Xiao-Hua Zheng
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Xiao-Hua Zheng has a total of 38 co-authors. Here are the top co-authors by number of shared publications:
Fang-Er Yang
College of Materials Science and Engineering, Zhejiang University of Technology 1 , Hangzhou 310014, China
3 shared publications- Fang-Er Yang
College of Materials Science and Engineering, Zhejiang University of Technology, Hangzhou, China
3 shared publications Gong-Qi Wang
Technical Department of Constant Velocity Drive Shaft Factory, Wanxiang Qianchao Co., Ltd. 2 , Hangzhou 311215, China
3 shared publicationsFanger Yang
College of Materials Science and Engineering, Zhejiang University of Technology, Hangzhou, China
2 shared publicationsShuo-Yan Yang
2 shared publicationsTao Liu
2 shared publications
Latest Publications
- 16 June 2025
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 34 (24) , 29868-29879
Preparation, Microstructure, and Electrical Contact Performance of Ag/LaNixCo1-xO3 Electrical Contact Materials
- 16 June 2025
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 34 (24) , 29868-29879
Preparation, Microstructure, and Electrical Contact Performance of Ag/LaNixCo1-xO3 Electrical Contact Materials
- 7 May 2024
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 35 (13) , 1-16
Interfacial wettability and electrical properties of Ni-doped Ag/Bi2Sn2O7 electrical contact materials
- 7 May 2024
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 35 (13) , 1-16
Interfacial wettability and electrical properties of Ni-doped Ag/Bi2Sn2O7 electrical contact materials
- Open Access
High Temperature Tribological Behavior of Electroless Plating Ni-P-Si3N4-WS2 Composite Coatings
Electroless nickel composite coatings have the potential for high-temperature tribological applications, and a combination of high wear resistance and low friction factor is one of the desirable solutions but still a tricky problem. The addition of self-lubricating WS2 and hard Si3N4 nanoparticles to the Ni-P coatings is expected to obtain good high-temperature tribological performance. In this work, Ni-P-Si3N4-WS2 composite coatings with various contents of WS2 nanoparticles were prepared using electroless plating and subsequently annealed at 400 °C in an inert atmosphere. The tribological properties of the coatings were evaluated using a ball-on-disc wear instrument at operating temperatures from 25 to 600 °C. The microstructure, chemical composition, and surface morphology of the coatings were characterized by X-ray diffractometry (XRD), energy disperse spectroscopy (EDS), and scanning electron microscopy (SEM). Upon increasing the WS2 dosage in the bath, the WS2 content in the coating increased and the micro-hardness of the as-plated coating increased from 539 to 717 HV. After heat treatment, the coating underwent a crystallization process, and the hardness increased from 878 to 1094 HV. The main wear mechanism of the coating changed from adhesive wear in the as-plated state to abrasive wear in the annealed state. The annealed Ni-P-Si3N4-WS2 coating with a WS2 dosage of 2.5 g/L in the bath exhibited excellent mechanical properties, with a hardness of 10.9 GPa, a friction coefficient of ~0.51, and a wear rate of 8.4 × 10−15 m3N−1⋅m−1 at room temperature, and maintained optimal performance at high temperatures. At operating temperatures of 200, 400, and 600 °C, the form of wear was adhesive wear for coatings with a WS2 dosage 2 dosage ≥1.5 g/L. The synergism of WS2 and Si3N4 particles refined the grains of the Ni-P matrix in as-plated coatings and obviously reduced the friction coefficient of friction pairs in annealed coatings at all operating temperatures.
