VPVadim Ya. Pokrovskii

Vadim Ya. Pokrovskii

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article

Previous Organizations / Institutes

The organizations / institutes from the scholar's other articles in the past ten years


Vadim Ya. Pokrovskii has a total of 133 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Laboratory technology of micromanipulation using micropincers with shape memory effect to create suspended microstructures based on whiskers of functional materials

    by S.R. Romanov, V.V. Koledov, M.V. Nikitin, A.P. Orlov, V.YA. Pokrovsky, A.V. Shelyakov, D.A. Khachatryan, A.V. Kletsov, A.K. Pogorelov

    A technology for manipulating whisker-like single crystals (whiskers) of quasi-one-dimensional charge-density-wave (Q1D CDW) semiconductors was developed for the fabrication of suspended structures. A current-controlled microgripper based on shape memory alloy (SMA) composite ribbons was created. A technique for capturing and fixing whiskers using a micromanipulator and a tungsten probe was developed, together with a method for contact formation employing a mask transferred by the microgripper followed by metal deposition. Resonant modes of high-frequency electromechanical oscillations in a suspended TaS₃ whisker were detected and investigated using the heterodyne method.

  • Structural transformation of NbS 3 -I whiskers and formation of perfect NbS 3 -II interlayers with charge density waves

    by V Ya Pokrovskii, V P Martovitskii, M V Nikitin, S G Zybtsev

    X-ray studies of monoclinic NbS 3 (NbS 3 -I) whiskers in conventional and grazing geometry reveal layers of II and IV polytypes alternating along the c axis. The formation of layers is explained by partial spinodal decomposition initiated by stresses between twins. The samples demonstrate exceptionally perfect structure, in concordance with the monoclinic angle β = 105.3° of phase II corresponding to minimal stresses between twins. In the whiskers from the higher-temperature growth zone extremely thin layers of phase IV (about two lattice parameters c ) are revealed. This suggests the existence of similar layers of phase II. The coherent sliding of 2D charge density wave (CDW) in NbS 3 -II layers has been confirmed earlier by transport studies at room temperature. The whiskers from the lower-temperature growth zone show numerous individual fibers split off from the body of the whisker. They are misoriented about the whisker axis b by ±30°. A comparison of the lattice parameters of the whiskers and the inclusions shows that all whiskers are compressed in the longitudinal direction b and expanded along c . The compression along b can stimulate the formation of CDWs in NbS 3 -II. We are suggesting a general picture: the monoclinic angle of NbS 3 , and, therefore, the polytype, is determined by the concentration of sulfur vacancies. Shortage of sulfur in the layers of phase II is directly evidenced by the temperature dependence of resistance. The concept of spinodal decomposition, as well as its coupling with vacancies concentration, would logically apply to the large family of layered tri- and dichalcogenides, which are currently being widely studied.

  • Open Access

    Dynamics of a Charge Density Wave in the Field of an Acoustic Wave

    by D. Yu. Saltykova, M. V. Nikitin, V. Ya. Pokrovskii, S. G. Zybtsev, V. V. Kolesov, V. V. Kashin, I. E. Kuznetsova, I. A. Nedospasov

    Whiskers of a quasi-one-dimensional TaS 3 conductor with a charge density wave have been fixed (arranged) on the surface of a lithium niobate wafer. Upon excitation of acoustic waves of various types with a wavelength of λ = 3 mm in the wafer, Shapiro steps (ShSWs) are observed in the current–voltage characteristics of the whiskers, indicating synchronization of the sliding of the charge density wave with the acoustic waves. For a sample with a length of L = 740 μm ≈ λ/4, the ShSWs differ significantly in structure and amplitude dependence from the Shapiro steps ShSVs observed when a voltage at the same frequency is applied directly to the sample and reflect a more inhomogeneous character of the sliding of the charge density wave in the synchronization mode. When studying segments of the same sample with a length of L $$ \ll $$ λ, the differences between the ShSWs and ShSVs almost disappear. It has been concluded that the features of ShSWs in long samples are attributed to the spatial inhomogeneity of the high-frequency electric and/or elastic field. The obtained results open up broad possibilities for combining acoustoelectronic devices and quasi-one-dimensional conductors with the charge density wave.

