Leposava Sidjanin
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Research Interests
Leposava Sidjanin has a total of 26 co-authors. Here are the top co-authors by number of shared publications:
- Dragan Rajnovic
Department of Production Engineering, Faculty of Technical Science, University of Novi Sad, Trg Dositeja Obradovica 6, 21000 Novi Sad, Serbia
8 shared publications - Petar Janjatovic
Department of Production Engineering, Faculty of Technical Sciences, University of Novi Sad, Trg Dositeja Obradovića 6, 21000 Novi Sad, Serbia
7 shared publications - Sebastian Balos
Faculty of Technical Sciences, University of Novi Sad, Trg Dositeja Obradovica 6, 21000 Novi Sad, Serbia
7 shared publications - Borislav Savkovic
University of Novi Sad
2 shared publications - Danka Labus Zlatanovic
Department of Production Technology, Technische Universität Ilmenau, 98693 Ilmenau, Germany
2 shared publications - Lihui Lang
School of Mechanical Engineering and Automation, Beihang University, Beijing 100191, China
2 shared publications
Latest Publications
- Open Access
- 1 January 2024
- Published by Društvo za unapređivanje zavarivanja u Srbiji - DUZS in Zavarivanje i zavarene konstrukcije
- Vol. 69 (1) , 17-23
Activated flux based on TiO2 nano and micro particles for A-TIG welding
In this paper, the A-TIG welding technology, a variation of the TIG welding process with an activated flux, was presented. An experimental investigation of an innovative flux based on a mixture of nano and micron oxide particles in solvent was shown. The zeta potential of the flux, the macro test, the microstructure and microhardness test were performed. Also, based on the obtained results, a model of the liquid metal flow in the weld metal is shown, where the increase in depth occurs due to a change in the direction of liquid metal flow from the edge to the middle of the weld metal. It has been shown that the mixture of nano and micron particles has the highest efficiency, due to the grinding effect of agglomerated nano particles.
- 1 January 2024
- Published by Društvo za unapređivanje zavarivanja u Srbiji - DUZS in Zavarivanje i zavarene konstrukcije
- Vol. 69 (1) , 17-23
Open AccessActivated flux based on TiO2 nano and micro particles for A-TIG welding
In this paper, the A-TIG welding technology, a variation of the TIG welding process with an activated flux, was presented. An experimental investigation of an innovative flux based on a mixture of nano and micron oxide particles in solvent was shown. The zeta potential of the flux, the macro test, the microstructure and microhardness test were performed. Also, based on the obtained results, a model of the liquid metal flow in the weld metal is shown, where the increase in depth occurs due to a change in the direction of liquid metal flow from the edge to the middle of the weld metal. It has been shown that the mixture of nano and micron particles has the highest efficiency, due to the grinding effect of agglomerated nano particles.
- Open Access
- 2 December 2023
- Published by Faculty of Technical Sciences in Advanced Technologies & Materials
- Vol. 48 (2) , 37-43
Influence of Strain Rate on Metallurgical and Mechanical Properties of Friction Stir Spot Welded Aluminium Joints
Nowadays, the substitution of copper with aluminium is widely pursued in order to save weight and material costs, for battery components and wire connectors. Additionally, cost reductions can be further enhanced with effective reduction of energy consumption through efficient manufacturing. Therefore, friction stir spot welding as a solid-state welding technique is a potential choice with low energy demands and high joining performances. However, the joining of aluminium and its alloys with solid-state welding techniques is still a challenging task due to a persistent and chemically stable aluminium oxide layer formed at the sheets prior to the welding, due to the reaction between aluminium and atmospheric oxygen. In this paper, the influence of strain rate induced during friction stir spot welding process on the metallurgical, mechanical and electrical properties of friction stir spot welding of AA 5754-H111 was studied. The strain rate was calculated according to the rotational speed of the tool and the effective (average) radius and depth of the stir zone. It was observed that the specimens welded with a lower strain rate endured a 15 % higher average strain failure load compared to the specimens welded at a higher share rate. The microhardness profiles of the specimens obtained at low strain rates imply strain hardening mechanisms in the weld zone, while the microhardness of specimens welded at high strain rates expressed thermal softening. It was also found that the friction welded sheets, regardless of the strain rate, show increased electrical resistance compared to the base material, however, it decreases with an increase in strain rate. Microstructural analysis reveals a stress-induced metallurgical transformation in the narrow zone around the weld-faying interface.
