Lee Aucott
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Lee Aucott has a total of 52 co-authors. Here are the top co-authors by number of shared publications:
- Hongbiao Dong
School of Metallurgy and Materials, University of Birmingham, Birmingham, UK
7 shared publications Shuwen Wen
Tata Steel, Research & Development, Swindon Technology Centre, Rotherham, S60 3AR, UK
3 shared publicationsA. C. F. Cocks
University of Oxford
2 shared publications- Alexander Rack
ESRF – The European Synchrotron, Grenoble, France
2 shared publications Anton Kidess
Department of Chemical Engineering, Delft University of Technology, 2629HZ, Delft, The Netherlands
2 shared publicationsChris R. Kleijn
Department of Chemical Engineering, Delft University of Technology, 2629HZ, Delft, The Netherlands
2 shared publications
Latest Publications
- Open Access
- 11 March 2024
- Published by Elsevier in Journal of the Mechanics and Physics of Solids
- Vol. 186
Thermal cracking: Clarifying the effects of phases, voids and grains through characterisation and crystal plasticity modelling
- 11 March 2024
- Published by Elsevier in Journal of the Mechanics and Physics of Solids
- Vol. 186
Open AccessThermal cracking: Clarifying the effects of phases, voids and grains through characterisation and crystal plasticity modelling
- 15 September 2023
- Published by Elsevier in Fusion Engineering and Design
- Vol. 196
Stress-strain curve mapping by nanoindentation – a technique to qualify diffusion-bonded window assemblies for ITER
- 15 September 2023
- Published by Elsevier in Fusion Engineering and Design
- Vol. 196
Stress-strain curve mapping by nanoindentation – a technique to qualify diffusion-bonded window assemblies for ITER
- Open Access
- 1 May 2019
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 529 (1) , 012026
Solidification cracking during welding of steel: In situ X-ray observation
Solidification cracking is an important issue during welding, casting and some of the additive manufacturing process. In order to illuminate the failure mechanisms, solidification cracking during arc welding of steel are investigated in situ with high-speed, high energy, synchrotron X-ray radiography approach. Analysis of the in situ radiography sequence revealed the solidification cracking initiates in the weld sub-surface trailing the welding electrode at relatively low true strain of about 3.1% in the form of micro-cavities. Although both material type and bending speed influence solidification cracking, cracks propagate from the core of the weld towards the free surface along the solidifying grain boundaries was found at a speed of between 1.7 - 2.6 × 10−3 m s−1 for three different steels. In addition, a three-stage mechanistic model for solidification cracking during welding of steel is proposed.
- 1 May 2019
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 529 (1) , 012026
Open AccessSolidification cracking during welding of steel: In situ X-ray observation
Solidification cracking is an important issue during welding, casting and some of the additive manufacturing process. In order to illuminate the failure mechanisms, solidification cracking during arc welding of steel are investigated in situ with high-speed, high energy, synchrotron X-ray radiography approach. Analysis of the in situ radiography sequence revealed the solidification cracking initiates in the weld sub-surface trailing the welding electrode at relatively low true strain of about 3.1% in the form of micro-cavities. Although both material type and bending speed influence solidification cracking, cracks propagate from the core of the weld towards the free surface along the solidifying grain boundaries was found at a speed of between 1.7 - 2.6 × 10−3 m s−1 for three different steels. In addition, a three-stage mechanistic model for solidification cracking during welding of steel is proposed.
- Top Cited PapersOpen Access
- 21 December 2018
- Published by Springer Nature in Nature Communications
- Vol. 9 (1) , 1-7
Revealing internal flow behaviour in arc welding and additive manufacturing of metals
Internal flow behaviour during melt-pool-based metal manufacturing remains unclear and hinders progression to process optimisation. In this contribution, we present direct time-resolved imaging of melt pool flow dynamics from a high-energy synchrotron radiation experiment. We track internal flow streams during arc welding of steel and measure instantaneous flow velocities ranging from 0.1 m s−1 to 0.5 m s−1. When the temperature-dependent surface tension coefficient is negative, bulk turbulence is the main flow mechanism and the critical velocity for surface turbulence is below the limits identified in previous theoretical studies. When the alloy exhibits a positive temperature-dependent surface tension coefficient, surface turbulence occurs and derisory oxides can be entrapped within the subsequent solid as result of higher flow velocities. The widely used arc welding and the emerging arc additive manufacturing routes can be optimised by controlling internal melt flow through adjusting surface active elements.
