Yun‐Qiao Wang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Yun‐Qiao Wang has a total of 35 co-authors. Here are the top co-authors by number of shared publications:
D.T. Zhang
4 shared publicationsM. Yue
4 shared publicationsD. Wu
3 shared publicationsH.G. Zhang
3 shared publicationsMing Yue
3 shared publicationsW.Q. Liu
3 shared publications
Latest Publications
- Open Access
- 1 December 2019
- Published by AIP Publishing in AIP Advances
- Vol. 9 (12) , 125142
Effect of ingot cooling rate on Cu distribution and magnetic properties of Sm(CobalFe0.28Cu0.07Zr0.03)7.6 magnets
The Sm(CobalFe0.28Cu0.07Zr0.03)7.6 magnets were made by a casting process with two different cooling rates. X-ray diffraction analysis shows that the main phase of the two as-cast alloys consist of 1:5, 1:7, and 2:17 (hexagonal) phase. While a few of rhombohedral 2:17 phases appear in the ingots with the lower cooling rate. The electron probe micro-analysis and corresponding wavelength dispersive x-ray results indicate that a higher cooling rate of the as-cast alloy is helpful to the uniformity of Cu element distribution in the ingots and magnets, especially for suppressing the formation of 2:17 R phase in ingots. The coercivity and squareness of magnet prepared from ingot with higher cooling rate increase by 72 and 48 percentage, respectively. The microstructure observation shows that some cell boundaries are destroyed in the magnet made by lower cooling rate, while the cell boundaries are well developed in the magnet made by higher cooling rate.
- 1 December 2019
- Published by AIP Publishing in AIP Advances
- Vol. 9 (12) , 125142
Open AccessEffect of ingot cooling rate on Cu distribution and magnetic properties of Sm(CobalFe0.28Cu0.07Zr0.03)7.6 magnets
The Sm(CobalFe0.28Cu0.07Zr0.03)7.6 magnets were made by a casting process with two different cooling rates. X-ray diffraction analysis shows that the main phase of the two as-cast alloys consist of 1:5, 1:7, and 2:17 (hexagonal) phase. While a few of rhombohedral 2:17 phases appear in the ingots with the lower cooling rate. The electron probe micro-analysis and corresponding wavelength dispersive x-ray results indicate that a higher cooling rate of the as-cast alloy is helpful to the uniformity of Cu element distribution in the ingots and magnets, especially for suppressing the formation of 2:17 R phase in ingots. The coercivity and squareness of magnet prepared from ingot with higher cooling rate increase by 72 and 48 percentage, respectively. The microstructure observation shows that some cell boundaries are destroyed in the magnet made by lower cooling rate, while the cell boundaries are well developed in the magnet made by higher cooling rate.
- 30 April 2019
- Published by Wiley in Rare Metals
- Vol. 39 (3) , 250-255
In‐situ observation of magnetization reversal process of Sm(Co,Cu,Fe,Zr) z magnets with different Fe contents
Sm(Co,Cu,Fe,Zr) z magnets have drawn much attention for high‐temperature applications due to their high Curie temperature, strong corrosion resistance and thermal stability. The effect of increasing Fe content on the distribution of elements and squareness ( S r ) of demagnetization curves were investigated for two kinds of magnets with different nominal compositions of Sm(Co bal Fe 0.15 Cu 0.07 Zr 0.03 ) 7.8 and Sm(Co bal Fe 0.28 Cu 0.07 Zr 0.03 ) 6.6 in this work. The magnetic properties of the magnets with higher Fe content fluctuate greatly after different solution treatments, indicating that they are more sensitive to the process temperature. The increase in Fe content can obviously enhance the cellular phase size. Meanwhile, inhomogeneous Cu distribution is observed in the Sm(Co bal Fe 0.28 Cu 0.07 Zr 0.03 ) 6.6 magnet, resulting in the different cellular structures and corresponding magnetic domain patterns in different regions in the inner grains. Furthermore, the lower Cu content regions are responsible for the wider magnetic domain, which have weaker resistance to applied magnetic field. As a result, S r of demagnetization curve decreases with the increase in Fe content due to the inhomogeneous Cu distribution, which was confirmed by in‐situ observation of electron probe micro‐analyzer (EPMA) and magneto‐optical Kerr optical microscope (MOKE).
