Liang Qi
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Liang Qi has a total of 69 co-authors. Here are the top co-authors by number of shared publications:
Chengcong Huang
Jiangxi Univ Sci & Technol, Fac Mat Met & Chem, Ganzhou 341000, Peoples R China
4 shared publicationsHongjin Zhao
4 shared publicationsJinbing Hu
4 shared publicationsZhen Ge
Faculty of Materials Metallurgy and Chemistry, Jiangxi University of Science and Technology 1 , Ganzhou 341000
4 shared publications- Zhigang Wang
School of Materials Science and Engineering, Jiangxi University of Science and Technology, Ganzhou 341000, China
4 shared publications Jiqiang Chen
3 shared publications
Latest Publications
- Open Access
- 2 July 2026
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 43, 4309-4323
Strength–ductility balance of AFSD-processed 7075 aluminum alloy: Synergistic roles of AFSD-induced dispersion and TiC nanoparticle modification
- 2 July 2026
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 43, 4309-4323
Open AccessStrength–ductility balance of AFSD-processed 7075 aluminum alloy: Synergistic roles of AFSD-induced dispersion and TiC nanoparticle modification
- 10 February 2025
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 1017
Additive friction stir deposition of Al-Ce alloy:Microstructure evolution, strengthening and fracture mechanism
- 10 February 2025
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 1017
Additive friction stir deposition of Al-Ce alloy:Microstructure evolution, strengthening and fracture mechanism
- 1 February 2025
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 927
Wire-arc directed energy deposited Al-Ce alloy: Microstructure evolution and mechanical properties
- 1 February 2025
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 927
Wire-arc directed energy deposited Al-Ce alloy: Microstructure evolution and mechanical properties
- 9 December 2024
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 43 (1)
Effect of Mg content on corrosion resistance of Zn-11Al-XMg coatings
Zn-Al-Mg is one of the most important coating types in hot dipped galvanization. This surface coating also provides surface barrier protection and galvanic protection, which improves the esthetics and service life of the material. In this paper, the corrosion resistance of Zn-11Al-XMg coatings with Mg content (wt. %) of 0, 1, 2, 3 was studied, and the effect of Mg content on the corrosion resistance of Zn-11Al-XMg coatings was analyzed. The results show that Zn-11Al coating is composed of an eutectoid Al-rich phase and a Zn-rich phase. When the Mg content is less than 2 wt. %, the increase of Mg content is accompanied by the decrease of the Al-rich and Zn-rich phases and the increase of the ternary eutectic content. When the Mg content is more than 2 wt. %, the increase of Mg content is accompanied by the decrease of the ternary eutectic content and the increase of the primary MgZn2 phase content. The results of corrosion experiments show that the Zn-11Al-XMg coating is mainly composed of an Al-rich phase and an Mg2Zn11 phase in ternary eutectic as the main anode. The coating after adding Mg forms a denser corrosion product film, among which the Zn-11Al-2Mg coating close to the eutectic point has the best corrosion resistance.
- 9 December 2024
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 43 (1)
Effect of Mg content on corrosion resistance of Zn-11Al-XMg coatings
Zn-Al-Mg is one of the most important coating types in hot dipped galvanization. This surface coating also provides surface barrier protection and galvanic protection, which improves the esthetics and service life of the material. In this paper, the corrosion resistance of Zn-11Al-XMg coatings with Mg content (wt. %) of 0, 1, 2, 3 was studied, and the effect of Mg content on the corrosion resistance of Zn-11Al-XMg coatings was analyzed. The results show that Zn-11Al coating is composed of an eutectoid Al-rich phase and a Zn-rich phase. When the Mg content is less than 2 wt. %, the increase of Mg content is accompanied by the decrease of the Al-rich and Zn-rich phases and the increase of the ternary eutectic content. When the Mg content is more than 2 wt. %, the increase of Mg content is accompanied by the decrease of the ternary eutectic content and the increase of the primary MgZn2 phase content. The results of corrosion experiments show that the Zn-11Al-XMg coating is mainly composed of an Al-rich phase and an Mg2Zn11 phase in ternary eutectic as the main anode. The coating after adding Mg forms a denser corrosion product film, among which the Zn-11Al-2Mg coating close to the eutectic point has the best corrosion resistance.
- Open Access
Study of Aging Temperature on the Thermal Compression Behaviors and Microstructure of a Novel Ni-Cr-Co-Based Superalloy
Nickel-based superalloys have been widely used in the aerospace industry, and regulating the reinforcing phases is the key to improving the high-temperature strength of the alloy. In this study, a series of aging treatments (650 °C, 750 °C, 850 °C and 950 °C for 8 h) were designed to study different thermal deformation behaviors and microstructure evolutions for a novel nickel-based superalloy. Among the aged samples, the 950 °C aged sample achieved the peak stress of ~323 MPa during the thermal deformation and the highest microhardness of ~315 HV after thermal compression, which were the greatest differences compared to before deformation. In addition, the grains of the 950 °C sample exhibit deformed fibrous shapes, and the grain orientation is isotropic, while the other samples exhibited isotropy. In the 850 °C and 950 °C high-temperature aging samples, the γ′ precipitate (about 20 nm in size) is gradually precipitated, which inhibits the movement of dislocation in the grain during compression, thus inhibiting the occurrence of dynamic recrystallization and improving the high-temperature mechanical properties of the alloy.
