Hediye Aydin
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Hediye Aydin has a total of 19 co-authors. Here are the top co-authors by number of shared publications:
Benan Elmusa
Department of Metallurgy and Material Engineering, Kütahya Dumlupinar University, Kütahya, Turkey
2 shared publications- Esad Kaya
Eskisehir Osmangazi University
2 shared publications G. Tokatas
2 shared publications- Pelin Çağım Tokat Birgin
Kutahya Dumlupinar Universitesi
2 shared publications Aysun Şavk
1 shared publicationEsad Kaya
Department of Mechanical Engineering, Eskisehir Osmangazi University, Eskişehir, Turkey
1 shared publication
Latest Publications
- 10 July 2026
- Published by Springer Nature in Chemical Papers
- Vol. 80 (11) , 13689-13701
Morphological and structural evolution of boron-containing electrospun nanofibers toward B4C formation
- 10 July 2026
- Published by Springer Nature in Chemical Papers
- Vol. 80 (11) , 13689-13701
Morphological and structural evolution of boron-containing electrospun nanofibers toward B4C formation
- Open Access
- 3 June 2026
- Published by Afyon Kocatepe Universitesi Fen Ve Muhendislik Bilimleri Dergisi in Afyon Kocatepe University Journal of Sciences and Engineering
- Vol. 26 (3) , 751-760
Spark Plasma Sintered B₄C-Based Composites with WC and Y₂O₃ Additives: Phase Evolution, Densification and Microstructural Analysis
B₄C matrix composites were produced using the spark plasma sintering (SPS) method at a temperature of 1900°C and a pressure of 40 MPa. In the production process, WC additives at volumes of 15%, 17.5%, and 20% and Y₂O₃ additives at volumes of 2.5% and 5% were used. The mechanical properties of composites produced using the SPS method have been investigated in relation to the effect of secondary phases on the structure. The sintered ceramic matrix composites exhibited a high fracture toughness of 8.1 MPa⋅ m¹/² and a Vickers hardness of 23.5 GPa. This remarkable improvement is attributed to the reduction in grain size, the formation of secondary phases, and energy loss mechanisms resulting from fracture along grain boundaries.
- 3 June 2026
- Published by Afyon Kocatepe Universitesi Fen Ve Muhendislik Bilimleri Dergisi in Afyon Kocatepe University Journal of Sciences and Engineering
- Vol. 26 (3) , 751-760
Open AccessSpark Plasma Sintered B₄C-Based Composites with WC and Y₂O₃ Additives: Phase Evolution, Densification and Microstructural Analysis
B₄C matrix composites were produced using the spark plasma sintering (SPS) method at a temperature of 1900°C and a pressure of 40 MPa. In the production process, WC additives at volumes of 15%, 17.5%, and 20% and Y₂O₃ additives at volumes of 2.5% and 5% were used. The mechanical properties of composites produced using the SPS method have been investigated in relation to the effect of secondary phases on the structure. The sintered ceramic matrix composites exhibited a high fracture toughness of 8.1 MPa⋅ m¹/² and a Vickers hardness of 23.5 GPa. This remarkable improvement is attributed to the reduction in grain size, the formation of secondary phases, and energy loss mechanisms resulting from fracture along grain boundaries.
- Open Access
- 17 May 2026
- Published by Folium Publishing Company in Металловедение и термическая обработка металлов
- No. 5,p. 20
Effect of cryogenic treatment on the properties of high molybdenum alloy steel
Исследовано влияние глубокой криогенной обработки на микроструктуру и механические свойства инструментальной стали SLD Magic (Cr8Mo2) и проанализирована взаимосвязь между микроструктурой и свойствами. После высокотемпературного отжига и аустенитизации проводили криогенную обработку стали Cr8Mo2 при –145 и –196 °C в течение различного времени выдержки: 12, 24, 36 и 48 ч. После криогенной обработки образцы стали каждой группы с разным временем выдержки подвергали отпуску при 200 и 520 °C в течение 1 ч. Изучена микроструктура и фазовый состав, измерена микротвердость. Выполнены испытания на абразивный износ и ударную вязкость стали в различных состояниях.
