rapid formation of hexagonal‐plate‐like Ca3Al2O6·6H2O crystals, while that in PC was dominated by needle‐like calcium‐silicate‐hydrate gels and columnar‐shaped Ca(OH)2 crystals. The late stage of setting in mMTA was dominated by calcium‐silicate‐hydrate gels and Ca(OH)2 crystals, while that in PC was dominated by Ca3Al2O6·6H2O crystals. The compressive strengths of mMTA and PC after 30 min of setting were 4.5 and 0.2 MPa, respectively. The results suggest that mMTA has potential to be used as a filling material for accidental pulp‐exposure or pulpal floor perforation cases that require rapid setting capacity and initial good strength. © 2018 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater 107B: 1440–1451, 2019.
- 1 October 2018
- Published by Wiley in Journal of Biomedical Materials Research Part B: Applied Biomaterials
- Vol. 107 (5) , 1440-1451
Synthesis of a Ca3SiO5–Ca2SiO4–Ca3Al2O6 cement system with rapid setting capacity by spray‐pyrolysis coupled with sol–gel method
A modified mineral‐trioxide‐aggregate (mMTA) with rapid setting capacity was newly synthesized by spray‐pyrolysis following a sol–gel reaction. Its faster setting capacity and initially higher compressive strength compared with Portland cement (PC) were evaluated. The precursor solution of the mMTA was prepared through condensation following hydrolysis among Ca(NO3)2·4H2O, Si(OC2H5)4, and Al(NO3)3·9H2O under nitric acid. The mMTA powder was then synthesized by spray‐pyrolysis at 1500°C. The particle shape was spherical with an average particle size of 0.8 ± 0.3 μm, while PC particles were irregular and 3.9 ± 3.0 μm in size. The mMTA consisted of mostly Ca3SiO5, Ca3Al2O6, and partial Ca2SiO4 phases, while the PC comprised mainly Ca3SiO5, Ca2SiO4, and partial Ca3Al2O6 phases. The final setting times of mMTA and PC measured under 95% relative humidity were about 11 min and 3 h, respectively. The early stage of setting in mMTA was dominated by the rapid formation of hexagonal‐plate‐like Ca3Al2O6·6H2O crystals, while that in PC was dominated by needle‐like calcium‐silicate‐hydrate gels and columnar‐shaped Ca(OH)2 crystals. The late stage of setting in mMTA was dominated by calcium‐silicate‐hydrate gels and Ca(OH)2 crystals, while that in PC was dominated by Ca3Al2O6·6H2O crystals. The compressive strengths of mMTA and PC after 30 min of setting were 4.5 and 0.2 MPa, respectively. The results suggest that mMTA has potential to be used as a filling material for accidental pulp‐exposure or pulpal floor perforation cases that require rapid setting capacity and initial good strength. © 2018 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater 107B: 1440–1451, 2019.
- 21 March 2017
- Published by Wiley in Journal of Biomedical Materials Research Part A
- Vol. 105 (7) , 1973-1983
Preparation of a non‐woven poly(ε‐caprolactone) fabric with partially embedded apatite surface for bone tissue engineering applications by partial surface melting of poly(ε‐caprolactone) fibers
This article describes a novel method for the preparation of a biodegradable non‐woven poly(ε‐caprolactone) fabric with a partially embedded apatite surface designed for application as a scaffold material for bone tissue engineering. The non‐woven poly(ε‐caprolactone) fabric was generated by the electro‐spinning technique and then apatite was coated in simulated body fluid after coating the PVA solution containing CaCl2·2H2O. The apatite crystals were partially embedded or fully embedded into the thermoplastic poly(ε‐caprolactone) fibers by controlling the degree of poly(ε‐caprolactone) fiber surface melting in a convection oven. Identical apatite‐coated poly(ε‐caprolactone) fabric that did not undergo heat‐treatment was used as a control. The features of the embedded apatite crystals were evaluated by FE‐SEM, AFM, EDS, and XRD. The adhesion strengths of the coated apatite layers and the tensile strengths of the apatite coated fabrics with and without heat‐treatment were assessed by the tape‐test and a universal testing machine, respectively. The degree of water absorbance was assessed by adding a DMEM droplet onto the fabrics. Moreover, cell penetrability was assessed by seeding preosteoblastic MC3T3‐E1 cells onto the fabrics and observing the degrees of cell penetration after 1 and 4 weeks by staining nuclei with DAPI. The non‐woven poly(ε‐caprolactone) fabric with a partially embedded apatite surface showed good water absorbance, cell penetrability, higher apatite adhesion strength, and higher tensile strength compared with the control fabric. These results show that the non‐woven poly(ε‐caprolactone) fabric with a partially embedded apatite surface is a potential candidate scaffold for bone tissue engineering due to its strong apatite adhesion strength and excellent cell penetrability. © 2016 Wiley Periodicals, Inc. J Biomed Mater Res Part A: 105A: 1973–1983, 2017.