- 2 December 2023
- Published by Faculty of Technical Sciences in Advanced Technologies & Materials
- Vol. 48 (2) , 37-43
Open AccessInfluence of Strain Rate on Metallurgical and Mechanical Properties of Friction Stir Spot Welded Aluminium Joints
Nowadays, the substitution of copper with aluminium is widely pursued in order to save weight and material costs, for battery components and wire connectors. Additionally, cost reductions can be further enhanced with effective reduction of energy consumption through efficient manufacturing. Therefore, friction stir spot welding as a solid-state welding technique is a potential choice with low energy demands and high joining performances. However, the joining of aluminium and its alloys with solid-state welding techniques is still a challenging task due to a persistent and chemically stable aluminium oxide layer formed at the sheets prior to the welding, due to the reaction between aluminium and atmospheric oxygen. In this paper, the influence of strain rate induced during friction stir spot welding process on the metallurgical, mechanical and electrical properties of friction stir spot welding of AA 5754-H111 was studied. The strain rate was calculated according to the rotational speed of the tool and the effective (average) radius and depth of the stir zone. It was observed that the specimens welded with a lower strain rate endured a 15 % higher average strain failure load compared to the specimens welded at a higher share rate. The microhardness profiles of the specimens obtained at low strain rates imply strain hardening mechanisms in the weld zone, while the microhardness of specimens welded at high strain rates expressed thermal softening. It was also found that the friction welded sheets, regardless of the strain rate, show increased electrical resistance compared to the base material, however, it decreases with an increase in strain rate. Microstructural analysis reveals a stress-induced metallurgical transformation in the narrow zone around the weld-faying interface.
- Open Access
- 27 March 2023
- Published by MDPI AG in Journal of Manufacturing and Materials Processing
- Vol. 7 (2) , 72
The Chip Formation Process When Cutting High-Speed Steels and Ti3SiC2 Ceramics
The paper presents the microstructural characterization of the chip roots in high-speed steels and ceramic Ti3SiC2. The process of chip formation and the obtaining of adequate samples were carried out using the quick-stop method. The tests were carried out during the milling process; the “quick stop” method was carried out in order to obtain samples of the chip roots. This method was developed in-house by the authors. The chip roots were microscopically studied by means of a light microscope (LM) and a scanning electron microscope (SEM). Before the actual analysis, preparation was performed based on the standard metallographic technique. The analysis of the high-speed steels samples showed that, for the used cutting conditions, a discontinuous chip with a built-up edge (BUE) was formed. During the processing of the Ti3SiC2 ceramic, a significant difference was manifested in the chip formation process and a powder-like chip was produced. After utilizing a careful cutting process, a chip pattern was observed, from which it is evident that chip breakage during ceramic processing occurs without prior plastic deformation. In addition, the cutting force Fc was also measured during the milling process of the high-speed steels and the ceramic, and it was correlated with the cutting speed, feed per tooth and depth of cut.
