A. S. Demin
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
A. S. Demin has a total of 63 co-authors. Here are the top co-authors by number of shared publications:
- V. N. Pimenov
Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences, Moscow, Russia
8 shared publications - E. V. Morozov
Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences, Moscow, Russia
7 shared publications - N. A. Epifanov
Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences, Moscow, Russia
7 shared publications - I. V. Borovitskaya
Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences, Moscow, Russia
6 shared publications - S. A. Maslyaev
Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences, Moscow, Russia
6 shared publications E. V. Morozov
Baikov Institute of Metallurgy and Material Science of RAS, Moscow, Russia
4 shared publications
Latest Publications
- 1 July 2025
- Published by Pleiades Publishing Ltd in Physics of Atomic Nuclei
- Vol. 88 (S1) , S67-S78
Damage of the Tungsten Surface Layer under Irradiation by Steady-State Ion and Pulsed Beam-Plasma Helium Fluxes
Comparative studies of tungsten surface damageability under irradiation with steady-state helium ion fluxes and pulsed helium ion and helium plasma fluxes in the ion-beam accelerator (ILU) and in the Vikhr Plasma Focus (PF) installation have been carried out. The parameters of irradiation with steady-state He+ ion fluxes in the ILU: helium ion energy of 30 keV; fluences of 1.0 × 1018 and 2.0 × 1018 cm–2; and target temperature during irradiation not exceeding ~500 K. For irradiation with pulsed fluxes of helium ions and helium plasma in the Vikhr PF installation, the samples were placed in the cathode zone of the Vikhr PF chamber at a distance of 2, 4, and 6 cm from the anode. Parameters of irradiation of samples in the Vikhr PF: duration of ion and plasma exposure of 10–30 and 50–200 ns, respectively; power density of plasma in the range of ∼107–109 W/cm2 and ions in the range of ~109–1010 W/cm2; number of pulses N = 5, 15, and 30; helium ion energy of ~100 keV; and plasma temperature of ~1 keV. Under irradiation with steady-state He+ ion fluxes with a fluence of 1018 cm–2, formation of blisters with peripheral rupture of caps characteristic of brittle materials is observed. An increase in the irradiation fluence by a factor of two leads to a change in the mechanism of surface failure; i.e., exfoliation of layers (flaking) is observed. During irradiation of samples in the Vikhr PF installation, melting of the surface layer occurs, resulting in a wavy surface relief with the appearance of cracks and craters, i.e., traces of helium gas release and unopened blisters. The sizes of craters are ∼1–2 µm, which is comparable to the dimensions of blisters observed after He+ ion implantation in the ILU accelerator. Numerical modeling of the impact of a fast helium ion beam on tungsten in the Vikhr PF installation has been performed. Using methods of X-ray diffraction analysis, the following effects are observed: a decrease in lattice parameters under all modes of ion and plasma flux exposure; varying degrees of changes in the size of the coherent scattering region (CSR) and the magnitude of lattice microstrain and texture. A decrease in the microhardness of tungsten samples after treatment with helium plasma and He+ ions in the Vikhr PF installation is detected, which may result from the influence of two competing factors: annealing of defects under intense thermal loads (reduces Hμ ) and thermal stresses arising during the crystallization and cooling of the melted surface layer (increases Hμ ). The mechanisms of the observed phenomena are discussed.
- 1 July 2025
- Published by Pleiades Publishing Ltd in Physics of Atomic Nuclei
- Vol. 88 (S1) , S67-S78
Damage of the Tungsten Surface Layer under Irradiation by Steady-State Ion and Pulsed Beam-Plasma Helium Fluxes
Comparative studies of tungsten surface damageability under irradiation with steady-state helium ion fluxes and pulsed helium ion and helium plasma fluxes in the ion-beam accelerator (ILU) and in the Vikhr Plasma Focus (PF) installation have been carried out. The parameters of irradiation with steady-state He+ ion fluxes in the ILU: helium ion energy of 30 keV; fluences of 1.0 × 1018 and 2.0 × 1018 cm–2; and target temperature during irradiation not exceeding ~500 K. For irradiation with pulsed fluxes of helium ions and helium plasma in the Vikhr PF installation, the samples were placed in the cathode zone of the Vikhr PF chamber at a distance of 2, 4, and 6 cm from the anode. Parameters of irradiation of samples in the Vikhr PF: duration of ion and plasma exposure of 10–30 and 50–200 ns, respectively; power density of plasma in the range of ∼107–109 W/cm2 and ions in the range of ~109–1010 W/cm2; number of pulses N = 5, 15, and 30; helium ion energy of ~100 keV; and plasma temperature of ~1 keV. Under irradiation with steady-state He+ ion fluxes with a fluence of 1018 cm–2, formation of blisters with peripheral rupture of caps characteristic of brittle materials is observed. An increase in the irradiation fluence by a factor of two leads to a change in the mechanism of surface failure; i.e., exfoliation of layers (flaking) is observed. During irradiation of samples in the Vikhr PF installation, melting of the surface layer occurs, resulting in a wavy surface relief with the appearance of cracks and craters, i.e., traces of helium gas release and unopened blisters. The sizes of craters are ∼1–2 µm, which is comparable to the dimensions of blisters observed after He+ ion implantation in the ILU accelerator. Numerical modeling of the impact of a fast helium ion beam on tungsten in the Vikhr PF installation has been performed. Using methods of X-ray diffraction analysis, the following effects are observed: a decrease in lattice parameters under all modes of ion and plasma flux exposure; varying degrees of changes in the size of the coherent scattering region (CSR) and the magnitude of lattice microstrain and texture. A decrease in the microhardness of tungsten samples after treatment with helium plasma and He+ ions in the Vikhr PF installation is detected, which may result from the influence of two competing factors: annealing of defects under intense thermal loads (reduces Hμ ) and thermal stresses arising during the crystallization and cooling of the melted surface layer (increases Hμ ). The mechanisms of the observed phenomena are discussed.
