Jorma Vihinen
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Jorma Vihinen has a total of 72 co-authors. Here are the top co-authors by number of shared publications:
- Petri Vuoristo
Materials Science and Environmental Engineering, Faculty of Engineering and Natural Sciences, Tampere University, P.O. Box 589, FI-33014 Tampere, Finland
4 shared publications - Yasuhiro Okamoto
Okayama University
4 shared publications - Erkki Levänen
Faculty of Engineering and Natural Sciences, Tampere University, Korkeakoulunkatu 6, P. O. Box 589, Tampere, 33014, Finland
3 shared publications Jarno Kangastupa
3 shared publicationsTero Kumpulainen
Automation Technology and Mechanical Engineering, Tampere University, Finland
3 shared publicationsAkira Okada
2 shared publications
Latest Publications
- Open Access
- 1 October 2021
- Published by Elsevier in Optics & Laser Technology
- Vol. 142, 107278
Interference system for high pressure environment
- 1 October 2021
- Published by Elsevier in Optics & Laser Technology
- Vol. 142, 107278
Open AccessInterference system for high pressure environment
- Open Access
- 18 July 2019
- Published by Medical Journals Sweden AB in Biomaterial Investigations in Dentistry
- Vol. 6 (1) , 23-31
Three-dimensional printing of zirconia: characterization of early stage material properties
Objective: The aim of this study was to evaluate the mechanical properties of 3D printed zirconia (ZrO2). Materials and Methods: The test specimens were produced with a 3D printer that uses lithography-based ceramic manufacturing (LCM) technique with two different parameters in horizontal and vertical printing orientations. Altogether four groups of nine specimens were printed and examined. Mechanical characterization was performed using 3-point bending test (ISO 10477) and surface microhardness (Vickers) test. Grain structure, porosity and printing layer morphology were examined with optical and scanning electron microscopy (SEM). Additionally fractography analysis was done to investigate and evaluate features of fracture initiation site. Numeric results were statistically analyzed with ANOVA (a = 0.05). Results : The average flexural strength reached for printed zirconia was 499 MPa (+/−75 MPa) for specimens printed in horizontal orientation and 575 MPa (+/−69 MPa) for specimens printed in vertical orientation. Optical microscopy and SEM analysis revealed that fractures initiated between the printing layers or from a local porosity. Printing layer thickness varied from under 13 μm to over 20 μm. Conclusions : The study revealed that 3D printed zirconia has challenges in regards to layer integration. Based on this study, 3D printed zirconia still suffers from low mechanical strength, which together with long carbon-debinding time, does not make 3D printed zirconia a potential material for dental appliances at this stage. Further research is needed to create more suitable zirconia precursor slurries and to optimize printing parameters and sintering conditions to be able to 3D print zirconia with higher mechanical properties.
- 18 July 2019
- Published by Medical Journals Sweden AB in Biomaterial Investigations in Dentistry
- Vol. 6 (1) , 23-31
Open AccessThree-dimensional printing of zirconia: characterization of early stage material properties
Objective: The aim of this study was to evaluate the mechanical properties of 3D printed zirconia (ZrO2). Materials and Methods: The test specimens were produced with a 3D printer that uses lithography-based ceramic manufacturing (LCM) technique with two different parameters in horizontal and vertical printing orientations. Altogether four groups of nine specimens were printed and examined. Mechanical characterization was performed using 3-point bending test (ISO 10477) and surface microhardness (Vickers) test. Grain structure, porosity and printing layer morphology were examined with optical and scanning electron microscopy (SEM). Additionally fractography analysis was done to investigate and evaluate features of fracture initiation site. Numeric results were statistically analyzed with ANOVA (a = 0.05). Results : The average flexural strength reached for printed zirconia was 499 MPa (+/−75 MPa) for specimens printed in horizontal orientation and 575 MPa (+/−69 MPa) for specimens printed in vertical orientation. Optical microscopy and SEM analysis revealed that fractures initiated between the printing layers or from a local porosity. Printing layer thickness varied from under 13 μm to over 20 μm. Conclusions : The study revealed that 3D printed zirconia has challenges in regards to layer integration. Based on this study, 3D printed zirconia still suffers from low mechanical strength, which together with long carbon-debinding time, does not make 3D printed zirconia a potential material for dental appliances at this stage. Further research is needed to create more suitable zirconia precursor slurries and to optimize printing parameters and sintering conditions to be able to 3D print zirconia with higher mechanical properties.
