Maria Gombotz
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Maria Gombotz has a total of 14 co-authors. Here are the top co-authors by number of shared publications:
- Martin Wilkening
Institute of Chemistry and Technology of Materials, Graz University of Technology (NAWI Graz), Stremayrgasse 9, A-8010 Graz, Austria
4 shared publications - Ilie Hanzu
Institute for Chemistry and Technology of Materials Graz University of Technology Graz Austria
2 shared publications - Bernhard Gadermaier
Institute of Chemistry and Technology of Materials (NAWI Graz), Graz University of Technology, Stremayrgasse 9, 8010 Graz, Austria
1 shared publication - Daniel Rettenwander
NTNU Norwegian University of Science and Technology
1 shared publication Florian Preishuber-Pflügl
Christian Doppler Laboratory for Lithium Batteries, and Institute for Chemistry and Technology of Materials, Graz University of Technology (NAWI Graz), 8010 Graz, Austria
1 shared publication- Klebson Lucenildo Da Silva
Universidade Estadual de Maringá
1 shared publication
Latest Publications
- 6 September 2021
- Published by Walter de Gruyter GmbH in Zeitschrift für Physikalische Chemie
- Vol. 236 (6-8) , 1077-1088
Ionic transport in K2Ti6O13
The increasing demand for batteries forced the development of energy storage systems that rely on materials consisting of abundant elements in the Earth’s crust. Switching from Li+ to K+ as the main ionic charge carrier needs highly conducting potassium-bearing electrolytes to realize K+ ion batteries (PIBs). The knowledge gained from the design of Li-ion batteries (LIBs) and Na-ion batteries (NIBs) may conceptually inspire also the establishment of PIBs. Considering, for instance, the hexatitanates Na2Ti6O13, Li2Ti6O13, and H2Ti6O13, which were previously investigated as components for LIBs and NIBs, here we investigated ion dynamics in the K-analog K2Ti6O13. Ionic transport in polycrystalline samples of K2Ti6O13 was studied in a moisture-free atmosphere by broadband impedance spectroscopy in a temperature range from 20 °C to 450 °C. The current study aims at establishing a correlation between structural features of K2Ti6O13 and long-range ionic transport. As expected for K+ transport in K2Ti6O13 with its geometrically obstructed structure, the overall activation energy of ion transport in the ternary oxide takes a rather high value of 0.97(2) eV. Almost the same result (0.95(3) eV) is obtained for the migration activation energy, which we extracted from the analysis of crossover frequencies of the corresponding conductivity isotherms. By comparing our results with those of Na2Ti6O13 (0.82 eV), Li2Ti6O13 (0.65 eV), and H2Ti6O13, we clearly see how the size of the mobile cation correlates with both specific conductivities and activation energies. This comparison points to K+ being the main charge carrier in K2Ti6O13. It also helps in laying the foundations to derive the relevant structure-property relationships in this class of materials.
- 6 September 2021
- Published by Walter de Gruyter GmbH in Zeitschrift für Physikalische Chemie
- Vol. 236 (6-8) , 1077-1088
Ionic transport in K2Ti6O13
The increasing demand for batteries forced the development of energy storage systems that rely on materials consisting of abundant elements in the Earth’s crust. Switching from Li+ to K+ as the main ionic charge carrier needs highly conducting potassium-bearing electrolytes to realize K+ ion batteries (PIBs). The knowledge gained from the design of Li-ion batteries (LIBs) and Na-ion batteries (NIBs) may conceptually inspire also the establishment of PIBs. Considering, for instance, the hexatitanates Na2Ti6O13, Li2Ti6O13, and H2Ti6O13, which were previously investigated as components for LIBs and NIBs, here we investigated ion dynamics in the K-analog K2Ti6O13. Ionic transport in polycrystalline samples of K2Ti6O13 was studied in a moisture-free atmosphere by broadband impedance spectroscopy in a temperature range from 20 °C to 450 °C. The current study aims at establishing a correlation between structural features of K2Ti6O13 and long-range ionic transport. As expected for K+ transport in K2Ti6O13 with its geometrically obstructed structure, the overall activation energy of ion transport in the ternary oxide takes a rather high value of 0.97(2) eV. Almost the same result (0.95(3) eV) is obtained for the migration activation energy, which we extracted from the analysis of crossover frequencies of the corresponding conductivity isotherms. By comparing our results with those of Na2Ti6O13 (0.82 eV), Li2Ti6O13 (0.65 eV), and H2Ti6O13, we clearly see how the size of the mobile cation correlates with both specific conductivities and activation energies. This comparison points to K+ being the main charge carrier in K2Ti6O13. It also helps in laying the foundations to derive the relevant structure-property relationships in this class of materials.
