Tao Gui
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Tao Gui has a total of 23 co-authors. Here are the top co-authors by number of shared publications:
Xue Bai
3 shared publicationsBo Song
School of Metallurgical and Ecological Engineering University of Science and Technology Beijing 100083 Beijing China
2 shared publicationsLei Yang
Division of Metallurgy and Materials for Rare Metals General Research Institute for Nonferrous Metals 100088 Beijing China
2 shared publicationsXingming Wang
2 shared publications- Xingqi Wang
National Engineering Research Center of Environment-Friendly Metallurgy in Producing Premium Non-ferrous Metals, GRINM Group Co., Ltd., Beijing 101407, China
2 shared publications Yuyang Liu
2 shared publications
Latest Publications
- Open Access
- 22 May 2024
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 30, 8591-8598
Investigation of the effects of rare earth element doping on the thermophysical properties of Gd2Zr2O7 by first principles
- 22 May 2024
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 30, 8591-8598
Open AccessInvestigation of the effects of rare earth element doping on the thermophysical properties of Gd2Zr2O7 by first principles
- Open Access
Preparation of AlON Powder by Carbothermal Reduction and Nitridation with Assisting by Silane Coupling Agent
In the preparation processes of aluminum oxynitride (AlON) powders by carbothermal reduction and nitridation, the homogeneity of mixed raw powders between Al2O3 and C is a critical factor by which the final composition and related properties of AlON transparent ceramic will be decided. In this paper, a silane coupling agent was used as a dispersant to optimize the distribution uniformity of raw material of Al2O3 and C, and the preparation of AlON powder with controllable composition and its distribution is investigated. The results show that the silane dispersant could effectively improve the distribution uniformity of raw material. The silane coupling agent contains functional groups of −SiH3 and −CnH2n+1O. XPS showed that the silane could react with C and Al2O3 to form the Si–C bond and C–Al2O3 bond, respectively. The silane coupling agent provides a connected bridge for raw material powders. When the amount of the silane was 5 wt%, the mixed powder had a great distribution uniformity. The addition of silane coupling agent improved the reactivity of raw materials and decreased the synthesis temperature of AlON. The single-phase AlON powder was obtained after the Al2O3/C mixed powder was kept at 1670 °C for 30 min. Furthermore, the grain size of AlON powder was 100–200 nm with an AlN content of 27.5 mol%. With the increase of holding time to 4 h, the grain size increased to 15 μm, indicating that sintering between particles occurred, which may reduce the sintering activity of the powder.
Open AccessPreparation of AlON Powder by Carbothermal Reduction and Nitridation with Assisting by Silane Coupling Agent
In the preparation processes of aluminum oxynitride (AlON) powders by carbothermal reduction and nitridation, the homogeneity of mixed raw powders between Al2O3 and C is a critical factor by which the final composition and related properties of AlON transparent ceramic will be decided. In this paper, a silane coupling agent was used as a dispersant to optimize the distribution uniformity of raw material of Al2O3 and C, and the preparation of AlON powder with controllable composition and its distribution is investigated. The results show that the silane dispersant could effectively improve the distribution uniformity of raw material. The silane coupling agent contains functional groups of −SiH3 and −CnH2n+1O. XPS showed that the silane could react with C and Al2O3 to form the Si–C bond and C–Al2O3 bond, respectively. The silane coupling agent provides a connected bridge for raw material powders. When the amount of the silane was 5 wt%, the mixed powder had a great distribution uniformity. The addition of silane coupling agent improved the reactivity of raw materials and decreased the synthesis temperature of AlON. The single-phase AlON powder was obtained after the Al2O3/C mixed powder was kept at 1670 °C for 30 min. Furthermore, the grain size of AlON powder was 100–200 nm with an AlN content of 27.5 mol%. With the increase of holding time to 4 h, the grain size increased to 15 μm, indicating that sintering between particles occurred, which may reduce the sintering activity of the powder.
- 20 November 2018
- Published by Wiley in Rare Metals
- Vol. 37 (12) , 1076-1081
Synthesis and densification of zirconium diboride prepared by carbothermal reduction
Using boron powder as additive, the preparation of zirconium diboride (ZrB 2 ) by carbothermal reduction was investigated. The results show that the carbothermal reduction cannot be completely done until the temperature is more than 1900 °C. The ZrB 2 particles prepared without boron (B) additive at 1900 °C for 3 h are rodlike and show a preferential grain growth along [001] direction. B additive changes the heat effect of the raw materials. With B additive, the morphology of ZrB 2 particles turns to be regular shape. The average particle size is about 3.6 μm with 2.5 wt% B additives. With more B additive, the shape of particles turns to be round like and the average particle size is decreased to 2.3 μm when 5 wt% B is added. The existence of oxides in grain boundary is a key factor to keep ZrB 2 ceramic from deep densification. Using ZrB 2 powder prepared with 5 wt% B additives, by controlling carbon content in ZrB 2 powder, ZrB 2 ceramic with 93% relative density is hot‐pressed.
- 20 November 2018
- Published by Wiley in Rare Metals
- Vol. 37 (12) , 1076-1081
Synthesis and densification of zirconium diboride prepared by carbothermal reduction
Using boron powder as additive, the preparation of zirconium diboride (ZrB 2 ) by carbothermal reduction was investigated. The results show that the carbothermal reduction cannot be completely done until the temperature is more than 1900 °C. The ZrB 2 particles prepared without boron (B) additive at 1900 °C for 3 h are rodlike and show a preferential grain growth along [001] direction. B additive changes the heat effect of the raw materials. With B additive, the morphology of ZrB 2 particles turns to be regular shape. The average particle size is about 3.6 μm with 2.5 wt% B additives. With more B additive, the shape of particles turns to be round like and the average particle size is decreased to 2.3 μm when 5 wt% B is added. The existence of oxides in grain boundary is a key factor to keep ZrB 2 ceramic from deep densification. Using ZrB 2 powder prepared with 5 wt% B additives, by controlling carbon content in ZrB 2 powder, ZrB 2 ceramic with 93% relative density is hot‐pressed.
- 18 April 2018
- Published by Springer Nature
- p. 517-527
Deep Densification of ZrB2 by Hot Pressing
- 17 March 2012
- Published by Wiley
- p. 663-670
Biosorption Characteristics of Pb(II) from Aqueous Solution onto Poplar Cotton
- 17 March 2012
- Published by Wiley
- p. 663-670
Biosorption Characteristics of Pb(II) from Aqueous Solution onto Poplar Cotton