XLXia Li

Xia Li

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Xia Li has a total of 10 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Improved Properties of Ceramic Shells by Optimizing the Surface Composition from Lanthanide-Based Composites

    by Minghui Li, Jianbo Yu, Xia Li, Zhigang Yang, Zhongming Ren, Xiaoxin Zhang

    The precision casting of nickel-based single-crystal superalloys imposes stringent requirements on the high-temperature stability and chemical inertness of ceramic shell face coats. To address the issue of traditional EC95 shells (95% Al2O3–5% SiO2) being prone to react with the alloy melt at elevated temperatures, thereby inducing casting defects, this study proposes a lanthanide oxide-based ceramic face coat material. Three distinct powders—LaAlO3 (LA), LaAlO3/La2Si2O7 (LAS), and LaAl11O18/La2Si2O7/Al2O3 (LA11S)—are successfully prepared through solid-phase sintering of the La2O3-Al2O3-SiO2 ternary system. Their slurry properties, shell sintering processes, and high-temperature performance are systematically investigated. The results demonstrate that optimal slurry coating effectiveness is achieved when LA powder is processed with a liquid-to-powder ratio of 3:1 and a particle size of 300 mesh. While LA shells show no cracking at 1300 °C, their face coats fail above 1400 °C due to the formation of a La2Si2O7 phase. In contrast, LAS and LA11S shells suppress cracking through the La2Si2O7 and LaAl11O18 phases, respectively, exhibiting exceptionally high-temperature stability at 1400 °C and 1500 °C. All three shells meet the high-temperature strength requirements for CMSX-4 single-crystal alloy casting. Interfacial reaction analysis and Gibbs free energy calculations reveal that Al2O3-forming reactions occur between the novel shells and alloy melt, accompanied by minor dissolution erosion without other chemical side reactions. This work provides a high-performance face coat material solution for investment casting of nickel-based superalloys.

  • Open Access

    Manganese Removal from Liquid Nickel by Hydrogen Plasma Arc Melting

    by Xiliang Guo, Jianbo Yu, Yuan Hou, Yujia Zhang, Jiang Wang, Xia Li, Hanlin Liao, Zhongming Ren

    In this work, the removal of manganese from nickel melts by Ar and (10%, 20% and 40%) H2 plasma arc melting under various pressures (0.01–0.02, 0.04–0.05 and 0.09–0.1 MPa) was investigated experimentally. The results show that only a slight reduction in the manganese content is obtained by Ar plasma arc melting (PAM). By contrast, the manganese content of liquid nickel decreases noticeably upon the addition of hydrogen to plasma gas, and the rate of manganese removal increases with increasing hydrogen volume fraction. In addition, the reduction in the pressure enhances the efficiency of manganese removal from liquid nickel by hydrogen plasma arc melting (HPAM). The process of manganese removal by HPAM was found to obey a first-order rate law. From kinetic analysis, the rate of reduction in the manganese content increases proportionally to the 0.73–0.75th power of the hydrogen volume fraction in the plasma gas. However, the rate of the manganese content reduction increases proportionally to approximately 0.88th power of %H2 in the plasma gas for the initial manganese content of 0.89 mass%, which is slightly higher than that for the initial manganese concentration of 0.45 mass%. Thermodynamic analysis indicates that the volatilization of manganese benefits from negative pressure and the presence of active hydrogen atoms that act as the transfer media of the metal vapor in the gas boundary layer.