- Open Access
- 25 February 2020
- Published by Frontiers Media SA in Frontiers in Chemistry
- Vol. 8, 100
Lithium-Ion Transport in Nanocrystalline Spinel-Type Li[InxLiy]Br4 as Seen by Conductivity Spectroscopy and NMR
Currently, a variety of solid Li+ conductors are being discussed that could potentially serve as electrolytes in all-solid-state Li-ion batteries and batteries using metallic Li as the anode. Besides oxides, sulfides and thioposphates, and also halogenides, such as Li3YBr6, belong to the group of such promising materials. Here, we report on the mechanosynthesis of ternary, nanocrystalline (defect-rich) Li[InxLiy]Br4, which crystallizes with a spinel structure. We took advantage of a soft mechanochemical synthesis route that overcomes the limitations of classical solid-state routes, which usually require high temperatures to prepare the product. X-ray powder diffraction, combined with Rietveld analysis, was used to collect initial information about the crystal structure; it turned out that the lithium indium bromide prepared adopts cubic symmetry (). The overall and electronic conductivity were examined via broadband conductivity spectroscopy and electrical polarization measurements. While electric modulus spectroscopy yielded information on long-range ion transport, 7Li nuclear magnetic resonance (NMR) spin-lattice relaxation measurements revealed rapid, localized ionic hopping processes in the ternary bromide. Finally, we studied the influence of thermal treatment on overall conductivity, as the indium bromide might find applications in cells that are operated at high temperatures (330 K and above).- 25 February 2020
- Published by Frontiers Media SA in Frontiers in Chemistry
- Vol. 8, 100
Open AccessLithium-Ion Transport in Nanocrystalline Spinel-Type Li[InxLiy]Br4 as Seen by Conductivity Spectroscopy and NMR
Currently, a variety of solid Li+ conductors are being discussed that could potentially serve as electrolytes in all-solid-state Li-ion batteries and batteries using metallic Li as the anode. Besides oxides, sulfides and thioposphates, and also halogenides, such as Li3YBr6, belong to the group of such promising materials. Here, we report on the mechanosynthesis of ternary, nanocrystalline (defect-rich) Li[InxLiy]Br4, which crystallizes with a spinel structure. We took advantage of a soft mechanochemical synthesis route that overcomes the limitations of classical solid-state routes, which usually require high temperatures to prepare the product. X-ray powder diffraction, combined with Rietveld analysis, was used to collect initial information about the crystal structure; it turned out that the lithium indium bromide prepared adopts cubic symmetry (). The overall and electronic conductivity were examined via broadband conductivity spectroscopy and electrical polarization measurements. While electric modulus spectroscopy yielded information on long-range ion transport, 7Li nuclear magnetic resonance (NMR) spin-lattice relaxation measurements revealed rapid, localized ionic hopping processes in the ternary bromide. Finally, we studied the influence of thermal treatment on overall conductivity, as the indium bromide might find applications in cells that are operated at high temperatures (330 K and above). - Open Access
- 25 October 2019
- Published by MDPI AG in Nanomaterials
- Vol. 9 (11) , 1517
Fluoride-Ion Batteries: On the Electrochemical Stability of Nanocrystalline La0.9Ba0.1F2.9 against Metal Electrodes