- 27 March 2023
- Published by MDPI AG in Journal of Manufacturing and Materials Processing
- Vol. 7 (2) , 72
Open AccessThe Chip Formation Process When Cutting High-Speed Steels and Ti3SiC2 Ceramics
The paper presents the microstructural characterization of the chip roots in high-speed steels and ceramic Ti3SiC2. The process of chip formation and the obtaining of adequate samples were carried out using the quick-stop method. The tests were carried out during the milling process; the “quick stop” method was carried out in order to obtain samples of the chip roots. This method was developed in-house by the authors. The chip roots were microscopically studied by means of a light microscope (LM) and a scanning electron microscope (SEM). Before the actual analysis, preparation was performed based on the standard metallographic technique. The analysis of the high-speed steels samples showed that, for the used cutting conditions, a discontinuous chip with a built-up edge (BUE) was formed. During the processing of the Ti3SiC2 ceramic, a significant difference was manifested in the chip formation process and a powder-like chip was produced. After utilizing a careful cutting process, a chip pattern was observed, from which it is evident that chip breakage during ceramic processing occurs without prior plastic deformation. In addition, the cutting force Fc was also measured during the milling process of the high-speed steels and the ceramic, and it was correlated with the cutting speed, feed per tooth and depth of cut.
- 15 December 2022
- Published by Faculty of Technical Sciences in Advanced Technologies & Materials
- Vol. 47 (2) , 17-20
Pitting Corrosion of Austenitic Stainless Steel Weld in Brewing Industry: Case Study
In this paper, a case study of pitting corrosion of austenitic stainless steel weld of a pipe in brewing industry is presented. Pitting corrosion caused leakage and the cause of corrosion was sought to be found. After a comprehensive investigation, comprising of visual inspection, chemical composition, hardness, tensile and metallographic testing. It was found that there are two reasons that influenced the occurrence of pitting corrosion, both related to welding process. The first is the unnecessary cleaning of the inside of the pipe by wire brush tool on the power drill, introducing creases that held the acidic cleaning agent. The concentration of the acid rose after evaporation that caused the corrosion, aided by the tinting of the weld zone. Tinting was caused by insufficient oxygen purging from the inside of the pipe by shielding gas. After welding, no passivation was performed, which left the heat tinting layer with compromised corrosion resistance
- 15 December 2022
- Published by Faculty of Technical Sciences in Advanced Technologies & Materials
- Vol. 47 (2) , 17-20
Pitting Corrosion of Austenitic Stainless Steel Weld in Brewing Industry: Case Study
In this paper, a case study of pitting corrosion of austenitic stainless steel weld of a pipe in brewing industry is presented. Pitting corrosion caused leakage and the cause of corrosion was sought to be found. After a comprehensive investigation, comprising of visual inspection, chemical composition, hardness, tensile and metallographic testing. It was found that there are two reasons that influenced the occurrence of pitting corrosion, both related to welding process. The first is the unnecessary cleaning of the inside of the pipe by wire brush tool on the power drill, introducing creases that held the acidic cleaning agent. The concentration of the acid rose after evaporation that caused the corrosion, aided by the tinting of the weld zone. Tinting was caused by insufficient oxygen purging from the inside of the pipe by shielding gas. After welding, no passivation was performed, which left the heat tinting layer with compromised corrosion resistance
- Open Access
The Effect of Water Concentration in Ethyl Alcohol on the Environmentally Assisted Embrittlement of Austempered Ductile Irons
Austempered ductile iron (ADI) is an advanced cast iron material that has a broad field of application and, among others, it is used in contact and for conveyance of fluids. However, it is noticed that in contact with some fluids, especially water, ADI material becomes brittle. The most significant decrease is established for the elongation. However, the influence of water and the cause of this phenomenon is still not fully understood. For that reason, in this paper, the influence of different water concentrations in ethyl alcohol on the mechanical properties of ADI materials was studied. The test was performed on two different types of ADI materials in 0.2, 4, 10, and 100 vol.% water concentration environments, and in dry condition. It was found that even the smallest concentration of water (0.2 vol.%) causes formation of the embrittled zone at fracture surface. However, not all mechanical properties were affected equally and not all water concentrations have been critical. The highest deterioration was established in the elongation, followed by the ultimate tensile strength, while the proof strength was affected least.