- 1 April 2025
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 16 (2) , 317-325
Features of the Use of Plasma Focus Installations in Radiation and Space Materials Science
The features of the use of Plasma Focus (PF) devices in the field of radiation and space materials science related to the specific generation of several types of radiation in the working chambers of the PF are considered. It is noted that the main role in the damage and modification of the structural state of the surface layers of materials irradiated in the cathode zone of the PF working chamber is played by powerful pulsed beams of working gas ions and flows of high-temperature plasma in the nano- and microsecond range of pulse duration. It is shown that, in addition to the common combined beam-plasma effect on a target sample, PF installations allow the possibility of separate irradiation of the target material with ion and plasma flows. Three methods for separating pulsed flows of hot plasma and fast ions in space and time in a PF installation, described in the literature, are presented. It is noted that PF installations are a promising tool for solving fundamental and applied problems in radiation and space materials science, including for simulation experiments focused on problems of thermonuclear energy and aerospace engineering. It is also indicated that hard X-ray pulses with a duration in the nanosecond range, arising from pulsed discharges in the PF chamber, can be used for diagnosing fast processes, in particular, for nondestructive flaw detection of machines and mechanisms during their operation.
- 1 April 2025
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 16 (2) , 317-325
Features of the Use of Plasma Focus Installations in Radiation and Space Materials Science
The features of the use of Plasma Focus (PF) devices in the field of radiation and space materials science related to the specific generation of several types of radiation in the working chambers of the PF are considered. It is noted that the main role in the damage and modification of the structural state of the surface layers of materials irradiated in the cathode zone of the PF working chamber is played by powerful pulsed beams of working gas ions and flows of high-temperature plasma in the nano- and microsecond range of pulse duration. It is shown that, in addition to the common combined beam-plasma effect on a target sample, PF installations allow the possibility of separate irradiation of the target material with ion and plasma flows. Three methods for separating pulsed flows of hot plasma and fast ions in space and time in a PF installation, described in the literature, are presented. It is noted that PF installations are a promising tool for solving fundamental and applied problems in radiation and space materials science, including for simulation experiments focused on problems of thermonuclear energy and aerospace engineering. It is also indicated that hard X-ray pulses with a duration in the nanosecond range, arising from pulsed discharges in the PF chamber, can be used for diagnosing fast processes, in particular, for nondestructive flaw detection of machines and mechanisms during their operation.
- 9 October 2024
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 15 (5) , 1265-1273
Effect of Pulsed Helium Ion and Helium Plasma Flows on Austenitic Chromium–Manganese Steel Preirradiated with Deuterium
The effect of sequential action of pulsed helium ion and helium plasma flows on low-activated austenitic 25Cr12Mn20W chromium–manganese steel samples cut from a hexagonal pipe preirradiated with the deuterium ion and deuterium plasma flows in different modes at the Plasma Focus PF-1000 facility has been studied. Two deuterium irradiation modes have been implemented: a relatively soft mode with a power density of q ~ 107–108 W/cm2 and a hard mode with q ~ 109–1010 W/cm2 with a pulse length of τ = 100 ns and number N = 4 of pulse discharges in both cases. It has been shown that the effect of the helium ion and helium plasma flows at the PF Vikhr facility with irradiation parameters of q ~ 107–108 W/cm2, τ = 100 ns, and N = 15 on the inner surface of a steel pipe sample depends on the mode of its preirradiation with deuterium ion and deuterium plasma flows. In the relatively soft mode of pre-exposure to deuterium ion and deuterium plasma flows with a power density of q ~ 107–108 W/cm2, the subsequent pulsed irradiation with helium causes slight changes in the damageability of the surface layer: smoothing of the wavelike surface relief, an increase in pore formation in the surface layer, appearance of microcracks in it, and formation of spherical particles consisting of basic and impurity elements of the steel composition. The presence of niobium deposited from the anode of the PF facility has also been observed. The impact of the helium ions and helium plasma flows on the inner surface of a steel pipe sample after its preirradiation with deuterium ion and deuterium plasma flows in the hard mode at q ~ 109–1010 W/cm2 increases the damageability of the surface layer. Implantation of helium into the material facilitates an increase in the number and size of open cavities (tens of microns) emerging in the surface layer at the stage of preirradiation of the pipe with deuterium, formation of numerous small (up to ~5 μm) bubbles and pores in it, and emergence of spherical particles of different phases on the irradiated surface. An increase in the damageability of the surface layer in the investigated steel sample after its subsequent pulsed irradiation with helium is accompanied by a significant increase in the intensity of erosion of the material as compared with the situation implemented in the softer mode of pre-irradiation of the sample. The enhanced erosion leads to a noticeable decrease in the content of niobium deposited onto the irradiated surface.
