    Fabrications of High-Capacity Alpha-Ni(OH)2

    by Kwo-Hsiung Young, Lixin Wang, Shuli Yan, Xingqun Liao, Tiejun Meng, Haoting Shen, William C. Mays

    Three different methods were used to produce α-Ni(OH)2 with higher discharge capacities than the conventional β-Ni(OH)2, specifically a batch process of co-precipitation, a continuous process of co-precipitation with a phase transformation step (initial cycling), and an overcharge at low temperature. All three methods can produce α-Ni(OH)2 or α/β mixed-Ni(OH)2 with capacities higher than that of conventional β-Ni(OH)2 and a stable cycle performance. The second method produces a special core–shell β-Ni(OH)2/α-Ni(OH)2 structure with an excellent cycle stability in the flooded half-cell configuration, is innovative and also already mass-production ready. The core–shell structure has been investigated by both scanning and transmission electron microscopies. The shell portion of the particle is composed of α-Ni(OH)2 nano-crystals embedded in a β-Ni(OH)2 matrix, which helps to reduce the stress originating from the lattice expansion in the β-α transformation. A review on the research regarding α-Ni(OH)2 is also included in the paper.


  • Open Access

    Ionic Liquid-Based Non-Aqueous Electrolytes for Nickel/Metal Hydride Batteries

    by Tiejun Meng, Kwo-Hsiung Young, Diana F. Wong, Jean Nei

    The voltage of an alkaline electrolyte-based battery is often limited by the narrow electrochemical stability window of water (1.23 V). As an alternative to water, ionic liquid (IL)-based electrolyte has been shown to exhibit excellent proton conducting properties and a wide electrochemical stability window, and can be used in proton conducting batteries. In this study, we used IL/acid mixtures to replace the 30 wt % KOH aqueous electrolyte in nickel/metal hydride (Ni/MH) batteries, and verified the proton conducting character of these mixtures through electrochemical charge/discharge experiments. Dilution of ILs with acetic acid was found to effectively increase proton conductivity. By using 2 M acetic acid in 1-ethyl-3-methylimidazolium acetate, stable charge/discharge characteristics were obtained, including low charge/discharge overpotentials, a discharge voltage plateau at ~1.2 V, a specific capacity of 161.9 mAh·g−1, and a stable cycling performance for an AB5 metal hydride anode with a (Ni,Co,Zn)(OH)2 cathode.


  • Open Access

    Clean Grain Boundary Found in C14/Body-Center-Cubic Multi-Phase Metal Hydride Alloys

    by Hao-Ting Shen, Kwo-Hsiung Young, Tiejun Meng, Leonid A. Bendersky

    The grain boundaries of three Laves phase-related body-center-cubic (bcc) solid-solution, metal hydride (MH) alloys with different phase abundances were closely examined by scanning electron microscopy (SEM), transmission electron microscopy (TEM), and more importantly, electron backscatter diffraction (EBSD) techniques. By using EBSD, we were able to identify the alignment of the crystallographic orientations of the three major phases in the alloys (C14, bcc, and B2 structures). This finding confirms the presence of crystallographically sharp interfaces between neighboring phases, which is a basic assumption for synergetic effects in a multi-phase MH system.


  • Open Access

    Failure Mechanisms of Nickel/Metal Hydride Batteries with Cobalt-Substituted Superlattice Hydrogen-Absorbing Alloy Anodes at 50 °C

    by Tiejun Meng, Kwo-Hsiung Young, John Koch, Taihei Ouchi, Shigekazu Yasuoka

    The incorporation of a small amount of Co in the A2B7 superlattice hydrogen absorbing alloy (HAA) can benefit its electrochemical cycle life performance at both room temperature (RT) and 50 °C. The electrochemical properties of the Co-substituted A2B7 and the failure mechanisms of cells using such alloys cycled at RT have been reported previously. In this paper, the failure mechanisms of the same alloys cycled at 50 °C are reported. Compared to that at RT, the trend of the cycle life at 50 °C versus the Co content in the Co-substituted A2B7 HAAs is similar, but the cycle life is significantly shorter. Failure analysis of the cells at 50 °C was performed using X-ray diffraction (XRD), scanning electron microscopy (SEM), X-ray energy dispersive spectroscopy (EDS), and inductively coupled plasma (ICP) analysis. It was found that the elevated temperature accelerates electrolyte dry-out and the deterioration (both pulverization and oxidation) of the A2B7 negative electrode, which are major causes of cell failure when cycling at 50 °C. Cells from HAA with higher Co-content also showed micro-shortage in the separator from the debris of the corrosion of the negative electrode.


