Hsin Jen Hoh
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Hsin Jen Hoh has a total of 21 co-authors. Here are the top co-authors by number of shared publications:
- Kin Shun Tsang
School of Mechanical & Aerospace Engineering, Nanyang Technological University, 50 Nanyang Avenue, Singapore 639798, Singapore
6 shared publications J. Luo
5 shared publications- Zhongmin Xiao
School of Mechanical and Aerospace Engineering, Nanyang Technological University, Singapore, Singapore
4 shared publications Bin Song
Nanyang Technological University
3 shared publicationsJohn H.L. Pang
3 shared publicationsJohn Hock Lye Pang
3 shared publications
Latest Publications
- 16 July 2019
- Published by Wiley in Fatigue & Fracture of Engineering Materials & Structures
- Vol. 43 (1) , 119-136
Dynamic finite element modeling and fatigue damage analysis of thermite welds
- 16 July 2019
- Published by Wiley in Fatigue & Fracture of Engineering Materials & Structures
- Vol. 43 (1) , 119-136
Dynamic finite element modeling and fatigue damage analysis of thermite welds
- 1 January 2017
- Published by Elsevier in International Journal of Fatigue
- Vol. 94, 158-165
Fatigue crack propagation analysis for multiple weld toe cracks in cut-out fatigue test specimens from a girth welded pipe
- 1 January 2017
- Published by Elsevier in International Journal of Fatigue
- Vol. 94, 158-165
Fatigue crack propagation analysis for multiple weld toe cracks in cut-out fatigue test specimens from a girth welded pipe
- 1 July 2016
- Published by Elsevier in Marine Structures
- Vol. 48, 1-14
3D stress intensity factors for weld toe semi-elliptical surface cracks using XFEM
- 1 July 2016
- Published by Elsevier in Marine Structures
- Vol. 48, 1-14
3D stress intensity factors for weld toe semi-elliptical surface cracks using XFEM
- 19 June 2016
- Published by ASME International
Fatigue Algorithm for Modeling Many Weld Toe Cracks Propagating at Welded Joints
Fatigue crack growth at welded joints often propagates from as many as tens to hundreds of small weld toe cracks along the weld toe line in offshore welded structures. This paper will present a fatigue algorithm for modeling many small weld toe cracks propagating from a welded joint. Cracks usually initiate at the weld toe region of the structures and propagate as surface cracks at the stress concentration regions of the weld-toe line. The presence of such weld defects or crack-like flaws can have a severe detrimental effect on their fatigue life and fracture resistance. Currently, there is a lack of studies that considers the effects of multiple cracks and their distribution density in welded joints. This work focuses on the fatigue analysis and modeling of multiple weld toe cracks, specifically in T-butt joints. Fatigue crack growth prediction is usually determined by the stress intensity factor range and crack propagation rate through Paris law. To predict the Stress Intensity Factor (SIF) of a weld toe crack, the magnification (Mk) factor was used. The Mk factor is influenced by the size of the welded attachment, as well as the size and depth of the weld toe crack. Simplified solutions for practical prediction of Mk factors were determined from 3D extended finite element method (XFEM) by modelling a semi-elliptical weld toe crack in a T-butt weld for cracks of different dimensions. The accuracy of the Mk factor solutions was verified by comparison to HSE fatigue data on 16 mm thick tubular joints. The Mk factor solutions were used to predict the growth of fatigue cracks using a model based on Paris Law and SIF solutions by Newman and Raju with plastic zone size corrections. Fatigue life was predicted for plates with and without attachments. It could be seen that the predicted life of a weld toe crack was severely reduced with the addition of a welded attachment. The model was extended to the multiple surface cracks commonly observed at the weld toe, where each crack is treated as independent, following established code procedures. The multiple cracks will coalesce as they propagate, until a single dominant crack emerges and fracture occurs. In this paper, the relationship between the fatigue life and the number and density distribution of the initial cracks was investigated. Fatigue life was predicted for plates with attachments with 1, 2, 10 and 100 cracks initially. The results show that as the number of cracks increases, the predicted fatigue life decreases.