- 21 December 2018
- Published by Springer Nature in Nature Communications
- Vol. 9 (1) , 1-7
Top Cited PapersOpen AccessRevealing internal flow behaviour in arc welding and additive manufacturing of metals
Internal flow behaviour during melt-pool-based metal manufacturing remains unclear and hinders progression to process optimisation. In this contribution, we present direct time-resolved imaging of melt pool flow dynamics from a high-energy synchrotron radiation experiment. We track internal flow streams during arc welding of steel and measure instantaneous flow velocities ranging from 0.1 m s−1 to 0.5 m s−1. When the temperature-dependent surface tension coefficient is negative, bulk turbulence is the main flow mechanism and the critical velocity for surface turbulence is below the limits identified in previous theoretical studies. When the alloy exhibits a positive temperature-dependent surface tension coefficient, surface turbulence occurs and derisory oxides can be entrapped within the subsequent solid as result of higher flow velocities. The widely used arc welding and the emerging arc additive manufacturing routes can be optimised by controlling internal melt flow through adjusting surface active elements.
- Open Access
- 2 March 2018
- Published by Springer Nature in Metallurgical and Materials Transactions A
- Vol. 49 (5) , 1674-1682
A Three-Stage Mechanistic Model for Solidification Cracking During Welding of Steel
- 2 March 2018
- Published by Springer Nature in Metallurgical and Materials Transactions A
- Vol. 49 (5) , 1674-1682
Open AccessA Three-Stage Mechanistic Model for Solidification Cracking During Welding of Steel
- Open Access
- 11 January 2017
- Published by Springer Nature in Scientific Reports
- Vol. 7 (1) , 40255
Initiation and growth kinetics of solidification cracking during welding of steel
Solidification cracking is a key phenomenon associated with defect formation during welding. To elucidate the failure mechanisms, solidification cracking during arc welding of steel are investigated in situ with high-speed, high-energy synchrotron X-ray radiography. Damage initiates at relatively low true strain of about 3.1% in the form of micro-cavities at the weld subsurface where peak volumetric strain and triaxiality are localised. The initial micro-cavities, with sizes from 10 × 10−6 m to 27 × 10−6m, are mostly formed in isolation as revealed by synchrotron X-ray micro-tomography. The growth of micro-cavities is driven by increasing strain induced to the solidifying steel. Cavities grow through coalescence of micro-cavities to form micro-cracks first and then through the propagation of micro-cracks. Cracks propagate from the core of the weld towards the free surface along the solidifying grain boundaries at a speed of 2–3 × 10−3 m s−1.
- 11 January 2017
- Published by Springer Nature in Scientific Reports
- Vol. 7 (1) , 40255
Open AccessInitiation and growth kinetics of solidification cracking during welding of steel
Solidification cracking is a key phenomenon associated with defect formation during welding. To elucidate the failure mechanisms, solidification cracking during arc welding of steel are investigated in situ with high-speed, high-energy synchrotron X-ray radiography. Damage initiates at relatively low true strain of about 3.1% in the form of micro-cavities at the weld subsurface where peak volumetric strain and triaxiality are localised. The initial micro-cavities, with sizes from 10 × 10−6 m to 27 × 10−6m, are mostly formed in isolation as revealed by synchrotron X-ray micro-tomography. The growth of micro-cavities is driven by increasing strain induced to the solidifying steel. Cavities grow through coalescence of micro-cavities to form micro-cracks first and then through the propagation of micro-cracks. Cracks propagate from the core of the weld towards the free surface along the solidifying grain boundaries at a speed of 2–3 × 10−3 m s−1.