Open AccessHigh Temperature Tribological Behavior of Electroless Plating Ni-P-Si3N4-WS2 Composite Coatings
Electroless nickel composite coatings have the potential for high-temperature tribological applications, and a combination of high wear resistance and low friction factor is one of the desirable solutions but still a tricky problem. The addition of self-lubricating WS2 and hard Si3N4 nanoparticles to the Ni-P coatings is expected to obtain good high-temperature tribological performance. In this work, Ni-P-Si3N4-WS2 composite coatings with various contents of WS2 nanoparticles were prepared using electroless plating and subsequently annealed at 400 °C in an inert atmosphere. The tribological properties of the coatings were evaluated using a ball-on-disc wear instrument at operating temperatures from 25 to 600 °C. The microstructure, chemical composition, and surface morphology of the coatings were characterized by X-ray diffractometry (XRD), energy disperse spectroscopy (EDS), and scanning electron microscopy (SEM). Upon increasing the WS2 dosage in the bath, the WS2 content in the coating increased and the micro-hardness of the as-plated coating increased from 539 to 717 HV. After heat treatment, the coating underwent a crystallization process, and the hardness increased from 878 to 1094 HV. The main wear mechanism of the coating changed from adhesive wear in the as-plated state to abrasive wear in the annealed state. The annealed Ni-P-Si3N4-WS2 coating with a WS2 dosage of 2.5 g/L in the bath exhibited excellent mechanical properties, with a hardness of 10.9 GPa, a friction coefficient of ~0.51, and a wear rate of 8.4 × 10−15 m3N−1⋅m−1 at room temperature, and maintained optimal performance at high temperatures. At operating temperatures of 200, 400, and 600 °C, the form of wear was adhesive wear for coatings with a WS2 dosage 2 dosage ≥1.5 g/L. The synergism of WS2 and Si3N4 particles refined the grains of the Ni-P matrix in as-plated coatings and obviously reduced the friction coefficient of friction pairs in annealed coatings at all operating temperatures.
- Open Access
CO2 Pressure-Dependent Microstructure and Morphology of Carbon for Energy Storage: Unraveling the Role of CO2 in Green Synthesis of Carbon Materials
Advanced carbon materials have played an important function in the field of energy conversion and storage. The green and low-carbon synthesis of elemental carbon with controllable morphology and microstructure is the main problem for carbon materials. Herein, we develop a green and low-carbon method to synthesize porous carbon by reacting CO2 with LiAlH4 at low temperatures. The starting reaction temperatures are as low as 142, 121, and 104 °C for LiAlH4 reacting with 1, 30, and 60 bar CO2, respectively. For the elemental carbon, the porosity of elemental carbon gradually decreased, whereas its graphitization degree increased as the CO2 pressure increased from 1 bar to 60 bar. CO2 serves as one of the two reactants and the CO2 pressure can adjust the thermodynamic and kinetic properties of the formation reaction for synthesizing elemental carbon. The mechanism for CO2 pressure-dependent microstructure and morphology of carbon is discussed on the basis of the formation reaction of elemental carbon and gas blowing effect of H2 and CO2. The elemental carbon with different morphology and microstructure exhibits distinct electrochemical lithium storage performance including reversible capacity, rate capability, cycling stability, and Coulombic efficiency, owing to their different lithium storage mechanism. The elemental carbon synthesized at 30 bar CO2 delivers the highest reversible capacity of 506 mAh g−1 after 1000 cycles even at 1.0 A g−1. Advanced energy storage technology based on the green and low-carbon synthesis of carbon materials is a requisite for providing a stable and sustainable energy supply to meet the ever-growing demand for energy.