- 1 August 2018
- Published by Elsevier in Journal of Materials Processing Technology
- Vol. 258, 180-188
High surface quality welding of aluminum using adjustable ring-mode fiber laser
- 1 August 2018
- Published by Elsevier in Journal of Materials Processing Technology
- Vol. 258, 180-188
High surface quality welding of aluminum using adjustable ring-mode fiber laser
- 23 May 2018
- Published by Wiley in Journal of Mechanical Design
- Vol. 140 (8) , 081101
A Conceptual Design and Modeling Framework for Integrated Additive Manufacturing
Modeling and simulation for additive manufacturing (AM) is commonly used in industry. Nevertheless, a central issue remaining is the integration of different models focusing on different objectives and targeting different levels of details. The objective of this work is to increase the prediction capability of characteristics and performances of additively manufactured parts and to co-design parts and processes. The paper contributes to this field of research by integrating part's performance model and additive technology process model into a single early integrated model. The paper uses the dimensional analysis conceptual modeling (DACM) framework in an AM perspective to generate causal graphs integrating the AM equipment and the part to be printed. DACM offers the possibility of integrating existing knowledge in the model. The framework supported by a computer tool produces a set of governing equations representing the relationships among the influencing variables of the integrated model. The systematic identification of the weaknesses and contradictions in the system and qualitative simulation of the system are some of the potential uses of the model. Ultimately, it is a way to create better designs of machines and parts, to control and qualify the manufacturing process, and to control three-dimensional (3D) printing processes. The DACM framework is tested on two cases of a 3D printer using the fused filament fabrication (FFF) powder bed fusion. The analysis, applied to the global system formed of the 3D printer and the part, illustrates the existence of contradictions. The analysis supports the early redesign of both parts and AM process (equipment) and later optimization of the control parameters.
- 23 May 2018
- Published by Wiley in Journal of Mechanical Design
- Vol. 140 (8) , 081101
A Conceptual Design and Modeling Framework for Integrated Additive Manufacturing
Modeling and simulation for additive manufacturing (AM) is commonly used in industry. Nevertheless, a central issue remaining is the integration of different models focusing on different objectives and targeting different levels of details. The objective of this work is to increase the prediction capability of characteristics and performances of additively manufactured parts and to co-design parts and processes. The paper contributes to this field of research by integrating part's performance model and additive technology process model into a single early integrated model. The paper uses the dimensional analysis conceptual modeling (DACM) framework in an AM perspective to generate causal graphs integrating the AM equipment and the part to be printed. DACM offers the possibility of integrating existing knowledge in the model. The framework supported by a computer tool produces a set of governing equations representing the relationships among the influencing variables of the integrated model. The systematic identification of the weaknesses and contradictions in the system and qualitative simulation of the system are some of the potential uses of the model. Ultimately, it is a way to create better designs of machines and parts, to control and qualify the manufacturing process, and to control three-dimensional (3D) printing processes. The DACM framework is tested on two cases of a 3D printer using the fused filament fabrication (FFF) powder bed fusion. The analysis, applied to the global system formed of the 3D printer and the part, illustrates the existence of contradictions. The analysis supports the early redesign of both parts and AM process (equipment) and later optimization of the control parameters.
- Open Access
- 19 April 2018
- Published by Oxford University Press (OUP) in Bioinformatics
- Vol. 34 (17) , 3013-3021
Comparative analysis of tissue reconstruction algorithms for 3D histology
Digital pathology enables new approaches that expand beyond storage, visualization or analysis of histological samples in digital format. One novel opportunity is 3D histology, where a three-dimensional reconstruction of the sample is formed computationally based on serial tissue sections. This allows examining tissue architecture in 3D, for example, for diagnostic purposes. Importantly, 3D histology enables joint mapping of cellular morphology with spatially resolved omics data in the true 3D context of the tissue at microscopic resolution. Several algorithms have been proposed for the reconstruction task, but a quantitative comparison of their accuracy is lacking. We developed a benchmarking framework to evaluate the accuracy of several free and commercial 3D reconstruction methods using two whole slide image datasets. The results provide a solid basis for further development and application of 3D histology algorithms and indicate that methods capable of compensating for local tissue deformation are superior to simpler approaches. Code: https://github.com/BioimageInformaticsTampere/RegBenchmark. Whole slide image datasets: http://urn.fi/urn: nbn: fi: csc-kata20170705131652639702. Supplementary data are available at Bioinformatics online.