- 17 May 2026
- Published by Folium Publishing Company in Металловедение и термическая обработка металлов
- No. 5,p. 20
Open AccessEffect of cryogenic treatment on the properties of high molybdenum alloy steel
Исследовано влияние глубокой криогенной обработки на микроструктуру и механические свойства инструментальной стали SLD Magic (Cr8Mo2) и проанализирована взаимосвязь между микроструктурой и свойствами. После высокотемпературного отжига и аустенитизации проводили криогенную обработку стали Cr8Mo2 при –145 и –196 °C в течение различного времени выдержки: 12, 24, 36 и 48 ч. После криогенной обработки образцы стали каждой группы с разным временем выдержки подвергали отпуску при 200 и 520 °C в течение 1 ч. Изучена микроструктура и фазовый состав, измерена микротвердость. Выполнены испытания на абразивный износ и ударную вязкость стали в различных состояниях.
- Open Access
- 21 October 2025
- Published by American Chemical Society (ACS) in ACS Omega
- Vol. 10 (43) , 50914-50927
Experimental Analysis of Micro-Tribomechanical and Thermal Oxidation Properties of Ceramic-Reinforced Copper-Graphite Composites
Using the powder metallurgy process, this study focused on the impact of varying concentrations of SiC and graphite additions on microstructural, tribomechanical, and thermophysical properties. The resulting composites had a high relative density (>90%). The reinforcement particles exhibited a homogeneous distribution in the copper matrix. No compound developed between the reinforcing and copper phases. There was good interfacial bonding between the graphite and SiC structures. The composites’ overall structural hardness increased by 1.04 to 1.25 times. From 1.13 to 1.40 times, the empirical elasticity modulus increased. With SiC and graphite reinforcement, wear resistance was increased 10-fold to 12-fold for the wear tests. Lean graphite reduced friction by around 2.4 times. The samples that were chosen based on their tribomechanical characteristics underwent oxidation testing. The application of graphite and SiC together resulted in a mere 2.5 times improvement in oxidation resistance, while bare SiC reinforcement enhanced it by almost 30 times compared to pure copper. Lean graphite and graphite added to the structure in combination with SiC had no discernible impact on oxidation resistance. For Cu matrix composites, the operating temperature was critical. Graphite-SiC reinforced samples demonstrated superior properties at temperatures below 300 °C, while lean SiC reinforced samples had superior tribomechanical properties at temperatures over 300 °C.
- 21 October 2025
- Published by American Chemical Society (ACS) in ACS Omega
- Vol. 10 (43) , 50914-50927
Open AccessExperimental Analysis of Micro-Tribomechanical and Thermal Oxidation Properties of Ceramic-Reinforced Copper-Graphite Composites
Using the powder metallurgy process, this study focused on the impact of varying concentrations of SiC and graphite additions on microstructural, tribomechanical, and thermophysical properties. The resulting composites had a high relative density (>90%). The reinforcement particles exhibited a homogeneous distribution in the copper matrix. No compound developed between the reinforcing and copper phases. There was good interfacial bonding between the graphite and SiC structures. The composites’ overall structural hardness increased by 1.04 to 1.25 times. From 1.13 to 1.40 times, the empirical elasticity modulus increased. With SiC and graphite reinforcement, wear resistance was increased 10-fold to 12-fold for the wear tests. Lean graphite reduced friction by around 2.4 times. The samples that were chosen based on their tribomechanical characteristics underwent oxidation testing. The application of graphite and SiC together resulted in a mere 2.5 times improvement in oxidation resistance, while bare SiC reinforcement enhanced it by almost 30 times compared to pure copper. Lean graphite and graphite added to the structure in combination with SiC had no discernible impact on oxidation resistance. For Cu matrix composites, the operating temperature was critical. Graphite-SiC reinforced samples demonstrated superior properties at temperatures below 300 °C, while lean SiC reinforced samples had superior tribomechanical properties at temperatures over 300 °C.