Open AccessCO2 Pressure-Dependent Microstructure and Morphology of Carbon for Energy Storage: Unraveling the Role of CO2 in Green Synthesis of Carbon Materials
Advanced carbon materials have played an important function in the field of energy conversion and storage. The green and low-carbon synthesis of elemental carbon with controllable morphology and microstructure is the main problem for carbon materials. Herein, we develop a green and low-carbon method to synthesize porous carbon by reacting CO2 with LiAlH4 at low temperatures. The starting reaction temperatures are as low as 142, 121, and 104 °C for LiAlH4 reacting with 1, 30, and 60 bar CO2, respectively. For the elemental carbon, the porosity of elemental carbon gradually decreased, whereas its graphitization degree increased as the CO2 pressure increased from 1 bar to 60 bar. CO2 serves as one of the two reactants and the CO2 pressure can adjust the thermodynamic and kinetic properties of the formation reaction for synthesizing elemental carbon. The mechanism for CO2 pressure-dependent microstructure and morphology of carbon is discussed on the basis of the formation reaction of elemental carbon and gas blowing effect of H2 and CO2. The elemental carbon with different morphology and microstructure exhibits distinct electrochemical lithium storage performance including reversible capacity, rate capability, cycling stability, and Coulombic efficiency, owing to their different lithium storage mechanism. The elemental carbon synthesized at 30 bar CO2 delivers the highest reversible capacity of 506 mAh g−1 after 1000 cycles even at 1.0 A g−1. Advanced energy storage technology based on the green and low-carbon synthesis of carbon materials is a requisite for providing a stable and sustainable energy supply to meet the ever-growing demand for energy.
- 19 August 2022
- Published by Springer Nature in Research on Chemical Intermediates
- Vol. 48 (10) , 4163-4182
Z-scheme Ag-loaded g-C3N4/CuNb2O6 composite photocatalyst for RhB dye degradation
- 19 August 2022
- Published by Springer Nature in Research on Chemical Intermediates
- Vol. 48 (10) , 4163-4182
Z-scheme Ag-loaded g-C3N4/CuNb2O6 composite photocatalyst for RhB dye degradation
- 18 March 2021
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 39 (3) , 033404
Enhancement in the tribological performance of WSx/a-C multilayer films with Al sublayers in vacuum
The manufacturing of multilayer films with improved mechanical and tribological properties has attracted attention recently for enabling their space applications. In this study, we aim to optimize the manufacturing process of WSx/a-C multilayer films by alternately depositing WS2, amorphous carbon (a-C), and Al metal on silicon substrates through magnetron sputtering. The microstructure and morphology of the multilayer films were investigated by x-ray diffractometry, scanning electron microscopy, and x-ray photoelectron spectroscopy. The mechanical and tribological properties of the films were evaluated in vacuum using a nanoindentation tester, ball-on-disk tribometer, and scratch tester. The results showed that the addition of an Al layer with an optimal thickness refined the microstructure of the films. The tribological properties of the films deteriorated with increasing thickness of the Al single layer. When the thickness of the Al film was 1 nm, the tribological properties of the films were optimal, and the adhesion was maximum (49.1 N). Hardness of the films gradually decreased with an increase in the thickness. Wear rate of the films decreased initially and then increased, and the wear rate was lowest when the thickness of the Al single layer was 2 nm (1.41 × 10−15 m3 N−1 m−1). By manufacturing films with optimal thickness, suitable tribological properties for vacuum applications can be achieved.
- 18 March 2021
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 39 (3) , 033404
Enhancement in the tribological performance of WSx/a-C multilayer films with Al sublayers in vacuum
The manufacturing of multilayer films with improved mechanical and tribological properties has attracted attention recently for enabling their space applications. In this study, we aim to optimize the manufacturing process of WSx/a-C multilayer films by alternately depositing WS2, amorphous carbon (a-C), and Al metal on silicon substrates through magnetron sputtering. The microstructure and morphology of the multilayer films were investigated by x-ray diffractometry, scanning electron microscopy, and x-ray photoelectron spectroscopy. The mechanical and tribological properties of the films were evaluated in vacuum using a nanoindentation tester, ball-on-disk tribometer, and scratch tester. The results showed that the addition of an Al layer with an optimal thickness refined the microstructure of the films. The tribological properties of the films deteriorated with increasing thickness of the Al single layer. When the thickness of the Al film was 1 nm, the tribological properties of the films were optimal, and the adhesion was maximum (49.1 N). Hardness of the films gradually decreased with an increase in the thickness. Wear rate of the films decreased initially and then increased, and the wear rate was lowest when the thickness of the Al single layer was 2 nm (1.41 × 10−15 m3 N−1 m−1). By manufacturing films with optimal thickness, suitable tribological properties for vacuum applications can be achieved.
