Hao Zhang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Research Interests
Hao Zhang has a total of 57 co-authors. Here are the top co-authors by number of shared publications:
- Yang Liu
Yangzhou University College of Electrical, Energy and Power Engineering Yangzhou
11 shared publications - Jiajie Fan
Fudan University
5 shared publications Guoqi Zhang
EEMCS Faculty, Delft University of Technology, 2628CD, Delft, The Netherlands
4 shared publicationsFenglian Sun
School of Materials Science and Engineering, Harbin University of Science and Technology, Harbin 150040, China
3 shared publications- Xuejun Fan
Department of Mechanical Engineering, Lamar University, Beaumont, USA
3 shared publications - Fenglian Sun
School of Materials Science and Chemical Engineering, Harbin University of Science and Technology, Harbin 150080, China
2 shared publications
Latest Publications
- 11 January 2024
- Published by Elsevier in Composite Structures
- Vol. 331, 117903
Thermal-mechanical coupling in drilling high-performance CFRP: Scale-span modeling and experimental validation
- 11 January 2024
- Published by Elsevier in Composite Structures
- Vol. 331, 117903
Thermal-mechanical coupling in drilling high-performance CFRP: Scale-span modeling and experimental validation
- 25 August 2022
- Published by American Chemical Society (ACS) in ACS Applied Nano Materials
- Vol. 5 (9) , 12876-12886
Copper-Nanoparticle-Coated Fabrics for Rapid and Sustained Antibacterial Activity Applications
- 25 August 2022
- Published by American Chemical Society (ACS) in ACS Applied Nano Materials
- Vol. 5 (9) , 12876-12886
Copper-Nanoparticle-Coated Fabrics for Rapid and Sustained Antibacterial Activity Applications
- 19 May 2020
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Components, Packaging and Manufacturing Technology
- Vol. 10 (7) , 1101-1109
Experimental Investigation on the Sintering Kinetics of Nanosilver Particles Used in High-Power Electronic Packaging
Better mechanical, thermal properties and longer lifetimes are needed for the die attach layer in high power electronic packaging. As traditional Sn-Ag-Cu (SAC) solders have many limitations, the sintered nanosilver materials are becoming one of substitutes for high power electronic packaging. However, high performance of sintered nanosilver materials is only achieved when its fine sintering densification is formed. This work investigates the sintering densification process of nanosilver particles based on the design of orthogonal experiments and sintering kinetics modeling in which both the macro-properties and micro-morphology are linked and analyzed. The results lead to several conclusions, such as: (1) The orthogonal experiments consider the effects of sintering temperature, dwell time, and sample preparation pressure on the sintering relative shrinkage and relative density—the results show that the most critical impact factor on sintering densification is the sintering temperature; (2) In the sintering kinetic experiments, the sintering densification rates obtained by fitting the relative density v.s. dwell time curves during 175 - 250°C follow the Arrhenius model and the apparent activation energy of sintering kinetics is calculated to be 36kJ/mol, while it is calculated from the particle size is 38.1 kJ/mol; (3) Through modeling the relationship between particle size, line shrinkage and porosity, the line shrinkage and porosity first increase at the initial stage, While since the particle size increases and the macroscopic volume decreases at the end of sintering, the porosity decreases.
- 19 May 2020
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Components, Packaging and Manufacturing Technology
- Vol. 10 (7) , 1101-1109
Experimental Investigation on the Sintering Kinetics of Nanosilver Particles Used in High-Power Electronic Packaging
Better mechanical, thermal properties and longer lifetimes are needed for the die attach layer in high power electronic packaging. As traditional Sn-Ag-Cu (SAC) solders have many limitations, the sintered nanosilver materials are becoming one of substitutes for high power electronic packaging. However, high performance of sintered nanosilver materials is only achieved when its fine sintering densification is formed. This work investigates the sintering densification process of nanosilver particles based on the design of orthogonal experiments and sintering kinetics modeling in which both the macro-properties and micro-morphology are linked and analyzed. The results lead to several conclusions, such as: (1) The orthogonal experiments consider the effects of sintering temperature, dwell time, and sample preparation pressure on the sintering relative shrinkage and relative density—the results show that the most critical impact factor on sintering densification is the sintering temperature; (2) In the sintering kinetic experiments, the sintering densification rates obtained by fitting the relative density v.s. dwell time curves during 175 - 250°C follow the Arrhenius model and the apparent activation energy of sintering kinetics is calculated to be 36kJ/mol, while it is calculated from the particle size is 38.1 kJ/mol; (3) Through modeling the relationship between particle size, line shrinkage and porosity, the line shrinkage and porosity first increase at the initial stage, While since the particle size increases and the macroscopic volume decreases at the end of sintering, the porosity decreases.