- 21 March 2017
- Published by Wiley in Journal of Biomedical Materials Research Part A
- Vol. 105 (7) , 1973-1983
Preparation of a non‐woven poly(ε‐caprolactone) fabric with partially embedded apatite surface for bone tissue engineering applications by partial surface melting of poly(ε‐caprolactone) fibers
This article describes a novel method for the preparation of a biodegradable non‐woven poly(ε‐caprolactone) fabric with a partially embedded apatite surface designed for application as a scaffold material for bone tissue engineering. The non‐woven poly(ε‐caprolactone) fabric was generated by the electro‐spinning technique and then apatite was coated in simulated body fluid after coating the PVA solution containing CaCl2·2H2O. The apatite crystals were partially embedded or fully embedded into the thermoplastic poly(ε‐caprolactone) fibers by controlling the degree of poly(ε‐caprolactone) fiber surface melting in a convection oven. Identical apatite‐coated poly(ε‐caprolactone) fabric that did not undergo heat‐treatment was used as a control. The features of the embedded apatite crystals were evaluated by FE‐SEM, AFM, EDS, and XRD. The adhesion strengths of the coated apatite layers and the tensile strengths of the apatite coated fabrics with and without heat‐treatment were assessed by the tape‐test and a universal testing machine, respectively. The degree of water absorbance was assessed by adding a DMEM droplet onto the fabrics. Moreover, cell penetrability was assessed by seeding preosteoblastic MC3T3‐E1 cells onto the fabrics and observing the degrees of cell penetration after 1 and 4 weeks by staining nuclei with DAPI. The non‐woven poly(ε‐caprolactone) fabric with a partially embedded apatite surface showed good water absorbance, cell penetrability, higher apatite adhesion strength, and higher tensile strength compared with the control fabric. These results show that the non‐woven poly(ε‐caprolactone) fabric with a partially embedded apatite surface is a potential candidate scaffold for bone tissue engineering due to its strong apatite adhesion strength and excellent cell penetrability. © 2016 Wiley Periodicals, Inc. J Biomed Mater Res Part A: 105A: 1973–1983, 2017.
- Open Access
- 1 January 2017
- Published by Korean Association of Orthodontists in The Korean Journal of Orthodontics
- Vol. 47 (4) , 229-237
Comparison of mechanical and biological properties of zirconia and titanium alloy orthodontic micro-implants
Choi HW, et al. Korean J Orthod. 2017 Jul;47(4):229-237. https://doi.org/10.4041/kjod.2017.47.4.229
- 1 January 2017
- Published by Korean Association of Orthodontists in The Korean Journal of Orthodontics
- Vol. 47 (4) , 229-237
Open AccessComparison of mechanical and biological properties of zirconia and titanium alloy orthodontic micro-implants
Choi HW, et al. Korean J Orthod. 2017 Jul;47(4):229-237. https://doi.org/10.4041/kjod.2017.47.4.229