Open AccessThe Effect of Water Concentration in Ethyl Alcohol on the Environmentally Assisted Embrittlement of Austempered Ductile Irons
Austempered ductile iron (ADI) is an advanced cast iron material that has a broad field of application and, among others, it is used in contact and for conveyance of fluids. However, it is noticed that in contact with some fluids, especially water, ADI material becomes brittle. The most significant decrease is established for the elongation. However, the influence of water and the cause of this phenomenon is still not fully understood. For that reason, in this paper, the influence of different water concentrations in ethyl alcohol on the mechanical properties of ADI materials was studied. The test was performed on two different types of ADI materials in 0.2, 4, 10, and 100 vol.% water concentration environments, and in dry condition. It was found that even the smallest concentration of water (0.2 vol.%) causes formation of the embrittled zone at fracture surface. However, not all mechanical properties were affected equally and not all water concentrations have been critical. The highest deterioration was established in the elongation, followed by the ultimate tensile strength, while the proof strength was affected least.
- Open Access
Effect of Rotation of the Principal Stress Axes Relative to the Material on the Evolution of Material Properties in Severe Plastic Deformation Processes
Severe plastic deformation (SPD) processes are widely used for improving material properties. A distinguishing feature of many SPD processes is that the principal axes of the stress tensor intensively rotate relative to the material. Nevertheless, no measure of this rotation is involved in the constitutive equations that predict the evolution of material properties. In particular, a typical way of describing the effect of SPD processes on material properties is to show the dependence of various parameters that characterize these properties on the equivalent strain. However, the same level of the equivalent strain can be achieved in a process in which the principal axes of the stress tensor do not rotate relative to the material. It is, therefore, vital to understand which properties are dependent and which properties are independent of the rotation of the principal axes of the stress tensor relative to the material. In the present paper, a new multistage SPD process is designed such that the principal stress axes do not rotate relative to the material during each stage of the process but the directions of the major and minor principal stresses interchange between two subsequent stages. The process is practically plane strain, and it may be named the process of upsetting by V-shape dies. In addition, axisymmetric compression by Rastegaev’s method is conducted. In this case, the principal stress axes are fixed in the material throughout the entire process of deformation. Material properties and microstructure generated in the two processes above are compared to reveal the effect of the rotation of the principal stress axes relative to the material on the evolution of these properties.
Open AccessEffect of Rotation of the Principal Stress Axes Relative to the Material on the Evolution of Material Properties in Severe Plastic Deformation Processes
Severe plastic deformation (SPD) processes are widely used for improving material properties. A distinguishing feature of many SPD processes is that the principal axes of the stress tensor intensively rotate relative to the material. Nevertheless, no measure of this rotation is involved in the constitutive equations that predict the evolution of material properties. In particular, a typical way of describing the effect of SPD processes on material properties is to show the dependence of various parameters that characterize these properties on the equivalent strain. However, the same level of the equivalent strain can be achieved in a process in which the principal axes of the stress tensor do not rotate relative to the material. It is, therefore, vital to understand which properties are dependent and which properties are independent of the rotation of the principal axes of the stress tensor relative to the material. In the present paper, a new multistage SPD process is designed such that the principal stress axes do not rotate relative to the material during each stage of the process but the directions of the major and minor principal stresses interchange between two subsequent stages. The process is practically plane strain, and it may be named the process of upsetting by V-shape dies. In addition, axisymmetric compression by Rastegaev’s method is conducted. In this case, the principal stress axes are fixed in the material throughout the entire process of deformation. Material properties and microstructure generated in the two processes above are compared to reveal the effect of the rotation of the principal stress axes relative to the material on the evolution of these properties.
- Open Access
Determination of the Grain Size in Single-Phase Materials by Edge Detection and Concatenation
This paper presents a novel approach for edge detection and concatenation. It applies the proposed method on a set of optical microscopy images of aluminium alloy Al 99.5% (ENAW1050A) samples with different grain size values. The performance of the proposed approach is evaluated based on the intercept method and compared with the manual grain size determination method. Edge detection filters have proven inefficient in grain boundaries’ detection of the presented microscopy images. To some extent only the Canny edge-detection filter was able to compute grain boundaries of lower-resolution images adequately, while the presented method proved to be superior, especially in high-resolution images. The proposed method has proven its applicability, and it implies higher automatisation and lower processing times compared to manual optical microscopy image processing.
