Fengyuan Shu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Fengyuan Shu has a total of 50 co-authors. Here are the top co-authors by number of shared publications:
Binshi Xu
National Key Laboratory for Remanufacturing Beijing 100072 People's Republic of China
4 shared publicationsHongyun Zhao
Shandong Provincial Key Laboratory of Special Welding Technology Harbin Institute of Technology at Weihai Weihai 264209 People's Republic of China
3 shared publicationsShaohua Sui
Harbin Institute of Technology - Weihai, Weihai, Shandong, CHINA
3 shared publicationsBin Liu
2 shared publicationsJian Zhao
College of Materials Engineering, Shanghai University of Engineering Science, Shanghai, China
2 shared publicationsPeng He
2 shared publications
Latest Publications
- 15 May 2024
- Published by Springer Nature in Journal of Thermal Spray Technology
- Vol. 33 (5) , 1630-1642
Research on Mechanical Properties and Corrosion Behavior of (Co34Fe8Cr29Ni8Si7)100−xBx High Entropy Alloy Coating
- 15 May 2024
- Published by Springer Nature in Journal of Thermal Spray Technology
- Vol. 33 (5) , 1630-1642
Research on Mechanical Properties and Corrosion Behavior of (Co34Fe8Cr29Ni8Si7)100−xBx High Entropy Alloy Coating
- 18 January 2022
- Published by SAGE Publications in Science and Technology of Welding and Joining
- Vol. 27 (3) , 176-185
Microstructure and mechanical properties of nanosecond pulsed laser welded Al–Cu–steel laminated structures
Al–Cu–steel laminated structures with configurations of Al/Cu/steel and steel/Cu/Al were obtained via nanosecond pulsed laser welding. Cavities occurred at the bottom welds in two joints. Full-penetration welds occurred more easily in steel/Cu/Al joints compared to Al/Cu/steel joints. The metallurgical reaction of Al and Fe was impeded by Cu. The eutectic (α-Al+θ) and θ-CuAl2 phases were predominant at the Al/Cu interface in the steel/Cu/Al joints, while (Cu, Fe) was the main phase in Al/Cu/steel joint. The average lap shear force of the Al/Cu/steel joints (51.2 N) was superior to that of steel/Cu/Al joints (37.2 N). The fracture for both joins occurred at the Al/Cu interface. The fracture morphologies indicated that smaller connection width and Al/Cu IMCs caused the weld pullout failure (WPF) mode in steel/Cu/Al joints. The larger connection area and presence of (Cu, Fe) solid solution were responsible for the interfacial shear failure (ISF) mode in Al/Cu/steel joints.
- 18 January 2022
- Published by SAGE Publications in Science and Technology of Welding and Joining
- Vol. 27 (3) , 176-185
Microstructure and mechanical properties of nanosecond pulsed laser welded Al–Cu–steel laminated structures
Al–Cu–steel laminated structures with configurations of Al/Cu/steel and steel/Cu/Al were obtained via nanosecond pulsed laser welding. Cavities occurred at the bottom welds in two joints. Full-penetration welds occurred more easily in steel/Cu/Al joints compared to Al/Cu/steel joints. The metallurgical reaction of Al and Fe was impeded by Cu. The eutectic (α-Al+θ) and θ-CuAl2 phases were predominant at the Al/Cu interface in the steel/Cu/Al joints, while (Cu, Fe) was the main phase in Al/Cu/steel joint. The average lap shear force of the Al/Cu/steel joints (51.2 N) was superior to that of steel/Cu/Al joints (37.2 N). The fracture for both joins occurred at the Al/Cu interface. The fracture morphologies indicated that smaller connection width and Al/Cu IMCs caused the weld pullout failure (WPF) mode in steel/Cu/Al joints. The larger connection area and presence of (Cu, Fe) solid solution were responsible for the interfacial shear failure (ISF) mode in Al/Cu/steel joints.
