Mitsuru Ohtake
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Mitsuru Ohtake has a total of 46 co-authors. Here are the top co-authors by number of shared publications:
- Masaaki Futamoto
Faculty of Science and Engineering, Chuo University, Tokyo, Japan
8 shared publications Fumiyoshi Kirino
5 shared publicationsMasaaki Futamoto
Yokohama National University
5 shared publicationsNobuyuki Inaba
5 shared publications- Yuta Nakamura
Yokohama National University
5 shared publications - Kosuke Imamura
Yokohama National University
4 shared publications
Latest Publications
- 13 November 2026
- Published by IOP Publishing in Japanese Journal of Applied Physics
- Vol. 65 (21) , 21SP11
Crystal-axis dependence of nonreciprocal spin-wave transmission in asymmetric Fe/MgO/NiFe trilayers
We investigated the crystal-axis dependence of nonreciprocal spin-wave transmission in asymmetric Fe/MgO/NiFe trilayer waveguides. Spin-wave transmission was measured in the Damon–Eshbach geometry for two configurations: the easy-axis configuration, with the magnetic field applied along Fe[100], and the hard-axis configuration, with the field along Fe[110]. The transmission spectra exhibited propagation-direction-dependent differences in both amplitude and frequency. In particular, the directional amplitude difference of one experimentally observed branch reversed its polarity upon reversal of the external magnetic field in both configurations. Micromagnetic simulations showed propagation-direction-dependent localization of the dynamic magnetization and revealed that the spectral separation between the Fe-like and NiFe-like branches depended on the orientation relative to the Fe crystal axes. These results demonstrate the important role of the Fe crystal axes in nonreciprocal spin-wave transmission in asymmetric magnetic multilayers.
- 13 November 2026
- Published by IOP Publishing in Japanese Journal of Applied Physics
- Vol. 65 (21) , 21SP11
Crystal-axis dependence of nonreciprocal spin-wave transmission in asymmetric Fe/MgO/NiFe trilayers
We investigated the crystal-axis dependence of nonreciprocal spin-wave transmission in asymmetric Fe/MgO/NiFe trilayer waveguides. Spin-wave transmission was measured in the Damon–Eshbach geometry for two configurations: the easy-axis configuration, with the magnetic field applied along Fe[100], and the hard-axis configuration, with the field along Fe[110]. The transmission spectra exhibited propagation-direction-dependent differences in both amplitude and frequency. In particular, the directional amplitude difference of one experimentally observed branch reversed its polarity upon reversal of the external magnetic field in both configurations. Micromagnetic simulations showed propagation-direction-dependent localization of the dynamic magnetization and revealed that the spectral separation between the Fe-like and NiFe-like branches depended on the orientation relative to the Fe crystal axes. These results demonstrate the important role of the Fe crystal axes in nonreciprocal spin-wave transmission in asymmetric magnetic multilayers.
- 1 October 2026
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Magnetics
- Vol. 62 (10) , 2002405
Effect of Annealing on the Microstructure and the Magnetostrictive Property of Nanogranular Fe-B-N Alloy Thin Film
- 1 October 2026
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Magnetics
- Vol. 62 (10) , 2002405
Effect of Annealing on the Microstructure and the Magnetostrictive Property of Nanogranular Fe-B-N Alloy Thin Film
- Open Access
- 25 March 2025
- Published by Institute of Electronics, Information and Communications Engineers (IEICE) in IEICE Electronics Express
- Vol. 22 (6) , 20250031
Tuning magnetic properties by microstructure control of nanocrystalline thin films for compact vibration energy harvesters
The vibration energy harvesting properties of Fe-based nanocrystalline soft magnetostrictive material (Fe-Si-B-P-Cu-C) thin films were systematically investigated. Thin films were deposited using rotational sputtering and subsequently annealed. Nanocrystallization occurred in the samples annealed at 100-110% of the crystallization temperature. This nanocrystallization process enhanced soft magnetic properties, however, decrease saturation magnetostriction reflecting the influence of the negative magnetostrictive α-Fe phase. The film annealed at 105% of the crystallization temperature exhibited the highest vibration power generation performance. This superior performance was attributed to the combination of enhanced soft magnetic properties, high saturation magnetic flux density, and a relatively large saturation magnetostriction.