- Open Access
- 26 June 2025
- Published by Springer Nature in Metals and Materials International
- Vol. 32 (1) , 230-250
Wear and Corrosion Behaviour of TiO2/Graphite Hybrid Reinforced Copper-Based Composites
This study focused on the fabrication and characterisation of TiO 2 /Graphite reinforced Cu-based composite produced by powder metallurgy. The effects of varying amounts of TiO 2 combined with 2% (w/w) graphite on the wear and corrosion behavior of stoichiometric copper (Cu) were investigated using various characterization techniques. The phase analysis revealed that Cu was the main phase. At low doping ratios, graphite peaks were found in trace amounts, while rutile phases of TiO 2 were detected. The microstructure and phase properties of the produced matrix and fracture surfaces were examined by scanning electron microscopy. As a result of the measurements made with the Vickers hardness tester, it was observed that the TiO 2 additive improved the hardness of the composites. Corrosion tests in 3.5 wt% NaCl solution showed that the addition of TiO 2 /Graphite to copper shifted the corrosion potential in the anodic (more noble) direction, while graphite alone shifted it in the cathodic (less noble) direction. However, graphite-reinforced Cu composites exhibited a better protective oxide film than those TiO 2 /Graphite reinforced Cu-based composite, attributed to the uniform distribution of graphite throughout the material. Although TiO 2 or TiO 2 /Graphite with graphite improved the corrosion potential, the corrosion current density was higher than that of unreinforced Cu due to the formation of micro-galvanic cells within the composite. Additionally, the high amount of TiO 2 added positively influenced the corrosion resistance. Using graphite's ability to make the composite self-lubricate when used with metals or ceramics, adding graphite to TiO₂ particles at all volume ratios significantly increased the wear resistance of the composite. Graphical Abstract
- 26 June 2025
- Published by Springer Nature in Metals and Materials International
- Vol. 32 (1) , 230-250
Open AccessWear and Corrosion Behaviour of TiO2/Graphite Hybrid Reinforced Copper-Based Composites
This study focused on the fabrication and characterisation of TiO 2 /Graphite reinforced Cu-based composite produced by powder metallurgy. The effects of varying amounts of TiO 2 combined with 2% (w/w) graphite on the wear and corrosion behavior of stoichiometric copper (Cu) were investigated using various characterization techniques. The phase analysis revealed that Cu was the main phase. At low doping ratios, graphite peaks were found in trace amounts, while rutile phases of TiO 2 were detected. The microstructure and phase properties of the produced matrix and fracture surfaces were examined by scanning electron microscopy. As a result of the measurements made with the Vickers hardness tester, it was observed that the TiO 2 additive improved the hardness of the composites. Corrosion tests in 3.5 wt% NaCl solution showed that the addition of TiO 2 /Graphite to copper shifted the corrosion potential in the anodic (more noble) direction, while graphite alone shifted it in the cathodic (less noble) direction. However, graphite-reinforced Cu composites exhibited a better protective oxide film than those TiO 2 /Graphite reinforced Cu-based composite, attributed to the uniform distribution of graphite throughout the material. Although TiO 2 or TiO 2 /Graphite with graphite improved the corrosion potential, the corrosion current density was higher than that of unreinforced Cu due to the formation of micro-galvanic cells within the composite. Additionally, the high amount of TiO 2 added positively influenced the corrosion resistance. Using graphite's ability to make the composite self-lubricate when used with metals or ceramics, adding graphite to TiO₂ particles at all volume ratios significantly increased the wear resistance of the composite. Graphical Abstract
- Open Access
- 1 January 2025
- Published by Afyon Kocatepe Universitesi Fen Ve Muhendislik Bilimleri Dergisi in Afyon Kocatepe University Journal of Sciences and Engineering
- Vol. 25 (2) , 423-432
Improving the mechanical and wear performance of AISI D2 steel with a cryogenic treatment
This research investigated the effect of cryogenic treatment on the notch impact strength, wear behaviour, microstructure, and hardness of AISI D2 steels. The study aimed to determine the impact of chemical composition and cryogenic treatment process on the material's mechanical properties. The samples prepared in the research were subjected to cryogenic treatment four times (12-48 hours) at -145°C and -196°C after heat treatment to achieve the desired mechanical improvement. Afterward, the specimens were tempered for an hour at two different temperatures, 200°C and 520°C. After cryogenic treatment, microhardness, microstructural investigations, wear, and notch impact tests were conducted and compared with the untreated material. Under optimum conditions, the cryogenic treatment caused a maximum increase of 4% in the microhardness of AISI D2 steels. After notch impact tests, the fracture energy of the material decreased at different rates in all groups except for the tempered sample with a holding time of 12 hours. Following cryogenic treatment at -196°C for 12 hours and then tempering at 520°C for 1 hour, the wear resistance of specimen D11 increased by up to 88%.
