Xianyou Wu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Xianyou Wu has a total of 10 co-authors. Here are the top co-authors by number of shared publications:
Antong Ma
Key Laboratory of High‐performance Synthetic Rubber and its Composite Materials, Changchun Institute of Applied Chemistry Chinese Academy of Sciences Changchun 130022 People's Republic of China
2 shared publicationsChao Fu
Key Laboratory of High‐performance Synthetic Rubber and its Composite Materials, Changchun Institute of Applied Chemistry Chinese Academy of Sciences Changchun 130022 People's Republic of China
2 shared publications- Wei Nie
Laboratory of Polymer Materials for Extreme Conditions, Changchun Institute of Applied Chemistry, Chinese Academy of Sciences, Changchun 130022, China
2 shared publications - Xianghai Ran
Lab of Polymer Composites Engineering, Changchun Institute of Applied Chemistry, Chinese Academy of Sciences, Changchun, China
2 shared publications Yixing Gao
Key Laboratory of High‐performance Synthetic Rubber and its Composite Materials, Changchun Institute of Applied Chemistry Chinese Academy of Sciences Changchun 130022 People's Republic of China
2 shared publicationsZhongyang Tan
Key Laboratory of High‐performance Synthetic Rubber and its Composite Materials, Changchun Institute of Applied Chemistry Chinese Academy of Sciences Changchun 130022 People's Republic of China
2 shared publications
Latest Publications
- 21 October 2019
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 137 (16)
A triple‐shape memory material fabricated by in situ crosslinking of poly(butylene adipate‐co‐terephthalate)/ε‐polycaprolactone via electron‐beam irradiation and its triple‐shape memory effects
In this work, we fabricated a triple‐shape memory polymeric material though in situ crosslinking of poly(butylene adipate‐co‐terephthalate)/ε‐polycaprolactone blends induced by electron beam irradiation. The intrinsic property of irradiation crosslinking, crosslinking rule in this heterogeneous system, formation of interfacial bridge molecular, and the resulted interfacial strength were investigated. No obvious interfacial slips were observed in tensile test, and the elongation at break was above 900%. The high‐temperature relaxation and recovery experiments at nonlinear region confirmed the excellent hyperelasticity and recovery ratios (Rr) can be as high as 95% for samples irradiated above 96 kGy. The mismatch between heating rate and relaxation kinetics resulted in both instable temporary shapes and heating‐mode dependent recovery behavior during the recovery process. Self‐stability of the temporary shape at middle temperature was also emphasized in view of the phenomenon that the second Rr was above 100% in our experiments. © 2019 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2020, 137, 48588.
- 21 October 2019
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 137 (16)
A triple‐shape memory material fabricated by in situ crosslinking of poly(butylene adipate‐co‐terephthalate)/ε‐polycaprolactone via electron‐beam irradiation and its triple‐shape memory effects
In this work, we fabricated a triple‐shape memory polymeric material though in situ crosslinking of poly(butylene adipate‐co‐terephthalate)/ε‐polycaprolactone blends induced by electron beam irradiation. The intrinsic property of irradiation crosslinking, crosslinking rule in this heterogeneous system, formation of interfacial bridge molecular, and the resulted interfacial strength were investigated. No obvious interfacial slips were observed in tensile test, and the elongation at break was above 900%. The high‐temperature relaxation and recovery experiments at nonlinear region confirmed the excellent hyperelasticity and recovery ratios (Rr) can be as high as 95% for samples irradiated above 96 kGy. The mismatch between heating rate and relaxation kinetics resulted in both instable temporary shapes and heating‐mode dependent recovery behavior during the recovery process. Self‐stability of the temporary shape at middle temperature was also emphasized in view of the phenomenon that the second Rr was above 100% in our experiments. © 2019 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2020, 137, 48588.