  • Open Access

    Interaction between Charge Density Waves in the Monoclinic Phase of NbS3

    by V. Ya. Pokrovskii, A. L. Vasiliev, N. B. Bolotina, A. G. Ivanova, S. V. Zaitsev-Zotov, S. G. Zybtsev, A. A. Sinchenko

    In the monoclinic polytype NbS3-II, the monoclinic b-axis of which coincides with the direction of greatest conductivity, two charge density waves (CDWs) have been observed at room temperature: CDW-0 with the wave vector q 0 = 0.5a* + 0.352b* + 0.5c* and CDW-1 with the wave vector q 1 = 0.5a* + 0.298b* + 0.5c*. X‑ray diffraction patterns obtained in the temperature range of 90–500 K have shown that the vectors q 0 and q 1 depend on the temperature, but their b* coordinates satisfy the relation $$2q_{0}^{{{\mathbf{b}}\text{*}}}(T) + q_{1}^{{{\mathbf{b}}\text{*}}}(T) = {\text{const}} = 1$$ . It has been concluded that the wave vector q 1 of CDW-1 is determined not only by the nesting of Fermi surfaces, but also by the vector q 0, because CDW-1 is adjusted to the second harmonic of CDW-0, which indicates the interaction between charge density waves. This conclusion has been confirmed by structural studies of NbS3-II samples, the lattice of which is strongly deformed due to a high concentration of twins. In these samples, CDW-0 is conserved, and the wave vector of CDW-1 has the b* component not related to q 0.


  • Effect of the Deformation on the Conductivity of the Quasi-One-Dimensional Conductor K0.3MoO3 in the Peierls State

    by S. G. Zybtsev, V. Ya. Pokrovskii, S. V. Zaitsev-Zotov

    The conductivity σ of the quasi-one-dimensional conductor K0.3MoO3 in low fields has been studied as a function of the temperature and uniaxial strain ε. It has been found that the Peierls transition temperature decreases under tensile strain and increases under compressive strain. A hysteresis is observed on the dependences σ(ε) for the Peierls state. The dependences indicate a strain-induced change in the wave vector of a charge density wave. This result seems to contradict the absence of a decrease in Young’s modulus in K0.3MoO3 at the depinning of the charge density wave. It has been shown that this contradiction is resolved by taking into account the transverse components in the deformation of the charge density wave and the lattice and the three-dimensional nature of their interaction.


  • Spektry propuskaniya infrakrasnogo izlucheniya v TiS3: kray fundamental'nogo pogloshcheniya, fonony i eksitony

    by K. N Boldyrev, E. V Mostovshchikova, A. N Titov, V. Ya Pokrovskiy, I. G. Gorlova, Мостовщикова Е. В, Покровский В. Я

    Исследованы спектры пропускания инфракрасного и видимого излучения монокристаллическими вискерами TiS3 при разных поляризациях света в диапазоне температур от комнатной до гелиевой. Определены абсолютные значения коэффициента поглощения. В области дальнего инфракрасного излучения наблюдались неизвестные ранее фононные моды. Изучена зависимость ширины запрещенной зоны E g от температуры и показано, что E g увеличивается на 50 мэВ при охлаждении от 300 до 5К. Сравнение спектров, снятых при разных направлениях поляризации, указывает на анизотропию оптической щели. Ниже ∼150К обнаружен пик поглощения с энергией 1.28 эВ, который объясняется возбуждением экситонов.

  • Open Access

    Infrared Transmission Spectra of TiS3: Fundamental Absorption Edge, Phonons, and Excitons

    by K. N. Boldyrev, E. V. Mostovshchikova, A. N. Titov, V. Ya. Pokrovskii, I. G. Gorlova

    Transmission spectra of TiS3 single crystal whiskers in the infrared and optical bands have been studied at various light polarizations in the temperature range from room to liquid helium. The absolute absorption coefficients have been determined. Previously unknown phonon modes have been observed in the far infrared region. The study of the temperature dependence of the band gap width $${{\mathcal{E}}_{{\text{g}}}}$$ has shown that it increases by 50 meV under cooling from 300 to 5 K. The comparison of spectra measured at different polarization directions indicates that the optical gap is anisotropic. A 1.28-eV absorption peak has been detected below ~150 K and has been attributed to the excitation of excitons.