Open AccessDetermination of the Grain Size in Single-Phase Materials by Edge Detection and Concatenation
This paper presents a novel approach for edge detection and concatenation. It applies the proposed method on a set of optical microscopy images of aluminium alloy Al 99.5% (ENAW1050A) samples with different grain size values. The performance of the proposed approach is evaluated based on the intercept method and compared with the manual grain size determination method. Edge detection filters have proven inefficient in grain boundaries’ detection of the presented microscopy images. To some extent only the Canny edge-detection filter was able to compute grain boundaries of lower-resolution images adequately, while the presented method proved to be superior, especially in high-resolution images. The proposed method has proven its applicability, and it implies higher automatisation and lower processing times compared to manual optical microscopy image processing.
- Open Access
Metallographic Determination of Strain Distribution in Cold Extruded Aluminum Gear-Like Element
In this study, an experimental, metallographic method for determining strain distribution in a cold extruded aluminum gear-like element, based on the dependence of recrystallized grain size on prior deformation, was devised in order to overcome design problems in manufacturing of complex parts where critical values of strain and stress could cause a fracture. The method was applied on a 99.5% aluminum bar subjected to cold, radial extrusion, in order to produce complex gear-like element. To reveal the strain and stress distribution in specimens, the calibration and flow curves were first obtained by uniaxial compression (Rastegaev test). Afterwards, the grain size in different parts of the gear section was examined, the strain and stress distributions were calculated, and the results were confirmed by microhardness measurements. It was found that grain size, strain, stress, and microhardness considerably differed throughout the cross-section of the gear. The coarsest grain, and thus the lowest strain zone, was obtained in the central part of the tooth and in the zone between teeth. Conversely, the finest grains appeared in the highest strain zone at the specimen surface, particularly in the root of the teeth. Furthermore, results were supported by microhardness measurements, i.e., microhardness corresponded to grain size and strain hardening. Finally, the real view of material flow in the complex extruded part was successfully obtained by the metallographic method.
Open AccessMetallographic Determination of Strain Distribution in Cold Extruded Aluminum Gear-Like Element
In this study, an experimental, metallographic method for determining strain distribution in a cold extruded aluminum gear-like element, based on the dependence of recrystallized grain size on prior deformation, was devised in order to overcome design problems in manufacturing of complex parts where critical values of strain and stress could cause a fracture. The method was applied on a 99.5% aluminum bar subjected to cold, radial extrusion, in order to produce complex gear-like element. To reveal the strain and stress distribution in specimens, the calibration and flow curves were first obtained by uniaxial compression (Rastegaev test). Afterwards, the grain size in different parts of the gear section was examined, the strain and stress distributions were calculated, and the results were confirmed by microhardness measurements. It was found that grain size, strain, stress, and microhardness considerably differed throughout the cross-section of the gear. The coarsest grain, and thus the lowest strain zone, was obtained in the central part of the tooth and in the zone between teeth. Conversely, the finest grains appeared in the highest strain zone at the specimen surface, particularly in the root of the teeth. Furthermore, results were supported by microhardness measurements, i.e., microhardness corresponded to grain size and strain hardening. Finally, the real view of material flow in the complex extruded part was successfully obtained by the metallographic method.