- 9 October 2024
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 15 (5) , 1265-1273
Effect of Pulsed Helium Ion and Helium Plasma Flows on Austenitic Chromium–Manganese Steel Preirradiated with Deuterium
The effect of sequential action of pulsed helium ion and helium plasma flows on low-activated austenitic 25Cr12Mn20W chromium–manganese steel samples cut from a hexagonal pipe preirradiated with the deuterium ion and deuterium plasma flows in different modes at the Plasma Focus PF-1000 facility has been studied. Two deuterium irradiation modes have been implemented: a relatively soft mode with a power density of q ~ 107–108 W/cm2 and a hard mode with q ~ 109–1010 W/cm2 with a pulse length of τ = 100 ns and number N = 4 of pulse discharges in both cases. It has been shown that the effect of the helium ion and helium plasma flows at the PF Vikhr facility with irradiation parameters of q ~ 107–108 W/cm2, τ = 100 ns, and N = 15 on the inner surface of a steel pipe sample depends on the mode of its preirradiation with deuterium ion and deuterium plasma flows. In the relatively soft mode of pre-exposure to deuterium ion and deuterium plasma flows with a power density of q ~ 107–108 W/cm2, the subsequent pulsed irradiation with helium causes slight changes in the damageability of the surface layer: smoothing of the wavelike surface relief, an increase in pore formation in the surface layer, appearance of microcracks in it, and formation of spherical particles consisting of basic and impurity elements of the steel composition. The presence of niobium deposited from the anode of the PF facility has also been observed. The impact of the helium ions and helium plasma flows on the inner surface of a steel pipe sample after its preirradiation with deuterium ion and deuterium plasma flows in the hard mode at q ~ 109–1010 W/cm2 increases the damageability of the surface layer. Implantation of helium into the material facilitates an increase in the number and size of open cavities (tens of microns) emerging in the surface layer at the stage of preirradiation of the pipe with deuterium, formation of numerous small (up to ~5 μm) bubbles and pores in it, and emergence of spherical particles of different phases on the irradiated surface. An increase in the damageability of the surface layer in the investigated steel sample after its subsequent pulsed irradiation with helium is accompanied by a significant increase in the intensity of erosion of the material as compared with the situation implemented in the softer mode of pre-irradiation of the sample. The enhanced erosion leads to a noticeable decrease in the content of niobium deposited onto the irradiated surface.
- 1 April 2023
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 14 (2) , 310-316
Simulated Irradiation of 16Cr–4Al–2W–0.3Ti–0.3Y2O3 ODS Steel Promising for Fusion Reactors in Vikhr Plasma Focus Facility
This article discusses radiation thermal resistance of 16Cr–4Al–2W–0.3Ti–0.3Y2O3 oxide dispersion strengthened (ODS) ferritic steel promising for application in nuclear fusion facilities under the impact of intense pulsed flows of helium ions and helium plasma using Vikhr Plasma Focus facility. The power density of high velocity helium ions and flows of high temperature helium plasma was ~108 and 107 W/cm2 at the impact duration of ~50 and 100 ns, respectively. The number of impact pulses N was varied in the range from 10 to 30. The rate of radiative sputtering varied slightly with increase in the number of impact pulses of energy flow on material and amounted to h ≈ 0.01–0.02 μm/pulse. The irradiated surface after repeated melting under the action of pulsed radiation thermal load by intense energy flows acquired a wavelike pattern with inclusion of disperse microparticles of the second phase containing mainly yttrium, oxygen, aluminum, iron, and titanium. At the same time, in contrast to the refractory metals (W, Mo, Ti) previously studied under the same conditions, no micro- and macrocracks were formed on the surface facing plasma. The Vikhr Plasma Focus facility has proven to be an efficient tool for simulation tests of candidate materials of fusion reactors with magnetic and inertial plasma confinement.