- 25 March 2025
- Published by Institute of Electronics, Information and Communications Engineers (IEICE) in IEICE Electronics Express
- Vol. 22 (6) , 20250031
Open AccessTuning magnetic properties by microstructure control of nanocrystalline thin films for compact vibration energy harvesters
The vibration energy harvesting properties of Fe-based nanocrystalline soft magnetostrictive material (Fe-Si-B-P-Cu-C) thin films were systematically investigated. Thin films were deposited using rotational sputtering and subsequently annealed. Nanocrystallization occurred in the samples annealed at 100-110% of the crystallization temperature. This nanocrystallization process enhanced soft magnetic properties, however, decrease saturation magnetostriction reflecting the influence of the negative magnetostrictive α-Fe phase. The film annealed at 105% of the crystallization temperature exhibited the highest vibration power generation performance. This superior performance was attributed to the combination of enhanced soft magnetic properties, high saturation magnetic flux density, and a relatively large saturation magnetostriction.
- 21 March 2025
- Published by Springer Nature
- p. 1-28
Magnetostriction
- 17 March 2025
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Magnetics
- Vol. 61 (9) , 1-5
Influences of Magnetic Properties of Beam Electroplated With 3d Ferromagnetic Transition Metal Film on the Output Characteristics in Magnetostrictive and Perpendicular Magnetic Field-Assisted Vibration Powered Generators
Cu base plates are electroplated with Fe100-xCox and Fe100-yNiy ($x =0$ –95 and$y =1$ –100 at.%) films of about$30~\mu $ m thickness. They are applied to beam materials in electromagnetic vibration powered generators with inverse magnetostrictive and perpendicular magnetic field-assisted types. The influences of magnetic properties of coated film on the output characteristic are investigated. The Fe100-xCox beams with around$x =30$ –55 show high saturation magnetizations of about 1.650 kemu/cm3, moderately low coercivities of less than 10 Oe, and large saturation magnetostrictions of more than$+ 30\times 10^{-6}$ . However, high output characteristics are not obtained in both types of generations. The reason is that the Fe100-xCox beams exhibit only less than 20% of their potentials due to that their magnetocrystalline anisotropies are not so low. On the other hand, very low coercivities of less than 1 Oe are recognized for the Fe100-yNiy beams with around$y =35$ –70. As a result, the Fe100-yNiy films show high output voltages of 5–7 V and powers of 0.5–1.1 mW, which correspond to more than 60% of their potentials. The present study has shown that low magnetocrystalline anisotropy is essential in enhancing the output characteristic for both types of generators.- 17 March 2025
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Magnetics
- Vol. 61 (9) , 1-5
Influences of Magnetic Properties of Beam Electroplated With 3d Ferromagnetic Transition Metal Film on the Output Characteristics in Magnetostrictive and Perpendicular Magnetic Field-Assisted Vibration Powered Generators
Cu base plates are electroplated with Fe100-xCox and Fe100-yNiy ($x =0$ –95 and$y =1$ –100 at.%) films of about$30~\mu $ m thickness. They are applied to beam materials in electromagnetic vibration powered generators with inverse magnetostrictive and perpendicular magnetic field-assisted types. The influences of magnetic properties of coated film on the output characteristic are investigated. The Fe100-xCox beams with around$x =30$ –55 show high saturation magnetizations of about 1.650 kemu/cm3, moderately low coercivities of less than 10 Oe, and large saturation magnetostrictions of more than$+ 30\times 10^{-6}$ . However, high output characteristics are not obtained in both types of generations. The reason is that the Fe100-xCox beams exhibit only less than 20% of their potentials due to that their magnetocrystalline anisotropies are not so low. On the other hand, very low coercivities of less than 1 Oe are recognized for the Fe100-yNiy beams with around$y =35$ –70. As a result, the Fe100-yNiy films show high output voltages of 5–7 V and powers of 0.5–1.1 mW, which correspond to more than 60% of their potentials. The present study has shown that low magnetocrystalline anisotropy is essential in enhancing the output characteristic for both types of generators.- Open Access
