Furong Cao
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Furong Cao has a total of 28 co-authors. Here are the top co-authors by number of shared publications:
- Nanpan Guo
School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China
3 shared publications - Shuting Kong
School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China
3 shared publications Hua Ding
College of Materials and Metallurgy, Northeastern University, Shenyang 110819, China
2 shared publications- Huihui Shang
School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China
2 shared publications Jinrui Liang
School of Materials Science and Engineering, Northeastern University, Shenyang, People’s Republic of China
2 shared publicationsBi Jin Zhou
Northeastern University
1 shared publication
Latest Publications
- 8 October 2024
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 34 (14) , 14535-14550
Microstructural Evolution, Mechanical Property, and Strengthening in a Lightweight Mg-Y-Zn-Mn Alloy Fabricated by Multidirectional Forging and Hot Rolling
- 8 October 2024
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 34 (14) , 14535-14550
Microstructural Evolution, Mechanical Property, and Strengthening in a Lightweight Mg-Y-Zn-Mn Alloy Fabricated by Multidirectional Forging and Hot Rolling
- Open Access
Room Temperature Strengthening and High-Temperature Superplasticity of Mg-Li-Al-Sr-Y Alloy Fabricated by Asymmetric Rolling and Friction Stir Processing
Magnesium-lithium alloy is the lightest alloy to date. To explore its room temperature strength and high-temperature ductility, a plate of a new fine-grained Mg-9.13Li-3.74Al-0.31Sr-0.11Y alloy was fabricated by asymmetric rolling, and the rolled plate was subjected to friction stir processing (FSP). The microstructure and mechanical properties at room and elevated temperatures were investigated by optical microscopy, X-ray diffraction (XRD), energy dispersive spectroscopy (EDS), and tensile tester. Grain refinement with an average grain size in the α-Mg phase of 1.65 μm and an average grain size in the β-Li phase of 4.24 μm was achieved in the water-cooled FSP alloy. For room temperature behavior, the ultimate tensile strength of 208 ± 4 MPa, yield strength of 193 ± 2 MPa, and elongation of 48.2% were obtained in the water-cooled FSP alloy. XRD and EDS analyses revealed that the present alloy consists of α-Mg and β-Li phases, Al2Y, Al4Sr, MgLi2Al, and AlLi intermetallic compounds. For high-temperature behavior, the maximum superplasticity or ductility of 416% was demonstrated in this fine-grained alloy with an average grain size of 10 μm at 573 K and 1.67 × 10−3 s−1. A power-law constitutive equation was established. The stress exponent was 2.29 (≈2) (strain rate sensitivity 0.44), and the deformation activation energy was 162.02 kJ/mol. This evidence confirmed that the dominant deformation mechanism at elevated temperatures is grain boundary and interphase boundary sliding controlled by lattice diffusion.
Open AccessRoom Temperature Strengthening and High-Temperature Superplasticity of Mg-Li-Al-Sr-Y Alloy Fabricated by Asymmetric Rolling and Friction Stir Processing
Magnesium-lithium alloy is the lightest alloy to date. To explore its room temperature strength and high-temperature ductility, a plate of a new fine-grained Mg-9.13Li-3.74Al-0.31Sr-0.11Y alloy was fabricated by asymmetric rolling, and the rolled plate was subjected to friction stir processing (FSP). The microstructure and mechanical properties at room and elevated temperatures were investigated by optical microscopy, X-ray diffraction (XRD), energy dispersive spectroscopy (EDS), and tensile tester. Grain refinement with an average grain size in the α-Mg phase of 1.65 μm and an average grain size in the β-Li phase of 4.24 μm was achieved in the water-cooled FSP alloy. For room temperature behavior, the ultimate tensile strength of 208 ± 4 MPa, yield strength of 193 ± 2 MPa, and elongation of 48.2% were obtained in the water-cooled FSP alloy. XRD and EDS analyses revealed that the present alloy consists of α-Mg and β-Li phases, Al2Y, Al4Sr, MgLi2Al, and AlLi intermetallic compounds. For high-temperature behavior, the maximum superplasticity or ductility of 416% was demonstrated in this fine-grained alloy with an average grain size of 10 μm at 573 K and 1.67 × 10−3 s−1. A power-law constitutive equation was established. The stress exponent was 2.29 (≈2) (strain rate sensitivity 0.44), and the deformation activation energy was 162.02 kJ/mol. This evidence confirmed that the dominant deformation mechanism at elevated temperatures is grain boundary and interphase boundary sliding controlled by lattice diffusion.