- 15 October 2019
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 137 (16)
Tunable triple‐shape memory composite fabricated by selective crosslinking of polycaprolactone/poly(butylene adipate‐co‐terephthalate)/bentonite
In this work, we fabricated a triple‐shape memory polymeric composite (TSMPc) by electron beam irradiation of ε‐polycaprolactone (ε‐PCL)/poly(butylene adipate‐co‐terephthalate) (PBAT)/bentonite(50/50/4) (wt %). The 95 ± 5 kGy was confirmed to be the saturated irradiation dose by both high‐temperature storage modulus and the equilibrated relaxation modulus at nonlinear elastic region. Further results demonstrated that sample exposed to 41.4 kGy exhibited excellent triple‐shape memory effect (TSME) though there existed slight plastic flow in PBAT. The two fixity ratios and total recovery ratio can be as high as 99.9, 98.3, and 94.7%. Besides, the strength of irradiated PBAT was improved because of the synergistic mechanical coupling effect from PCL and bentonite. In the meantime, this synergistic effect also improved the integral TSME and the stability of all shapes. Eventually, we made a comparison among the controllable factors, the crosslinking density and amount of deformation ΔεB → C were believed to have more influences on the stability of temporary shapes and the recovery behavior during the shape memory cycle “A → B → C → Br → Ar.” © 2019 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2020, 137, 48577.
- 15 October 2019
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 137 (16)
Tunable triple‐shape memory composite fabricated by selective crosslinking of polycaprolactone/poly(butylene adipate‐co‐terephthalate)/bentonite
In this work, we fabricated a triple‐shape memory polymeric composite (TSMPc) by electron beam irradiation of ε‐polycaprolactone (ε‐PCL)/poly(butylene adipate‐co‐terephthalate) (PBAT)/bentonite(50/50/4) (wt %). The 95 ± 5 kGy was confirmed to be the saturated irradiation dose by both high‐temperature storage modulus and the equilibrated relaxation modulus at nonlinear elastic region. Further results demonstrated that sample exposed to 41.4 kGy exhibited excellent triple‐shape memory effect (TSME) though there existed slight plastic flow in PBAT. The two fixity ratios and total recovery ratio can be as high as 99.9, 98.3, and 94.7%. Besides, the strength of irradiated PBAT was improved because of the synergistic mechanical coupling effect from PCL and bentonite. In the meantime, this synergistic effect also improved the integral TSME and the stability of all shapes. Eventually, we made a comparison among the controllable factors, the crosslinking density and amount of deformation ΔεB → C were believed to have more influences on the stability of temporary shapes and the recovery behavior during the shape memory cycle “A → B → C → Br → Ar.” © 2019 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2020, 137, 48577.
- 1 December 2007
- Published by American Scientific Publishers in Journal of Biobased Materials and Bioenergy
- Vol. 1 (3) , 341-350
Influence of the Processing Conditions on the Mechanical Properties of Chitin Whisker Reinforced Poly(caprolactone) Nanocomposites
Nanocomposite materials obtained from chitin whiskers and polycaprolactone (PCL) were produced by evaporation, freeze drying and melt-compounding in a mini-extruder followed by hot pressing. Chitin whiskers were obtained from crab shell by removing the protein matrix that held them in the shell structure. The chitin whiskers obtained in this way were characterised with fourier transform infrared spectroscopy (FTIR) and transmission electron microscopy (TEM). The thermal, tensile and dynamic mechanical properties of the composites were also investigated. The thermal stability of the nanocomposites was higher than that of the pure PCL, as revealed by thermogravimetric analysis (TGA). The highest increase in Young's moduli was obtained for a chitin whisker content of 10 wt%. Higher chitin whisker contents resulted in a more brittle failure behaviour of the nanocomposites which was accompanied by a reduced tensile strength and elongation at break. Melt-compounded specimens showed improved mechanical properties compared with those processed by evaporation and freeze drying techniques.
- 1 December 2007
- Published by American Scientific Publishers in Journal of Biobased Materials and Bioenergy
- Vol. 1 (3) , 341-350
Influence of the Processing Conditions on the Mechanical Properties of Chitin Whisker Reinforced Poly(caprolactone) Nanocomposites
Nanocomposite materials obtained from chitin whiskers and polycaprolactone (PCL) were produced by evaporation, freeze drying and melt-compounding in a mini-extruder followed by hot pressing. Chitin whiskers were obtained from crab shell by removing the protein matrix that held them in the shell structure. The chitin whiskers obtained in this way were characterised with fourier transform infrared spectroscopy (FTIR) and transmission electron microscopy (TEM). The thermal, tensile and dynamic mechanical properties of the composites were also investigated. The thermal stability of the nanocomposites was higher than that of the pure PCL, as revealed by thermogravimetric analysis (TGA). The highest increase in Young's moduli was obtained for a chitin whisker content of 10 wt%. Higher chitin whisker contents resulted in a more brittle failure behaviour of the nanocomposites which was accompanied by a reduced tensile strength and elongation at break. Melt-compounded specimens showed improved mechanical properties compared with those processed by evaporation and freeze drying techniques.