- 1 April 2023
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 14 (2) , 310-316
Simulated Irradiation of 16Cr–4Al–2W–0.3Ti–0.3Y2O3 ODS Steel Promising for Fusion Reactors in Vikhr Plasma Focus Facility
This article discusses radiation thermal resistance of 16Cr–4Al–2W–0.3Ti–0.3Y2O3 oxide dispersion strengthened (ODS) ferritic steel promising for application in nuclear fusion facilities under the impact of intense pulsed flows of helium ions and helium plasma using Vikhr Plasma Focus facility. The power density of high velocity helium ions and flows of high temperature helium plasma was ~108 and 107 W/cm2 at the impact duration of ~50 and 100 ns, respectively. The number of impact pulses N was varied in the range from 10 to 30. The rate of radiative sputtering varied slightly with increase in the number of impact pulses of energy flow on material and amounted to h ≈ 0.01–0.02 μm/pulse. The irradiated surface after repeated melting under the action of pulsed radiation thermal load by intense energy flows acquired a wavelike pattern with inclusion of disperse microparticles of the second phase containing mainly yttrium, oxygen, aluminum, iron, and titanium. At the same time, in contrast to the refractory metals (W, Mo, Ti) previously studied under the same conditions, no micro- and macrocracks were formed on the surface facing plasma. The Vikhr Plasma Focus facility has proven to be an efficient tool for simulation tests of candidate materials of fusion reactors with magnetic and inertial plasma confinement.
- 30 September 2022
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 13 (5) , 1238-1246
Features of Niobium Damage by Pulsed Laser Radiation in Comparison with Beam-Plasma Impact
The features of damageability of niobium by pulsed fluxes of laser radiation (LR) in free-running (power density qFR = 105–106 W/cm2 with pulse duration τFR = 700 μs) and Q-switched (q = 108–109 W/cm2, τQS = 80 ns) modes in comparison with pulsed effects of helium ion (HI) and helium plasma (HP) fluxes in the Plasma Focus (PF) setup at a flux power density qi ~ 108 W/cm2 and qp ~ 107 W/cm2, respectively, and pulse durations τi ≈ 30–50 ns and τp ≈ 100 ns were studied. LR fluxes were exposed to Nb in air; the working gas in the PF chamber was helium. It is shown that, in contrast to the effect of helium ion and helium plasma fluxes on niobium in the PF installation, which contribute to the erosion of the material, irradiation of niobium with pulsed LR in air fluxes under the implemented conditions does not cause noticeable surface erosion. When Nb is exposed to pulsed LR in the FR mode, the melt interacts with air and forms a thin film of elements of liquid and gas phases on the irradiated surface. A similar nature of Nb damageability under conditions of laser and beam-plasma treatment was found: a wavy relief of the irradiated surface with the presence of droplike fragments on it, extended wave crests, and microcracks. Irradiation of Nb with pulsed LR fluxes in the FR mode leads to formation of sections with block and cellular structures in the surface layer (SL), which are also formed after experiments in the PF chamber. It was found that, after laser treatment in the FR and Q-switched modes, bubbles (blisters) are not formed in the SL of niobium, which are always present on the irradiated surface when exposed to pulsed fluxes of HI and HP in the PF chamber owing to implantation of helium ions into Nb. It is noted that, in laser experiments, there is no possibility of implanting working gas ions into the material, which is typical of beam-plasma impacts in PF devices, which affects damageability parameters and modification of the structure of the irradiated SL.
- 30 September 2022
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 13 (5) , 1238-1246
Features of Niobium Damage by Pulsed Laser Radiation in Comparison with Beam-Plasma Impact
The features of damageability of niobium by pulsed fluxes of laser radiation (LR) in free-running (power density qFR = 105–106 W/cm2 with pulse duration τFR = 700 μs) and Q-switched (q = 108–109 W/cm2, τQS = 80 ns) modes in comparison with pulsed effects of helium ion (HI) and helium plasma (HP) fluxes in the Plasma Focus (PF) setup at a flux power density qi ~ 108 W/cm2 and qp ~ 107 W/cm2, respectively, and pulse durations τi ≈ 30–50 ns and τp ≈ 100 ns were studied. LR fluxes were exposed to Nb in air; the working gas in the PF chamber was helium. It is shown that, in contrast to the effect of helium ion and helium plasma fluxes on niobium in the PF installation, which contribute to the erosion of the material, irradiation of niobium with pulsed LR in air fluxes under the implemented conditions does not cause noticeable surface erosion. When Nb is exposed to pulsed LR in the FR mode, the melt interacts with air and forms a thin film of elements of liquid and gas phases on the irradiated surface. A similar nature of Nb damageability under conditions of laser and beam-plasma treatment was found: a wavy relief of the irradiated surface with the presence of droplike fragments on it, extended wave crests, and microcracks. Irradiation of Nb with pulsed LR fluxes in the FR mode leads to formation of sections with block and cellular structures in the surface layer (SL), which are also formed after experiments in the PF chamber. It was found that, after laser treatment in the FR and Q-switched modes, bubbles (blisters) are not formed in the SL of niobium, which are always present on the irradiated surface when exposed to pulsed fluxes of HI and HP in the PF chamber owing to implantation of helium ions into Nb. It is noted that, in laser experiments, there is no possibility of implanting working gas ions into the material, which is typical of beam-plasma impacts in PF devices, which affects damageability parameters and modification of the structure of the irradiated SL.