- 20 December 2019
- Published by Faculty of Technical Sciences in Advanced Technologies & Materials
- Vol. 44 (2) , 7-11
Ballistic behavior of multilayer wire mesh application armor
In this paper, an attempt was made to increase the ballistic protection of the armor system by combining non-homogenous spaced armor in form of multilayer wire mesh with rolled homogenous armor steel base plate. Different angles of incidence were tested: 0, 20, 25 and 35o, by using 12.7 mm armor piercing incendiary ammunition from 100 m. It was found that the inclination of the armor system has a negative effect on ballistic resistance due to variations in wire body-to-body distance, some of which can increase, causing a decreased contact with the projectile and an insufficient yaw. The yaw causes a sideways impact on the base plate. However, the non-penetrating hits in vertical armor cause a more severe damage on the base plate compared to the inclined armor system. This effect is due to the inclination itself, which is a common behavior of increasing effectiveness of sloped armor.
- 20 December 2019
- Published by Faculty of Technical Sciences in Advanced Technologies & Materials
- Vol. 44 (2) , 7-11
Ballistic behavior of multilayer wire mesh application armor
In this paper, an attempt was made to increase the ballistic protection of the armor system by combining non-homogenous spaced armor in form of multilayer wire mesh with rolled homogenous armor steel base plate. Different angles of incidence were tested: 0, 20, 25 and 35o, by using 12.7 mm armor piercing incendiary ammunition from 100 m. It was found that the inclination of the armor system has a negative effect on ballistic resistance due to variations in wire body-to-body distance, some of which can increase, causing a decreased contact with the projectile and an insufficient yaw. The yaw causes a sideways impact on the base plate. However, the non-penetrating hits in vertical armor cause a more severe damage on the base plate compared to the inclined armor system. This effect is due to the inclination itself, which is a common behavior of increasing effectiveness of sloped armor.
- Open Access
- 1 January 2019
- Published by FapUNIFESP (SciELO) in Matéria (Rio de Janeiro)
- Vol. 24 (3)
Tensile and fatigue properties, machinability and machined surface roughness of Al-Si-Cu alloys
In this paper, the aim was to determine if ASC91 (9 % Al, 1 % Cu) could be replaced with ASC73 (7 % Al, 3 % Cu) aluminium alloy, with presumably improved machinability due to lower silicon content (9 to 7 %) and retained mechanical properties due to a higher copper content (1 to 3 %). The test samples were excised from cylinder heads produced by the lost-foam casting technique in industrial conditions. The tensile properties (proof strength, ultimate tensile strength, elongation and modulus of elasticity), fatigue performance, microstructure and machinability of two as-cast aluminium alloys were examined. The results of the fatigue tests were statistically analyzed using the stair-case method described in the UNI 3964 standard. Tensile properties of the ASC91 were higher, while fatigue properties were higher in the ASC73 alloy. The resultant force was lower for the ASC73, while roughness was lower for the ASC73 alloy, if the feed per tooth is higher than 0.21 mm/t. Two main factors that influence such behaviour are the amount of eutectic silicon and the α-solid solution adhesion to the cutting tool.
- 1 January 2019
- Published by FapUNIFESP (SciELO) in Matéria (Rio de Janeiro)
- Vol. 24 (3)
Open AccessTensile and fatigue properties, machinability and machined surface roughness of Al-Si-Cu alloys
In this paper, the aim was to determine if ASC91 (9 % Al, 1 % Cu) could be replaced with ASC73 (7 % Al, 3 % Cu) aluminium alloy, with presumably improved machinability due to lower silicon content (9 to 7 %) and retained mechanical properties due to a higher copper content (1 to 3 %). The test samples were excised from cylinder heads produced by the lost-foam casting technique in industrial conditions. The tensile properties (proof strength, ultimate tensile strength, elongation and modulus of elasticity), fatigue performance, microstructure and machinability of two as-cast aluminium alloys were examined. The results of the fatigue tests were statistically analyzed using the stair-case method described in the UNI 3964 standard. Tensile properties of the ASC91 were higher, while fatigue properties were higher in the ASC73 alloy. The resultant force was lower for the ASC73, while roughness was lower for the ASC73 alloy, if the feed per tooth is higher than 0.21 mm/t. Two main factors that influence such behaviour are the amount of eutectic silicon and the α-solid solution adhesion to the cutting tool.