- 1 March 2025
- Published by AIP Publishing in AIP Advances
- Vol. 15 (3)
Relationship between chemical bonding state and magnetostriction in Fe–Al–N alloy system
N atoms are added to Fe100−xAlx (x=10.0, 20.0, and 30.0 at. %) alloys to form preferential Al–N bonding in crystal lattice and then to reduce their magnetostriction. Single-crystal (Fe100−xAlx)1−0.01yNy(001) film samples (y ≤ 11.0 at. %) are employed to investigate the fundamental magnetic properties. bcc-based disordered A2 phase is formed for x = 10.0 and 20.0, whereas ordered B2 phase is involved for x = 30.0. As a result, the N content dependences of magnetocrystalline anisotropy and magnetostriction for x = 30.0 are different from those for x = 10.0 and 20.0. Low magnetocrystalline anisotropy constants, K1, on the order of 105 erg/cm3 are obtained for x = 10.0 and 20.0, even when N atoms are added. The saturation magnetostrictive coefficients along [100] direction, λ100, for x = 10.0 and 20.0 drastically decrease from +33.7 × 10−6 to +15.5 × 10−6 and from +64.9 × 10−6 to +16.4 × 10−6 with increasing the N content, respectively. The reduction is possibly attributed to bonding of N atoms placed at octahedral interstitial sites with Al atoms located at substitutional sites along 〈100〉 directions. On the other hand, the magnetostrictive coefficients along [111], λ111, for x = 10.0 and 20.0 do not almost vary depending on the N content in ranges between −18.4 × 10−6 and −17.0 × 10−6 and between −16.9 × 10−6 and −6.5 × 10−6, respectively. The magnetostrictive values of randomly-oriented polycrystalline materials, λrandom, are also estimated by using the relation of λrandom = (2/5)λ100 + (3/5)λ111. Low λrandom values on the order of 10−6 are achieved in ranges of y ≥ 0 for x = 10.0 and y ≥ 3.2 for x = 20.0. The present study has shown that reducing in magnetostriction of Fe–Al alloy to the order of λrandom = 10−6 while keeping low magnetocrystalline anisotropy is possible by N atom addition and control of its chemical bonding state.
- 1 March 2025
- Published by AIP Publishing in AIP Advances
- Vol. 15 (3)
Open AccessRelationship between chemical bonding state and magnetostriction in Fe–Al–N alloy system
N atoms are added to Fe100−xAlx (x=10.0, 20.0, and 30.0 at. %) alloys to form preferential Al–N bonding in crystal lattice and then to reduce their magnetostriction. Single-crystal (Fe100−xAlx)1−0.01yNy(001) film samples (y ≤ 11.0 at. %) are employed to investigate the fundamental magnetic properties. bcc-based disordered A2 phase is formed for x = 10.0 and 20.0, whereas ordered B2 phase is involved for x = 30.0. As a result, the N content dependences of magnetocrystalline anisotropy and magnetostriction for x = 30.0 are different from those for x = 10.0 and 20.0. Low magnetocrystalline anisotropy constants, K1, on the order of 105 erg/cm3 are obtained for x = 10.0 and 20.0, even when N atoms are added. The saturation magnetostrictive coefficients along [100] direction, λ100, for x = 10.0 and 20.0 drastically decrease from +33.7 × 10−6 to +15.5 × 10−6 and from +64.9 × 10−6 to +16.4 × 10−6 with increasing the N content, respectively. The reduction is possibly attributed to bonding of N atoms placed at octahedral interstitial sites with Al atoms located at substitutional sites along 〈100〉 directions. On the other hand, the magnetostrictive coefficients along [111], λ111, for x = 10.0 and 20.0 do not almost vary depending on the N content in ranges between −18.4 × 10−6 and −17.0 × 10−6 and between −16.9 × 10−6 and −6.5 × 10−6, respectively. The magnetostrictive values of randomly-oriented polycrystalline materials, λrandom, are also estimated by using the relation of λrandom = (2/5)λ100 + (3/5)λ111. Low λrandom values on the order of 10−6 are achieved in ranges of y ≥ 0 for x = 10.0 and y ≥ 3.2 for x = 20.0. The present study has shown that reducing in magnetostriction of Fe–Al alloy to the order of λrandom = 10−6 while keeping low magnetocrystalline anisotropy is possible by N atom addition and control of its chemical bonding state.