- 1 February 2022
- Published by Pleiades Publishing Ltd in Journal of Surface Investigation: X-Ray, Synchrotron and Neutron Techniques
- Vol. 16 (1) , 33-41
Influence of Pulsed Flows of Deuterium Ions and Deuterium Plasma on Cu–Ni and Cu–Ni–Ga Alloys
Experiments on the irradiation of Cu–4 wt % Ni and Cu–4 wt % Ni–10 wt % Ga copper alloys by high-power pulsed flows of deuterium plasma and deuterium ions are carried out in the Plasma Focus PF-1000 installation. The alloys are irradiated in two modes: the hard mode of combined action of deuterium plasma flows at qpl = 108–109 W/cm2, τpl = 100 ns and deuterium ions at qi = 109–1010 W/cm2, τi = 50 ns and also in more soft conditions: the Cu–4 wt % Ni alloy is irradiated with a deuterium plasma flow at a power density of qi = 2 × 107 W/cm2 and pulse duration of τpl = 100 ns; the Cu–4 wt % Ni–10 wt % Ga alloy, at qpl = 5 ×107–108 W/cm2 and qi = 108–109 W/cm2 and the same values of the pulse duration. The nature of the damage for Cu–4 wt % Ni and Cu–4 wt % Ni–10 wt % Ga alloys in the irradiation modes implemented is approximately the same and is determined by the wavy surface relief, the presence of craters, micropores, droplet-like fragments, and the absence of microcracks. Unlike the Cu–4 wt % Ni alloy, the surface structure of the Cu–4 wt % Ni–10 wt % Ga copper alloys has, after irradiation, a cellular or cellular–dendritic character. The parameters of the formation of such a structure depend on the regime of pulsed irradiation of the sample target and the conditions of subsequent directed crystallization of the molten surface layer. The formation of this structure is also significantly affected by alloying of the binary copper–nickel alloy with a third element (gallium) and probably the dendritic structure of the alloy in the initial state of the alloys. Plastic deformation is observed in the surface layer of each of the studied alloys after exposure to the flows of deuterium plasma and deuterium ions, which proceed by the sliding mechanism along the planes of the densest packing {111}, typical of materials with a face-centered cubic (fcc) lattice. The ductile copper Cu–Ni and Cu–Ni–Ga alloys under study, as well as the Cu–10 wt % Ga alloy studied previously, exhibit very high crack resistance to the effects of high-power pulsed radiation-thermal loads generated in a Plasma Focus PF-1000 installation, as compared to the refractory metals W, Mo, and V.
- 1 February 2022
- Published by Pleiades Publishing Ltd in Journal of Surface Investigation: X-Ray, Synchrotron and Neutron Techniques
- Vol. 16 (1) , 33-41
Influence of Pulsed Flows of Deuterium Ions and Deuterium Plasma on Cu–Ni and Cu–Ni–Ga Alloys
Experiments on the irradiation of Cu–4 wt % Ni and Cu–4 wt % Ni–10 wt % Ga copper alloys by high-power pulsed flows of deuterium plasma and deuterium ions are carried out in the Plasma Focus PF-1000 installation. The alloys are irradiated in two modes: the hard mode of combined action of deuterium plasma flows at qpl = 108–109 W/cm2, τpl = 100 ns and deuterium ions at qi = 109–1010 W/cm2, τi = 50 ns and also in more soft conditions: the Cu–4 wt % Ni alloy is irradiated with a deuterium plasma flow at a power density of qi = 2 × 107 W/cm2 and pulse duration of τpl = 100 ns; the Cu–4 wt % Ni–10 wt % Ga alloy, at qpl = 5 ×107–108 W/cm2 and qi = 108–109 W/cm2 and the same values of the pulse duration. The nature of the damage for Cu–4 wt % Ni and Cu–4 wt % Ni–10 wt % Ga alloys in the irradiation modes implemented is approximately the same and is determined by the wavy surface relief, the presence of craters, micropores, droplet-like fragments, and the absence of microcracks. Unlike the Cu–4 wt % Ni alloy, the surface structure of the Cu–4 wt % Ni–10 wt % Ga copper alloys has, after irradiation, a cellular or cellular–dendritic character. The parameters of the formation of such a structure depend on the regime of pulsed irradiation of the sample target and the conditions of subsequent directed crystallization of the molten surface layer. The formation of this structure is also significantly affected by alloying of the binary copper–nickel alloy with a third element (gallium) and probably the dendritic structure of the alloy in the initial state of the alloys. Plastic deformation is observed in the surface layer of each of the studied alloys after exposure to the flows of deuterium plasma and deuterium ions, which proceed by the sliding mechanism along the planes of the densest packing {111}, typical of materials with a face-centered cubic (fcc) lattice. The ductile copper Cu–Ni and Cu–Ni–Ga alloys under study, as well as the Cu–10 wt % Ga alloy studied previously, exhibit very high crack resistance to the effects of high-power pulsed radiation-thermal loads generated in a Plasma Focus PF-1000 installation, as compared to the refractory metals W, Mo, and V.