- 1 January 2025
- Published by Afyon Kocatepe Universitesi Fen Ve Muhendislik Bilimleri Dergisi in Afyon Kocatepe University Journal of Sciences and Engineering
- Vol. 25 (2) , 423-432
Open AccessImproving the mechanical and wear performance of AISI D2 steel with a cryogenic treatment
This research investigated the effect of cryogenic treatment on the notch impact strength, wear behaviour, microstructure, and hardness of AISI D2 steels. The study aimed to determine the impact of chemical composition and cryogenic treatment process on the material's mechanical properties. The samples prepared in the research were subjected to cryogenic treatment four times (12-48 hours) at -145°C and -196°C after heat treatment to achieve the desired mechanical improvement. Afterward, the specimens were tempered for an hour at two different temperatures, 200°C and 520°C. After cryogenic treatment, microhardness, microstructural investigations, wear, and notch impact tests were conducted and compared with the untreated material. Under optimum conditions, the cryogenic treatment caused a maximum increase of 4% in the microhardness of AISI D2 steels. After notch impact tests, the fracture energy of the material decreased at different rates in all groups except for the tempered sample with a holding time of 12 hours. Following cryogenic treatment at -196°C for 12 hours and then tempering at 520°C for 1 hour, the wear resistance of specimen D11 increased by up to 88%.
- Open Access
- 1 January 2025
- Published by National Library of Serbia in Science of Sintering
- Vol. 57 (1) , 1-15
Synthesis of Y2O3 and graphite-added copper-based hybrid composites by powder metallurgy: Mechanical properties and tribological behavior
In the presented study, Y2O3 and graphite-reinforced Cu matrix hybrid composite materials were prepared using the powder metallurgy method. The aim is to compare the microstructure, density, hardness, and wear behavior of composites with different yttria contents (5, 10, and 15 wt%) and graphite (2 wt%) reinforcements. An increase in the Y2O3 ratio, along with the addition of graphite, resulted in an observed increase in the hardness values of the composites. Additionally, it was observed that Y2O3 and graphite are homogeneously distributed in the copper matrix in the SEM-EDX spectra. Upon examining the microstructures of the composites, it was determined that with the increase in yttrium oxide content, partially yttrium oxide agglomerations formed in some regions. The addition of Y2O3 resulted in a copper sample that is 1.34 times harder than pure copper. Addition of Y2O3 -graphite, samples with 3.301?22.3 % higher wear resistance were obtained.
- 1 January 2025
- Published by National Library of Serbia in Science of Sintering
- Vol. 57 (1) , 1-15
Open AccessSynthesis of Y2O3 and graphite-added copper-based hybrid composites by powder metallurgy: Mechanical properties and tribological behavior
In the presented study, Y2O3 and graphite-reinforced Cu matrix hybrid composite materials were prepared using the powder metallurgy method. The aim is to compare the microstructure, density, hardness, and wear behavior of composites with different yttria contents (5, 10, and 15 wt%) and graphite (2 wt%) reinforcements. An increase in the Y2O3 ratio, along with the addition of graphite, resulted in an observed increase in the hardness values of the composites. Additionally, it was observed that Y2O3 and graphite are homogeneously distributed in the copper matrix in the SEM-EDX spectra. Upon examining the microstructures of the composites, it was determined that with the increase in yttrium oxide content, partially yttrium oxide agglomerations formed in some regions. The addition of Y2O3 resulted in a copper sample that is 1.34 times harder than pure copper. Addition of Y2O3 -graphite, samples with 3.301?22.3 % higher wear resistance were obtained.
- 29 March 2021
- Published by Springer Nature in Journal of the Australian Ceramic Society
- Vol. 57 (3) , 1003
Correction: Fabrication and characterization of Al2O3-TiB2 nanocomposite powder by mechanochemical processing
- 29 March 2021
- Published by Springer Nature in Journal of the Australian Ceramic Society
- Vol. 57 (3) , 1003
Correction: Fabrication and characterization of Al2O3-TiB2 nanocomposite powder by mechanochemical processing
- 17 February 2021
- Published by Springer Nature in Journal of the Australian Ceramic Society
- Vol. 57 (3) , 731-741
Fabrication and characterization of Al2O3-TiB2 nanocomposite powder by mechanochemical processing
- 17 February 2021
- Published by Springer Nature in Journal of the Australian Ceramic Society
- Vol. 57 (3) , 731-741
Fabrication and characterization of Al2O3-TiB2 nanocomposite powder by mechanochemical processing
- 14 May 2020
- Published by Springer Nature in Journal of the Australian Ceramic Society
- Vol. 56 (4) , 1271-1281
Mechanochemical-assisted synthesis and characterization of Al2O3/B4C ceramics
- 14 May 2020
- Published by Springer Nature in Journal of the Australian Ceramic Society
- Vol. 56 (4) , 1271-1281
Mechanochemical-assisted synthesis and characterization of Al2O3/B4C ceramics