- 30 April 2019
- Published by Wiley in Rare Metals
- Vol. 39 (3) , 250-255
In‐situ observation of magnetization reversal process of Sm(Co,Cu,Fe,Zr) z magnets with different Fe contents
Sm(Co,Cu,Fe,Zr) z magnets have drawn much attention for high‐temperature applications due to their high Curie temperature, strong corrosion resistance and thermal stability. The effect of increasing Fe content on the distribution of elements and squareness ( S r ) of demagnetization curves were investigated for two kinds of magnets with different nominal compositions of Sm(Co bal Fe 0.15 Cu 0.07 Zr 0.03 ) 7.8 and Sm(Co bal Fe 0.28 Cu 0.07 Zr 0.03 ) 6.6 in this work. The magnetic properties of the magnets with higher Fe content fluctuate greatly after different solution treatments, indicating that they are more sensitive to the process temperature. The increase in Fe content can obviously enhance the cellular phase size. Meanwhile, inhomogeneous Cu distribution is observed in the Sm(Co bal Fe 0.28 Cu 0.07 Zr 0.03 ) 6.6 magnet, resulting in the different cellular structures and corresponding magnetic domain patterns in different regions in the inner grains. Furthermore, the lower Cu content regions are responsible for the wider magnetic domain, which have weaker resistance to applied magnetic field. As a result, S r of demagnetization curve decreases with the increase in Fe content due to the inhomogeneous Cu distribution, which was confirmed by in‐situ observation of electron probe micro‐analyzer (EPMA) and magneto‐optical Kerr optical microscope (MOKE).
- 1 March 2019
- Published by Elsevier in Journal of Magnetism and Magnetic Materials
- Vol. 474, 417-423
Correlation between Fe content and z value in Sm(CobalFexCu0.06Zr0.025)z permanent magnets
- 1 March 2019
- Published by Elsevier in Journal of Magnetism and Magnetic Materials
- Vol. 474, 417-423
Correlation between Fe content and z value in Sm(CobalFexCu0.06Zr0.025)z permanent magnets
- 1 February 2019
- Published by Elsevier in Acta Materialia
- Vol. 164, 196-206
Attractive-domain-wall-pinning controlled Sm-Co magnets overcome the coercivity-remanence trade-off
- 1 February 2019
- Published by Elsevier in Acta Materialia
- Vol. 164, 196-206
Attractive-domain-wall-pinning controlled Sm-Co magnets overcome the coercivity-remanence trade-off
- 1 April 2018
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 741, 495-500
Effect of Cu redistribution in grain boundary on magnetic properties of Sm(Co0.665Fe0.25Cu0.06Zr0.025)7 permanent magnets
- 1 April 2018
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 741, 495-500
Effect of Cu redistribution in grain boundary on magnetic properties of Sm(Co0.665Fe0.25Cu0.06Zr0.025)7 permanent magnets
- 1 March 2018
- Published by Elsevier in Scripta Materialia
- Vol. 146, 231-235
Microstructure modification induced giant coercivity enhancement in Sm(CoFeCuZr)z permanent magnets
- 1 March 2018
- Published by Elsevier in Scripta Materialia
- Vol. 146, 231-235
Microstructure modification induced giant coercivity enhancement in Sm(CoFeCuZr)z permanent magnets
- 1 November 2015
- Published by Elsevier in Journal of Magnetism and Magnetic Materials
- Vol. 393, 551-554
Effects of CE substitution on the microstructures and intrinsic magnetic properties of Nd–Fe–B alloy
- 1 November 2015
- Published by Elsevier in Journal of Magnetism and Magnetic Materials
- Vol. 393, 551-554
Effects of CE substitution on the microstructures and intrinsic magnetic properties of Nd–Fe–B alloy
- 1 September 2015
- Published by Elsevier in Journal of Rare Earths
- Vol. 33 (9) , 961-964
Effects of lanthanum substitution on microstructures and intrinsic magnetic properties of Nd-Fe-B alloy
- 1 September 2015
- Published by Elsevier in Journal of Rare Earths
- Vol. 33 (9) , 961-964
Effects of lanthanum substitution on microstructures and intrinsic magnetic properties of Nd-Fe-B alloy