- 19 April 2018
- Published by Oxford University Press (OUP) in Bioinformatics
- Vol. 34 (17) , 3013-3021
Open AccessComparative analysis of tissue reconstruction algorithms for 3D histology
Digital pathology enables new approaches that expand beyond storage, visualization or analysis of histological samples in digital format. One novel opportunity is 3D histology, where a three-dimensional reconstruction of the sample is formed computationally based on serial tissue sections. This allows examining tissue architecture in 3D, for example, for diagnostic purposes. Importantly, 3D histology enables joint mapping of cellular morphology with spatially resolved omics data in the true 3D context of the tissue at microscopic resolution. Several algorithms have been proposed for the reconstruction task, but a quantitative comparison of their accuracy is lacking. We developed a benchmarking framework to evaluate the accuracy of several free and commercial 3D reconstruction methods using two whole slide image datasets. The results provide a solid basis for further development and application of 3D histology algorithms and indicate that methods capable of compensating for local tissue deformation are superior to simpler approaches. Code: https://github.com/BioimageInformaticsTampere/RegBenchmark. Whole slide image datasets: http://urn.fi/urn: nbn: fi: csc-kata20170705131652639702. Supplementary data are available at Bioinformatics online.
- 15 November 2016
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 879, 984-989
Structures and Properties of Laser-Assisted Cold-Sprayed Aluminum Coatings
In the cold spray process, solid particles impact on a surface with high kinetic energy, deform plastically and form a coating. This enables the formation of pure and dense coating structures. Even more, coating performance and deposition efficiency can be improved by assisting the process with a laser. Laser-assisted cold spraying (LACS) has shown its potential to improve coating properties compared with traditional cold spraying. In this study, coating quality improvement was obtained by using a co-axial laser spray (COLA) process which offers a new, cost-effective laser-assisted cold spray technique, for high-quality deposition and repair. In the COLA process, the sprayed surface is laser heated while particles hit the surface. This assists the better bonding between particles and substrate and leads to the formation of tight coating structures. This study focuses on the evaluation of the microstructural characteristics and mechanical properties (e.g., hardness and bond strength) of LACS metallic coatings.
- 15 November 2016
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 879, 984-989
Structures and Properties of Laser-Assisted Cold-Sprayed Aluminum Coatings
In the cold spray process, solid particles impact on a surface with high kinetic energy, deform plastically and form a coating. This enables the formation of pure and dense coating structures. Even more, coating performance and deposition efficiency can be improved by assisting the process with a laser. Laser-assisted cold spraying (LACS) has shown its potential to improve coating properties compared with traditional cold spraying. In this study, coating quality improvement was obtained by using a co-axial laser spray (COLA) process which offers a new, cost-effective laser-assisted cold spray technique, for high-quality deposition and repair. In the COLA process, the sprayed surface is laser heated while particles hit the surface. This assists the better bonding between particles and substrate and leads to the formation of tight coating structures. This study focuses on the evaluation of the microstructural characteristics and mechanical properties (e.g., hardness and bond strength) of LACS metallic coatings.
- Open Access
- 5 October 2016
- Published by Springer Nature in Discover Nano
- Vol. 11 (1) , 1-9
Pulsed Laser Ablation-Induced Green Synthesis of TiO2 Nanoparticles and Application of Novel Small Angle X-Ray Scattering Technique for Nanoparticle Size and Size Distribution Analysis
This paper aims to introduce small angle X-ray scattering (SAXS) as a promising technique for measuring size and size distribution of TiO2 nanoparticles. In this manuscript, pulsed laser ablation in liquids (PLAL) has been demonstrated as a quick and simple technique for synthesizing TiO2 nanoparticles directly into deionized water as a suspension from titanium targets. Spherical TiO2 nanoparticles with diameters in the range 4–35 nm were observed with transmission electron microscopy (TEM). X-ray diffraction (XRD) showed highly crystalline nanoparticles that comprised of two main photoactive phases of TiO2: anatase and rutile. However, presence of minor amounts of brookite was also reported. The traditional methods for nanoparticle size and size distribution analysis such as electron microscopy-based methods are time-consuming. In this study, we have proposed and validated SAXS as a promising method for characterization of laser-ablated TiO2 nanoparticles for their size and size distribution by comparing SAXS- and TEM-measured nanoparticle size and size distribution. SAXS- and TEM-measured size distributions closely followed each other for each sample, and size distributions in both showed maxima at the same nanoparticle size. The SAXS-measured nanoparticle diameters were slightly larger than the respective diameters measured by TEM. This was because SAXS measures an agglomerate consisting of several particles as one big particle which slightly increased the mean diameter. TEM- and SAXS-measured mean diameters when plotted together showed similar trend in the variation in the size as the laser power was changed which along with extremely similar size distributions for TEM and SAXS validated the application of SAXS for size distribution measurement of the synthesized TiO2 nanoparticles.