- Open Access
- 1 April 2020
- Published by DEStech Publications in DEStech Transactions on Environment, Energy and Earth Sciences
- No. peems
The Influence of Solder Void on IGBT Temperature
The void in solder layer is the main factor that causes bad heat dissipation of IGBT (Insulated Gate Bipolar Transistor) module. Based on the seven-layer structure of IGBT, this article established a three-dimensional finite element model of IGBT module packaging structure and carried out its thermal analysis, then had a study on the effect of welding layer void on the temperature of IGBT chip. The overall distribution of IGBT module with or without solder hole is compared, meanwhile the article analyzed the effects of void type, size, shape, number and distribution on the temperature distribution of IGBT chips. The results show that the void in the solder layer of the chip has a great influence on the temperature of the chip. The influence of penetrating voids on chip temperature is greater than that of non-penetrating voids, the bigger the single hole is, the higher the temperature of IGBT chip. Voids of the same shape have greater influence on chip temperature at edge and corner positions than those inside the welding layer. The more concentrated the distribution of multiple holes, the higher the chip’s temperature. Therefore, in order to improve the reliability of IGBT, it is necessary to avoid voids in the chip welding layer during the packaging process.
- 1 April 2020
- Published by DEStech Publications in DEStech Transactions on Environment, Energy and Earth Sciences
- No. peems
Open AccessThe Influence of Solder Void on IGBT Temperature
The void in solder layer is the main factor that causes bad heat dissipation of IGBT (Insulated Gate Bipolar Transistor) module. Based on the seven-layer structure of IGBT, this article established a three-dimensional finite element model of IGBT module packaging structure and carried out its thermal analysis, then had a study on the effect of welding layer void on the temperature of IGBT chip. The overall distribution of IGBT module with or without solder hole is compared, meanwhile the article analyzed the effects of void type, size, shape, number and distribution on the temperature distribution of IGBT chips. The results show that the void in the solder layer of the chip has a great influence on the temperature of the chip. The influence of penetrating voids on chip temperature is greater than that of non-penetrating voids, the bigger the single hole is, the higher the temperature of IGBT chip. Voids of the same shape have greater influence on chip temperature at edge and corner positions than those inside the welding layer. The more concentrated the distribution of multiple holes, the higher the chip’s temperature. Therefore, in order to improve the reliability of IGBT, it is necessary to avoid voids in the chip welding layer during the packaging process.
- Open Access
Random Voids Generation and Effect of Thermal Shock Load on Mechanical Reliability of Light-Emitting Diode Flip Chip Solder Joints
To make the light-emitting diode (LED) more compact and effective, the flip chip solder joint is recommended in LED chip-scale packaging (CSP) with critical functions in mechanical support, heat dissipation, and electrical conductivity. However, the generation of voids always challenges the mechanical strength, thermal stability, and reliability of solder joints. This paper models the 3D random voids generation in the LED flip chip Sn96.5–Ag3.0–Cu0.5 (SAC305) solder joint, and investigates the effect of thermal shock load on its mechanical reliability with both simulations and experiments referring to the JEDEC thermal shock test standard (JESD22-A106B). The results reveal the following: (1) the void rate of the solder joint increases after thermal shock ageing, and its shear strength exponentially degrades; (2) the first principal stress of the solder joint is not obviously increased, however, if the through-hole voids emerged in the corner of solder joints, it will dramatically increase; (3) modelling of the fatigue failure of solder joint with randomly distributed voids utilizes the approximate model to estimate the lifetime, and the experimental results confirm that the absolute prediction error can be controlled around 2.84%.
Open AccessRandom Voids Generation and Effect of Thermal Shock Load on Mechanical Reliability of Light-Emitting Diode Flip Chip Solder Joints
To make the light-emitting diode (LED) more compact and effective, the flip chip solder joint is recommended in LED chip-scale packaging (CSP) with critical functions in mechanical support, heat dissipation, and electrical conductivity. However, the generation of voids always challenges the mechanical strength, thermal stability, and reliability of solder joints. This paper models the 3D random voids generation in the LED flip chip Sn96.5–Ag3.0–Cu0.5 (SAC305) solder joint, and investigates the effect of thermal shock load on its mechanical reliability with both simulations and experiments referring to the JEDEC thermal shock test standard (JESD22-A106B). The results reveal the following: (1) the void rate of the solder joint increases after thermal shock ageing, and its shear strength exponentially degrades; (2) the first principal stress of the solder joint is not obviously increased, however, if the through-hole voids emerged in the corner of solder joints, it will dramatically increase; (3) modelling of the fatigue failure of solder joint with randomly distributed voids utilizes the approximate model to estimate the lifetime, and the experimental results confirm that the absolute prediction error can be controlled around 2.84%.