- 20 July 2020
- Published by Taylor & Francis in Composite Interfaces
- Vol. 28 (6) , 593-607
Micro-structure and tribological behaviors of magnetron sputtered WSx/Fe/a-C/Fe multi-layer films with various Fe layer thicknesses
The WS x /Fe/a-C/Fe multi-layer films with various Fe layer thicknesses were prepared by using magnetron sputtering and alternate deposition of WS x , Fe, and a-C layers on the silicon substrates. The morphology, micro-structure, and composition of the films were characterized by scanning electron microscope, energy dispersive spectroscopy, electron probe micro-analyzer, X-ray diffraction, and X-ray photoelectron spectroscopy. The mechanical and tribological properties of the fabricated films were evaluated by using nano-indenter, film stress tester, scratch tester, and ball-on-disk tribotester. According to the obtained results, all the multi-layer films revealed a featureless micro-structure with a smooth and dense surface. As the thickness of Fe layer increased, the S/W ratio of the films was decreased from 1.38 to 1.16, the hardness, elastic modulus, and adhesion of the films were gradually improved. Both the steady-state friction coefficient and wear rate were declined first and, then, enhanced. The film with the Fe-layer thickness of 4 nm exhibited the highest hardness (10.6 GPa) and adhesion (38.0 N); whereas, film with the Fe-layer thickness of 2 nm showed the best tribological performance with a steady-state friction coefficient of 0.218 and wear rate of 1.63 × 10−15m3 N−1 m−1.
- 20 July 2020
- Published by Taylor & Francis in Composite Interfaces
- Vol. 28 (6) , 593-607
Micro-structure and tribological behaviors of magnetron sputtered WSx/Fe/a-C/Fe multi-layer films with various Fe layer thicknesses
The WS x /Fe/a-C/Fe multi-layer films with various Fe layer thicknesses were prepared by using magnetron sputtering and alternate deposition of WS x , Fe, and a-C layers on the silicon substrates. The morphology, micro-structure, and composition of the films were characterized by scanning electron microscope, energy dispersive spectroscopy, electron probe micro-analyzer, X-ray diffraction, and X-ray photoelectron spectroscopy. The mechanical and tribological properties of the fabricated films were evaluated by using nano-indenter, film stress tester, scratch tester, and ball-on-disk tribotester. According to the obtained results, all the multi-layer films revealed a featureless micro-structure with a smooth and dense surface. As the thickness of Fe layer increased, the S/W ratio of the films was decreased from 1.38 to 1.16, the hardness, elastic modulus, and adhesion of the films were gradually improved. Both the steady-state friction coefficient and wear rate were declined first and, then, enhanced. The film with the Fe-layer thickness of 4 nm exhibited the highest hardness (10.6 GPa) and adhesion (38.0 N); whereas, film with the Fe-layer thickness of 2 nm showed the best tribological performance with a steady-state friction coefficient of 0.218 and wear rate of 1.63 × 10−15m3 N−1 m−1.
- 1 January 2017
- Published by Elsevier in Surface and Coatings Technology
- Vol. 309, 187-194
Microstructure and tribological properties of WS x /a-C multilayer films with various layer thickness ratios in different environments
- 1 January 2017
- Published by Elsevier in Surface and Coatings Technology
- Vol. 309, 187-194
Microstructure and tribological properties of WS x /a-C multilayer films with various layer thickness ratios in different environments
- 1 November 2014
- Published by Elsevier in Surface and Coatings Technology
- Vol. 258, 716-721
Microstructure and mechanical properties of a-CN films prepared by bias voltage assisted PLD with carbon nitride target
- 1 November 2014
- Published by Elsevier in Surface and Coatings Technology
- Vol. 258, 716-721
Microstructure and mechanical properties of a-CN films prepared by bias voltage assisted PLD with carbon nitride target