  • Logarifmicheskaya relaksatsiya fotoprovodimosti kvaziodnomernogo poluprovodnika TiS3

    by I. G. Gorlova, S. G. Zybtsev, V. Ya Pokrovskiy, S. A Nikonov, S. V Zaytsev-Zotov, A. N Titov, Покровский В. Я

    Исследованы переходные процессы в фотопроводимости монокристаллов TiS3 при подаче на образец прямоугольных импульсов света в области длин волн λ = 405−940 нм. Установлено, что спад фотопроводимости после выключения излучения при температурах от 180 до 78К описывается логарифмическим законом в интервале от 10-3 до 102 с, т.е. при изменении времени на 5 порядков. Это означает, что процесс релаксации характеризуется временами, распределенными в диапазоне от десятков микросекунд до десятков минут, как минимум. Показано, что релаксация имеет преимущественно последовательный характер: барьер для рекомбинации повышается по мере приближения проводимости к равновесному значению.

  • Spinodal'nyy raspad viskerov NbS3 c volnami zaryadovoy plotnosti

    by V. P Martovitskiy, M. V Nikitin, V. Ya Pokrovskiy, Мартовицкий В. П, Покровский В. Я

    Рентгенодифракционное исследование в скользящей геометрии вискеров NbS3 II фазы с волнами зарядовой плотности показало, что в них вместо одиночных пиков (h0l) присутствуют пары уширенных рефлексов от двух близких фаз с углами моноклинности β1 и β2. Фаза с меньшим углом моноклинности β1 = 95.9 ÷ 97.2° близка по структурным параметрам к фазе I без волн зарядовой плотности. Фаза II с β2 = 99.9 ÷ 100.0° имеет пониженное значение параметра решетки вдоль сильнейшей связи (оси b), что предполагает повышенную концентрацию вакансий серы в этой фазе по сравнению с фазой I. Сделан вывод, что в исследованных вискерах произошел спинодальный распад c перераспределением вакансий серы, в результате которого наблюдается чередование фаз в направлении поперек слоев (001). В лучшем по структурному совершенству вискере II фазы наблюдается сателлитная структура, свидетельствующая об образовании сверхрешетки с периодом 35.2 нм в этом направлении. Спинодальный распад сочетается с высокими внутренними напряжениями, присутствующими в вискерах с моноклинной решеткой. Частичный спинодальный распад наблюдается и в некоторых вискерах I фазы без волн зарядовой плотности с появлением тонких прослоек фазы IV и фазы II с углом моноклинности β = 104°. Существование тонких слоев фазы II в объеме фазы I таких образцов подтверждается наблюдением ступенек Шапиро на вольт-амперных характеристиках при подаче высокочастотного напряжения. Фактор спинодального распада необходимо учитывать при описании свойств вискеров NbS3, номинально относящихся к тому или иному политипу.

  • Logarithmic Relaxation of the Photoconductivity of a Quasi-One-Dimensional TiS3 Semiconductor

    by I. G. Gorlova, S. G. Zybtsev, V. Ya. Pokrovskii, S. A. Nikonov, S. V. Zaitsev-Zotov, A. N. Titov

    Transient processes in the photoconductivity of TiS3 single crystals exposed to rectangular light pulses in the wavelength range of λ = 405–940 nm are investigated. It is established that the decay in the photoconductivity after switching the light off at temperatures from 78 to 180 K is described by a logarithmic law in the range from 10–3 to 102 s (i.e., when time changes by five orders of magnitude). This means that the relaxation process is characterized by times ranging, at least, from several tens of microseconds to several tens of minutes. It is shown that the relaxation is basically successive: the recombination barrier increases while the conductivity approaches the equilibrium value.