- 26 July 2023
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Magnetics
- Vol. 59 (11) , 1-5
Formulation of Electric Voltage for Vibration Generation Device Using Magnetostriction Material
A study on vibration power generation using magnetostriction material is carried out in both experimental and theoretical sides, and the power generation voltage is formulated using an analytical formula. The damping constant is obtained from experiments, and the bending at free end is described by the equation of motion of forced oscillation using the damping constant. Power generation is achieved through the variation in the longitudinal magnetization of cantilever beam. The magnetization curve where the magnetization is saturated at tensile stress and is approaching to zero at compressive stress is described by using an arctangent function. By assuming that magnetoelastic energy caused by stress is equivalent to magnetic energy, the energy can be converted into an effective magnetic field by using the function. The operating point on magnetization curve is set by the shape magnetic anisotropy of cantilever beam, and the magnetization variation due to the effective magnetic field is calculated around the operating point. The calculated variation in magnetization is differentiated by time to obtain the generated voltage. The generated voltage calculated by using the formulation well explains the experimental results of the dependence of generated voltage on bias magnetic field, and the characteristics of waveform are similar to the experiments.
- 26 July 2023
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Magnetics
- Vol. 59 (11) , 1-5
Formulation of Electric Voltage for Vibration Generation Device Using Magnetostriction Material
A study on vibration power generation using magnetostriction material is carried out in both experimental and theoretical sides, and the power generation voltage is formulated using an analytical formula. The damping constant is obtained from experiments, and the bending at free end is described by the equation of motion of forced oscillation using the damping constant. Power generation is achieved through the variation in the longitudinal magnetization of cantilever beam. The magnetization curve where the magnetization is saturated at tensile stress and is approaching to zero at compressive stress is described by using an arctangent function. By assuming that magnetoelastic energy caused by stress is equivalent to magnetic energy, the energy can be converted into an effective magnetic field by using the function. The operating point on magnetization curve is set by the shape magnetic anisotropy of cantilever beam, and the magnetization variation due to the effective magnetic field is calculated around the operating point. The calculated variation in magnetization is differentiated by time to obtain the generated voltage. The generated voltage calculated by using the formulation well explains the experimental results of the dependence of generated voltage on bias magnetic field, and the characteristics of waveform are similar to the experiments.
- 30 June 2023
- Published by Elsevier in Journal of Magnetism and Magnetic Materials
- Vol. 585
Large magnetostriction in γʹ-Fe4N single-crystal thin film
- 30 June 2023
- Published by Elsevier in Journal of Magnetism and Magnetic Materials
- Vol. 585
Large magnetostriction in γʹ-Fe4N single-crystal thin film
- 19 June 2023
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Magnetics
- Vol. 59 (11) , 1-5
Anisotropic FMR Peak Widths in Fe-Co Single Crystal Thin Films
We investigated Q-band ( f =35 GHz) and X-band ( f =9 GHz) ferromagnetic resonance (FMR) spectra of Fe 1-x Co x single crystal thin films ( x Fe-Co film plane in terms of magnetostriction. The FMR peak width Δ H(f) and the magnetostriction λ had the maximum and minimum values at the 〈100〉 and the 〈110〉 directions of the specimens. The periodic variations of Δ H(f) were due to the anisotropic variations of the frequency independent part Δ H 0 in Δ H(f) . The linear relationship existed between Δ H 0 and λ.
- 19 June 2023
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Magnetics
- Vol. 59 (11) , 1-5
Anisotropic FMR Peak Widths in Fe-Co Single Crystal Thin Films
We investigated Q-band ( f =35 GHz) and X-band ( f =9 GHz) ferromagnetic resonance (FMR) spectra of Fe 1-x Co x single crystal thin films ( x Fe-Co film plane in terms of magnetostriction. The FMR peak width Δ H(f) and the magnetostriction λ had the maximum and minimum values at the 〈100〉 and the 〈110〉 directions of the specimens. The periodic variations of Δ H(f) were due to the anisotropic variations of the frequency independent part Δ H 0 in Δ H(f) . The linear relationship existed between Δ H 0 and λ.