- 5 October 2016
- Published by Springer Nature in Discover Nano
- Vol. 11 (1) , 1-9
Open AccessPulsed Laser Ablation-Induced Green Synthesis of TiO2 Nanoparticles and Application of Novel Small Angle X-Ray Scattering Technique for Nanoparticle Size and Size Distribution Analysis
This paper aims to introduce small angle X-ray scattering (SAXS) as a promising technique for measuring size and size distribution of TiO2 nanoparticles. In this manuscript, pulsed laser ablation in liquids (PLAL) has been demonstrated as a quick and simple technique for synthesizing TiO2 nanoparticles directly into deionized water as a suspension from titanium targets. Spherical TiO2 nanoparticles with diameters in the range 4–35 nm were observed with transmission electron microscopy (TEM). X-ray diffraction (XRD) showed highly crystalline nanoparticles that comprised of two main photoactive phases of TiO2: anatase and rutile. However, presence of minor amounts of brookite was also reported. The traditional methods for nanoparticle size and size distribution analysis such as electron microscopy-based methods are time-consuming. In this study, we have proposed and validated SAXS as a promising method for characterization of laser-ablated TiO2 nanoparticles for their size and size distribution by comparing SAXS- and TEM-measured nanoparticle size and size distribution. SAXS- and TEM-measured size distributions closely followed each other for each sample, and size distributions in both showed maxima at the same nanoparticle size. The SAXS-measured nanoparticle diameters were slightly larger than the respective diameters measured by TEM. This was because SAXS measures an agglomerate consisting of several particles as one big particle which slightly increased the mean diameter. TEM- and SAXS-measured mean diameters when plotted together showed similar trend in the variation in the size as the laser power was changed which along with extremely similar size distributions for TEM and SAXS validated the application of SAXS for size distribution measurement of the synthesized TiO2 nanoparticles.
- 21 August 2016
- Published by ASME International
A Network Based Modelling Approach Using the Dimensional Analysis Conceptual Modeling (DACM) Framework for Additive Manufacturing Technologies
The application of additive manufacturing technologies in the industry is growing fast. This leads to an increasing need for reliable modeling techniques in the field of additive manufacturing. A methodology is proposed to systematically assess the influence of process parameters on the final characteristics of additively manufactured parts. The current study aims at presenting a theoretical framework dedicated to the modeling of the additive manufacturing technology. More specifically, the framework is used in the context of the study to plan and optimize the experimental process to minimize the amount of experiments required to populate the model. The framework presented is based on the Dimensional Analysis Conceptual Modelling framework (DACM). DACM is an approach supporting the production of models. This approach is designing networks representing a system architecture and behavior using an approach sharing similarities with neural networks. Based on the proposed approach, it is possible to detect where supplementary experimental data have to be collected to complete the model generated by the DACM approach. The modeling of the Direct Material Deposition process is conducted as an illustrative case study. The scope of the approach is vast and supported by validated scientific methods combined to form the core of the DACM method. The DACM framework is step by step extracting information from a description of the system architecture to create semi-automatically a model that can be simulated and used for multiple types of analyses associated for example with innovation and design improvement. The current paper will focus on the usage of the DACM framework, recently developed in a project, in the field of additive manufacturing.
