Bruce Ford
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Bruce Ford has a total of 8 co-authors. Here are the top co-authors by number of shared publications:
- Bronwyn J. Lowe
University of Otago, Dunedin, New Zealand
1 shared publication Capucine Korenberg
Department of Scientific Research, The British Museum, London, UK
1 shared publication- Catherine Ann Smith
Archaeology School of Social Science University of Otago/Te Whare Wānanga o Otāgo Dunedin New Zealand
1 shared publication Frances Daroux
Centre for Materials Science and Technology, University of Otago, PO Box 56, Dunedin 9054, New Zealand
1 shared publication- Keith Christopher Gordon
Department of Chemistry University of Otago Dunedin New Zealand
1 shared publication - Rachel A. Paterson
Norwegian Institute for Nature Research, Trondheim, Norway
1 shared publication
Latest Publications
- 23 March 2023
- Published by Taylor & Francis in Studies in Conservation
- Vol. 69 (3) , 209-220
Manufacturing Variations in ISO Blue Wool Fading Standards under Microfading Exposure Conditions
As is the case for other accelerated light-ageing methods, microfade test results are usually rated against the responses of the International Standards Organisation’s Blue Wool Fading Standards, the production of which is regulated by the International Standards Organisation. The suitability and convenience of the ISO Blue Wools for this purpose have been questioned on various grounds, including wavelength sensitivity, manufacturing or batch response variations, and the effect of their woven texture on systematic errors. In the present article, the effect of manufacturing variations was assessed by carrying out microfade testing on samples of ISO Blue Wools from various suppliers and manufacturers spanning more than 20 years. Our results confirm that the first three ISO Blue Wools, which are of most relevance to locating colourants at risk of significant light-fading on display in museums, had measurable batch-to-batch and/or manufacturer variations in fading rates, most significantly in the case of Blue Wool 2. Different batches were often also distinguishable by their colour and the texture of the wool fabric. It is argued that while texture-related systematic errors and manufacturing variations are inconvenient, they are not significant in light of the other potential sources of disparity between the results of accelerated exposure tests of any kind and fading at ambient light levels, and it is concluded that the advantages of the use of ISO Blue Wools as internal standards for microfade testing outweigh their disadvantages.
- 23 March 2023
- Published by Taylor & Francis in Studies in Conservation
- Vol. 69 (3) , 209-220
Manufacturing Variations in ISO Blue Wool Fading Standards under Microfading Exposure Conditions
As is the case for other accelerated light-ageing methods, microfade test results are usually rated against the responses of the International Standards Organisation’s Blue Wool Fading Standards, the production of which is regulated by the International Standards Organisation. The suitability and convenience of the ISO Blue Wools for this purpose have been questioned on various grounds, including wavelength sensitivity, manufacturing or batch response variations, and the effect of their woven texture on systematic errors. In the present article, the effect of manufacturing variations was assessed by carrying out microfade testing on samples of ISO Blue Wools from various suppliers and manufacturers spanning more than 20 years. Our results confirm that the first three ISO Blue Wools, which are of most relevance to locating colourants at risk of significant light-fading on display in museums, had measurable batch-to-batch and/or manufacturer variations in fading rates, most significantly in the case of Blue Wool 2. Different batches were often also distinguishable by their colour and the texture of the wool fabric. It is argued that while texture-related systematic errors and manufacturing variations are inconvenient, they are not significant in light of the other potential sources of disparity between the results of accelerated exposure tests of any kind and fading at ambient light levels, and it is concluded that the advantages of the use of ISO Blue Wools as internal standards for microfade testing outweigh their disadvantages.
- 2 January 2018
- Published by Taylor & Francis in AICCM Bulletin
- Vol. 39 (1) , 26-34
A microfading survey of the lightfastness of blue, black and red ballpoint pen inks in ambient and modified environments
The lightfastness of approximately 100 randomly selected red, black and blue inks was surveyed using the microfade technique. The inks’ responses were recorded at 55% and at 1% relative humidity (RH) in air, and in a low oxygen environment (2) at 55% RH. Their light sensitivity in air was highly unpredictable, ranging from the detection limit of the technique to several times greater than the most fugitive ISO Blue Wool Fading Standard (BW1). With very few exceptions, the response of blue and black inks was markedly suppressed in anoxia, and the opposite was true of a significant proportion of red inks tested. The correlation between RH and light-sensitivity in air was weak, with highly variable responses in both directions. The results show that it is not possible to make useful display (light exposure) recommendations for ballpoint pen inks without prior fade-testing.
- 2 January 2018
- Published by Taylor & Francis in AICCM Bulletin
- Vol. 39 (1) , 26-34
A microfading survey of the lightfastness of blue, black and red ballpoint pen inks in ambient and modified environments
The lightfastness of approximately 100 randomly selected red, black and blue inks was surveyed using the microfade technique. The inks’ responses were recorded at 55% and at 1% relative humidity (RH) in air, and in a low oxygen environment (2) at 55% RH. Their light sensitivity in air was highly unpredictable, ranging from the detection limit of the technique to several times greater than the most fugitive ISO Blue Wool Fading Standard (BW1). With very few exceptions, the response of blue and black inks was markedly suppressed in anoxia, and the opposite was true of a significant proportion of red inks tested. The correlation between RH and light-sensitivity in air was weak, with highly variable responses in both directions. The results show that it is not possible to make useful display (light exposure) recommendations for ballpoint pen inks without prior fade-testing.
- 1 March 2017
- Published by Elsevier in Journal of Cultural Heritage
- Vol. 24, 60-68
Light-ageing characteristics of Māori textiles: Colour, strength and molecular change
- 1 March 2017
- Published by Elsevier in Journal of Cultural Heritage
- Vol. 24, 60-68
Light-ageing characteristics of Māori textiles: Colour, strength and molecular change