- 19 June 2016
- Published by ASME International
Fatigue Algorithm for Modeling Many Weld Toe Cracks Propagating at Welded Joints
Fatigue crack growth at welded joints often propagates from as many as tens to hundreds of small weld toe cracks along the weld toe line in offshore welded structures. This paper will present a fatigue algorithm for modeling many small weld toe cracks propagating from a welded joint. Cracks usually initiate at the weld toe region of the structures and propagate as surface cracks at the stress concentration regions of the weld-toe line. The presence of such weld defects or crack-like flaws can have a severe detrimental effect on their fatigue life and fracture resistance. Currently, there is a lack of studies that considers the effects of multiple cracks and their distribution density in welded joints. This work focuses on the fatigue analysis and modeling of multiple weld toe cracks, specifically in T-butt joints. Fatigue crack growth prediction is usually determined by the stress intensity factor range and crack propagation rate through Paris law. To predict the Stress Intensity Factor (SIF) of a weld toe crack, the magnification (Mk) factor was used. The Mk factor is influenced by the size of the welded attachment, as well as the size and depth of the weld toe crack. Simplified solutions for practical prediction of Mk factors were determined from 3D extended finite element method (XFEM) by modelling a semi-elliptical weld toe crack in a T-butt weld for cracks of different dimensions. The accuracy of the Mk factor solutions was verified by comparison to HSE fatigue data on 16 mm thick tubular joints. The Mk factor solutions were used to predict the growth of fatigue cracks using a model based on Paris Law and SIF solutions by Newman and Raju with plastic zone size corrections. Fatigue life was predicted for plates with and without attachments. It could be seen that the predicted life of a weld toe crack was severely reduced with the addition of a welded attachment. The model was extended to the multiple surface cracks commonly observed at the weld toe, where each crack is treated as independent, following established code procedures. The multiple cracks will coalesce as they propagate, until a single dominant crack emerges and fracture occurs. In this paper, the relationship between the fatigue life and the number and density distribution of the initial cracks was investigated. Fatigue life was predicted for plates with attachments with 1, 2, 10 and 100 cracks initially. The results show that as the number of cracks increases, the predicted fatigue life decreases.
- 19 June 2016
- Published by ASME International
Fatigue Modelling of Semi-Elliptical Surface Cracks in Welded Pipe Geometries
Offshore pipelines and risers transfer oil and gas across long distances, from seabed to production facility to the surface. The long pipelines are formed by welding together pipe segments. The welded joints formed are a source of stress concentration and defects from which fatigue cracks can grow. Hence, it is imperative that the effect of the weld geometry on the stress concentration be understood so that appropriate measures can be taken to assess the potential remaining service life of the welded structure. The effects can be understood by the linear elastic fracture mechanics approach, where the stress intensity factors quantify the stress concentration. While the classical equations of Newman and Raju have been long available for semi-elliptical surface cracks in plates, no similarly elegant stress intensity factor solutions are available for pipes. There have been solutions in tabular form which can be cumbersome in practice. Moreover, solutions of welded pipe geometries have not been developed. The objectives of the current work are to develop closed-form solutions for stress intensity factors for external semi-elliptical surface cracks in plates. The welded pipe geometry will also be studied to develop solutions for the weld toe magnification factors of welded pipe geometries. The stress intensity factors can be used to determine the propagation rate of cracks in pipe or welded pipe geometries. The stress intensity factors are obtained by the J-integral output of the three-dimensional finite element method. First, a plate with a circular crack is modelled. The initial step transforms the model to a plate with a semi-elliptical crack with the appropriate crack aspect ratio and width. A second transformation follows to transform the geometry to pipe form. The main parameters studied are the relative crack depth to thickness, crack aspect ratio, radius and thickness. The developed stress intensity factor solutions can be reduced to the classical equations. The new solutions show good agreement compared to previous work. A similar approach is developed to study the welded pipe geometry to develop weld toe magnification factor solutions. The weld toe magnification factor solutions for certain geometries are presented as a function of the relative crack depth. The stress intensity factor solutions are then applied to predict the crack growth rates of cracks in pipe geometries. The prediction was conducted by a program written to assess the fatigue life of single and multiple cracks in pipes and welded pipes. The fatigue life assessment of welded pipes using the weld toe magnification factor solutions shows how significantly the weld geometry affects fatigue life.
- 19 June 2016
- Published by ASME International
Fatigue Modelling of Semi-Elliptical Surface Cracks in Welded Pipe Geometries
Offshore pipelines and risers transfer oil and gas across long distances, from seabed to production facility to the surface. The long pipelines are formed by welding together pipe segments. The welded joints formed are a source of stress concentration and defects from which fatigue cracks can grow. Hence, it is imperative that the effect of the weld geometry on the stress concentration be understood so that appropriate measures can be taken to assess the potential remaining service life of the welded structure. The effects can be understood by the linear elastic fracture mechanics approach, where the stress intensity factors quantify the stress concentration. While the classical equations of Newman and Raju have been long available for semi-elliptical surface cracks in plates, no similarly elegant stress intensity factor solutions are available for pipes. There have been solutions in tabular form which can be cumbersome in practice. Moreover, solutions of welded pipe geometries have not been developed. The objectives of the current work are to develop closed-form solutions for stress intensity factors for external semi-elliptical surface cracks in plates. The welded pipe geometry will also be studied to develop solutions for the weld toe magnification factors of welded pipe geometries. The stress intensity factors can be used to determine the propagation rate of cracks in pipe or welded pipe geometries. The stress intensity factors are obtained by the J-integral output of the three-dimensional finite element method. First, a plate with a circular crack is modelled. The initial step transforms the model to a plate with a semi-elliptical crack with the appropriate crack aspect ratio and width. A second transformation follows to transform the geometry to pipe form. The main parameters studied are the relative crack depth to thickness, crack aspect ratio, radius and thickness. The developed stress intensity factor solutions can be reduced to the classical equations. The new solutions show good agreement compared to previous work. A similar approach is developed to study the welded pipe geometry to develop weld toe magnification factor solutions. The weld toe magnification factor solutions for certain geometries are presented as a function of the relative crack depth. The stress intensity factor solutions are then applied to predict the crack growth rates of cracks in pipe geometries. The prediction was conducted by a program written to assess the fatigue life of single and multiple cracks in pipes and welded pipes. The fatigue life assessment of welded pipes using the weld toe magnification factor solutions shows how significantly the weld geometry affects fatigue life.
