Bartłomiej SZWED
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Bartłomiej SZWED has a total of 7 co-authors. Here are the top co-authors by number of shared publications:
- Marek Konieczny
Department of Metals Science and Materials Technologies, Kielce University of Technology, Kielce, Poland
3 shared publications - Hubert Danielewski
Laser Research Centre, Faculty of Mechatronics and Mechanical Engineering, Kielce University of Technology, Al. Tysiąclecia P.P. 7, 25-314 Kielce, Poland
2 shared publications - Piotr Kurp
Laser Research Centre, Faculty of Mechatronics and Mechanical Engineering, Kielce University of Technology, Al. Tysiąclecia P.P. 7, 25-314 Kielce, Poland
2 shared publications - Andrej Zrak
University of Zilina, Zilina, Slovakia
1 shared publication - Krzysztof Borkowski
Department of Automation and Robotics, Kielce University of Technology, 25-314 Kielce, Poland
1 shared publication - Oksana P. Gaponova
Department of Experimental Mechanics, Institute of Fundamental Technological Research Polish Academy of Sciences, Pawińskiego 5B, 02-106 Warsaw, Poland
1 shared publication
Latest Publications
- Open Access
- 6 April 2023
- Published by University of Zilina in Communications - Scientific letters of the University of Zilina
- Vol. 25 (2) , B110-B117
Discussion about Metal Expansion Joints Manufacturing Technology of Preventing Thermal Deformation Pipelines Intended for the Fluids Transport
In this paper, the authors discuss the method of deformations compensation (resulting from the impact of variable temperatures and pressure) in pipelines intended for fluids transport (liquids and gases). Classical methods of compensation thro...
- 6 April 2023
- Published by University of Zilina in Communications - Scientific letters of the University of Zilina
- Vol. 25 (2) , B110-B117
Open AccessDiscussion about Metal Expansion Joints Manufacturing Technology of Preventing Thermal Deformation Pipelines Intended for the Fluids Transport
In this paper, the authors discuss the method of deformations compensation (resulting from the impact of variable temperatures and pressure) in pipelines intended for fluids transport (liquids and gases). Classical methods of compensation thro...
- Open Access
- 1 January 2023
- Published by TANGER Ltd.
- Vol. 2023, 258-262
Technology and experimental results of metal expansion joints fabrication
- 1 January 2023
- Published by TANGER Ltd.
- Vol. 2023, 258-262
Open AccessTechnology and experimental results of metal expansion joints fabrication
- Open Access
- 10 December 2018
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 461 (1) , 012081
Evaluation of corrosion resistance of titanium/stainless steel diffusion joints bonded by interlayers made of pure metals
The purpose of this study is to compare corrosion resistance of the joints between commercially pure titanium (Grade 2) and stainless steel (X5CrNi18-10) bonded by interlayers made of pure metals. Three different interlayers were used in the study, which were made of aluminium (Al 99.5), copper (Cu 99.99) and nickel (Ni 99.6). The diffusion bonding process has been employed to join those dissimilar materials. The microstructure of the joints were investigated using scanning electron microscopy equipped with an energy dispersive X-ray system (EDS). The phases of the reaction layers in the diffusion zone were identified by means of an X-ray diffraction (XRD).The structures of the joints varied importantly depending on the interlayer. The galvanic corrosion test was carried out in two solutions one in a 3,5% NaCl and second one in 1M Na2SO4 solution. The potentiodynamic polarization curves in a 3,5% NaCl solution show that the higher corrosion potential as well as a lower corrosion current were registered for the joints performed by nickel. The test carried out in 1M Na2SO4 solution show that that the lowest corrosion current was registered for the joints performed by copper and also all investigated samples have a tendency towards passivation.
- 10 December 2018
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 461 (1) , 012081
Open AccessEvaluation of corrosion resistance of titanium/stainless steel diffusion joints bonded by interlayers made of pure metals
The purpose of this study is to compare corrosion resistance of the joints between commercially pure titanium (Grade 2) and stainless steel (X5CrNi18-10) bonded by interlayers made of pure metals. Three different interlayers were used in the study, which were made of aluminium (Al 99.5), copper (Cu 99.99) and nickel (Ni 99.6). The diffusion bonding process has been employed to join those dissimilar materials. The microstructure of the joints were investigated using scanning electron microscopy equipped with an energy dispersive X-ray system (EDS). The phases of the reaction layers in the diffusion zone were identified by means of an X-ray diffraction (XRD).The structures of the joints varied importantly depending on the interlayer. The galvanic corrosion test was carried out in two solutions one in a 3,5% NaCl and second one in 1M Na2SO4 solution. The potentiodynamic polarization curves in a 3,5% NaCl solution show that the higher corrosion potential as well as a lower corrosion current were registered for the joints performed by nickel. The test carried out in 1M Na2SO4 solution show that that the lowest corrosion current was registered for the joints performed by copper and also all investigated samples have a tendency towards passivation.