Open AccessStudy of Aging Temperature on the Thermal Compression Behaviors and Microstructure of a Novel Ni-Cr-Co-Based Superalloy
Nickel-based superalloys have been widely used in the aerospace industry, and regulating the reinforcing phases is the key to improving the high-temperature strength of the alloy. In this study, a series of aging treatments (650 °C, 750 °C, 850 °C and 950 °C for 8 h) were designed to study different thermal deformation behaviors and microstructure evolutions for a novel nickel-based superalloy. Among the aged samples, the 950 °C aged sample achieved the peak stress of ~323 MPa during the thermal deformation and the highest microhardness of ~315 HV after thermal compression, which were the greatest differences compared to before deformation. In addition, the grains of the 950 °C sample exhibit deformed fibrous shapes, and the grain orientation is isotropic, while the other samples exhibited isotropy. In the 850 °C and 950 °C high-temperature aging samples, the γ′ precipitate (about 20 nm in size) is gradually precipitated, which inhibits the movement of dislocation in the grain during compression, thus inhibiting the occurrence of dynamic recrystallization and improving the high-temperature mechanical properties of the alloy.
- Open Access
Different Heat-Exposure Temperatures on the Microstructure and Properties of Dissimilar GH4169/IC10 Superalloy Vacuum Electron Beam Welded Joint
Vacuum electron-beam welding (EBW) was used to join the precipitation-strengthened GH4169 superalloy and a new nickel-based superalloy IC10 to fabricate the turbine blade discs. In this study, a solid solution (1050 °C/2 h for GH4169 and 1150 °C/2 h for IC10) and different heat-exposure temperatures (650 °C, 750 °C, 950 °C and 1050 °C/200 h, respectively) were used to study the high-temperature tensile properties and microstructure evolution of welded joints; meanwhile, the formation and evolution of the second phases of the joints were analyzed. After EBW, the welded joint exhibited a typical nail morphology, and the fusion zone (FZ) consisted of columnar and cellular structures. During the solidification process of the molten pool, Mo elements are enriched in the dendrites and inter-dendrites, and that of Nb and Ti elements was enriched in the dendrites, which lead to forming a non-uniform distribution of Laves eutectic and MC carbides in the FZ. The microhardness of the FZ gradually increased during thermal exposure at 650 °C and reached 300–320 HV, and the γ′ and γ″ phases were gradually precipitated with size of about 50 nm. Meanwhile, the microhardness of the FZ decreased to 260–280 HV at 750 °C, and the higher temperature resulted in the coarsening of the γ″ phase (with a final size of about 100 nm) and the formation of the acicular δ-phase. At 950 °C and 1050 °C, the microhardness of FZ decreased sharply, reaching up to 170~190 HV and 160~180 HV, respectively. Moreover, the Laves eutectic and MC carbides are dissolved to a greater extent without the formation of γ″ and δ phases; as a result, the absent of γ″ and δ phases are attributed to the significant improvement of segregation at higher temperatures.
Open AccessDifferent Heat-Exposure Temperatures on the Microstructure and Properties of Dissimilar GH4169/IC10 Superalloy Vacuum Electron Beam Welded Joint
Vacuum electron-beam welding (EBW) was used to join the precipitation-strengthened GH4169 superalloy and a new nickel-based superalloy IC10 to fabricate the turbine blade discs. In this study, a solid solution (1050 °C/2 h for GH4169 and 1150 °C/2 h for IC10) and different heat-exposure temperatures (650 °C, 750 °C, 950 °C and 1050 °C/200 h, respectively) were used to study the high-temperature tensile properties and microstructure evolution of welded joints; meanwhile, the formation and evolution of the second phases of the joints were analyzed. After EBW, the welded joint exhibited a typical nail morphology, and the fusion zone (FZ) consisted of columnar and cellular structures. During the solidification process of the molten pool, Mo elements are enriched in the dendrites and inter-dendrites, and that of Nb and Ti elements was enriched in the dendrites, which lead to forming a non-uniform distribution of Laves eutectic and MC carbides in the FZ. The microhardness of the FZ gradually increased during thermal exposure at 650 °C and reached 300–320 HV, and the γ′ and γ″ phases were gradually precipitated with size of about 50 nm. Meanwhile, the microhardness of the FZ decreased to 260–280 HV at 750 °C, and the higher temperature resulted in the coarsening of the γ″ phase (with a final size of about 100 nm) and the formation of the acicular δ-phase. At 950 °C and 1050 °C, the microhardness of FZ decreased sharply, reaching up to 170~190 HV and 160~180 HV, respectively. Moreover, the Laves eutectic and MC carbides are dissolved to a greater extent without the formation of γ″ and δ phases; as a result, the absent of γ″ and δ phases are attributed to the significant improvement of segregation at higher temperatures.