Over the past years, ceramic fluorine ion conductors with high ionic conductivity have stepped into the limelight of materials research, as they may act as solid-state electrolytes in fluorine-ion batteries (FIBs). A factor of utmost importance, which has been left aside so far, is the electrochemical stability of these conductors with respect to both the voltage window and the active materials used. The compatibility with different current collector materials is important as well. In the course of this study, tysonite-type La Ba F , which is one of the most important electrolyte in first-generation FIBs, was chosen as model substance to study its electrochemical stability against a series of metal electrodes viz. Pt, Au, Ni, Cu and Ag. To test anodic or cathodic degradation processes we carried out cyclic voltammetry (CV) measurements using a two-electrode set-up. We covered a voltage window ranging from −1 to 4 V, which is typical for FIBs, and investigated the change of the response of the CVs as a function of scan rate (2 mV/s to 0.1 V/s). It turned out that Cu is unstable in combination with La Ba F , even before voltage was applied. The cells with Au and Pt electrodes show reactions during the CV scans; in the case of Au the irreversible changes seen in CV are accompanied by a change in color of the electrode as investigated by light microscopy. Ag and Ni electrodes seem to suffer from contact issues which, most likely, also originate from side reactions with the electrode material. The experiments show that the choice of current collectors in future FIBs will become an important topic if we are to develop long-lasting FIBs. Most likely, protecting layers between the composite electrode material and the metal current collector have to be developed to prevent any interdiffusion or electrochemical degradation processes.- 25 October 2019
- Published by MDPI AG in Nanomaterials
- Vol. 9 (11) , 1517
Open AccessFluoride-Ion Batteries: On the Electrochemical Stability of Nanocrystalline La0.9Ba0.1F2.9 against Metal Electrodes
Over the past years, ceramic fluorine ion conductors with high ionic conductivity have stepped into the limelight of materials research, as they may act as solid-state electrolytes in fluorine-ion batteries (FIBs). A factor of utmost importance, which has been left aside so far, is the electrochemical stability of these conductors with respect to both the voltage window and the active materials used. The compatibility with different current collector materials is important as well. In the course of this study, tysonite-type La Ba F , which is one of the most important electrolyte in first-generation FIBs, was chosen as model substance to study its electrochemical stability against a series of metal electrodes viz. Pt, Au, Ni, Cu and Ag. To test anodic or cathodic degradation processes we carried out cyclic voltammetry (CV) measurements using a two-electrode set-up. We covered a voltage window ranging from −1 to 4 V, which is typical for FIBs, and investigated the change of the response of the CVs as a function of scan rate (2 mV/s to 0.1 V/s). It turned out that Cu is unstable in combination with La Ba F , even before voltage was applied. The cells with Au and Pt electrodes show reactions during the CV scans; in the case of Au the irreversible changes seen in CV are accompanied by a change in color of the electrode as investigated by light microscopy. Ag and Ni electrodes seem to suffer from contact issues which, most likely, also originate from side reactions with the electrode material. The experiments show that the choice of current collectors in future FIBs will become an important topic if we are to develop long-lasting FIBs. Most likely, protecting layers between the composite electrode material and the metal current collector have to be developed to prevent any interdiffusion or electrochemical degradation processes. - Open Access
- 9 January 2019
- Published by Royal Society of Chemistry (RSC) in Physical Chemistry Chemical Physics
- Vol. 21 (4) , 1872-1883
Spatial confinement – rapid 2D F − diffusion in micro- and nanocrystalline RbSn 2 F 5
NMR and conductivity spectroscopy reveal 2D diffusion in both microcrystalline and nanocrystalline RbSn 2 F 5 .
- 9 January 2019
- Published by Royal Society of Chemistry (RSC) in Physical Chemistry Chemical Physics
- Vol. 21 (4) , 1872-1883
Open AccessSpatial confinement – rapid 2D F − diffusion in micro- and nanocrystalline RbSn 2 F 5
NMR and conductivity spectroscopy reveal 2D diffusion in both microcrystalline and nanocrystalline RbSn 2 F 5 .