- Open Access
- 10 December 2018
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 461 (1) , 012082
Structural changes during the formation of diffusion bonded joints between titanium and stainless steel
In the present investigation, transient liquid-phase bonding was performed between pure titanium (Grade 2) and stainless steel (X5CrNi 18-10) using nickel foil as an intermediate material. The process was carried out at the temperatures of: 950, 975 and 1000 ° C for 60 minutes under the compressive stress of 2 MPa in a vacuum. The microstructure was investigated using light microscopy and scanning electron microscopy equipped EDS. The metallographic examination shows that the diffusion interfaces are free from cracks. However, Kirkendall voids were observed at the borders of materials. Especially large voids were formed in middle section of the joint prepared using the highest bonding temperature. The structure of the joints on the titanium side was composed of the eutectoid mixture αTi+Ti2Ni and layers of intermetallic phases Ti2Ni, TiNi and TiNi3. The nickel interlayer blocked the diffusion of titanium to stainless steel side at 950 °C bonding temperature and prevented from formation of the Fe-Ti intermetallic layers. The layer of a solid solution γFe+Ni between nickel and stainless steel was observed at the 950 °C processing temperature. The mixture of λ+FeTi+Ti, FeTi+Ti, λ+αFe and λ+χ+αFe phases was formed at 975 and 1000 °C at the nickel-stainless steel interlayer.
- 10 December 2018
- Published by IOP Publishing in IOP Conference Series: Materials Science and Engineering
- Vol. 461 (1) , 012082
Open AccessStructural changes during the formation of diffusion bonded joints between titanium and stainless steel
In the present investigation, transient liquid-phase bonding was performed between pure titanium (Grade 2) and stainless steel (X5CrNi 18-10) using nickel foil as an intermediate material. The process was carried out at the temperatures of: 950, 975 and 1000 ° C for 60 minutes under the compressive stress of 2 MPa in a vacuum. The microstructure was investigated using light microscopy and scanning electron microscopy equipped EDS. The metallographic examination shows that the diffusion interfaces are free from cracks. However, Kirkendall voids were observed at the borders of materials. Especially large voids were formed in middle section of the joint prepared using the highest bonding temperature. The structure of the joints on the titanium side was composed of the eutectoid mixture αTi+Ti2Ni and layers of intermetallic phases Ti2Ni, TiNi and TiNi3. The nickel interlayer blocked the diffusion of titanium to stainless steel side at 950 °C bonding temperature and prevented from formation of the Fe-Ti intermetallic layers. The layer of a solid solution γFe+Ni between nickel and stainless steel was observed at the 950 °C processing temperature. The mixture of λ+FeTi+Ti, FeTi+Ti, λ+αFe and λ+χ+αFe phases was formed at 975 and 1000 °C at the nickel-stainless steel interlayer.
- Open Access
- 1 June 2016
- Published by Walter de Gruyter GmbH in Archives of Metallurgy and Materials
- Vol. 61 (2) , 997-1001
Microstructure and Mechanical Properties of Joints of Titanium with Stainless Steel Performed using Nickel Filler
Diffusion brazing was performed between titanium (Grade 2) and stainless steel (X5CrNi18-10) using as a filler a nickel foil at the temperatures of 850, 900, 950 and 1000°C. The microstructure was investigated using light microscopy and scanning electron microscopy equipped with an energy dispersive X-ray system (EDS). The structure of the joints on the titanium side was composed of the eutectoid mixture αTi+Ti2Ni and layers of intermetallic phases Ti2Ni, TiNi and TiNi3. The stainless steel-nickel interface is free from any reaction layer at 850°C, above this temperature thin layer of reaction appears. The microhardness measured across the joints reaches higher values than for titanium and stainless steel, and it achieves value from 260 to 446 HV. The highest shear strength (214 MPa) was achieved for joints brazed at 900°C
- 1 June 2016
- Published by Walter de Gruyter GmbH in Archives of Metallurgy and Materials
- Vol. 61 (2) , 997-1001
Open AccessMicrostructure and Mechanical Properties of Joints of Titanium with Stainless Steel Performed using Nickel Filler
Diffusion brazing was performed between titanium (Grade 2) and stainless steel (X5CrNi18-10) using as a filler a nickel foil at the temperatures of 850, 900, 950 and 1000°C. The microstructure was investigated using light microscopy and scanning electron microscopy equipped with an energy dispersive X-ray system (EDS). The structure of the joints on the titanium side was composed of the eutectoid mixture αTi+Ti2Ni and layers of intermetallic phases Ti2Ni, TiNi and TiNi3. The stainless steel-nickel interface is free from any reaction layer at 850°C, above this temperature thin layer of reaction appears. The microhardness measured across the joints reaches higher values than for titanium and stainless steel, and it achieves value from 260 to 446 HV. The highest shear strength (214 MPa) was achieved for joints brazed at 900°C