  • Gamma-Activation Analysis of Selenium at the Microtron-ST Electron Accelerator

    by V. I. Tovtin, V. N. Kolokoltsev, N. N. Dogadkin, E. E. Starostin

    Gamma activation analysis of Se was performed during its irradiation with bremsstrahlung gamma radiation at the Microtron-ST cyclic electron accelerator (E = 21 MeV). Irradiation was carried out at room temperature for 1 h and gamma quanta intensity of ~5 × 1013 γ/s. Se samples in the form of granules (balls) weighing 5–10 mg and microparticles (powder) were studied. Microparticle samples were suspended in distilled water in a plastic capsule. After irradiation of samples with gamma quanta, the induced radioactivity was measured on an SBS-75 gamma spectrometer with a semiconductor detector. Energy spectra of selenium radionuclides were obtained. Analysis of spectra of radionuclides showed the absence of impurity chemical elements in the selenium samples.

  • Deposition of thin refractory-metal-films onto glasses through diaphragms at plasma focus facility

    by V. N. Kolokoltsev, V. Ya. Nikulin, P. V. Silin, I. V. Borovitskaya, E. N. Peregudova, A. I. Gaidar, L. I. Kobeleva, A. M. Mezrin, A. A. Eriskin

    The results of experiments are presented on the deposition onto silicate glasses of thin refractorymetal- films: molybdenum, tantalum and tungsten. The technique used for manufacturing films was based on the deposition of metal-containing plasma formed when exposing the surface of foils made of refractory metals to high-power plasma and ion pulses. For generation of such pulses, the facility of plasma focus type was used, which makes it possible to obtain ion beams and plasma flows with the energy flux density in the range of 1010—1012 W/cm2. The most intense central part of the ion-plasma flow was separated using metal diaphragms with aperture diameters of 2.5, 3.5, and 4.5 mm. Metal Mo, Ta and W films with dimensions of ∅ 3—5 mm were obtained on the surfaces of glasses. Metal films are characterized by good adhesion, since they coalesce with the glass surface. It was discovered that the planarity of films becomes violated due to the drift of molten metal particles under the glass surface. The relief of films is non-uniform, which can be explained by the presence of micrometer-sized metal particles in the plasma flow.

  • Deposition of Thin Refractory-Metal-Films onto Glasses through Diaphragms at Plasma Focus Facility

    by V. N. Kolokoltsev, V. Ya. Nikulin, P. V. Silin, I. V. Borovitskaya, E. N. Peregudova, A. I. Gaidar, L. I. Kobeleva, A. M. Mezrin, A. A. Eriskin

    The results of experiments are presented on the deposition onto silicate glasses of thin refractory-metal-films: molybdenum, tantalum and tungsten. The technique used for manufacturing films was based on the deposition of metal-containing plasma formed when exposing the surface of foils made of refractory metals to high-power plasma and ion pulses. For generation of such pulses, the facility of plasma focus type was used, which makes it possible to obtain ion beams and plasma flows with the energy flux density in the range of 1010–1012 W/cm2. The most intense central part of the ion-plasma flow was separated using metal di-aphragms with aperture diameters of 2.5, 3.5, and 4.5 mm. Metal Mo, Ta and W films with dimensions of ∅3–5 mm were obtained on the surfaces of glasses. Metal films are characterized by good adhesion, since they coalesce with the glass surface. It was discovered that the planarity of films becomes violated due to the drift of molten metal particles under the glass surface. The relief of films is non-uniform, which can be explained by the presence of micrometer-sized metal particles in the plasma flow.

  • Open Access

    Elemental Composition of Copper Films Deposited on the Surface of Metals Fe, V, and Ti at the Plasma Focus Facility

    by Aleksandr Eriskin, Aleksandr Kobzev, Vyacheslav Kolokoltsev, Georgy Sprygin, Pavel Silin, Valerii Nikulin, Alexei Mezrin, Elena Peregudova, Sergiy Lyubchyk, Alisa Tatarinova, et al.

    Thin Cu films with a thickness of ~0.5-2.5 mkm were obtained on the surface of Fe, V, and Ti metals using the Plasma Focus (PF) setup. The Cu film thickness was determined on an Ambios XP-200 profilometer. The distribution profiles of Cu, C, О2, N2 and H2 in initial metal samples: Fe, V, and Ti were studied by layer-by-layer analysis on a GDS 850A atomic emission spectrometer. It is shown that the distribution profile and the depth of occurrence of elements depend on the type of metal. Using the method of Rutherford Backscattering Spectrometry (RBS) of 4He+ ions, it was shown that for Cu atoms the depth of occurrence in Fe, V, and Ti, accordingly, is ~106, ~120, and ~160 nm. The depth of occurrence of C atoms in metals: Fe, V, and Ti is ~150, ~120, and ~200 nm, accordingly. From the data of layer-by-layer analysis on an atomic emission spectrometer in the initial samples of metals: Fe, V and Ti, a transition layer with a thickness of ~0.01, accordingly, was found; 0.5 and 1 mm. The presence of this layer is connected with the mechanical processing of metal samples, and the presence of a large number of admixtures in the thin layer of the metal. Thus, Cu atoms are located in the transition layer under the metal surface, which imparts adhesion and electrophysical properties of Cu films.

  • Production of Aqueous Colloidal Se Solution by Mechanical Dispersion

    by V. N. Kolokoltsev, G. E. Folmanis, M. A. Fedotov

    Owing to its antioxidant properties, selenium is an essential trace element for human life which enters the body mainly from foods of plant origin. To obtain selenium nanoparticles for the preparation of functional foods enriched in selenium, in this work, the method of mechanical dispersion was used. Colloidal solutions of selenium nanoparticles ranging in size from 20 to 100 nm were obtained by mechanical dispersion of selenium granules in distilled water using a vibrating machine of the Metapolan-2 type at a frequency of 100 Hz. The Se concentration in the solution was measured by means of atomic emission spectroscopy and reached from 2 to 10 mg/L. It has been established that the properties of colloidal selenium solutions prepared by mechanical dispersion largely depend on the material of the weighing bottle in which they are obtained. Selenium colloidal solutions obtained in plastic bottles have acidic properties, while solutions obtained in glass bottles are alkaline. Using the method of electron microscopy, it is shown that the evaporation of colloidal solutions leads to the formation of fractal structures.


  • Open Access

    Production of the thin carbon films using a Plasma Focus Installation

    by V N Kolokoltsev, I V Borovitskaya, S A Maslyaev, V F Degtyarev

    In the paper, the possibility of obtaining thin carbon (C) films on glass substrates using the Plasma focus installation is considered. The films were sprayed through a slit diaphragm made of graphite under the action of nitrogen plasma. The obtained films were inhomogeneous, which is due to the no uniform energy distribution in the plasma jet. The measured transmission spectra and temperature dependences of the surface electrical resistivity (in the temperature range 78-300K) indicate the cluster formation of films on glass substrates. At 300K, the resistance of the films with is from 105 to 107 Ohms.