- 1 January 2022
- Published by Pleiades Publishing Ltd in Russian Metallurgy (Metally)
- Vol. 2022 (1) , 48-56
Effect of High-Temperature Pulsed Deuterium Plasma on the Structure and Mechanical Properties of the Surface of Cu–Ga and Cu–Ga–Ni Alloys
The changes in the mechanical properties and the texture of the surface layers in Cu–10Ga and Cu–10Ga–4Ni alloys are studied under the powerful pulsed radiation-thermal and shock-wave loads characteristic of pulsed thermonuclear fusion plants. Samples are irradiated by pulsed high-temperature plasma and ions in the 600-kJ Plasma Focus (PF) PF-1000 (Poland) plant, and deuterium is used as a working gas. The deuterium plasma power density is varied from 107 to 109 W/cm2 at the plasma pulse duration of ~10–7 s, and the deuterium ion flux power density is from 108 to 1011 W/cm2 at an ion flux incident time of ~5 × 10–8 s. Irradiation under the experimental conditions is found to change the texture of the surface layers to a depth of several micrometers, which is likely to be caused by directional solidification at a high temperature gradient oriented normal to the irradiated sample surface. There is a correlation between the type of texture formed in this case and the character of propagating slip lines with formation of a block structure. The lattice parameter in the irradiated surface layers decreases, which is related, supposedly, with the action of residual macroscopic stresses, since substantial changes in the surface layer composition have not been observed. A general tendency toward a decrease in the Vickers microhardness is noted in copper alloy samples as a result of their irradiation in the PF plant under the experimental conditions. A possible cause is thermal effect, since the concentration of alloying elements in the alloys decreases insignificantly after irradiation. The elastic modulus E of the Cu–10Ga alloy decreases insignificantly (to 14%) after irradiation. At the same time, in the Cu–10Ga–4Ni alloy, i.e., after alloying of the Cu–10Ga alloy with nickel (element with higher E as compared to that of copper), the elastic modulus of the initial surface layer remains almost the same after irradiation in PF.
- 1 January 2022
- Published by Pleiades Publishing Ltd in Russian Metallurgy (Metally)
- Vol. 2022 (1) , 48-56
Effect of High-Temperature Pulsed Deuterium Plasma on the Structure and Mechanical Properties of the Surface of Cu–Ga and Cu–Ga–Ni Alloys
The changes in the mechanical properties and the texture of the surface layers in Cu–10Ga and Cu–10Ga–4Ni alloys are studied under the powerful pulsed radiation-thermal and shock-wave loads characteristic of pulsed thermonuclear fusion plants. Samples are irradiated by pulsed high-temperature plasma and ions in the 600-kJ Plasma Focus (PF) PF-1000 (Poland) plant, and deuterium is used as a working gas. The deuterium plasma power density is varied from 107 to 109 W/cm2 at the plasma pulse duration of ~10–7 s, and the deuterium ion flux power density is from 108 to 1011 W/cm2 at an ion flux incident time of ~5 × 10–8 s. Irradiation under the experimental conditions is found to change the texture of the surface layers to a depth of several micrometers, which is likely to be caused by directional solidification at a high temperature gradient oriented normal to the irradiated sample surface. There is a correlation between the type of texture formed in this case and the character of propagating slip lines with formation of a block structure. The lattice parameter in the irradiated surface layers decreases, which is related, supposedly, with the action of residual macroscopic stresses, since substantial changes in the surface layer composition have not been observed. A general tendency toward a decrease in the Vickers microhardness is noted in copper alloy samples as a result of their irradiation in the PF plant under the experimental conditions. A possible cause is thermal effect, since the concentration of alloying elements in the alloys decreases insignificantly after irradiation. The elastic modulus E of the Cu–10Ga alloy decreases insignificantly (to 14%) after irradiation. At the same time, in the Cu–10Ga–4Ni alloy, i.e., after alloying of the Cu–10Ga alloy with nickel (element with higher E as compared to that of copper), the elastic modulus of the initial surface layer remains almost the same after irradiation in PF.