- 1 January 2015
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 622, 194-203
The role of Ti carbonitride precipitates on fusion zone strength-toughness in submerged arc welded linepipe joints
- 1 January 2015
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 622, 194-203
The role of Ti carbonitride precipitates on fusion zone strength-toughness in submerged arc welded linepipe joints
- 8 June 2014
- Published by ASME International
On the Relationship of Microstructure, Toughness, and Hardness Properties in a Submerged Arc Welded API-5L Grade X65 Pipeline Steel Section
In order to further improve welded pipeline performance, a detailed knowledge of the key and interlinking relationships between the chemistry, microstructure and mechanical properties of the weld joint is needed. In this paper, the results of optical emission spectroscopy analysis on the as welded chemical properties of a submerged arc welded API-5L grade X65 linepipe are first presented. The microstructure of the various weld regions is then assessed against the results of the chemical analysis using a series of microscopy techniques. A fine grained ferrite-degenerate pearlite microstructure was observed within the base metal of the linepipe along with large (1.5 μm) cuboidal Ti (C, N) precipitates. Within the heat affected zone (HAZ) close to the molten weld joint, grain growth occurred with small volume fractions of induced upper bainite present within the microstructure. The fusion zone of the submerged arc weld joint consists of predominantly acicular ferrite with a small volume of grain boundary phases and a high number of large (0.8 μm) spherical Ti (C, N) precipitates. The results of Vickers hardness tests carried out at two length scales (macro + micro) show clear relations between the hardening effects of the cementite enriched degenerate pearlite and induced upper bainite phases within the base metal and HAZ respectively. Fractography analysis of Charpy impact test samples across the submerged arc welded joint found that the large Ti (C, N) precipitates within the fusion zone appear to be acting as microvoid initiation sites for the ductile fracture and as such contributing to the relatively low toughness properties within the fusion zone. Finally, the potential benefits of reducing the Ti content in both the welding wires and X65 base metal for further improvement of the mechanical properties of the linepipe weld joint are discussed in regards to reducing the size of the coarse Ti (C, N) precipitates within the base metal, HAZ and fusion zone.
- 8 June 2014
- Published by ASME International
On the Relationship of Microstructure, Toughness, and Hardness Properties in a Submerged Arc Welded API-5L Grade X65 Pipeline Steel Section
In order to further improve welded pipeline performance, a detailed knowledge of the key and interlinking relationships between the chemistry, microstructure and mechanical properties of the weld joint is needed. In this paper, the results of optical emission spectroscopy analysis on the as welded chemical properties of a submerged arc welded API-5L grade X65 linepipe are first presented. The microstructure of the various weld regions is then assessed against the results of the chemical analysis using a series of microscopy techniques. A fine grained ferrite-degenerate pearlite microstructure was observed within the base metal of the linepipe along with large (1.5 μm) cuboidal Ti (C, N) precipitates. Within the heat affected zone (HAZ) close to the molten weld joint, grain growth occurred with small volume fractions of induced upper bainite present within the microstructure. The fusion zone of the submerged arc weld joint consists of predominantly acicular ferrite with a small volume of grain boundary phases and a high number of large (0.8 μm) spherical Ti (C, N) precipitates. The results of Vickers hardness tests carried out at two length scales (macro + micro) show clear relations between the hardening effects of the cementite enriched degenerate pearlite and induced upper bainite phases within the base metal and HAZ respectively. Fractography analysis of Charpy impact test samples across the submerged arc welded joint found that the large Ti (C, N) precipitates within the fusion zone appear to be acting as microvoid initiation sites for the ductile fracture and as such contributing to the relatively low toughness properties within the fusion zone. Finally, the potential benefits of reducing the Ti content in both the welding wires and X65 base metal for further improvement of the mechanical properties of the linepipe weld joint are discussed in regards to reducing the size of the coarse Ti (C, N) precipitates within the base metal, HAZ and fusion zone.
- 14 November 2012
- Published by Springer Nature in JOM
- Vol. 65 (1) , 99-106
Multiscale, Multiphysics Numerical Modeling of Fusion Welding with Experimental Characterization and Validation
- 14 November 2012
- Published by Springer Nature in JOM
- Vol. 65 (1) , 99-106
Multiscale, Multiphysics Numerical Modeling of Fusion Welding with Experimental Characterization and Validation