- 1 April 2019
- Published by Elsevier in Materials Letters
- Vol. 241, 108-110
Copper foam enhanced Sn58Bi solder joint with high performance for low temperature packaging
- 1 April 2019
- Published by Elsevier in Materials Letters
- Vol. 241, 108-110
Copper foam enhanced Sn58Bi solder joint with high performance for low temperature packaging
- 29 November 2018
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Components, Packaging and Manufacturing Technology
- Vol. 9 (5) , 963-972
Effects of Sintering Pressure on the Densification and Mechanical Properties of Nanosilver Double-Side Sintered Power Module
Modern power electronics has the increased demands in current density and high temperature reliability. However, these performance factors are limited due to the die attach materials used to affix power dies microchips to electric circuitry. Although several die attach materials and methods exist, nanosilver sintering technology has received much attention in attaching power dies due to its superior high temperature reliability. This paper investigated the sintering properties of nanosilver film in double side sintered power packages. X-ray diffraction (XRD) results revealed that the size of nanosilver particles increased after pressure-free sintering. Comparing with the pressure-free sintered nanosilver particles, the 5 MPa sintered particles showed a higher density. When increasing sintering pressure from 5 to 30 MPa, the shear strength of the sintered package increased from 8.71 MPa to 86.26 MPa. When sintering at pressures below 20 MPa, the fracture areas are mainly located between the sintered Ag layer and the surface metallization layer on the fast recovery diode (FRD) die. The fracture occurs through the FRD die and the metallization layer on bottom Mo substrate when sintering at 30 MPa.
- 29 November 2018
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Components, Packaging and Manufacturing Technology
- Vol. 9 (5) , 963-972
Effects of Sintering Pressure on the Densification and Mechanical Properties of Nanosilver Double-Side Sintered Power Module
Modern power electronics has the increased demands in current density and high temperature reliability. However, these performance factors are limited due to the die attach materials used to affix power dies microchips to electric circuitry. Although several die attach materials and methods exist, nanosilver sintering technology has received much attention in attaching power dies due to its superior high temperature reliability. This paper investigated the sintering properties of nanosilver film in double side sintered power packages. X-ray diffraction (XRD) results revealed that the size of nanosilver particles increased after pressure-free sintering. Comparing with the pressure-free sintered nanosilver particles, the 5 MPa sintered particles showed a higher density. When increasing sintering pressure from 5 to 30 MPa, the shear strength of the sintered package increased from 8.71 MPa to 86.26 MPa. When sintering at pressures below 20 MPa, the fracture areas are mainly located between the sintered Ag layer and the surface metallization layer on the fast recovery diode (FRD) die. The fracture occurs through the FRD die and the metallization layer on bottom Mo substrate when sintering at 30 MPa.
- Open Access
- 1 February 2018
- Published by Elsevier in Microelectronics Reliability
- Vol. 81, 143-149
A new hermetic sealing method for ceramic package using nanosilver sintering technology
- 1 February 2018
- Published by Elsevier in Microelectronics Reliability
- Vol. 81, 143-149
Open AccessA new hermetic sealing method for ceramic package using nanosilver sintering technology
- 8 September 2017
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 28 (24) , 19113-19120
Microstructure, hardness, and shear behavior of the as-soldered SnBi–SAC composite solder pastes
- 8 September 2017
- Published by Springer Nature in Journal of Materials Science: Materials in Electronics
- Vol. 28 (24) , 19113-19120
Microstructure, hardness, and shear behavior of the as-soldered SnBi–SAC composite solder pastes
- 1 September 2017
- Published by IOP Publishing in Journal of Semiconductors
- Vol. 38 (9) , 96003
Shear strength of LED solder joints using SAC-nano Cu solder pastes
The addition of Cu nanoparticles into the solder pastes by mechanical mixing method creates a positive effect on the microstructure refinement of the LED solder joints. The grain size of β-Sn and Cu6Sn5 decrease obviously due to the increasing concentration of the nanoparticles in the solder pastes. However, the addition of nanoparticles facilitates the formation of voids in the solder joints, especially when the concentration of nanoparticles is higher than 0.5 wt% in the solder pastes. Both the microstructure refinement and void percentage affect the shear strength of the solder joints. Since the increase of the void percentage is limited when the concentration of nanoparticles increases from 0 to 0.5 wt%, the microstructure refinement shows a dominant effect on the shear performance and thus improves the shear strength of the solder joints from 49.8 to 55 MPa. Further addition of nanoparticles in the solder pastes leads to a sharp increase of the void percentage. Consequently, the shear strength of the solder joints decreases from 55 to 48.8 MPa when the concentration of doped particles increases from 0.5 to 1 wt% in the solder pastes.
- 1 September 2017
- Published by IOP Publishing in Journal of Semiconductors
- Vol. 38 (9) , 96003
Shear strength of LED solder joints using SAC-nano Cu solder pastes
The addition of Cu nanoparticles into the solder pastes by mechanical mixing method creates a positive effect on the microstructure refinement of the LED solder joints. The grain size of β-Sn and Cu6Sn5 decrease obviously due to the increasing concentration of the nanoparticles in the solder pastes. However, the addition of nanoparticles facilitates the formation of voids in the solder joints, especially when the concentration of nanoparticles is higher than 0.5 wt% in the solder pastes. Both the microstructure refinement and void percentage affect the shear strength of the solder joints. Since the increase of the void percentage is limited when the concentration of nanoparticles increases from 0 to 0.5 wt%, the microstructure refinement shows a dominant effect on the shear performance and thus improves the shear strength of the solder joints from 49.8 to 55 MPa. Further addition of nanoparticles in the solder pastes leads to a sharp increase of the void percentage. Consequently, the shear strength of the solder joints decreases from 55 to 48.8 MPa when the concentration of doped particles increases from 0.5 to 1 wt% in the solder pastes.