- 1 September 2021
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 12 (5) , 1191-1195
Effect of Pulsed Ion-Plasma Impact and Electron Irradiation on Mechanical Properties of Precipitation-Hardened Inconel 718 Alloy
The effect of pulsed ion-plasma irradiation in the Plasma Focus Vikhr setup and irradiation with 20-MeV electrons at the Microtron-ST accelerator on the mechanical properties of the Inconel 718 precipitation-hardened alloy obtained by the selective laser fusion method has been studied. It was found that ion-plasma and electron irradiation does not affect the properties of the alloy, which is explained by the small thickness of the modified layer during irradiation at the Plasma Focus setup and insufficiently high electron fluence for the manifestation of radiation-stimulated process of redistribution and dissolution of dispersed precipitates of the strengthening phases. The results obtained bear evidence of a high resistance to crack propagation and the absence of a tendency of the studied alloy to embrittlement.
- 1 September 2021
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 12 (5) , 1191-1195
Effect of Pulsed Ion-Plasma Impact and Electron Irradiation on Mechanical Properties of Precipitation-Hardened Inconel 718 Alloy
The effect of pulsed ion-plasma irradiation in the Plasma Focus Vikhr setup and irradiation with 20-MeV electrons at the Microtron-ST accelerator on the mechanical properties of the Inconel 718 precipitation-hardened alloy obtained by the selective laser fusion method has been studied. It was found that ion-plasma and electron irradiation does not affect the properties of the alloy, which is explained by the small thickness of the modified layer during irradiation at the Plasma Focus setup and insufficiently high electron fluence for the manifestation of radiation-stimulated process of redistribution and dissolution of dispersed precipitates of the strengthening phases. The results obtained bear evidence of a high resistance to crack propagation and the absence of a tendency of the studied alloy to embrittlement.
- 1 May 2021
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 12 (3) , 601-609
Effect of Pulsed Fluxes of Deuterium Ions and Deuterium Plasma on Oxide Dispersion Strengthened Ferritic Steels
The effect of high-power pulsed fluxes of deuterium ions and deuterium plasma generated in the Plasma Focus PF-1000U device on oxide dispersion strengthened ferritic steel KP4-ODS (Fe–15 Cr–4 Al–2 W–0.35 Y2O3) was experimentally studied. When the samples were irradiated with two pulses (N = 2), the plasma flux power density was qpl ≈ 108 W/cm2 and that of ion beam qi × 109 W/cm2. At N = 9, qpl ≈ 2 ×108 W/cm2 and qi ≈ 5 × 109 W/cm2. The pulse duration of the plasma beams was τpl ≈ 100 ns and that of the ion beams τi ≈ 50 ns. It was shown that irradiation of the material in the soft mode (N = 2) leads to surface erosion due to evaporation of the material and is accompanied by the surface polishing effect. In this case, there is no significant change in the initial structural phase state of steel; only a small change in the crystal lattice parameters of solid solutions based on iron and chromium is observed. In the hard irradiation mode (N = 9), owing to the high heating of the surface layer, in addition to erosion, the material melts. In the structure of the surface layer of the ODS steel, a chromium-based solid solution disappears and only an iron-based solid solution remains, while the number of second-phase nanoparticles increases. The presence of a liquid phase formed upon exposure to fluxes of deuterium ions and deuterium plasma stimulates the possibility of complete dissolution of small (less than ~20 nm) nanoparticles of Y2O3 oxide and partial dissolution of larger (tens of nanometers) nanoparticles. Enhanced in comparison with the solid phase, the diffusion redistribution of elements in the molten surface layer contributes to the formation of Y2O3 nanoparticles and oxides of other elements that make up the ODS steel (Al2O3, Y–Al–O) upon cooling of the melt.