- Open Access
Room-Temperature Strengthening, Portevin-Le Chatelier Effect, High-Temperature Tensile Deformation Behavior, and Constitutive Modeling in a Lightweight Mg-Gd-Al-Zn Alloy
To explore room-temperature strengthening and high-temperature ductility, a lightweight novel Mg-1.85Gd-0.64Al-0.62Zn alloy was fabricated by innovative multidirectional forging and a hot-rolling technique. Microstructures and mechanical properties were studied at room and elevated temperatures with an optical microscope, an X-ray diffractometer, and a tensile tester. An ultimate tensile strength of 260 MPa, yield strength of 171 MPa, and elongation of 20.4% were demonstrated at room temperature. The room-temperature strengthening mechanisms were identified by strengthening the model estimation. A type C Portevin-Le Chatelier effect was discovered and elucidated in this alloy. X-ray diffraction analysis revealed that the phase composition is α-Mg solid solution and (Mg, Al)3Gd, Al7Zn3, and Al2Gd intermetallic compounds. Examination of the microstructure at elevated temperatures revealed that dynamic recrystallization and dynamic grain growth occur. In particular, it was discovered that bimodal microstructures or incomplete dynamic recrystallization microstructures exist in high-temperature deformation. A maximum quasi-superplasticity of 228.4% was demonstrated in this alloy at 673 K and 5.0 × 10−4 s−1. Flow stress curves showed that the present alloy exhibits Sotoudeh–Bate curves or a long intermediate strain-hardening stage followed by a strain-softening stage. A modified Zerilli–Armstrong constitutive equation incorporating the number of dislocations was established. The power-law constitutive equation was established to identify the deformation mechanism. Both constitutive models had good predictability. At 673 K and 5.0 × 10−4 s−1, the stress exponent was 4, and the average deformation activation energy was 104.42 kJ/mol. The number of dislocations inside a grain was 146. This characteristic evidence confirmed that dislocation motion controlled by pipe diffusion dominates the rate-controlling process under this condition.
Open AccessRoom-Temperature Strengthening, Portevin-Le Chatelier Effect, High-Temperature Tensile Deformation Behavior, and Constitutive Modeling in a Lightweight Mg-Gd-Al-Zn Alloy
To explore room-temperature strengthening and high-temperature ductility, a lightweight novel Mg-1.85Gd-0.64Al-0.62Zn alloy was fabricated by innovative multidirectional forging and a hot-rolling technique. Microstructures and mechanical properties were studied at room and elevated temperatures with an optical microscope, an X-ray diffractometer, and a tensile tester. An ultimate tensile strength of 260 MPa, yield strength of 171 MPa, and elongation of 20.4% were demonstrated at room temperature. The room-temperature strengthening mechanisms were identified by strengthening the model estimation. A type C Portevin-Le Chatelier effect was discovered and elucidated in this alloy. X-ray diffraction analysis revealed that the phase composition is α-Mg solid solution and (Mg, Al)3Gd, Al7Zn3, and Al2Gd intermetallic compounds. Examination of the microstructure at elevated temperatures revealed that dynamic recrystallization and dynamic grain growth occur. In particular, it was discovered that bimodal microstructures or incomplete dynamic recrystallization microstructures exist in high-temperature deformation. A maximum quasi-superplasticity of 228.4% was demonstrated in this alloy at 673 K and 5.0 × 10−4 s−1. Flow stress curves showed that the present alloy exhibits Sotoudeh–Bate curves or a long intermediate strain-hardening stage followed by a strain-softening stage. A modified Zerilli–Armstrong constitutive equation incorporating the number of dislocations was established. The power-law constitutive equation was established to identify the deformation mechanism. Both constitutive models had good predictability. At 673 K and 5.0 × 10−4 s−1, the stress exponent was 4, and the average deformation activation energy was 104.42 kJ/mol. The number of dislocations inside a grain was 146. This characteristic evidence confirmed that dislocation motion controlled by pipe diffusion dominates the rate-controlling process under this condition.
- Open Access
High Strain Rate Quasi-Superplasticity Behavior in an Ultralight Mg-9.55Li-2.92Al-0.027Y-0.026Mn Alloy Fabricated by Multidirectional Forging and Asymmetrical Rolling
To explore new approaches to severe plastic deformation and the ductility of a multicomponent magnesium–lithium alloy, an ultralight microduplex Mg-9.55Li-2.92Al-0.027Y-0.026Mn alloy was made by novel multidirectional forging and asymmetrical rolling, and the superplasticity behavior was investigated by optical microscope, hot tensile test, and modeling. The average grain size is 1.9 μm in this alloy after multidirectional forging and asymmetrical rolling. Remarkable grain refinement caused by such a forming, which turns the as-cast grain size of 144.68 μm into the as-rolled grain size of 1.9 μm, is achieved. The elongation to failure of 228.05% is obtained at 523 K and 1 × 10−2 s−1, which demonstrates the high strain rate quasi-superplasticity. The maximum elongation to failure of 287.12% was achieved in this alloy at 573 K and 5 × 10−4 s−1. It was found that strain-induced grain coarsening at 523 K is much weaker than the strain-induced grain coarsening at 573 K. Thus, the ductility of 228.05% is suitable for application in high strain rate superplastic forming. The stress exponent of 3 and the average activation energy for deformation of 50.06 kJ/mol indicate that the rate-controlling deformation mechanism is dislocation-glide controlled by pipe diffusion.