  • Open Access

    Studies on the Synergetic Effects in Multi-Phase Metal Hydride Alloys

    by Kwo-Hsiung Young, Taihei Ouchi, Tiejun Meng, Diana F. Wong

    The electrochemical reactions of multi-phase metal hydride (MH) alloys were studied using a series of Laves phase-related body-centered-cubic (BCC) Ti15.6Zr2.1V43Cr11.2Mn6.9Co1.4Ni18.5Al0.3X (X = V, B, Mg, Y, Zr, Nb, Mo, La, and Nd) alloys. These alloys are composed of BCC (major), TiNi (major), C14 (minor), and Ti2Ni (minor) phases. The BCC phase was found to be responsible for the visible equilibrium pressure plateau between 0.1 MPa and 1 MPa. The plateaus belonging to the other phases occurred below 0.005 MPa. Due to the synergetic effects of other non-BCC phases, the body-centered-tetragonal (BCT) intermediate step is skipped and the face-centered-cubic (FCC) hydride phase is formed directly. During hydrogenation in both gaseous phase and electrochemistry, the non-BCC phases were first charged to completion, followed by charging of the BCC phase. In the multi-phase system, the side with a higher work function along the grain boundary is believed to be the first region that becomes hydrogenated and will not be fully dehydrided after 8 h in vacuum at 300 °C. While there is a large step at approximately 50% of the maximum hydrogen storage for the equilibrium pressure measured in gaseous phase, the charge/discharge curves measured electrochemically are very smooth, indicating a synergetic effect between BCC and non-BCC phases in the presence of voltage and charge non-neutrality. Compared to the non-BCC phases, the C14 phase benefits while the TiNi phase deteriorates the high-rate dischargeability (HRD) of the alloys. These synergetic effects are explained by the preoccupied hydrogen sites on the side of the hydrogen storage phase near the grain boundary.


  • Open Access

    Studies on Incorporation of Mg in Zr-Based AB2 Metal Hydride Alloys

    by Shiuan Chang, Kwo-Hsiung Young, Taiehi Ouchi, Tiejun Meng, Jean Nei, Xin Wu

    Mg, the A-site atom in C14 (MgZn2), C15 (MgCu2), and C36 (MgNi2) Laves phase alloys, was added to the Zr-based AB2 metal hydride (MH) alloy during induction melting. Due to the high melting temperature of the host alloy (>1500 °C) and high volatility of Mg in the melt, the Mg content of the final ingot is limited to 0.8 at%. A new Mg-rich cubic phase was found in the Mg-containing alloys with a small phase abundance, which contributes to a significant increase in hydrogen storage capacities, the degree of disorder (DOD) in the hydride, the high-rate dischargeability (HRD), and the charge-transfer resistances at both room temperature (RT) and −40 °C. This phase also facilitates the activation process in measurement of electrochemical discharge capacity. Moreover, through a correlation study, the Ni content was found to be detrimental to the storage capacities, while Ti content was found to be more influential in HRD and charge-transfer resistance in this group of AB2 metal hydride (MH) alloys.


  • Open Access

    Electrochemical Open-Circuit Voltage and Pressure-Concentration-Temperature Isotherm Comparison for Metal Hydride Alloys

    by Negar Mosavati, Kwo-Hsiung Young, Tiejun Meng, K. Y. Simon Ng

    In this study we compared the electrochemical pressure-concentration-temperature (EPCT) method with the gaseous phase pressure-concentration-temperature (PCT) method and demonstrated the differences between the two. Experimentally, this was done by electrochemically charging/discharging the electrodes of four different metal hydride (MH) alloys. The results indicate that in the PCT curve is flatter with a smaller hysteresis and a higher storage capacity compared to the EPCT curve. Moreover, while the PCT curves (up to around one third of the hydrogen storage capacity) reside in between the charge and discharge EPCT curves, the rest of the PCT curves are below the EPCT curves. Finally, we demonstrated a new calibration method based on the inflection points observed in the EPCT isotherms of a physical mixture of more than one alloy. This turning point can be used to find a preset calibration point to determine the state-of-charge.