- 1 May 2021
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 12 (3) , 601-609
Effect of Pulsed Fluxes of Deuterium Ions and Deuterium Plasma on Oxide Dispersion Strengthened Ferritic Steels
The effect of high-power pulsed fluxes of deuterium ions and deuterium plasma generated in the Plasma Focus PF-1000U device on oxide dispersion strengthened ferritic steel KP4-ODS (Fe–15 Cr–4 Al–2 W–0.35 Y2O3) was experimentally studied. When the samples were irradiated with two pulses (N = 2), the plasma flux power density was qpl ≈ 108 W/cm2 and that of ion beam qi × 109 W/cm2. At N = 9, qpl ≈ 2 ×108 W/cm2 and qi ≈ 5 × 109 W/cm2. The pulse duration of the plasma beams was τpl ≈ 100 ns and that of the ion beams τi ≈ 50 ns. It was shown that irradiation of the material in the soft mode (N = 2) leads to surface erosion due to evaporation of the material and is accompanied by the surface polishing effect. In this case, there is no significant change in the initial structural phase state of steel; only a small change in the crystal lattice parameters of solid solutions based on iron and chromium is observed. In the hard irradiation mode (N = 9), owing to the high heating of the surface layer, in addition to erosion, the material melts. In the structure of the surface layer of the ODS steel, a chromium-based solid solution disappears and only an iron-based solid solution remains, while the number of second-phase nanoparticles increases. The presence of a liquid phase formed upon exposure to fluxes of deuterium ions and deuterium plasma stimulates the possibility of complete dissolution of small (less than ~20 nm) nanoparticles of Y2O3 oxide and partial dissolution of larger (tens of nanometers) nanoparticles. Enhanced in comparison with the solid phase, the diffusion redistribution of elements in the molten surface layer contributes to the formation of Y2O3 nanoparticles and oxides of other elements that make up the ODS steel (Al2O3, Y–Al–O) upon cooling of the melt.
- 1 January 2021
- Published by Intercontact Science in Physics and Chemistry of Materials Treatment
- No. 6,p. 5-17
Damage of niobium by pulse flows of helium ions and helium plasma
The damageability of niobium by pulsed fluxes of helium ions (HI) and helium plasma (HP) in the Plasma Focus (PF) setup was studied at a flux power density qi ~ 108 W/cm2 and qp ~ 107 W/cm2, respectively, and pulse duration τi ≈ 30 – 50 ns and τp ≈ 100 ns. In the implemented irradiation conditions the erosion of the material is observed associated with the evaporation of the surface layer (SL), which occurs somewhat more intensively in the central part of the irradiation zone under the action of the most high-energy fluxes of HI and HP. The typical features of the damageability of the niobium SL under the considered irradiation conditions are revealed. These include: melting of SL with the formation of a wavy surface relief and a large number of blisters of two types — gas-filled and with destroyed shells, as well as the presence of microcracks. The appearance of blisters was associated with the formation of complexes based on the combination of implanted helium atoms with vacancies and interstitial impurity atoms (C, O, N, etc.) and their subsequent growth and coagulation in the liquid phase under pulsed action of energy fluxes on the irradiated Nb surface. Some of the microcracks formed in the SL under the action of thermal stresses coincide with the sliding lines of the material that arise under the action of high-speed plastic deformation. A network of such microcracks creates a block structure on the Nb surface. In the irradiated surface layer of niobium, zones of columnar crystals and a cellular microstructure of the surface are found, in which the average cell size is ~ 100 nm. It was shown by the method of numerical simulation that in the indicated zones the process of solidification of the SL proceeded through directional crystallization at a high speed, which reached ~ 35 m/s near the irradiated surface.
- 1 January 2021
- Published by Intercontact Science in Physics and Chemistry of Materials Treatment
- No. 6,p. 5-17
Damage of niobium by pulse flows of helium ions and helium plasma
The damageability of niobium by pulsed fluxes of helium ions (HI) and helium plasma (HP) in the Plasma Focus (PF) setup was studied at a flux power density qi ~ 108 W/cm2 and qp ~ 107 W/cm2, respectively, and pulse duration τi ≈ 30 – 50 ns and τp ≈ 100 ns. In the implemented irradiation conditions the erosion of the material is observed associated with the evaporation of the surface layer (SL), which occurs somewhat more intensively in the central part of the irradiation zone under the action of the most high-energy fluxes of HI and HP. The typical features of the damageability of the niobium SL under the considered irradiation conditions are revealed. These include: melting of SL with the formation of a wavy surface relief and a large number of blisters of two types — gas-filled and with destroyed shells, as well as the presence of microcracks. The appearance of blisters was associated with the formation of complexes based on the combination of implanted helium atoms with vacancies and interstitial impurity atoms (C, O, N, etc.) and their subsequent growth and coagulation in the liquid phase under pulsed action of energy fluxes on the irradiated Nb surface. Some of the microcracks formed in the SL under the action of thermal stresses coincide with the sliding lines of the material that arise under the action of high-speed plastic deformation. A network of such microcracks creates a block structure on the Nb surface. In the irradiated surface layer of niobium, zones of columnar crystals and a cellular microstructure of the surface are found, in which the average cell size is ~ 100 nm. It was shown by the method of numerical simulation that in the indicated zones the process of solidification of the SL proceeded through directional crystallization at a high speed, which reached ~ 35 m/s near the irradiated surface.