- 21 August 2016
- Published by ASME International
A Network Based Modelling Approach Using the Dimensional Analysis Conceptual Modeling (DACM) Framework for Additive Manufacturing Technologies
The application of additive manufacturing technologies in the industry is growing fast. This leads to an increasing need for reliable modeling techniques in the field of additive manufacturing. A methodology is proposed to systematically assess the influence of process parameters on the final characteristics of additively manufactured parts. The current study aims at presenting a theoretical framework dedicated to the modeling of the additive manufacturing technology. More specifically, the framework is used in the context of the study to plan and optimize the experimental process to minimize the amount of experiments required to populate the model. The framework presented is based on the Dimensional Analysis Conceptual Modelling framework (DACM). DACM is an approach supporting the production of models. This approach is designing networks representing a system architecture and behavior using an approach sharing similarities with neural networks. Based on the proposed approach, it is possible to detect where supplementary experimental data have to be collected to complete the model generated by the DACM approach. The modeling of the Direct Material Deposition process is conducted as an illustrative case study. The scope of the approach is vast and supported by validated scientific methods combined to form the core of the DACM method. The DACM framework is step by step extracting information from a description of the system architecture to create semi-automatically a model that can be simulated and used for multiple types of analyses associated for example with innovation and design improvement. The current paper will focus on the usage of the DACM framework, recently developed in a project, in the field of additive manufacturing.
- Open Access
- 4 February 2015
- Published by Optica Publishing Group in Optics Express
- Vol. 23 (3) , 3427-3439
High speed, high strength microwelding of Si/glass using ps-laser pulses
A novel microwelding procedure to join Si-to-glass using ps-laser pulses with high repetition rates is presented. The procedure provides weld joint with mechanical strength as high as 85 MPa and 45 MPa in sample pairs of Si/aluminosilicate (Si/SW-Y) and Si/borosilicate (Si/Borofloat 33), respectively, which are higher than anodic bonding, at high spatial resolution (< 20 µm) and very high throughput without pre- and post-heating. Laser-matter interaction analysis indicates that excellent weld joint of Si/glass is obtained by avoiding violent evaporation of Si substrate using ps-laser pulses. Laser welded Si/glass samples can be singulated along the weld lines by standard blade dicer without defects, demonstrating welding by ps-laser pulses is applicable to wafer-level packaging.
- 4 February 2015
- Published by Optica Publishing Group in Optics Express
- Vol. 23 (3) , 3427-3439
Open AccessHigh speed, high strength microwelding of Si/glass using ps-laser pulses
A novel microwelding procedure to join Si-to-glass using ps-laser pulses with high repetition rates is presented. The procedure provides weld joint with mechanical strength as high as 85 MPa and 45 MPa in sample pairs of Si/aluminosilicate (Si/SW-Y) and Si/borosilicate (Si/Borofloat 33), respectively, which are higher than anodic bonding, at high spatial resolution (< 20 µm) and very high throughput without pre- and post-heating. Laser-matter interaction analysis indicates that excellent weld joint of Si/glass is obtained by avoiding violent evaporation of Si substrate using ps-laser pulses. Laser welded Si/glass samples can be singulated along the weld lines by standard blade dicer without defects, demonstrating welding by ps-laser pulses is applicable to wafer-level packaging.
- 1 September 2014
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 1-4
Novel glass welding technique for hermetic encapsulation
Conventional glass bonding methods do not fill all the requirements set by the industry. A novel hermetic room temperature glass welding technology was investigated. The aim was to avoid additive materials and multistep manufacturing process as well as minimize the heat affect. However, a good quality hermetic, mechanically sound bond was desired. In this study, a temperature cycling test was performed to glass samples welded with this novel technology. Notable advantages of using the novel welding technology were discovered: resistance of rapid temperature changes, excellent mechanical properties, room temperature welding, and hermetic encapsulation can be achieved. Use of only one material ensures that no problems with different temperature coefficients will be appeared. As a result, a newly develop glass welding technology can offer solution for the novel challenges set by the industry.
- 1 September 2014
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 1-4
Novel glass welding technique for hermetic encapsulation
Conventional glass bonding methods do not fill all the requirements set by the industry. A novel hermetic room temperature glass welding technology was investigated. The aim was to avoid additive materials and multistep manufacturing process as well as minimize the heat affect. However, a good quality hermetic, mechanically sound bond was desired. In this study, a temperature cycling test was performed to glass samples welded with this novel technology. Notable advantages of using the novel welding technology were discovered: resistance of rapid temperature changes, excellent mechanical properties, room temperature welding, and hermetic encapsulation can be achieved. Use of only one material ensures that no problems with different temperature coefficients will be appeared. As a result, a newly develop glass welding technology can offer solution for the novel challenges set by the industry.