- 1 June 2016
- Published by Elsevier in International Journal of Fatigue
- Vol. 87, 279-287
Stress intensity factors for fatigue analysis of weld toe cracks in a girth-welded pipe
- 1 June 2016
- Published by Elsevier in International Journal of Fatigue
- Vol. 87, 279-287
Stress intensity factors for fatigue analysis of weld toe cracks in a girth-welded pipe
- 15 March 2014
- Published by Springer Nature in Journal of Nondestructive Evaluation
- Vol. 33 (3) , 413-426
Fatigue Growth Analysis of Pre Induced Surface Defects Using Piezoelectric Wafer Based Impedance Method and Digital Image Correlation System
- 15 March 2014
- Published by Springer Nature in Journal of Nondestructive Evaluation
- Vol. 33 (3) , 413-426
Fatigue Growth Analysis of Pre Induced Surface Defects Using Piezoelectric Wafer Based Impedance Method and Digital Image Correlation System
- 12 March 2014
- Published by Trans Tech Publications, Ltd. in Advanced Materials Research
- Vol. 891-892, 551-556
Fatigue Monitoring of Double Surface Defects Using PZT Based Electromechanical Impedance and Digital Image Correlation Methods
Most of the engineering failures especially in mechanical and aerospace industry are due to the fatigue. Fatigue cracks and their propagation can be monitored by observing changes in the structural stiffness resulting from strength reduction as a function of the number of loading cycles. This monitoring can be observed using piezoceramic (PZT) transducer based electromechanical impedance (EMI) technique, and digital image correlation (DIC) system which uses variations on structural surface. The fatigue load usually aggravates the fracture if any defects pre-exist in the structure. The present work monitors multiple-crack emanating from electrode sparked multiple plane defects which are induced in to the specimens prior to the fatigue test, using EMI technique and DIC system. The fracture occurs much below the ultimate stress for the structures which already have defects as in the present case. EMI technique uses signature comparison of healthy and cracked state of the structure to depict crack growth. Initial detection of surface hair-line cracks from the corners of induced defects and their propagation till merging and subsequent failure were explained by signature variations and DIC techniques. Thus, a signal processing technique EMI, and image processing technology DIC were found to complement each other in prediction of early crack and their appearance on surface of the specimens.
- 12 March 2014
- Published by Trans Tech Publications, Ltd. in Advanced Materials Research
- Vol. 891-892, 551-556
Fatigue Monitoring of Double Surface Defects Using PZT Based Electromechanical Impedance and Digital Image Correlation Methods
Most of the engineering failures especially in mechanical and aerospace industry are due to the fatigue. Fatigue cracks and their propagation can be monitored by observing changes in the structural stiffness resulting from strength reduction as a function of the number of loading cycles. This monitoring can be observed using piezoceramic (PZT) transducer based electromechanical impedance (EMI) technique, and digital image correlation (DIC) system which uses variations on structural surface. The fatigue load usually aggravates the fracture if any defects pre-exist in the structure. The present work monitors multiple-crack emanating from electrode sparked multiple plane defects which are induced in to the specimens prior to the fatigue test, using EMI technique and DIC system. The fracture occurs much below the ultimate stress for the structures which already have defects as in the present case. EMI technique uses signature comparison of healthy and cracked state of the structure to depict crack growth. Initial detection of surface hair-line cracks from the corners of induced defects and their propagation till merging and subsequent failure were explained by signature variations and DIC techniques. Thus, a signal processing technique EMI, and image processing technology DIC were found to complement each other in prediction of early crack and their appearance on surface of the specimens.
- 1 July 2013
- Published by Elsevier in Mechanics of Materials
- Vol. 60, 144-158
A review of recent works on inclusions
- 1 July 2013
- Published by Elsevier in Mechanics of Materials
- Vol. 60, 144-158
A review of recent works on inclusions
- 1 February 2012
- Published by Elsevier in Mechanics of Materials
- Vol. 45, 1-9
On the fracture behavior of a Zener–Stroh crack with plastic zone correction in three-phase cylindrical composite material
- 1 February 2012
- Published by Elsevier in Mechanics of Materials
- Vol. 45, 1-9
On the fracture behavior of a Zener–Stroh crack with plastic zone correction in three-phase cylindrical composite material