- 1 May 2023
- Published by SAGE Publications in Materials Science and Technology
- Vol. 39 (8) , 1030-1038
Effects of Er addition and cooling rate on the corrosion resistance of Zn-5Al alloys
Galfan (Zn-5Al-RE) coating is widely used in high-strength steel wires. The effects of cooling rate and the adulteration of erbium (Er) on the microstructure and corrosion resistance of Zn-5Al alloys were investigated in this study. The results show that the Zn-5Al alloy is made up of the primary η-Zn phase and eutectic structure at a high cooling rate. As the cooling rate decreases, the corrosion current firstly increased and then decreased due to decrease of the primary η-Zn content, the appearance and grew of α-Al phase. Moreover, the addition of Er leads to the formation of Er-containing intermetallic compounds in the Zn-5Al alloy, reducing the size of the primary η-Zn and α-Al phase, decreasing the corrosion current density, and improving the density and compactness of the corrosion product.
- 1 May 2023
- Published by SAGE Publications in Materials Science and Technology
- Vol. 39 (8) , 1030-1038
Effects of Er addition and cooling rate on the corrosion resistance of Zn-5Al alloys
Galfan (Zn-5Al-RE) coating is widely used in high-strength steel wires. The effects of cooling rate and the adulteration of erbium (Er) on the microstructure and corrosion resistance of Zn-5Al alloys were investigated in this study. The results show that the Zn-5Al alloy is made up of the primary η-Zn phase and eutectic structure at a high cooling rate. As the cooling rate decreases, the corrosion current firstly increased and then decreased due to decrease of the primary η-Zn content, the appearance and grew of α-Al phase. Moreover, the addition of Er leads to the formation of Er-containing intermetallic compounds in the Zn-5Al alloy, reducing the size of the primary η-Zn and α-Al phase, decreasing the corrosion current density, and improving the density and compactness of the corrosion product.
- 1 November 2022
- Published by SAGE Publications in Materials Science and Technology
- Vol. 38 (17) , 1501-1509
Effect of erbium (Er) on the hot cracking behaviour of Al-5Cu alloy
In this paper, the effect of Er on the hot cracking behaviour of Al-5Cu alloy is investigated by the means of wedge moulds, differential hot analyzer, optical microscope, and scanning electron microscope. The results show that the percentage of intergranular low-melting-point eutectic structure is increased by approximately 8% on average per 0.3 wt-% Er additions. The increase of low-melting-point eutectic structure enhances the fluidity of the liquid film in the late solidification stage, resulting in the improvement of the hot cracking resistance of the alloy. Moreover, the Al-5Cu-0.6Er alloy has the best hot cracking resistance under wedge-shaped copper casting experiments.
- 1 November 2022
- Published by SAGE Publications in Materials Science and Technology
- Vol. 38 (17) , 1501-1509
Effect of erbium (Er) on the hot cracking behaviour of Al-5Cu alloy
In this paper, the effect of Er on the hot cracking behaviour of Al-5Cu alloy is investigated by the means of wedge moulds, differential hot analyzer, optical microscope, and scanning electron microscope. The results show that the percentage of intergranular low-melting-point eutectic structure is increased by approximately 8% on average per 0.3 wt-% Er additions. The increase of low-melting-point eutectic structure enhances the fluidity of the liquid film in the late solidification stage, resulting in the improvement of the hot cracking resistance of the alloy. Moreover, the Al-5Cu-0.6Er alloy has the best hot cracking resistance under wedge-shaped copper casting experiments.
- 1 September 2021
- Published by SAGE Publications in Materials Science and Technology
- Vol. 37 (13) , 1129-1138
Dynamic deformation behaviour of 0.51C–1.72Si–0.83Mn–0.56Co high-strength steel
In this paper, high-strength steel is prepared by different heat-treatment processes. Through split Hopkinson pressure bar experiment, optical microscope, scanning electron microscope and X-ray diffractometer, the microstructure evolution and mechanical behaviour under high strain rate were studied. The results show that the samples prepared by the two-step isothermal method have the highest compressive strength under the same strain rate, especially at 5000 s−1, the highest can reach 2097 MPa. The retained austenite undergoes transformation under high strain rate conditions, which improves the plastic deformation ability of the material. Compared with the one-step isothermal heat-treatment process, the two-step isothermal heat-treatment process can better control the strength and plasticity under high strain rate deformation conditions.
- 1 September 2021
- Published by SAGE Publications in Materials Science and Technology
- Vol. 37 (13) , 1129-1138
Dynamic deformation behaviour of 0.51C–1.72Si–0.83Mn–0.56Co high-strength steel
In this paper, high-strength steel is prepared by different heat-treatment processes. Through split Hopkinson pressure bar experiment, optical microscope, scanning electron microscope and X-ray diffractometer, the microstructure evolution and mechanical behaviour under high strain rate were studied. The results show that the samples prepared by the two-step isothermal method have the highest compressive strength under the same strain rate, especially at 5000 s−1, the highest can reach 2097 MPa. The retained austenite undergoes transformation under high strain rate conditions, which improves the plastic deformation ability of the material. Compared with the one-step isothermal heat-treatment process, the two-step isothermal heat-treatment process can better control the strength and plasticity under high strain rate deformation conditions.