- Open Access
- 1 July 2020
- Published by IOP Publishing in Materials Research Express
- Vol. 7 (7) , 075104
Research on microstructure of copper coatings on AlN ceramic surface by laser cladding and brazing
The preparation of Cu-based coatings on AlN ceramic surface was accomplished by laser cladding and brazing technology. The Cu-based coating was prepared by both copper powder and titanium powder on ceramic surface. The microstructure and properties were tested by x-ray diffraction, metallurgical microscope, scanning electron microscope, energy dispersive spectrometer and microhardness tester. The novelties of this paper in the method of laser cladding and brazing were used to prepare Cu-coating on ceramic surface and the addition of Ti could improve the properties of Cu-based coating. The addition of Ti improved the wettability of ceramic surface. According to the results of EDS, Ti could better get into the Cu-based coating and formed metallurgical bonding in the laser cladding. The microhardness of laser cladding was higher than brazing, which could be concluded that it was due to the rapid cooling rate during the laser cladding could restrain grain growth and element segregation.
- 1 July 2020
- Published by IOP Publishing in Materials Research Express
- Vol. 7 (7) , 075104
Open AccessResearch on microstructure of copper coatings on AlN ceramic surface by laser cladding and brazing
The preparation of Cu-based coatings on AlN ceramic surface was accomplished by laser cladding and brazing technology. The Cu-based coating was prepared by both copper powder and titanium powder on ceramic surface. The microstructure and properties were tested by x-ray diffraction, metallurgical microscope, scanning electron microscope, energy dispersive spectrometer and microhardness tester. The novelties of this paper in the method of laser cladding and brazing were used to prepare Cu-coating on ceramic surface and the addition of Ti could improve the properties of Cu-based coating. The addition of Ti improved the wettability of ceramic surface. According to the results of EDS, Ti could better get into the Cu-based coating and formed metallurgical bonding in the laser cladding. The microhardness of laser cladding was higher than brazing, which could be concluded that it was due to the rapid cooling rate during the laser cladding could restrain grain growth and element segregation.
- 16 March 2020
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 29 (3) , 1830-1840
Statistical and Metallurgical Analysis of Dissimilar Friction Stir Spot Welded Aluminum/Copper Metals
- 16 March 2020
- Published by Springer Nature in Journal of Materials Engineering and Performance
- Vol. 29 (3) , 1830-1840
Statistical and Metallurgical Analysis of Dissimilar Friction Stir Spot Welded Aluminum/Copper Metals
- 7 August 2019
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (10) , 106517
Effect of rare earth oxide CeO2 on microstructure and surface properties of laser cladded CoFeCrNiSiB high-entropy alloy coatings
- 7 August 2019
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (10) , 106517
Effect of rare earth oxide CeO2 on microstructure and surface properties of laser cladded CoFeCrNiSiB high-entropy alloy coatings
- Open Access
- 26 June 2019
- Published by Institution of Engineering and Technology (IET) in Micro & Nano Letters
- Vol. 14 (7) , 717-720
Strengthening mechanism and properties of Co–WC composite coatings deposited by plasma‐transferred arc welding
Cobalt (Co)‐based tungsten carbide (WC) wear‐resistant coatings with different content of WC were prepared on the surface of Q235 low carbon steel by plasma‐transferred arc welding. The properties of the coatings such as strengthening mechanism, microhardness and wear properties were tested by using a metallurgical microscope, scanning electron microscope, energy dispersive spectrometer, X‐ray diffraction, Rockwell hardness tester, and friction wear equipment. The results show that the main reasons for the strengthening of spray welding layer are the solution strengthening formed by α‐Co with supersaturated tungsten (W) and the dispersion strengthening caused by eutectic precipitated carbide and silicide. The proportion of the solid solution of W in α‐Co steadily ranges from 18.00 to 19.59%. The morphologies of rich W‐phase are mainly related to the content of W. With the content of W increasing, the evolution process of the shape is the amorphous form→damascene shape→star‐like shape→the polygon. Amorphous W‐rich phase can be obtained when the content of WC ranges from 20 to 30%, evenly distributed W‐rich phase in the shape of damascene or star can be obtained when the WC content ranges from 30 to 40%, and the polygonal W‐rich phase can be obtained at the percentage of 40–50%.