Open AccessHigh Strain Rate Quasi-Superplasticity Behavior in an Ultralight Mg-9.55Li-2.92Al-0.027Y-0.026Mn Alloy Fabricated by Multidirectional Forging and Asymmetrical Rolling
To explore new approaches to severe plastic deformation and the ductility of a multicomponent magnesium–lithium alloy, an ultralight microduplex Mg-9.55Li-2.92Al-0.027Y-0.026Mn alloy was made by novel multidirectional forging and asymmetrical rolling, and the superplasticity behavior was investigated by optical microscope, hot tensile test, and modeling. The average grain size is 1.9 μm in this alloy after multidirectional forging and asymmetrical rolling. Remarkable grain refinement caused by such a forming, which turns the as-cast grain size of 144.68 μm into the as-rolled grain size of 1.9 μm, is achieved. The elongation to failure of 228.05% is obtained at 523 K and 1 × 10−2 s−1, which demonstrates the high strain rate quasi-superplasticity. The maximum elongation to failure of 287.12% was achieved in this alloy at 573 K and 5 × 10−4 s−1. It was found that strain-induced grain coarsening at 523 K is much weaker than the strain-induced grain coarsening at 573 K. Thus, the ductility of 228.05% is suitable for application in high strain rate superplastic forming. The stress exponent of 3 and the average activation energy for deformation of 50.06 kJ/mol indicate that the rate-controlling deformation mechanism is dislocation-glide controlled by pipe diffusion.
- Open Access
- 10 March 2022
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 18, 962-977
Room temperature strengthening mechanisms, high temperature deformation behavior and constitutive modeling in an Al-3.25Mg-0.37Zr-0.28Mn-0.19Y alloy
- 10 March 2022
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 18, 962-977
Open AccessRoom temperature strengthening mechanisms, high temperature deformation behavior and constitutive modeling in an Al-3.25Mg-0.37Zr-0.28Mn-0.19Y alloy
- 14 November 2018
- Published by Springer Nature in Metals and Materials International
- Vol. 25 (3) , 570-583
High-Temperature Deformation Behavior of Duplex Mg–8.41Li–1.80Al–1.77Zn Alloy Processed by Friction Stir Processing
- 14 November 2018
- Published by Springer Nature in Metals and Materials International
- Vol. 25 (3) , 570-583
High-Temperature Deformation Behavior of Duplex Mg–8.41Li–1.80Al–1.77Zn Alloy Processed by Friction Stir Processing
- 1 September 2015
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 643, 169-174
Incorporating dislocation variables into Mohamed's and Kawasaki–Langdon's deformation mechanism maps containing superplasticity mechanism regimes
- 1 September 2015
- Published by Elsevier in Materials Science and Engineering: A
- Vol. 643, 169-174
Incorporating dislocation variables into Mohamed's and Kawasaki–Langdon's deformation mechanism maps containing superplasticity mechanism regimes
- 31 January 2013
- Published by Elsevier in Transactions of Nonferrous Metals Society of China
- Vol. 23 (1) , 201-207
Force analysis and experimental study of pure aluminum and Al–5%Ti–1%B alloy continuous expansion extrusion forming process
- 31 January 2013
- Published by Elsevier in Transactions of Nonferrous Metals Society of China
- Vol. 23 (1) , 201-207
Force analysis and experimental study of pure aluminum and Al–5%Ti–1%B alloy continuous expansion extrusion forming process
- 11 June 2010
- Published by China Science Publishing & Media Ltd. in ACTA METALLURGICA SINICA
- Vol. 46 (6) , 715-722
DISLOCATION CREEP IN SUPER--LIGHT α SOLID SOLUTION BASE Mg--6Li--3Zn ALLOY
- 11 June 2010
- Published by China Science Publishing & Media Ltd. in ACTA METALLURGICA SINICA
- Vol. 46 (6) , 715-722
DISLOCATION CREEP IN SUPER--LIGHT α SOLID SOLUTION BASE Mg--6Li--3Zn ALLOY