- 26 June 2019
- Published by Institution of Engineering and Technology (IET) in Micro & Nano Letters
- Vol. 14 (7) , 717-720
Open AccessStrengthening mechanism and properties of Co–WC composite coatings deposited by plasma‐transferred arc welding
Cobalt (Co)‐based tungsten carbide (WC) wear‐resistant coatings with different content of WC were prepared on the surface of Q235 low carbon steel by plasma‐transferred arc welding. The properties of the coatings such as strengthening mechanism, microhardness and wear properties were tested by using a metallurgical microscope, scanning electron microscope, energy dispersive spectrometer, X‐ray diffraction, Rockwell hardness tester, and friction wear equipment. The results show that the main reasons for the strengthening of spray welding layer are the solution strengthening formed by α‐Co with supersaturated tungsten (W) and the dispersion strengthening caused by eutectic precipitated carbide and silicide. The proportion of the solid solution of W in α‐Co steadily ranges from 18.00 to 19.59%. The morphologies of rich W‐phase are mainly related to the content of W. With the content of W increasing, the evolution process of the shape is the amorphous form→damascene shape→star‐like shape→the polygon. Amorphous W‐rich phase can be obtained when the content of WC ranges from 20 to 30%, evenly distributed W‐rich phase in the shape of damascene or star can be obtained when the WC content ranges from 30 to 40%, and the polygonal W‐rich phase can be obtained at the percentage of 40–50%.
- 20 May 2019
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (10) , 1065e1
Microstructure and mechanical properties of multi-pass TIG welded joint of thick Al–Zn–Mg alloy plate
The microstructure and impact mechanical properties of multi-layer multi-channel TIG welded joints of Al-Zn-Mg alloy plates were studied in this paper. The mechanical properties of the welded joint including microhardness and tensile performance were tested, respectively, while the microstructure was observed by scanning electron microscope, energy dispersive spectrometer, X-ray diffractor and transmission electron microscope. A short rod-shaped MgZn2 phase and a strip-shaped Al3Mg2 phase were found in the intergranular column of the weld seam, and an ellipsoidal MgZn2 phase was found in the intragranular column. The EDS test results of the micro-fracture and the fracture surface of the tensile specimen indicated that these particles could act as a strengthening phase or a crack source during the tensile fracture process. In addition, the distribution of microhardness in the weld zone was investigated.
- 20 May 2019
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (10) , 1065e1
Microstructure and mechanical properties of multi-pass TIG welded joint of thick Al–Zn–Mg alloy plate
The microstructure and impact mechanical properties of multi-layer multi-channel TIG welded joints of Al-Zn-Mg alloy plates were studied in this paper. The mechanical properties of the welded joint including microhardness and tensile performance were tested, respectively, while the microstructure was observed by scanning electron microscope, energy dispersive spectrometer, X-ray diffractor and transmission electron microscope. A short rod-shaped MgZn2 phase and a strip-shaped Al3Mg2 phase were found in the intergranular column of the weld seam, and an ellipsoidal MgZn2 phase was found in the intragranular column. The EDS test results of the micro-fracture and the fracture surface of the tensile specimen indicated that these particles could act as a strengthening phase or a crack source during the tensile fracture process. In addition, the distribution of microhardness in the weld zone was investigated.
- 1 May 2019
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 785, 846-854
Microstructure and mechanical properties of Co-based alloy coatings fabricated by laser cladding and plasma arc spray welding
- 1 May 2019
- Published by Elsevier in Journal of Alloys and Compounds
- Vol. 785, 846-854
Microstructure and mechanical properties of Co-based alloy coatings fabricated by laser cladding and plasma arc spray welding
- 1 January 2019
- Published by Elsevier in Surface and Coatings Technology
- Vol. 358, 667-675
Effects of laser power on microstructure and properties of laser cladded CoCrBFeNiSi high-entropy alloy amorphous coatings
- 1 January 2019
- Published by Elsevier in Surface and Coatings Technology
- Vol. 358, 667-675
Effects of laser power on microstructure and properties of laser cladded CoCrBFeNiSi high-entropy alloy amorphous coatings
- 1 August 2018
- Published by Elsevier in Applied Surface Science
- Vol. 450, 538-544
Effects of Fe-to-Co ratio on microstructure and mechanical properties of laser cladded FeCoCrBNiSi high-entropy alloy coatings
- 1 August 2018
- Published by Elsevier in Applied Surface Science
- Vol. 450, 538-544
Effects of Fe-to-Co ratio on microstructure and mechanical properties of laser cladded FeCoCrBNiSi high-entropy alloy coatings